Generally, ceramics are very difficult-to-cut materials because of its high strength and hardness. The machining process of ceramics can be characterized by cracking and brittle fracture. In the machining of ceramics, edge chipping and crack propagation are the principal reasons to cause surface integrity deterioration. Such phenomenon can cause not only poor dimensional and geometric accuracy, but also possible failure of the ceramic parts. Ceramics can be machined with traditional method such as grinding and polishing. However, such processes are generally cost-expensive and have low material removal rate. Thus, in this paper, to overcome these problems. BN powder, which gives good cutting property, is added for the fabrication of machinable ceramics by volume of 5,10,15,20,25 and 30%. And, mechanical properties, R-curve behavior and machining tests are carried out to evaluate the machining properties of the manufactured machinable ceramics.

키워드

참고문헌

  1. Cao, Y., 'Failure analysis of exit edges in ceramic machining using finite element analysis,' Engineering Failure Analysis, Vol. 8, pp. 325-338, 2001 https://doi.org/10.1016/S1350-6307(00)00024-8
  2. Zhang, G., Cao, Y. and Qi, L., 'Single point cutting of machinable glass ceramics,' Transactions of NAMRI/SME, Vol. XXVII, pp. 159-164, 1999
  3. Zhang, G., Qi, L. and Cao, Y., 'Assessment of machining performance of dental ceramics,' Transactions of NAMRI/SME, Vol. XXVI, pp. 105-110, 1998
  4. Wang, Z. Y., Rajurkar, K. P. and Murugappan, M., 'Cryogenic PCBN turning of ceramic($Si_3N_4$),' Wear, Vol. 196, pp. 1-6, 1996 https://doi.org/10.1016/0043-1648(95)06645-4
  5. Yan, B. H., Guang, F. Y., and Chow, H. M., 'Study on the turning characteristics of alumina-based ceramics,' Journal of Materials Processing Technology, Vol. 54, pp. 341-347, 1995 https://doi.org/10.1016/0924-0136(95)01798-4
  6. Liu, S. Y., and Chen, I. W., 'High Temperature Crack Growth in Silicon Nitride under Static and Cyclic Loading:Short-Crack Behavior and Brittle-Ductile Transition,' Acta mater, Vol. 44. No. 5, pp. 2079-2092, 1996 https://doi.org/10.1016/1359-6454(95)00307-X
  7. Zhang, Z. H., Zhang, J. H. Sun, K. M., and G. D. Wang, 'Study on the diamond tool drilling of engineering ceramics,' Journal Materials Processing Technology, Vol. 122, pp. 232-236 https://doi.org/10.1016/S0924-0136(02)00016-X