• Title/Summary/Keyword: $Ba_2In_2O_5$

Search Result 810, Processing Time 0.03 seconds

Heat Liberation in the Reaction of $YBa_2Cu_3O_{7-}\delta$, $Y_2BaCuO_5$, and Binary Compounds in the Ba-Cu-O System with Water ($YBa_2Cu_3O_{7-}\delta$, $Y_2BaCuO_5$ 및 Ba-Cu-O계 화합물의 수분과의 반응에 의한 열방출에 관한 연구)

  • 김배연
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.1
    • /
    • pp.83-89
    • /
    • 1995
  • YBa2Cu3O7-$\delta$, Y2BaCuO5, and binary compounds in the Ba-Cu-O system with the nominal composition of Ba2CuO3, BaCuO2, Ba3Cu4O7, Ba3Cu5O8 were synthesized to investigate the heat evolutions and crystalline phases in the hydration reaction of orthorhombic YBa2Cu3O7-$\delta$ phase. The observed crystalline phases were YBa2Cu3O7-$\delta$, Y2BaCuO5, and BaCuO2, or Ba2Cu3O5+x, and some amount of noncrystalline phase in the Ba-Cu system comounds. In contact with distilled water, YBa2Cu3O7-$\delta$ and Y2BaCuO5 did not have considerable heat liberation, but in the binary compounds of the Ba-Cu-O system, the amount of total heat liberation was increased with respect to the Cu content. It might be that the reaction of high temperature superconductor YBa2Cu3O7-$\delta$ with water and/or moisture originated from the unusual oxidation state of Cu ion and the presence of amorphous Ba-Cu oxide compound. The degradation of high Tc superconductor by moisture and water could be controlled by restricting the heterogeneous distribution of Tc comlposition and the formation of second phase, such as stable Y2BaCuO5, and the resulting unstable Ba-Cu oxide compound.

  • PDF

Phase Relation and Microwave Dielectric Properties of $BaO-(Nd, Sm)_2O_3-TiO_2$ Ceramic System ($BaO-(Nd, Sm)_2O_3-TiO_2$계 세라믹스의 상관계 및 마이크로파 유전특성)

  • 김희도;김진호;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.9
    • /
    • pp.995-1004
    • /
    • 1994
  • Phase relation and microwave dielectric properties of the system BaO.(Nd1-xSmx)2O3.TiO2 (n=4, 5) were studied. With n=5 (1 : 1 : 5), Ba2Ti9O20 and TiO2 formed in case of X$\leq$0.7, and Ba2Ti9O20 and Sm2Ti2O7 formed at X=1.0 as the second phases dispersed in fine-grained orthorhombic matrix phase. With n=4 (1 : 1 : 4). on the contrary, only fine grains of an ortho-rhombic phase were observed irrespective of Nd/Sm ratio. The compositions of these two stable orthorombic phases having distinct lattic constants even with the same Nd/Sm ratio were estimated as 4BaO.5(Nd1-xSmx)2O3.18TiO2 and BaO.(Nd1-xSmx)2O3.4TiO2 with n=5 and n=4 in the system BaO.(Nd1-xSmx)2O3.TiO2, respectively. Consequently the composition BaO.(Nd1-xSmx)2O3.5TiO2 lies in the compatible triangle of 4BaO.5(Nd1-xSmx)2O3.18TiO2 and the second phases mentioned above. The microwave dielectric properties (~4 GHz) of BaO.(Nd1-xSmx)2O3.5TiO2 can be controlled effectively by adjusting Sm content : with increasing X from 0 to 0.7, both dielectric constant and the temperature coefficient of resonant frequency decreased monotonically from 82 to 65 and from 91 (ppm/$^{\circ}C$) to -19(ppm/$^{\circ}C$), respectively, while unloaded Q(Qo) remained constant at about 2,600.

