The 2, 4, 6 and 8mol% Y2O3 doped-ZrO2 powders (20 kinds) with the addedtion of Al2O3 upto 8wt% were prepared by coprecipitation method using the zirconium oxyacetate, yttrium chloride and aluminum nitrate as starting materials. The coprecipitated powders were characterized by XRD, TG-DTA, FT-IR and SEM. The sintering properties of zirconia-alumina composites prepared by 2YSZ and 8YSZ powders containing various Al2O3 contents were also investigated. With increasing the yttria stabilizer contents, the amount of exothermic heat for zirconia crystallization decreased. And it was confirmed that the crystallizing temperature of coprecipitated zirconia powders increased and the crystallization process occurred in a wide temperature range, as Al2O3 content increased in 8YSZ.
A gem-quality yttria-stabilized zirconium oxide crystals were synthesized by the skull-melting method, using the RF electrical apparatus. Principal raw materials used were $ZrO_2$and 25 wt.% $Y_2O_3$as stabilizer and 0.03~0.05 wt.% $Nd_2O_3$decolorizing agent were added to it. The single crystals were approximately 20$\times$63 mm in size with chemical composition $Zr_{0.73}$$Y_{0.27}$$O_{1.87}$ . The crystals are isotropic with no appreciable anisotropism under a polarizing microscope. Their refractive indices are in the range of 2.15~2.18, specific gravity 5.85, Mohs' hardness 8~8.5, and reflectivity 13.47%. The zirconia crystals were confirmed to have cubic structure with Face-centered lattice(Z=4), space group Fm3m ($CaF_2$-type structure) and unit cell parameters are a=5.157 $\AA$. The optimal growing conditions for yttria-stabilized zirconia are 50 kW, 2.94 MHz in power and to use a crucible with 105 mm $\times$ 135 mm in size. When the lowering speed of the crucible was set 16mm/hr gave the best yield, 42%. Since the refractive index(2.15~2.18) of cubic zirconia is smaller than that of diamond, the angle between crown and pavilion should be fashioned to make it smaller than $40.5^{\circ}$ to show the maximum brilliancy and fire.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.20
no.6
/
pp.289-294
/
2010
Ni-YSZ (Yttria Stabilized Zirconia) composite powders for SOFC were fabricated by glycine nitrate process. $ZrO(NO_3)_2{\cdot}2H_2O$, $Y(NO_3)_3{\cdot}6H_2O$, $Ni(NO_3)_2{\cdot}6H_2O$ and glycine were chosen as the starting materials. The structural properties of the sintered Ni-YSZ cermets have been investigated with respect to the volume contents of Ni. A porous microstructure consisting of homogeneously distributed Ni and YSZ phases together with well-connected grains was observed. The sintered Ni-YSZ cermets showed a porous microstructure consists of homogeneously distributed Ni and YSZ phases and the grains were well-connected. It was found that the open porosity is sensitive to the volume content of Ni. The Ni-YSZ cermet containing 35 vol% Ni seems to be suitable for the electrode material of SOFC since it provides sufficient open porosity higher than 30%.
