In case that W/B is 20%, 30%, 40% respectively, the effects of additive and shrinkage reducing agent on the autogenous shrinkage for high strengthen concrete through the substitution of FA and SF analysis were obtained as following conclusions. When the ratio of FA increased, the compressive strength of high strengthen concrete is decreased in the early times. As the ratio of SF increase, the compressive strength also increased. Comparing with PC(Portland Cement) for 7 days curing, the strength is 13.8% of FA10 + SR0.5 and 19.2% of FA15 + SR0.5 decreased when W/B is 20%, and 6.1% of SF7.5 + SR0.5, 4.8% of SF15 + SR0.5, the strength are increased. In case that W/B is 30%, 13.1% of FA10 + SR0.5 19.1% of FA15 + SR0.5 the strength is decreased and 4.1% of SF 7.5 + SR0.5, 7.2% of SF15 + SR0.5 the strength are increased. In case of W/B 40%, 4.3% of FA10 + SR0.5, and 8.7% of FA15 + SR0.5, the strength is decreased and 3.3% of SF7.5 + SR0.5, 6.3% SF15 + SR0.5 the strength is increased. When the ratio of SR is 0.5%, autogenous shrinkage strain of OPC concrete appeared $-417{\times}10-6$ in 56days curing, the shrinkage strain is decreased 23.7%. The reducing effects of autogenous shrinkage when the mineral and shrinkage agent are used are the same as ones when only shrinkage agent used.

Keywords