The compounds associated with corrosion, in metallic archaeological samples of carbon steel of insular origin were evaluated to establish their degree of deterioration and structural damage against air pollution. The iron phases present in samples of archaeological artifacts were detected by Raman spectroscopy and confocal Raman microcopy. These samples mainly exhibited ing mainly ${\beta}$-FeO(OH) type goethite oxyhydroxides and small amounts of akaganeite ${\alpha}$-FeO(OH) lepidocrocite ${\gamma}$-FeO(OH) due to dominant chloride in a marine environment and non-stoichiometric oxyhydroxides Fe (II + / III +) as indicators of early corrosion. Some parts showed the presence of magnetic maghemite indicating high corrosion. ${\gamma}$-FeO(OH) is a precursor of phases associated with advanced marine corrosion. By studying its decomposition by Raman spectroscopy, it was synthesized with the following sequence: ${\gamma}-FeO(OH){\rightarrow}{\alpha}-FeO(OH)+{\gamma}-FeO(OH)$, ${\rightarrow}{\gamma}-Fe_2O_3+Fe_3O_4$. Ferric compounds provided evidence for the effect of intensity of laser on them, constituting a very useful input for the characterization of oxidation of iron in this type of artifacts. Thus, destructive analysis techniques should be avoided in addition to the use of small amounts of specimen.
The effect of hot-dip aluminizing on the corrosion of the low carbon steel was studied at $650-850^{\circ}C$ for 20-50 h in $N_2/0.5%\;H_2S$ gas. The aluminized steel consisted primarily of the Al topcoat and the underlying Al-Fe alloy layer. Aluminizing drastically improved the corrosion resistance by forming the ${\alpha}-Al_2O_3$ surface scale. Without aluminizing, the steel formed nonadherent, fragile, thick scales, which consisted of FeS as the major phase and iron oxides such as FeO, $Fe_3O_4$ and $Fe_2O_3$ as minor ones.
Proceedings of the Korea Association of Crystal Growth Conference
/
1997.10a
/
pp.173-179
/
1997
출발원료로 ferric nitrate, ethylene glycol, acethyl acetone 혼합용액을 사용하여 dip-coating된 $\alpha$-Fe$_2$O$_3$막을 제조하였다. coating을 위한 혼합용액의 시간의 경과에 따른 용액내의 가교(polymerization) 효과를 관찰하기 위해서 적외선 분광기(FT-IR)을 사용하였고, 막 형성 시 유기물 분해 및 결정화 시작 온도를 확인하기 위하여 FT-IR, XRD, DSC 등을 이용하여 분석을 행하였다. 또한 각 조건에서 제조된 막은 X-선 회절 분석을 통해 결정상을 확인 하였으며, SEM을 통하여 막의 두께 변화에 대하여 관찰하였다.
Proceedings of the Korea Association of Crystal Growth Conference
/
1998.09a
/
pp.65-70
/
1998
Fine powders of $\alpha$-Fe2O3 were prepared by precipitation method using iron (III) nitrate in ethanol solvent and the thick film using this powder was made by the screen printing technology. Effects of the reaction temperature and concentration of the iron (III) nitrate on the particle size and specific surface area were studied. Also, the relationship between the powder size and properties of the thick film was discussed.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.16
no.6
/
pp.532-537
/
2003
Crystallographic, electric, magnetic and heat transition properties of $\alpha$-Fe$_2$O$_3$ have been studied with a small addition of Eu impurities. Hematite($\alpha$-Fe$_2$O$_3$) is a basic ferromagnetic material having rhombohedral structure, which is similar to perovskites structure. Eu is a rare earth element that has an electric configuration of 4f$^{7}$ 6s$^2$. X-ray diffraction pattern of Fe$_{1-x}$ Eu$_{x}$O$_3$ (x = 0.00, 0.04, 0.06) shows an increament of a value when the amount of Eu impurities increased. The VSM data show an increment of magnetization by increasing the amount of Eu impurity. The one with x=0.06 shows the largest increment of magnetic remanence. The magnetic remanence varied from 0.49$\times$10$^{-3}$ emu/g to 0.62$\times$10$^{-3}$ emu/g when Eu impurity is increased by 2 %. Coercivity is decreased as Eu impurity is increased. Resistances is reduced significantly by Eu impurity. There is a clear difference in temperature-dependent resistance depending on the amount of Eu impurities. Especially, there are cusps between 150 K to 175 K. It indicates the change of electronic quantum states inside the atoms by rare earth impurities in rhombohedral structure. Temperature-dependent heat capacity shows that the most effective amount of Eu impurities is 6 %. %.