Proceedings of the Korean Vacuum Society Conference
/
1999.07a
/
pp.150-150
/
1999
재료의 광학적 특성을 변화시키기 위한 표면 코팅의 사용을 잘 알려져 있다. 그리고 이러한 광학 코팅은 우리가 주위에서 볼 수 있는 렌즈에서부터 레이저반사경 다 나아가 다양한 광학 필터에 이르기까지 빛의 간섭을 이용한 광학 박막의 코팅은 폭넓게 이용되고 있다. 그러한 응용가운데 불필요한 표면 반사를 방지함으로써 전체 투과율을 강화시키기 위한 무반사(Anti-Reflection) 코팅은 오늘날 광대역 무반사 특성 등 다양한 광학적 요구에 따라 하나 또는 그 이상의 층을 형성함으로써 극적으로 성취할 수 있다. 본 실험은 기존 많이 활용되는 증발법 그리고 스퍼터링 방법과는 달리 고진공하에서 증착 변수를 효과적으로 제어, 박막을 형성할 수 있는 자체 제작된 단일 IBS(Ion Beam Sputtering) 시스템을 이용하여 우수한 광학적 특성을 갖는 광학 재료로써 무반사용 다층박막 형성하기 앞서 MgF2, ZrO2 (yttria stabilized zirconia) 단층 박막을 제조하였으며, 각 증착 변수에 따른 결정학적 및 광학적 특성을 관찰하였다. 본 실험에 사용된 제조 장비로 Kaufman type 2.5inch의 이온 건이 장착된 Ion Beam sputtering 시스템으로 초기 진공도는 5$\times$10-6orr이며, 이온 빔의 전류 밀도는 Fareday cup을 이용했다. 6inch 크기의 ZrO2(yttria stabilized zirconia), MgF2 타겟트를 이용하여 Si(100), glass 기판위에 박막을 성장시켰다. 각 타겟트에 대한 증착변수로 이온 에너지, 기판온도, Ar 가스량을 변화시키면서 박막을 제조하였다. 제조된 박막의 광학적 특성으로 가시 영역에서 투과율의 변화는 자외/가시광선 분광 분석기 (UV/VIS specrophotometer)를 이용하여 측정했다. 그리고 박막의 조성 및 결정학적 구조는 AES EDS와 XRD로 확인하였다. 이온 빔 전압 500V, 빔 저류 55mA일 때 온도는 상온에서 30$0^{\circ}C$까지 승온 후 MgF2 박막의 XRD분석결과 우세한 결정성을 관찰할 수 없었으며, 이 때의 광 투과도는 가시영역에서 80~90%의 값으로 측정되었다. 추후 증착된 막의 결정성을 위해 열처리를 실시하고, 각 증착조건에 대한 결과는 학회 발표시 보고한다.
The optimum powder to ball ratio was examined, which is one of the important conditions in reactive mechanical grinding processing. Yttria (Y2O3)-stabilized zirconia (ZrO2) (YSZ), Ni, and graphene were chosen as additives to enhance the hydriding and dehydriding rates of Mg. Samples with a composition of 92.5 wt% Mg + 2.5 wt% YSZ + 2.5 wt% Ni + 2.5 wt% graphene (designated as Mg-2.5YSZ-2.5Ni-2.5graphene) were prepared by grinding in hydrogen atmosphere. Mg-2.5YSZ-2.5Ni-2.5graphene had a high effective hydrogen-storage capacity of almost 7 wt% (6.85 wt%) at 623 K in 12 bar H2 at the second cycle (n = 2). Mg-2.5YSZ-2.5Ni-2.5graphene contained Mg2Ni phase after hydriding-dehydriding cycling. Mg-2.5YSZ-2.5Ni-2.5graphene had a larger quantity of hydrogen absorbed for 60 min, Ha (60 min), than Mg-2.5Ni-2.5graphene and Mg-2.5graphene. The addition of YSZ also increased the initial dehydriding rate and the quantity of hydrogen released for 60 min, Hd (60 min), compared with those of Mg-2.5Ni-2.5graphene. Y2O3-stabilized ZrO2, Ni, and graphene-added Mg had a higher initial hydriding rate and a larger Ha (60 min) than Fe2O3, MnO, or Ni and Fe2O3-added Mg at n = 1.
