Abstract

The production of industrial wastes have increased due to the growth of population and industrial development. Among these wastes, especially amount of paper ash has been increased year after year. If it is possible to reuse industrial wastes, it will be beneficial not only economically but also environmentally. In this study, the possibility of the utilization of paper ash were investigated as a construction materials through a series of laboratory testing carried out to evaluate physical properties, compaction, consolidation, permeability and compressive strength characteristics. Concrete bricks with replacement ratio of paper ash at 2, 4, 6, 8, 10, 12, 14, 16, 18, 20%, and clayey bricks with replacement ratio of paper ash at 5, 10, 15, 20, 25, 30% were used in the test in order to evaluate its quality. As a result of tests, it were shown that the maximum replacement ratio of paper ash satisfying the quality standards of concrete bricks and clayey bricks were 11.5% and 12%, respectively.

인구증가와 산업발달로 인해 산업폐기물의 발생량은 매년 증가하고 있으며, 이들 폐기물 중 제지회의 발생량도 증가하고 있다. 산업폐기물을 재활용할 수 있다면 경제적 환경적으로 유익할 것이다. 따라서, 본 연구에서는 일련의 실내실험을 통하여 기본특성, 다짐, 압밀, 투수 및 압축강도 특성을 분석하여 제지회를 건설재료로서 활용하기 위한 방안을 연구하였다. 본 실험에서 콘크리트 벽돌과 점토 벽돌의 품질을 평가하기 위하여 제지회의 치환률을 2, 4, 6, 8, 10, 12, 14, 16, 18, 20%로 하여 제작한 콘크리트 벽돌과 제지회의 치환률을 5, 10, 15, 20, 25, 30%로 변화시키면서 제작한 점토 벽돌을 사용하였다. 시험결과, 콘크리트 벽돌과 점토 벽돌의 품질기준을 만족하는 제지회의 최대 치환률은 각각 11.5%와 12%로 나타났다.

Keywords