  • PDF

Luminescent Properties of BaSi2O5:Eu2+ Phosphor Film Fabricated by Spin-Coating of Ba-Eu Precursor on SiO2 Glass

  • Park, Je Hong;Kim, Jong Su;Kim, Jong Tae
    • Journal of the Optical Society of Korea
    • /
    • v.18 no.1
    • /
    • pp.45-49
    • /
    • 2014
  • Well-crystallized $BaSi_2O_5:Eu^{2+}$ phosphor films were synthesized by heat treatment of spin-coated BaO:Eu on $SiO_2$ glass. We investigated luminescence-structure properties of these phosphor films as a function of heat-treatment temperature. From x-ray diffraction patterns, our $BaSi_2O_5:Eu^{2+}$ phosphor films revealed that (111)- and (204)-crystal planes of $BaSi_2O_5$ crystal were dominantly increased with an increase of heat-treatment temperature. Photoluminescence intensities of $BaSi_2O_5:Eu^{2+}$ phosphor films were increased with amount of these crystal planes. It can be explained that $Eu^{2+}$ ions were stably occupied at specific crystal orientation of $BaSi_2O_5$ crystal, enhancing the luminescent intensities of $BaSi_2O_5:Eu^{2+}$ phosphor films. In addition, our $BaSi_2O_5:Eu^{2+}$ phosphor films had transmittance of 70% at 510 nm,.due to the dense morphology and specific crystallinity of $BaSi_2O_5:Eu^{2+}$ phosphor films.

The Structural and dielectric Properties of the $BaTiO_{3}+10wt%Nb_{2}O_{5}$ ceramics with the sintering temperature (소결온도에 따른 $BaTiO_{3}+10wt%Nb_{2}O_{5}$ 세라믹스의 구조 및 유전특성)

  • 이상철;이성갑;배선기;이영희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.402-405
    • /
    • 2001
  • The BaTiO$_3$+10wt%Nb$_2$O$_{5}$ ceramics were prepared by conventional mixed oxide method. The structural and dielectric properties of the BaTiO$_3$+10wt%Nb$_2$O$_{5}$ ceramics with the sintering temperature were investigated. Increasing the sintering temperature, the 2$\theta$ value of BaTiO$_3$peaks were shifted to the higher degree and intensity of the BaTiO$_3$and BaNbO$_3$peaks were increased. In the BaTiO$_3$+10wt%Nb$_2$O$_{5}$ ceramics sintered at 135$0^{\circ}C$ and 1375$^{\circ}C$, the grain was fine and uniform. Increasing the sintering temperature, the pore was decreased and the dielectric constant was increased. In the BaTiO$_3$+10wt%Nb$_2$O$_{5}$ ceramics sintered at 1375$^{\circ}C$, the dielectric constant and dielectric loss were 5424, 0.02 respectively.ctively.

  • PDF

Phase Separation and their Structures in $BaO-B_2O_3$ Glasses ($BaO-B_2O_3$계 유리의 상분리 현상과 유리의 구조)

  • 채수철;김철영
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.6
    • /
    • pp.25-32
    • /
    • 1986
  • Phase spearated glass is heterogeneous in microscopic point of view and the heterogeneities affect the structures of glasses. In the present work the phase separation of $BaO-B_2O_3$ glass system was investigated and the effect of $P_2O_5$ on the phase separation and crystallization was also studied in the above system. Experiments such as scanning electron microscopy X-ray diffraction and infrared spectroscopy were performed. Phase separation with $B_2O_3$ rich phase matrix and BaO rich phase droplet was observed for the glasses containing less than 6 mole% of BaO while the opposite morphology of phase separation was found for the glasses containing more than 7 mole% of BaO. Phase separation region was extended up to the glass with 22mole% of BaO when the amount of $P_2O_5$ was increased. The heat-treated glasses crystallized to BaO.$4B_2O_3$$P_2O_5$ hindered the glass from the crystalli-zation.

