For the development of superconducting fault current limiters(SFCLs) having large current capacity, we fabricated an SFCL element that consists of Bi-2212 superconductor and Cu-Ni alloy tubes. First, Ag was plated on the surface of the Bi-2212 for the enhancement of soldering process. On the Ag-plated Bi-2212 tube, a Cu-Ni alloy tube was soldered using optimized solders and soldering conditions. The BSCCO/Cu-Ni composite was processed mechanically to have a helical shape for the improvement of the SFCL characteristics. The total current path of the SFCL element was 1330 mm long with 12 turns, and had critical current of 340 A at 77 K. Finally, we carried out the fault test using the fabricated SFCL element. It showed successful current limiting performance under the fault condition of 50 $V_{rms}$ and 5.5 kA. From the results, the rated voltage of the SFCL element was decided to be 0.4 V/cm, and the power capacity was 12 kVA at 77 K. The fabrication process of the SFCL and the fault test results will be presented.

Keywords

References

  1. 유상임, "고온초전도 벌크재료의 기술개발 현황 및 전망", 초전도 저온공학, 4권 2호, 2002
  2. Steffen Elschner, Frank Breuer, Thomas Rettelbach, Heribert walter, and Joachim Bock, "Manufacturing and Testing of MCP 2212 Bifilar Coils for a 10 MVA Fault current Limiter", IEEE Trans. Applied. Superconductivity, 13, 1051-8223, 2003
  3. S. Elschner , F. Breuer , M. Noe, A. Wolf, J. Bock, "Qualification of MCP BSCCO 2212 bulk material for use in resistive current limiters", Physica C, 372-376, 2002
  4. Dae-Gon Kim, Seung-Boo Jung, "Interfacial reactions and growth kinetics for intermetallic compound layer between In-48Sn solder and bare cu substrate", Journal of Alloys and Compounds, 386, 151-156, 2005 https://doi.org/10.1016/j.jallcom.2004.05.055
  5. I. Shohji, S. Fujiwara, S. Kiyono and K. F. Kobayashi, "Intermetallic compound layer formation between Au and In-48Sn solder", Scripta Materialia, 40, 7, 815-820, 1999 https://doi.org/10.1016/S1359-6462(99)00007-X