$BaTiO_3/SrTiO_3$ Heterolayered Thin/Thick films Dielectric Properties

$BaTiO_3/SrTiO_3$ 이종층 박막/후막의 유전특성

  • Published : 2005.07.18

Abstract

$SrTiO_3$ and $BaTiO_3$ sol-liquids and powders were prepared by the sol-gel method. $SrTiO_3/BaTiO_3$ heterolayered thin/thick films have been prepared on the $Al_2O_3$ substrates by screen printing and spin-coating method. The thin films were sintered at $750^{\circ}C$ in the air for 1 hour and the thick films sintered at $1325^{\circ}C$ in the air for 2 hours, respectively. The $SrTiO_3/BaTiO_3$ thin/thick films's structural and dielectric properties were investigated. Increasing the spin-coating times, (110), (200), (211) peaks of the $SrTiO_3$ were increased. The X-ray diffraction(XRD) patterns and SEM photographs indicated that the $SrTiO_3$ phase were formed in the surface of $BaTiO_3$ thick films. The average thickness of a $BaTiO_3$ thick films and $SrTiO_3$ thin films were $50{\mu}m$ and 400nm, respectively The dielectric constant and dielectric loss of the $SrTiO_3/BaTiO_3$ thin/thick films with $SrTiO_3$ coated 5 times were 1598 and 0.0436 at 10KHz.

Keywords