The Electrical Characteristics of Ceramic Capacitor for High Voltage (고전압용 세라믹 커패시터의 전기적 특성)

  • 홍경진;김태성
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.13 no.1
    • /
    • pp.53-59
    • /
    • 1999
  • The ceramic capacitor was fabricated by $(Ba_{0.85}Ca_(0.15)TiO_3+ZnO$ + ZnO(from 0.1 to 0.4 mol ratio). The electrical and structural properties of ceramic capacitor for high voltage application was studied in this study. The relative rensity of ceramics capacitor has shown high in all specimen. The grain was a small size from $1.0[\mum]$ to $1.22[\mum]$ and it was increased with ZnO at 0.3 mol ratio. It was stabilized that the temperature coefficient of ceramic capacitor to change temperature had below 100[ppm] at 0.12~10[kHz]. The dielectric reIaxation time was decreased by interface polarization over $110[^{\circ}C]$ and it was increased by space polarization of paraelectric layer below $110[^{\circ}C]$. The insulating layer was increased with ZnO and dielectric constant to voltage was stabilized by 0.1[%].0.1[%].

  • PDF

Piezoelectric and Dielectric Properties of NKN-(1-x)BNT-xBT Ceramics (NKN-(1-x)BNT-xBT 세라믹스의 압전 및 유전특성)

  • Lee, Seung-Hwan;Nam, Sung-Pill;Lee, Sung-Gap;Lee, Young-Hie
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.10
    • /
    • pp.771-775
    • /
    • 2010
  • In this study, piezoelectric and dielectric properties of the $(Na_{0.5}K_{0.5})NbO_3-(1-x)(Bi_{0.5}Na_{0.5})TiO_3-xBaTiO_3$ [NKN-(1-x)BNT-xBT] ceramics were investigated. The lead-free NKN-(1-x)BNT-xBT ceramics were fabricated by a conventional mixed oxide method. The results indicate that the addition of $BaTiO_3$ significantly influences the sintering, microstructure, phase transition and electrical properties of NKN-BNT ceramics. A gradual change in the piezoelectric and dielectric properties was observed with the increase of BT contents. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased at the morphotropic phase boundary (MPB). The $d_{33}$=184 pC/N, $k_p$=0.38, dielectric constant=1455 with dielectric loss value of less than 1% were obtained for the NKN-0.95BNT-0.05BT ceramics sintered at $1150^{\circ}C$ for 2h. These results demonstrate that the NKN-(1-x)BNT-xBT ceramics is an attractive candidate for lead-free piezoelectric materials.

The effect of $MnO_2$ Addition to the PZT-PNN Piezoelectric Ceramics used in Ultrasonic Sensor (Receiver) (초음파 센서(수신기)용 PZT-PNN계 압전세라믹스에 $MnO_2$/ 첨가가 미치는 영향)

  • 조봉희;손은영;김현재;박창엽
    • Electrical & Electronic Materials
    • /
    • v.1 no.4
    • /
    • pp.311-318
    • /
    • 1988
  • 초음파센서(수신기)에 응용가능한 압전세라믹스를 제조하기 위하여 Ba변조된 Pb(ZR, Ti)O$_{3}$계 세라믹스에 MnO$_{2}$를 첨가하여 첨가량과 소성온도에 따른 영향을 조사하였다. 또한 제조된 압전세라믹스를 이용하여 초음파 수신기를 제작하여 수신특성을 확인하여 보았다. 그 겨로가 MnO$_{2}$가 0.4(wt%)첨가되었을 때 압전 g정수가 가장 크고 수신감도가 우수한 것으로 밝혀졌다.

  • PDF

Influence of Yb2O3 Doping Amount on Screen-printed Barium Strontium Calcium Titanate Thick Films

