• 제목/요약/키워드: wear coefficients

검색결과 170건 처리시간 0.021초

Macroscopic Wear Behavior of C/C and C/C-SiC Composites Coated with Hafnium Carbide

  • Lee, Kee Sung;Sihn, Ihn Cheol;Lim, Byung-Joo;Lim, Kwang Hyun
    • 한국세라믹학회지
    • /
    • 제52권6호
    • /
    • pp.429-434
    • /
    • 2015
  • This study investigates the macroscopic wear behaviors of C/C and C/C-SiC composites coated with hafnium carbide (HfC). To improve the wear resistance of C/C composites, low-pressure chemical vapor deposition (LPCVD) was used to obtain HfC coating. The CVD coatings were deposited at various deposition temperatures of 1300, 1400, and $1500^{\circ}C$. The effect of the substrate material (the C/C substrate, the C/C-CVR substrate, or the C/C-SiC substrate deposited by LSI) was also studied to improve the wear resistance. The experiment used the ball-on-disk method, with a tungsten carbide (WC) ball utilized as an indenter to evaluate the wear behavior. The HfC coatings were found to effectively improve the wear resistance of C/C and C/C-SiC composites, compared with the case of a non-coated C/C composite. The former showed lower friction coefficients and almost no wear loss during the wear test because of the presence of hard coatings. The wear scar width was relatively narrower for the C/C and C/C-SiC composites with hafnium coatings. Wear behavior was found to critically depend on the deposition temperature and the material. Thus, the HfC-coated C/C-SiC composites fabricated at deposition temperatures of $1500^{\circ}C$ showed the best wear resistance, a lower friction coefficient, and almost no loss during the wear test.

일방향성 배열을 가진 Sic whisker에 의해 강화된 알루미나 복합체의 Whisker orientation 에 따른 마모마찰 특성 (Tribological Behavior of the Alumina Reinforced with Unidirectionally Oriented SiC whiskers depending on whisker orientation)

  • 간태석;한병동;임대순
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.220-224
    • /
    • 1999
  • Sliding wear test was employed to determine the effect of whisker content and orientation on the firiction and wear behavior of SiC whisker reinforced alumina. Composites containing unidirectionally oriented whiskers were prepared by a modified tape casting followed by lamination, binder removal and hot pressing in order to align the whiskers in the tape casting direction. Wear coefficients on three directions were measured; parallel and normal to the tape casting direction on the tape casting surface and normal to lamination direction on surfnce normal to the tape casting direction. In the effect of whisker orientation, the highest wear rate was obtained in the direction parallel tape casting direction and the lowest in the direction normal to lamination direction at all temperatures. Silicon oxide layer amoothing the surface was detected by energy dispersive X-ray analysis on the worn surface.

  • PDF

광감쇄를 이용한 마모입자의 농도 측정 (Wear Debris Concentration Measurement by Laser Beam Attenuation)

  • 강기호;손정영;전형욱;윤의성;안효석
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1990년도 제12회 학술강연회초록집
    • /
    • pp.58-62
    • /
    • 1990
  • The size and concentration of wear debris in lubricating oil often reveal the operating condition of the rotating machinery. To evaluate the possible application of light attenuation measurement for the estimation of wear debris concentration in the lubricating oil, the light transmittance through the lubricating oil cell contaminated with various concentrations of diatomite particles was measured, the attenuation coefficient was estimated from the transmittance measurement and the coefficients were compared with those obtained from the scattering theory. The comparision showed good agreements between them. It is also noted that the experimentally determined attenuation coefficient showed almost linear relation with particle weight concentrations for the concentrations within the range of 2000 ppm. For the case of 0 ppm weight concentration of diatomite particles in the lubricating oil cell, the thickness of the cell required to give $100 \mu W$ light attenuation is 7.75 mm. This result indicates that the light attenuation method will be one of the possible candidates of machine failure diagnostic sensors for the estimation of wear debris concentration in the lubricating oil.

  • PDF

Ni-SiC 복합도금층의 내마모성에 관한 연구 (A study on the wear resistance of Ni-SiC composite plating)

  • 김성호;한혜원;장현구
    • 한국표면공학회지
    • /
    • 제29권1호
    • /
    • pp.26-35
    • /
    • 1996
  • The Ni-SiC composite plating was performed in a Watt nickel solution and the wear resistance of the composite layer was studied on a pin-on-flat type wear tester. The volume losses and friction coefficients were measured. It was found that the quantity of SiC powder in the composite layers was affected by SiC concentration, pH, temperature, and agitation speed in the Watt nickel solution. The hardness and wear resistance of the coatings increased with SiC content. The quantity of SiC powder in the coating from a nickel sulfamate solution is larger than that of the Watt nickel solution, because the amount of nickel ions absorbed on the SiC powder in the nickel sulfamate solution is greater than that in the Watt's solution.

