Ferroelectric Mg-doped SBT and Ti-doped SBT were successfully deposited on Pt/Ti/$SiO_2/Si$ substrate by using a sol-gel solution coating method. The solutions were prepared through out adding the metal alkoxide solutions to SBT solution. The typical hysteresis loop of the films was obtained at 5V. The measured $2P_r$ value were $16.50{\mu}C/cm^2$ for SBT, $18.98{\mu}C/cm^2$ and for Mg-doped SBT, and $17.10{\mu}C/cm^2$ for Ti-doped SBT at an applied voltage of 5V, respectively. And it is found that the leakage current densities are less than $10^{-7}A/cm^2$ when applied voltage is less than 10.8MV/cm, which indicates the excellent insulating characteristics.