• 제목/요약/키워드: wire-rod

검색결과 100건 처리시간 0.023초

선재공형이 주름흠에 미치는 영향 (The influence of roll caliber design on the wire rod's Wrinkle defect)

  • 김준영;조용근;김용호;임규환;이영석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.180-187
    • /
    • 1999
  • This document illustrates the relationship between the wire rod wrinkle defect and the roll caliber design. The wrinkle defect is caused by the incongruent rolling conditions of the roll caliber design, the roll adjustment, and the extracting temperature. In this document, we restrict the study scope to the roll caliber design's effect on wrinkle defect at the base of real condition of the No.2 Wire Rod mill, POSCO. There has been wrinkle defect problem in the No.2 Wire Rod Mill, POSCO for many years. The engineers of the wire rod mill have been making efforts to solve the problem. As one of the efforts, we take the samples of the wire rod in the each stands of the 2'nd wire rod mill and then analyze the samples. Through the analysis, we find out the problem of the roll caliber design. So, we suggest the roll caliber design method to be more effective to weaken the wrinkle defect.

  • PDF

냉각주형식 연속주조장치에 의한 일방향응고 Cu 선재의 제조 (Unidirectionally Solidified Cu Rod Fabrication Using Continuous Casting Apparatus with Cooled Mold)

  • 조훈;조인성
    • 한국주조공학회지
    • /
    • 제29권5호
    • /
    • pp.198-203
    • /
    • 2009
  • In order to manufacture copper ultra fine wire used for bonding wire in integrated circuit package, continuous casting process, which can produce high purity copper rod with small cross section, and wiredrawing process have to be optimized to prevent wire brakeage during entire manufacturing process of fine wire. The optimum condition for producing copper rod with mirror surface has to established by investigation of the effects of several parameters such as withdrawal speed, superheat and rod diameter on grain morphology of the cast rod and on its drawing characteristics to fine wire. The purpose of this study is to propose the optimized process parameters in continuous casting process in order to produce cast rod without internal defects, and to predict microstructure orientation suitable for wire drawing process.

펄스 TIG용접에서 필러 와이어 송급속도에 따른 아크압력 변동이 용입에 미치는 영향 (The Effects of the Arc Pressure Variation on the Penetration by the filler Wire Feed Rate in Pulsed TIG Welding)

  • 조상명;김진우
    • Journal of Welding and Joining
    • /
    • 제22권1호
    • /
    • pp.71-76
    • /
    • 2004
  • In the standpoint of the arc pressure, the effects of the filler wire feed rate on the penetration was investigated in this study. The pure Ar gas was used as a shield gas and the parameters investigated were the welding current and the filler wire feed rate. By making the experiment on the arc pressure, we could know that the arc pressure was fluctuated as the depth-into-arc of the tungsten rod. Instead of the filler wire, the tungsten rod was supplied into the molten pool to make this experiment. Because the filler wire melted in arc and then we couldn't measure the arc pressure. So, the tungsten rod - the highest melting point - was used. According to the depth-into-arc of the tungsten rod, the arc pressure could be measured by using the manometer. It was proved that the arc pressure got higher as the wire feed rate was slow. It is reported the arc pressure is proportion to welding voltage and the square of welding current. But, in the filler wire TIG welding, we could blow that arc pressure was fluctuated as the depth-into-arc of filler wire was changed. We could measure the arc pressure by the variation of the filler wire feed rate and could verify that it affected bead shape and penetration.

새로운 압연Process 구축을 통한 연화소둔 열처리생략강개발 (Development of Low Annealing treatment omission steel by new rolling process)

  • 김병홍;최규성;허춘열;김경원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.27-36
    • /
    • 2004
  • Contemporary objectives for steel rod rolling processing are increasingly complex and often contrasting i.e. obtaining a desired product with optimum combination of properties such as strength, toughness and formability at lower cost. Low-alloy steel rods have been produced with several heat treatments for drawing and forging processes at room temperature. In order to reduce these heat treatments much of the researches concerning of high temperature mechanical behavior of steel rods have been conducted at wire rod mill of POSCO. In this present work, optimizations of rolling temperature and cooling rate for JS-SCM435 are performed to eliminate softening heat treatment(Low Temperature Annealing) for drawing process. The results from the optimization changed the microstructure of rods after rod rolling from Bainite with high tensile strength of 1000Mpa to Pearlite and Ferrite with appropriate strength of 750Mpa that is equivalent tensile strength after softening heat treatment.

  • PDF

비전시스템에 의한 열간 선재 단면 측정 (Measurement of Hot WireRod Cross-Section by Vision System)

  • 박중조;탁영봉
    • 제어로봇시스템학회논문지
    • /
    • 제6권12호
    • /
    • pp.1106-1112
    • /
    • 2000
  • In this paper, we present a vision system which measures the cross-section of a hot wire-rod in the steel plant. We developed a mobile vision system capable of accurate measurement, which is strong to vibration and jolt when moving. Our system uses green laser light sources and CCD cameras as a sensor, where laser sheet beams form a cross-section contour on the surface of the hot wire-rod and the reflected light from the wire-rode is imaged on the CCD cameras. We use four lasers and four cameras to obtain the image with the complete cross-section contour without an occlusion region. We also perform camera calibrations to obtain each cameras physical parameters by using a single calibration pattern sheet. In our measuring algorithm, distorted four-camera images are corrected by using the camera calibration information and added to generate an image with the complete cross-section contour of the wire-rod. Then, from this image, the cross-section contour of the wire-rod is extracted by preprocessing and segmentation, and its height, width and area are measured.

