The Beating Properties of High Yield Pulp Treated Ozone(I) - Fiber Length Distribution of Ozonenation Pulp for Beating -

오존처리(處理) 고수율(高收率)펄프의 고해(叩解) 특성(特性)(I) - 오존처리(處理) 펄프 고해후(叩解後) 섬유장(纖維長) 분포(分布) -

  • Received : 1997.04.18
  • Published : 1997.06.30

Abstract

This research has been examined to measure the degree of the fiber damage of ozonenation high yield pulp in the beating process. Ozone treated the TMP(Thermomechanical Pulp) and CTMP(Chemithermomechanical Pulp) of spruce and the CTMP of birch has been beaten to be reached 200ml(freeness) of its content. It had been studied the forming of fiber distribution by treatment for long fiber, short fiber, fine with the above method. As ozone treatment time gets longer, the pulp has showed the tendency of increasing the fiber content of 28, 48mesh. Ozone treated fiber has been increased long fiber content by being added softness. By given longer ozone treatment time, the TMP and CTMP of spruce has showed the decreasing of fiber content. On the contrary, CTMP of birch has showed the increasing its fiber content. It had proved that the results of difference are rather closer to the species of tree than closer to the kinds of pulp. The fiber content of over 200mesh which has created in beating process demonstrates the decreasing of its fiber content by getting longer ozone treatment time. The softness of fiber can be extracted by the lignin of fiber surface that had been formed by ozone treatment. Thus we assume that the fiber in the process of beating obtains less physical damage.

Keywords