  • Noh, Hyun-Ji;Lee, Sung-Gap;Ahn, Byeong-Lib;Lee, Ju
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.6
    • /
    • pp.241-245
    • /
    • 2007
  • [ $(Ba_{0.9-x}Sr_xCa_{0.10})TiO_3$ ] (x=0.33, 0.36) powders were prepared by sol-gel method. $(Ba,Sr,Ca)TiO_3$(BSCT) thick films, undoped and doped with $MnCO_3$ and $Yb_2O_3(0.1{\sim}0.7mol%)$, were fabricated by the screen printing method on the alumina substrate. The coating and drying procedure was repeated 6-times. The Pt bottom electrode was screen printing method on the alumina substrate. These BSCT thick films were annealed at $1420^{\circ}C$ for 2 hr in atmosphere. The upper electrodes were fabricated by screen printing the Ag paste and then firing at $590^{\circ}C$ for 10 min. And then the structured and dielectric properties as a function of the doping amount of $Yb_2O_3$ were studied. As a result of the TG-DTA, exothermic peak was observed at around $670^{\circ}C$ due to the formation of the polycrystalline perovskite phase. All BSCT thick films showed XRD patterns of typical cubic peroveskite structure. The average thickness of BSCT thick films was about $70^{\mu}m$. The curie temperature and the dielectric constant decreased with increasing $Yb_2O_3$ doped content and the relative dielectric constant of the specimen, doped with 0.5 mol% $Yb_2O_3$ at BSCT(54/36/10), showed a best value of 5018 at curie temperature.

Effects of La2O3 on the Piezoelectric Properties of Lead-Free (Bi0.5Na0.5)0.94Ba0.06TiO3 Piezoelectric Ceramics (무연 BNBT 세라믹스의 압전특성에 미치는 La2O3의 영향)

  • Son Young-Jin;Yoon Man-Soon;Ur Soon-Chul
    • Korean Journal of Materials Research
    • /
    • v.15 no.12
    • /
    • pp.756-759
    • /
    • 2005
  • A lead free piezoelectric material, bismuth sodium barium titanate $(Bi_{0.5}Na_{0.5})_{0.94}Ba_{0.06}TiO_3$ (BNBT), was considered as an environment-friendly alternatives for the current PZT system. A perovskite BNBT was synthesized by conventional bulk ceramic processing technique. In order to improve piezoelectric properties, $La_2O_3$ as a dopant was incorporated into the BNBT system up to 0.025 moi, ana the effects on subsequent the piezoelectric ana dielectric properties were systematically investigated. With increasing $La_2O_3$ contents, the equilibrium grain shape was remarkably evidenced and sintered density was increased. Piezoelectric and dielectric properties were s]town to have maximum values at the $La_2O_3$ contents of 0.02 mol. $La^{3+}$ ions seemed to act as a softener in the BNBT system and to enhance dielectric and piezoelectric properties in this study.

A Study on Surface of BST Thin Films by Sol-Gel Methods (졸겔법으로 제작된 BST 박막의 구조적 특성)

  • 홍경진;민용기;조재철
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.377-380
    • /
    • 2001
  • The BST thin films to composite (Ba$\sub$x/Sr$\sub$l-x/)TiO$_3$ using sol-gel method were fabricated on Pt/Ti/SiO$_2$/Si substrate. The thin film capacitor to be ferroelectric materials was investigated by structural and electrical properties. BST solution was composited by moi ratio, and then spin-coated (from 3 times to 5 times coating on Pt/SiO$_2$/Si substrate. Thickness of BST ceramics thin films are about 2600∼2800[${\AA}$] in 3 times deposition. The property of leakage current was stable when the applied voltage was 3[V]. Leakage current of 3 times coated BST thin film was 10$\^$-9/∼10$\^$-11/[A] at 0∼3[V].

  • PDF

The effect of $Nd_2O_3$ addition on the microwave dielectric properties of the BSST ceramics (BSST계 세라믹스의 마이크로파 유전특성에 미치는 $Nd_2O_3$ 첨가 효과)

  • 박인길;류기원;배선기;이영희
    • Electrical & Electronic Materials
    • /
    • v.9 no.5
    • /
    • pp.439-444
    • /
    • 1996
  • 0.15(B $a_{0.95}$ S $r_{0.05}$)O-0.15(S $m_{2(1-x}$/N $d_{2x}$) $O_{3}$-0.7Ti $O_{2}$(x=0-10[m/o]) ceramics were fabricated by mixed oxide method. Microwave dielectric properties were investigated with contents of N $d_{2}$ $O_{3}$. In the case of specimen with N $d_{2}$ $O_{3}$(6[m/o]), dielectric constant, quality factor and temperature coefficient of resonant frequency were 78.14, 2938(at 3[GHz]) and +14.19[ppm/.deg. C], respectively. By comparison its properties with undoped specimen, dielectric constant and quality factor were highly improved, but the temperature coefficient of resonant frequency was increased to positive value......