  • PDF

3-Roll 선재압연에서의 결정립조대화 방지기술 (The Technology for Reducing Abnomal Grain Growth in 3- Roll Type Wire Rod Rolling)

  • 임규환;김병홍;김기환;권정석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.163-171
    • /
    • 1999
  • The abnormal grain coarsening in wire rolling induces detrimental defects, such as jagged size tolorance, severe bending after heat treatments and drawing troubles, in the following secondary processes. Neishi et al observed that there is a band type region where grain coarsenting occurs in the plastic strain vs. deformation temperature plot. Based on the finding, we have investigate whether grain sizes and ferrite volume fractions are correlation to deformation strain with three kinds of wire rod diameters as for the different average deformation conditions. The samples were chosen from the No.2 Wire Rod Mill of POSCO where 3-roll type of finishing mill stand are used. It was found in the present work that the grain size and ferrite volume fraction of the rolled and cooled microstructure were changed with rolling reduction and rolling temperature. Abnormally grown grains at various observed points were also found. To have homogeneously fine grains of microstructure from the No. 2 Wire Rod Mill, it will be easier to control finish rolling temperature at around 750$^{\circ}C$ rather than to find another rolling schedule.

  • PDF

Flow and Convective Heat Transfer Analysis Using RANS for A Wire-Wrapped Fuel Assembly

  • Ahmad, Imteyaz;Kim, Kwang-Yong
    • Journal of Mechanical Science and Technology
    • /
    • 제20권9호
    • /
    • pp.1514-1524
    • /
    • 2006
  • This work presents the three-dimensional analysis of flow and heat transfer performed for a wire-wrapped fuel assembly of liquid metal reactor using Reynolds-averaged Wavier-Stokes analysis in conjunction with 557 model as a turbulence closure. The whole fuel assembly has been analyzed for one period of the wire-spacer using periodic boundary conditions at inlet and outlet of the calculation domain. Three different assemblies, two 7-pin wire-spacer fuel assemblies and one bare rod bundle, apart from the pressure drop calculations for a 19-pin case, have been analyzed. Individual as well as a comparative analysis of the flow field and heat transfer have been discussed. Also, discussed is the position of hot spots observed in the wire-spacer fuel assembly. The flow field in the subchannels of a bare rod bundle and a wire-spacer fuel assembly is found to be different. A directional temperature gradient is found to exist in the subchannels of a wire-spacer fuel assembly Local Nusselt number in the subchannels of wire-spacer fuel assemblies is found to vary according to the wire-wrap position while in case of bare rod bundle, it's found to be constant.

An Experimental Study of Pressure Drop Correlations for Wire-Wrapped Fuel Assemblies

  • Chun, Moon-Hyun;Seo, Kyong-Won;Park, Seok-Ki;Nam, Ho-Yun
    • Journal of Mechanical Science and Technology
    • /
    • 제15권3호
    • /
    • pp.403-409
    • /
    • 2001
  • The main objective of the present study is to perform an experimental evaluation of five existing correlations for the subchannel pressure drop analysis of a wire-wrapped fuel assembly. For this purpose, a series of water experiments have been performed using a helical wire-wrapped 19-pin fuel assembly for various test parameters. Four different test sections with different pitch to rod diameter ratios (P/D) and wire lead length to rod diameter ratios (H/D) have been fabricated. A series of pressure drop measurements were made to obtain friction factors for these four test sections. The new data along with existing data are used to evaluate existing correlations. Both the original and the simplified Cheng and Todreas correlations give the best agreement with experimental data for all flow regions.

  • PDF

도시철도 통합접지망에서의 위험전압에 따른 연접접지봉의 최적 분기간격에 관한 연구 (A Study on the Optimal Divergence Spacing of the Connecting Grounding Rod to the Dangerous Voltage in the Global Earthing Network of Urban Rail Transit)

  • 정호성;박영;김형철;김진희;김재문;조대훈
    • 전기학회논문지
    • /
    • 제61권9호
    • /
    • pp.1374-1379
    • /
    • 2012
  • Urban rail transit tends to global grounding system in order to control ground potential rise and potential differences between electric equipments. In addition, global grounding system can discharge the large capacity surge current to the ground safely. Since some railway electric equipments are installed all section of line, the global grounding system connected with the connecting grounding wire is more effectively. However, if the fault occurred in the connecting grounding wire area, some dangerous voltage is generated. So, the installation of additional grounding rod will be required. In this study, the global grounding system is simulated using CDEGS program to analyze the divergence spacing of additional ground rod depending on dangerous electric potential characteristics. Grounding net of the each station is modelled in depending on the size of the platform, and the spacing of the connecting grounding rod are compared 50m, 100m, 250m and 400m. Simulation results considering of earth resistivity and underground condition of the connecting grounding wire, spacing of the connecting grounding rod is that less than 250m to spacing of the ground rod was appropriately confirmed.

비조질 선재 제품에 대한 소개 및 최근 연구개발 동향 (Introduction of Non-Heat Treated Steel Wire Rod Developed by POSCO)

  • 이유환;김동현;이상윤;이덕락
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.137-138
    • /
    • 2009
  • There is a growing interest to replace the commercial steels with non-heat treated steels, which does not involve the spheroidization and quenching-tempering treatment in the steel-wire industry production. However, non-heat treated steels should satisfy high strength and good formability without performing heat treatment. Therefore, it is important to investigate optimum materials showing a good combination of strength and formability after the cold drawing process. In this presentation, non-heat treated steel wire rod produced by POSCO will be introduced and discussed on detail technical concepts.