• Title/Summary/Keyword: $(La,Sr)MnO_3$

검색결과 205건 처리시간 0.086초

고효율 고체산화물 연료전지 개발을 위한 자발 착화 연소 합성법과 고상반응법에 의한 $La_ 0.7Sr_0.3MnO_3$ 양극재료 제조 및 물성에 관한 연구 (Studies on the fabrication and properties of $La_ 0.7Sr_0.3MnO_3$cathode contact prepared by glycine-nitrate process and solid state reaction method for the high efficient solid oxide fuel cells applications 0.3/Mn $O_{3}$)

  • 신웅선;박인식;김선재;박성
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권2호
    • /
    • pp.141-149
    • /
    • 1997
  • L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ powders were prepared by both GNP(Glycine-Nitrate Process) and solid state reaction method in various of calcination temperature(800-1000.deg. C) and time in air. Also, L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ cathode contacts on YSZ(Yttria-Stabilized Zirconia) substrate were prepared by screen printing and sintering method as a function of sintering temperature(1100-1450.deg. C) in air. Sintering behaviors have been investigated by SEM(Scanning Electron Microscope) and porosity measurement. Compositional and structural characterization were carried out by X-ray diffractometer and ICP AES(Inductively Coupled Plasma-Atomic Emission Spectrometry) analysis. Electrical characterization was carried out by the electrical conductivity with linear 4 point probe method. As the calcination period increased in solid state reaction method, L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ phase increased. Although L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ single phase was obtained only for 48hrs at 1000.deg. C, in GNP method it was easy to get single and ultra-fine L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ powders with submicron particle size at 650.deg. C for 30min. The particle size and thickness of L $a_{0.7}$S $r_{0.3}$Mn $O_{3}$ cathode contact by solid state reaction method did not change during the heat treatment, while those by GNP method showed good sintering characteristics because initial powder size fabricated from GNP method is smaller than that fabricated from solid state reaction method. Based on enthalpy change from thermodynamic data and ICP-AES analysis, it was suggested to make cathode contact in composition of (L $a_{0.7}$S $r_{0.3}$)$_{0.91}$ Mn $O_{3}$ which have little second phase (L $a_{2}$Z $r_{2}$ $O_{7}$) for high efficient solid oxide fuel cells applications. As (L $a_{0.7}$S $r_{0.3}$)$_{0.91}$Mn $O_{3}$ cathode contact on YSZ substrate was sintering at 1250.deg. C the temperature that liquid phase sintering did not occur. It was possible to obtain proper cathode contacts with electrical conductivity of 150(S/cm) and porosity content of 30-40%.m) and porosity content of 30-40%.

  • PDF

Magnetic and Magnetotransport Properties of (1-x) $La_{0.7}Sr_{0.3}MnO_3-xRE_2O_3$ (RE=La, Nd) Composites

  • Kim, Hyo-Jin;Kang, Young-Min;Yoo, Sang-Im
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2009년도 정기총회 및 동계학술연구발표회
    • /
    • pp.192-192
    • /
    • 2009
  • Magnetic and magnetotransport properties of (1-x) $La_{0.7}Sr_{0.3}MnO_3-xRE_2O_3$ (RE=La, Nd) (x = 0.025, 0.05, 0.075, 0.1, 0.2, 0.3) composite polycrystalline samples were systematically studied. Samples were prepared using conventional solid-state reaction. LSMO and $RE_2O_3$ react at high temperature and become chemically compatible. The ferromagnetic-paramagnetic transition temperatures ($T_c$) of the LSMO-$Nd_2O_3$ composite samples were decreased 313K~349K with increasing x, while the $T_c$ values of the LSMO-$La_2O_3$ composite samples were almost unaltered in the range of 355K~358K, representing that the ferromagnetism of LSMO might be more seriously degraded by Nd substitution on the ($La_{0.7}Sr_{0.3}$) site. However, LSMO-$RE_2O_3$ composite samples exhibit greatly enhanced low field magnetoresistance (LFMR) and dMR/dH value without an appreciable increase in its resistivity. Remarkably improved LFMR properties are attributed to LSMO grain boundaries acting as effective spin-dependent scattering centers. The relationship among the $RE_2O_3$ addition, microstructure, magnetic and magnetotransport properties will be discussed in this paper.

  • PDF

박막형 고온초전도 선재를 위한 산화물 완충층의 IBAD_MgO 기판에서의 성장과 특성 (Growth and characterization of oxide buffer layer on IBAD_MgO template for HTS coated conductors)

  • 고락길;장세훈;하홍수;김호섭;송규정;하동우;오상수;박찬;문승현;김영철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.297-297
    • /
    • 2008
  • Buffer layers play an important role in the development of high critical current density coated conductor. $LaMnO_3$, $SrTiO_3$ and $BaZrO_3$ buffer layers were compatible with MgO surfaces and also provide a good template for growing high current density REBCO(RE=Rare earth) films. Systematic studies on the influences of pulsed laser deposition parameters (deposition temperature, deposition pressure, processing gas, laser energy density, etc.) on microstructure and texture properties of $LaMnO_3$, $SrTiO_3$ and $BaZrO_3$ films as buffer layer deposited on ion-beam assisted deposition MgO (IBAD_MgO) template by pulse laser deposition method, were carried out. These results will be presented together with the discussion on the possible use of this material in HTS coated conductor as buffer.

