W/B 및 골재암종 변화에 따른 초고강도 콘크리트의 자기수축특성

Autogenous Shrinkage of Ultra-high Strength Concrete according to W/B and Aggregate Kinds

  • 정상운 (청주대학교 건축공학과) ;
  • 김태선 (청주대학교 건축공학과) ;
  • 이홍규 (청주대학교 건축공학과) ;
  • 한동엽 (청주대학교 산업과학연구소) ;
  • 한민철 (청주대학교 건축공학과) ;
  • 한천구 (청주대학교 건축공학과)
  • 발행 : 2014.11.14

초록

The aim of this research is selecting an economical aggregate type for ultra-high strength concrete with 80 to 120 MPa of compressive strength. As the tests, the effect of water-to-binder ratios and types of aggregate on autogenous shrinkage of ultra-high strength concrete were evaluated. as the results of a series of tests performed, the slump flow was satisfied the target range of 600 ± 100 mm, and the concrete mixture with RLA showed higher elastic modulus than the other cases. For the autogenous shrinkage preventing performance, in the case of water-to-binder ratio of 15, and 20 %, the mixture with BA showed slightly improved autogenous shrinkage reducing effect than the mixture with RLA while the mixture with RLA showed better performance at 25 % of water-to-binder ratio. Therefore, based on the tests results of slump flow, elastic modulus, and autogenous shrinkage, the RLA is considered as a better aggregate type for this purpose.

키워드