  • PDF

Geochemical Characteristics of Surface Sediments in the Keum River Estuary Adjacent to Coastal Area (금강하구 표층퇴적물의 지화학적 특성에 관한 연구)

  • Seo, Man-Seok;Park, Young-Seog
    • Journal of Fisheries and Marine Sciences Education
    • /
    • v.19 no.1
    • /
    • pp.1-7
    • /
    • 2007
  • The purpose of this study was to investigate geochemical characteristics of surface sediments in the Keum river estuary adjacent to coastal area. For this study we collected the 21 surface sediments samples. Mean size of surface samples was $3.24{\sim}6.65{\phi}$ on inner estuary and was $2.15{\sim}3.42{\phi}$ on outside estuary. Surface samples were composed of silt on inner estuary and were composed of sand which was more larger than $4{\phi}$ on outside estuary. Most major elements except CaO, $Na_2O$ showed good relationships between variation of contents and grain size. Contents of $Al_2O_3$, $Fe_2O_3$, MgO, $K_2O$, $TiO_2$, $P_2O_5$ and $M_nO$ were increased predominately owing to the variation of mean size of surface samples. Contents of Co, Cr, Cu, Li, Sr, Zn, La, Ce, Pb, Rb, Nd have a good relationships with grain size but Ba, Th, Sm have not. All of major and minor elements contents except $K_2O$ and Ba were less than world mean contents of shallow surface sediments but apprehend a high pollution possibility on silt sediments in the estuaries.

Piezoelectric and Electric Field Induced Strain Properties of PMW-PNN-PZT Ceramics with the Substitution of Ba (Ba 치환에 따른 PMW-PNN-PZT 세라믹스의 압전 및 전계유기왜형 특성)

  • 윤광희;김규수;최병수
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.1
    • /
    • pp.20-25
    • /
    • 2001
  • To develop the piezoelectric actuator, the structural, dielectric and piezoelectric properties and electric fieldinduced strain of the ceramics(Pb$\_$1-2/Ba$\_$x/)[Mg$\_$1/2/W$\_$1/2/)$\_$0.03/-Ni$\_$1/3/Nb$\_$2/3/)$\_$0.12/-(Zr$\_$0.5/Ti$\_$0.5/)$\_$0.85/]O$_3$(x=0, 0.01, 0.03, 0.05, 0.07, 0.1) were investigated with the substitution of Ba. The tetragonality of crystal structure and grain size decreased by the substitution of Ba. Curie temperature decreased due to the decrease of the tetragonality, and dielectric constants increased with the substitution of Ba. The coercive field, remnant polarization and electromechanical coupling factor also decreased, whereas the piezoelectric constatns d$\_$33/ and d$\_$31/ were showed the highest value of 430 and 209(x10$\^$-12/C/N), respectively, because of the increase of dielectric constant. The strain induced by 60Hz AC electric field had the maximum value of 204x10$\^$-6/Δℓ/ℓ at the substitution of Ba 3mol%. As the applied electric field approaches to the coercive field, the piezoelectric element is depolarized and the electric field induced strain revealed non-linearity.

  • PDF

A study on Dielectric and Electrical Properties using PMN Ceramics with $La_{2}O_{3}$ substitution ($La_{2}O_{3}$ 치환된 PMN계 세라믹스의 유전 및 전기적특성에 관한 연구)

  • Ji, S.H.;Kim, B.S.;Lee, N.H.;Lee, H.K.;Kim, Y.H.;Lee, D.C.
    • Proceedings of the KIEE Conference
    • /
    • 1996.07c
    • /
    • pp.1621-1623
    • /
    • 1996
  • The dielectric and polarizable properties of 0.85Pb$Mg_{1/3}Nb_{2/3}$)$O_3$-$0.125PbTiO_3$-$0.25BaTiO_3$ Ceramics have been investigated as a addition of the amount of $La_{2}O_{3}$($0{\leq}x{\geq}0.05$). The Temperature-dependant electrostictive characteristics of 0.85PMN-0.125PT-0.25BT relaxor ferroelectic system were improved by enhencing the extent of the diffuse phase transition(DPT). This was achieved using PMN-PT-BTceramics by the partial substitution of La at the Pb site. The curie temperature and the maximum dielectic permittivity decreased by substituting $La_{2}O_{3}$ and the electic field-related hysteresis phenomena decreased with increasing $La_{2}O_{3}$ substitution amount. It is showed decreasing in induced strain for electric field with increasing $La_{2}O_{3}$ substitution.

  • PDF