Abstract
Hardened concrete contains pores of varying types and sizes, and therefore the transport of air through concrete can be considered. The rate of permeability will not only depends on the continuity of pores, but also on the moisture contents in concrete and finishing material on concrete. Also it knows that the durability of reinforced concrete structure is concerned with air permeability which effects on the carbonation occurred by invasion of CO2 gas and the corrosion of steel bar occurred by O$_2$. In this paper, the effects of curing conditions and finishing materials on carbonation and air permeability are investigated according to the accelerated carbonation test. As results, carbonation velocity and air permeability are effected by curing conditions and finishing materials, and air permeability coefficient is effected by moisture content. Also the relationship between carbonation velocity coefficients and air permeability coefficients has been quite well established.
경화콘크리트는 골재와 시멘트 수화물에 의한 매트릭스 구조로 되어진 다공체이기 때문에 내부에 다양한 크기와 형태의 공극을 갖으며, 공기투과성을 갖게 된다. 이러한 투기성능은 탄산가스의 침투.확산에 따른 중성화속도와 산소와 물의 침투에 따른 철근의 부식속도를 결정하게 되어 철근콘크리트 구조물의 내구성과 밀접한 관련이 있는 것으로 보고되고 있다. 한편, 중성화속도 및 투기성능은 표면 마감재 및 콘크리트의 함수율에 의해 크게 영향을 받게 된다. 이에 본 연구는 물-시멘트비 및 마감재의 종류, 양생조건이 콘크리트의 중성화속도 및 투기성에 미치는 영향을 검토하고, 양생조건에 따른 함수상태가 투기성에 미치는 영향을 검토하였다. 본 실험결과 중성화속도 및 투기성은 물-시멘트비, 마감재의 유무 및 종류, 양생조건에 의해 크게 영향을 받으며, 콘크리트의 투기계수는 중성화속도계수와 밀접한 관련이 있는 것으로 나타나, 향후 중성화속도를 평가함에 있어서 투기계수를 요인으로 추정 가능할 것으로 사료된다.