Setting Properties of GGBS Powder According to Replacement of Ratio of CaO-Al2O3 Based Inorganic Binder

CaO-Al2O3계 무기결합재 사용량에 따른 고로슬래그 미분말의 응결특성

  • 최덕진 (공주대학교 친환경콘크리트연구소) ;
  • 이영재 (포항산업과학연구원) ;
  • 최세진 (포항산업과학연구원) ;
  • 김진만 (공주대학교 건축공학과)
  • Published : 2013.05.09

Abstract

As a part of study to maximize the amount used of the ground granulated blast-furnace slag, the study deals with setting properties of paste that is mixed the ground granulated blast-furnace slag with CaO-Al2O3 based inorganic blinder. The results of the experiment show that the setting time is most fast in the mix of 25% rate of CaO-Al2O3 based inorganic blinder. It is generally needed 2 hours for work time in precast concrete products. In this study, this requirement is achieved when using the retarder of 0.5%.