A TEM study on proeutectoid ${\alpha}$ reaction at sub-eutectoid temperatures has been made in hypoeutectoid Ti-3.gw/o Co and Ti-5.2w/o Fe alloys. Widmanstatten ${\alpha}$ plates were formed in both alloys within the ${\beta}$ matrix with some modification of degenerate forms. These degenerate plates were formed by the sympathetic nucleation of ${\alpha}$ plates at ${\alpha}:{\beta}$ interphase boundaries. Three types of sympathetic nucleation, i.e., edge-to-edge, face-to-edge, face-to-face, were found in both alloys. The edge-to-edge sympathetically nucleated crystals formed a low-angle boundary between two crystals. The ${\alpha}:{\beta}$ interphase boundaries were found to be partially coherent interfaces which consist of regularly spaced misfit dislocations. The growth of these interphase boundaries were accomplished by the lateral movement of growth ledges. The intersection points of two ${\alpha}$ plates or the low angle boundaries which had formed by edge-to-edge sympathetic nucleation played a role as the potential sources of growth ledges during the growth of plate. The interfacial structures and the spatial morphologies of the degenerate proeutectoid ${\alpha}$ plates would be expected to influence the nucleation and growth of the succeeding eutectoid decomposition process.
Thin film ethanol sensors made from ${\alpha}-Fe_2O_3$ decorated with multiwall carbon nanotubes(MWCNTs) were manufactured by the electron beam deposition method. The morphology of the decorated ${\alpha}-Fe_2O_3$/MWCNTs (25:1 weight ratios) nanocomposite powder was investigated using the scanning electron microscopy and X-ray diffraction techniques. The thickness of thin films has been determined from ellipsometric measurements. The response of manufactured sensors was investigated at different temperatures of the sensor work body and concentration of gas vapors. Good response of prepared sensors to ethanol vapors already at work body temperature of $150^{\circ}C$ was shown.
The addition of Ni leads to the formation of protective rust layer on steel and subsequently high corrosion resistance of steel in $Cl^-$-containing environment. $\alpha$-FeOOH, $\beta$-FeOOH, $\gamma$-FeOOH and $Fe_3O_4$ are formed mainly on steels exposed to $Cl^-$-containing environment. As the first work of this kind, this study reports the influence of Ni on the oxidation behavior of $Ni_xFe_{1-x}(OH)_2$ in $Cl^-$-containing solution at two different pH regions(condition I under which the solution pH is allowed to decrease and condition I under which solution pH is maintained at 8) where $\gamma$-FeOOH and $Fe_3O_4$ are predominantly formed, respectively, upon oxidation of $Fe(OH)_2$, In the presence of Ni(II) in the starting solution, the formation of $\beta$-FeOOH was facilitated and the formation of $\gamma$-FeOOH was suppressed with increasing Ni(II) content and with increasing oxidation rate of Fe(II). Ni(II) was found to have $Fe_3O_4$-suppressing effect under condition II.
Hematite iron oxide (${\alpha}$-$Fe_2O_3$) nanowalls were fabricated on aluminum substrate by a facile solvent-assisted hydrothermal oxidation process. The XRD and EDS patterns indicate that the sample has a rhombohedral phase of hematite $Fe_2O_3$. FE-SEM, TEM, HR-TEM, SA-ED were employed to characterize the resulting materials. $N_2$ adsorption-desorption isotherms was used to study a BET surface area. Their capability of catalytic degradation of titan yellow GR azo dye with air oxygen in aqueous solution over $Fe_2O_3$ catalysts was studied. The result indicates that the as-prepared product has a high catalytic activity, because it has a larger surface area. Langmuir and Freundlich isotherms of adsorption dye on the catalysts surface were investigated and the decomposition of titan yellow GR follows pseudo-first order kinetic.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.