  • PDF

Dielectric Relaxation Properties of 0.5Ba(Zr0.2Ti0.8)O3-0.5(Ba0.7Ca0.3)TiO3 Ceramics with CuO Addition (CuO 첨가에 따른 0.5Ba(Zr0.2Ti0.8)O3-0.5(Ba0.7Ca0.3)TiO3 세라믹스의 유전 이완 특성)

  • Bae, Seon Gi;Shin, Hyea-Kyoung;Lee, Suk-Jin;Im, In-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.28 no.2
    • /
    • pp.80-84
    • /
    • 2015
  • We investigated the dielectric relaxation properties $0.5Ba(Zr_{0.2}Ti_{0.8})O_3-0.5(Ba_{0.7}Ca_{0.3})TiO_3$ ceramics with CuO addition. With increasing CuO addition, the lattice parameter was increased by substitution of small amount $Cu^{2+}$ ion in B-site of $0.5Ba(Zr_{0.2}Ti_{0.8})O_3-0.5(Ba_{0.7}Ca_{0.3})TiO_3$ ceramics. Also the grain size and the maximum dielectric constant of $0.5Ba(Zr_{0.2}Ti_{0.8})O_3-0.5(Ba_{0.7}Ca_{0.3})TiO_3$ ceramics was decreased with increasing amounts of CuO addition. Moreover, the diffused phase transition properties (${\gamma}$) of $0.5Ba(Zr_{0.2}Ti_{0.8})O_3-0.5(Ba_{0.7}Ca_{0.3})TiO_3$ ceramics was increased by compositional fluctuation with increasing of CuO amount, changed from 1.45 at 1 wt% CuO addition to 1.94 at 7 wt% CuO addition.

A Study of the Synthesis and the Properties on Microwave Dielectric Material of BaO-Pr$_2$O$_3$-TiO$_2$ and BaO-(Nd,Pr)$_2$O$_3$-TiO$_2$ System (BaO-Pr$_2$O$_3$-TiO$_2$계 및 BaO-(Nd,Pr)$_2$O$_3$-TiO$_2$계 마이크로파 유전체의 합성 및 특성에 관한 연구)

  • 이용석;이재원;성학제;김준수;이병하
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.8
    • /
    • pp.775-782
    • /
    • 1998
  • This experiment is third study concerning BaO-{{{{ { { Pr}_{ 2} O}_{3 } }}-{{{{ { TiO}_{2 } }} (Ln=Sm, Nd, Pr, La..) system which is known to show a high dielectric constant and Q value in microwave dielectric materials. The process of cry-stallization and the microwave dielectric properties of the specimens sintered at 1220-140$0^{\circ}C$ for 2 hr was investigated in the BaO-(Na,{{{{ { { Pr})_{2 }O }_{3 } }}-{{{{ { TiO}_{2 } }} as well as BaO-{{{{ { { Pr}_{ 2} O}_{3 } }}-{{{{ { TiO}_{2 } }} system. The single phase BaPr2Ti5O14 and Ba(Nd,{{{{ { { Pr})_{2 }O }_{3 } }}Ti5O14 was finally formed from the Pr2Ti2O7 (Nd, Pr)2Ti2O7 as a secondary phase in the BaO-{{{{ { { Pr}_{ 2} O}_{3 } }}-{{{{ { TiO}_{2 } }} and BaO-(Nd, {{{{ { { Pr})_{2 }O }_{3 } }}-{{{{ { TiO}_{2 } }} system respectively The dielectric constant of the specimens sint-ered at 1280~131$0^{\circ}C$ showed the maximum value as 105(BaO-{{{{ { { Pr}_{ 2} O}_{3 } }}-{{{{ { TiO}_{2 } }} system) and 88 (BaO-(Nd,{{{{ { { Pr})_{2 }O }_{3 } }}-{{{{ { TiO}_{2 } }} system) and the Q values of them showed higher value than 1800 which are due to the maximum den-sity. However the dielectric properties of the specimens sintered at higher temperature than 131$0^{\circ}C$ were reduced due to the increases of pore which were resulted from the sudden grain growth.