Neutron single crystal and powder diffraction techniques have been applied to the structure analysis of yttria-stabilized zirconium, Z $r_{0.73}$$Y_{0.27}$$O_{1.87}$., prepared by the skull-melting method. The crystal structure has been determined to be cubic symmetry, space group Fm/equation omitted/ with a=5.155(2)$\AA$, V=136.99(5)$\AA$, Z=4, and R(F)=5.65%, $\omega$R(I)=10.57% for 70 integrated intensities of Bragg Peaks observed from single crystal of Z $r_{0.73}$$Y_{0.27}$$O_{1.87}$. The stabilizer atoms randomly occupy the zirconium sites and there are displacements of oxygen atoms with amplitudes of $\Delta$/a~0.033 and 0.11 along <110> and <100> directions from the ideal positions of the fluorite structure, respectively. There are no significant differences in crystallographic data between the single crystal and powder studies. Diffraction pattern after Rietveld refinement, using neutron powder data, has shown the evidence of a tetragonal impurity phase, or a slight tetragonal distortion.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.7
no.3
/
pp.377-383
/
1997
Yttria-stabilized TZP alloyed with pentavalent oxides $(Ta_2O_5,\;Nb_2O_5)$ were fabricated by the conventional sintering method at $1500^{\circ}C$ in air to construct the simplified ternary phase diagram. The phase stability of tetragonal -$ZrO_2$ from the quasi-binary system $ZrO_2-YTa(Nb)O_4$, which do not transform to monoclinic-$ZrO_2$ even for a wide range of grain size and annealing temperature, was investigated to determine composition region of the non-transformable $t-ZrO_2$ solid solution$(NT_{ss})$. Phase stability of $NT_{ss}$ was probably due to the enhanced stability of $_YTa(Nb)O4$ having the tetragonal fergusonite structure. It was experimentally found that mixtures having $NT_{ss}$ alloyed with $T_{ss}$ by weight%% showed both excellent phase stability of $t-ZrO_2$ and fracture toughness even though the calculated composition of the mixture /was located outside $NT_{ss}$ composition region.
New process development of nuclear fuel fabrication for nuclear power plant was attempted by induction plasma technology with yttria-stabilized-zirconia ($\textrm{ZrO}_{2}$-$\textrm{Y}_{2}\textrm{O}_{3}$)powder, similar to $\textrm{UO}_{2}$, in the respect of melting point and physicochemical characteristics. Extent of powder melting was affected greatly by plasma plate power and particle size. Being optimized such as, sheath gas composition, probe position, particle size and spraying distance, dense deposit of 97.91% T.D. with deposition rate 20mm/min was attained at the condition of 120/20$\ell$/min of Ar/$\textrm{H}_{2}$ flow rate, 80kw of plate power, 8cm of probe position, 200Torr of chamber pressure and 18cm of spraying distance. The pellet of 96.5% of theoretical density was formed with homogeneity and nice exterior view at the best condition of deposition experiments, and the possibility of new nuclear pellet fabrication process was confirmed. The main and interrelated effects on deposit density were assessed by ANOVA(Ana1ysis of Variance).
Considerable research efforts have been explored attempting to enhance the thermal durability of thermal barrier coatings (TBCs) at the high operating temperatures of gas turbines. In this study, the suspension plasma spray (SPS) process was applied to produce TBCs with a segmented structure by using an yttria-stabilized zirconia (YSZ) suspension. Four different experiment sets were carried out by controlling the ratio between surface roughness of the bond coat and feed stock size ($R_a/D_{50}$) in order to examine the effect of $R_a/D_{50}$ ratio on the microstructure of SPS-prepared coatings. When the $R_a/D_{50}$ had a high value of 11.8, a deposited thick coating turned out to have a cone-type columnar microstructure. In contrast, at the low $R_a/D_{50}$ values of 2.9 and 0.18, a deposited thick coating appeared to have a dense, vertically-cracked microstructure. However, with the very low $R_a/D_{50}$ value of 0.05 the coating was delaminated.
A full retention of the tetragonal phase with coarse grains $(50\~60\;{\mu}m)$ was possible with the specimen $ZrO_2-1.9\;mol\%\;Y_2O_3$. In these coarse grains, $\{101\}_t$ annealing twins were frequently observed, although they do not exist in the usual fine grained specimens. The morphology and growth rate of the isothermally formed individual products are studied at an optical microscopic level. The habit planes of both products are also identified by performing two-surface trace analysis on the grains whose orientations are determined by the Electron Back Scattering Pattern (EBSP) method. The morphologies of isothermal martensite were well-defined thin plates and lenticular types. The growth rate in their longitudinal directions was quite slow and temperature-dependent. A two-surface trace analysis, incorporated with the EBSP method, identified the habit planes near $\{013\}_c$, in agreement with previous reports obtained from TEM works.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.