  • PDF

부유대역용융법에 의한 $RE_{1-x}Ca_xMnO_3$ (RE=La, Nd)의 결정성장 (Crystal Growth of $RE_{1-x}Ca_xMnO_3$(RE=La, Nd) by Floating Zone Method)

  • 정준기;조남희;김철진;이태근
    • 한국결정학회지
    • /
    • 제11권4호
    • /
    • pp.231-237
    • /
    • 2000
  • CMR Materials RE/sub 1-x/Ca/sub x/MnO₃(RE=La, Nd, A=Ca, Sr) were grown using the floating zone image furnace with halogen lamps as heat source. The growth condition was at 2∼10 mm/hr growth rate in air atmosphere, were 445∼50 rpm and 20∼25 rpm of rotation rate of feedrod and growing crystal, respectively. The grown crystals showed shiny black color and annealed at 1500℃ in a box furnace to release the residual stress during cooling. Characterization analyses of the crystal were carried out using XRD and SEM. The crystal structure of Nd/sub 0.7/Ca/sub 0.3/MnO₃ was analyzed with smart CCD XRD was lattice parameter of a=5.425(4)Å, b=5.434(4)Å, and c=7.712(5)Å, an orthorombic system with space group of pbnm.

  • PDF

(La, Sr)MnO3을 이용한 가변 방사율 소재에 관한 연구 (Experimental Investigation of Variable Emittance Material Based on (La, Sr)MnO3)

  • 한선우;최봉수;송태호;김성진;이봉재
    • 대한기계학회논문집B
    • /
    • 제37권6호
    • /
    • pp.583-590
    • /
    • 2013
  • 가변 방사율 라디에이터는 우주환경에서 작동하는 장비의 온도가 낮을 때는 방사율이 낮아져 시스템의 외부로의 열 손실을 줄이고, 반대로 온도가 높은 때는 방사율이 높아져 장비의 열을 외부로 방출할 수 있어 효율적인 열제어가 가능하게 한다. 가변 방사율 소재로 보편적으로 이용하고 있는 것 중 하나인 감온변색 장치(thermochromics device)는 추가적인 장비 필요 없이 열제어가 가능하기 때문에 효율적이고 고장이 발생하지 않는 장점을 가지고 있다. 본 연구는 이와 같은 이유로 감온변색 장치의 소재 중 하나인 LSMO($La_{1-x}Sr_xMnO_3$)채택하여 졸-겔(sol-gel)방법을 이용하여 제작하고, 제작된 샘플의 가변방사 성능을 실험적으로 규명하였다. 또한, 진공환경과 극저온 환경에 반복 노출시켜 시편이 극심한 환경 변화 이후에도 방사율 값이 일정함을 확인하여 우주적합성을 판단하였다.

철을 미량 치환한 $La_{0. 67}Ba_{0.33}Mn_{1-x}^{57}Fe_xO_3$ (x=0.0, 0.005, 0.01)물질의 자기적 및 중성자 회절연구

  • 최강룡;안근영;심인보;김철성
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2002년도 동계연구발표회 논문개요집
    • /
    • pp.102-103
    • /
    • 2002
  • LaMnO$_3$에 Ca을 치환한 Mn계 perovskite 구조(ABO3)의 물질에서 초거대자기저항 현상이 발견된 이후 R$_{1-x}$$^{3+}$ A$_{x}$$^{2+}$MnO$_3$(R=La, Nd, Pr: 희토류금속, A=Ca, Sr, Ba, Cd, Pb; 2가 양이온)계의 Mn 산화물의 연구가 고감도 자기 저항 센서와 자기기록 등의 활용가능성을 중심으로 활발히 진행되고 있다. 자기적 특성이 뛰어난 초거대자기저항물질에 대한 미시적인 자성에 대한 연구는 그 메커니즘이 복잡하고 다양한 접근방식에 따른다. (중략)

  • PDF

저온 작동형 SOFC Lanthanum Ferrite계 공기극 소재의 전기적 특성 (Electrical Properties of the Lanthanum Ferrite-Based Cathode Materials for Low-Temperature SOFCs)

  • 강주현;최정운;심한별;유광수
    • 한국세라믹학회지
    • /
    • 제43권3호
    • /
    • pp.162-168
    • /
    • 2006
  • The perovskites with nominal compositions $La_{0.8}Sr_{0.2}Fe_{1-x}M_xO_3$ (M=Co, Mn, Ni, x=0.1-0.3) were fabricated by a solid-state reaction method as cathode materials of low-temperature operating Solid Oxide Fuel Cells (SOFCs). X-ray diffraction analysis and microstructure observation for the sintered samples were performed. The ac complex impedance were measured in the temperature range $600-900^{\circ}C$ in air and fitted with a Solatron ZView program. The electrical conductivity and polarization resistance of $La_{0.8}Sr_{0.2}Fe_{1-x}M_xO_3$ (M=Co, Mn, Ni, x=0.1-0.3) were characterized systematically. The porosities of the sintered samples were in the range of 25% to 38%. The polarization resistance of $La_{0.8}Sr_{0.2}Fe_{0.7}M_{0.3}O_3$ was $0.291{\Omega}cm^2\;at\;700^{\circ}C$.