  • PDF

The Effects of Ag and $Y_2BaCuO_5$ on Critical Characteristics of $YBa_2Cu_3O_X$ Fabricated by MPMG Method (Ag와 $Y_2BaCuO_5$ 가 고온초전도체의 임계특성에 미치는 영향)

  • 임성훈
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.6
    • /
    • pp.493-501
    • /
    • 1998
  • $YBa_2Cu_3O_X$ samples were fabricated by MPMG(Melt Powdered Melt Growth). Intitial composition of the mixed powders were prepared as follow ; $YBa_2Cu_3O_X$ : $Y_2BaCuO_5$ = 1:0, 1:0.2, 1:0.3, 1:0.4. After the first melt and cooling, 5wt% to 20wt% fo Ag power was added to the powder. Effects of the different initial $Y_2BaCuO_5$ and Ag addition amount on $J_c$ and magnetization of $YBa_2Cu_3O_X$ fabricated by MPMG method were investigated. The critical current density increased with the amount of $Y_2BaCuO_5$ and Ag. It was also observed that the difference between negative and positive magnetization in the magnetization hysteresis measurement at 77K was larger than the case where $Y_2BaCuO_5$and Ag were not added to the $YBa_2Cu_3O_X$ powders. It is concluded that $Y_2BaCuO_5$ sample with 40wt% amount of $Y_2BaCuO_5$ and 20wt% amount of Ag has not only the largest $J_c$ but also the improved pinning effect.

  • PDF

A Study on Solid Reaction of BaCO3-TiO2 System (BaCO3-TiO2계의 고상반응에 관한 연구)

  • 이응상;황성연;임대영
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.5
    • /
    • pp.484-490
    • /
    • 1987
  • Diffusion coupling experiment was done to study expansion of body and soild reaction in BaCO3-TiO2 system. Specimen of BaCO3 and TiO2 was formed with Pt-mark's method. Each specimen was fired at interval of 25℃ from 900℃ to 1000℃ for 2hrs. After that, specimen was fixed with resin and polished. Product layers of specimen were observed with SEM and EDS. The result were following; 1. Diffusion component is Ba2+, which diffuse toward TiO2. 2. Large crack between layer of BaCO3 and Ba2TiO4 was generated because of difference of thermal expansion coefficient. 3. Ba2TiO4 is formed to TiO2 body by the reaction of BaTiO3 and BaO and its structure is very porous. 4. BaTiO3 changes immediately to Ba2TiO4 by the reaction of BaO. But BaTiO3 which formed by the reaction of TiO2 and Ba2TiO4 exsists as layer because the diffusion distance of Ba2+ is far.

  • PDF

Fabrication of $BaTiO_3-PTCR$ Ceramic Resister Prepared by Direct Wet Process (습식 직접합성법을 이용한 PTCR 소자개발 연구)

  • 이경희;이병하;이희승
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.4
    • /
    • pp.61-65
    • /
    • 1985
  • $BaTiO_3$ powders doped with $BaTiO_3$ and $Nb_2O_5$ at 9$0^{\circ}C$ for 1hr. were synthesized by Direct Wet Process. These powders were very homogeneous and fine particle size. To obtain the highe PTCR effect AST($1/3Al_2O_3$.$3/4SiO_2$.$1/4TiO_2$) and $MnO_2$ were added in the semiconduc-ting $BaTiO_3$. In this case $Bi_2O_3$ and $MnO_2$ were used in the form of $Bi(NO)_3$ and $MnCl_2$.$4H_2O$ solution for Direct Wet Process. $BaTiO_3$ doped Nb2O5 and $MnO_2$ demostrated greater PTCR effect than $BaTiO_3$ doped $Nn_2O_5$ only.

  • PDF