  • PDF

광감쇄를 이용한 마모입자의 농도 측정 (Wear Debris Coacentration Measurement by Laser Beam Attenuation)

  • 강기호;손정영;전형욱;윤의성;안효석
    • Tribology and Lubricants
    • /
    • 제6권2호
    • /
    • pp.94-98
    • /
    • 1990
  • The size and concentration of wear debris in lubricating oil often reveal the operating condition of the rotating machinery. To evaluate the possible application of light attenuation measurement for the estimation of wear debris concentration in the lubricating oil, the light transmittance through the lubricating oil cell contaminated with various concentrations of diatomire particles was measured, the attenuation coefficient was estimated from the transmittance measurement and the coefficients were compared with those obtained from the scattering theory. The comparision showed good agreements between them. It is also noted that the experimentally determined attenuation coefficient showed almost linear relation with particle weight coucentrations for the concentrations within the range of 2000 ppm. For the case of 0 ppm weight concentration of diatomire particles in the lubricating oil cell, the thickness of the cell required to give $100 \muW$ light attenuation is 7.75 mm. This result indicates that the light attenuation method will be one of the possible candidates of machine failure diagnostic sensors for the estimation of wear debris concentration in the lubricating oil.

Ductile Cast Iron (DCI) 롤의 마모 특성 고찰 및 마모계수 도출을 위한 실험적 연구 (Experimental Study to Examine Wear Characteristics and Determine the Wear Coefficient of Ductile Cast Iron (DCI) Roll)

  • 변상민
    • Tribology and Lubricants
    • /
    • 제33권3호
    • /
    • pp.98-105
    • /
    • 2017
  • A pin-on-disk test is performed to measure the wear volume of a ductile cast iron (DCI) roll when it wears down using a high carbon steel and two alloy steels at different sliding velocities between the roll and the material (steel). Normal pressure is set as constant and test temperatures are 400, 500 and $600^{\circ}C$. In addition, thermal softening behavior of the DCI roll is examined using a high-temperature micro-hardness tester and the surface hardness variation of the DCI roll is expressed in terms of temperature and heating time. Based on experimental data, a wear coefficient used in Archard's wear model for each material is obtained. The wear volume is clearly observed when the test temperature is $400^{\circ}C$ and sliding velocity varies. However, it is not measured at temperatures of $500^{\circ}C$ and $600^{\circ}C$ even with variations in sliding velocity. From the optical photographs of the pin and disk, the abrasive wear is observed at $400^{\circ}C$ clearly, but no at $500^{\circ}C$ and $600^{\circ}C$. At higher temperatures, the pin surface is not smooth and has many tiny caves distributed on it. It is found that wear volume is dependent on the carbon contents rather than alloy contents. Results also reveal that the variations of wear coefficients are almost linearly proportional to the carbon contents of the material.

곡선 구간에서 철도 차량 휠의 마모 특성 해석 (A Wheel Wear Analysis of Railway Vehicle on a Curved Section)

  • 강주석
    • 대한기계학회논문집A
    • /
    • 제40권6호
    • /
    • pp.547-555
    • /
    • 2016
  • 철도차량의 휠의 마모는 주로 곡선 주행 시 발생한다. 휠의 형상 변화는 차량 동적 안정성에 중요한 영향을 미친다. 본 연구에서는 곡선 주행 시 휠 마모 특성 분석을 위해 곡선 반경 크기와 속도를 변경시키면서 휠 마모량을 계산하였다. 다물체 동역학 해석에 기초한 차량 동역학 해석결과로부터 마모인자를 계산하고 BRR(British Rail Research)에서 제시한 마모 모델을 이용하여 휠의 마모량을 계산하였다. 반경 300m에서의 마모량이 다른 반경과 비교하여 매우 큰 것으로 나타났다. 곡선 선로에 윤활유를 도유하는 경우 마모 특성 변화를 분석하기 위해 휠의 답면과 플랜지 부위의 마찰계수를 다르게 하여 휠 마모량을 계산하였다. 도유 시 휠 마모의 개선 효과를 여러 반경에서 계산하고 실제 도시철도구간에서 마모 개선 효과를 확인하였다.

C-N 코팅 스퍼기어의 마찰${\cdot}$마모 특성에 관한 연구 (A Study on the Friction and Wear Characteristics of C-N Coated Spur Gear)

  • 노용;류성기
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2004년도 학술대회지
    • /
    • pp.41-46
    • /
    • 2004
  • This study deals with the friction and wear characteristics of C-N coated spur gear. The PSII apparatus was built and a SCM415 test piece and test gear with steel substrate was treated with carbon nitrogen by this apparatus. The composition and structure of the surface layer were analyzed and compared with that of PVD coated TiN layer. It was found that both of friction coefficients of C-N coating and TiN coaling decreased with increasing load, however, C-N coating showed relatively lower friction coefficient than that of TiN coating. We was investigated the effect of C-N coating on hardness, friction and wear. The TiN coated gear showed more serious friction phenomena than that of C-N coated gear. It was considered that coating of TiN, which was conducted at a vacuum chamber at about $500^{\circ}C$ results in a tempering of base material that causes microstructure change, which in turn resulted in decreasing of hardness. The C-N coated gear and pinion had higher wear resistance that of TiN coated gear and pinion. C-N coating significantly improved the friction and wear resistance of the gear.

  • PDF

콜타르 핏치를 이용하여 제조된 탄소/탄소 복합재의 관성제동 마찰특성 (The Inertia Friction properties of the Carbon/Carbon Composites Manufactured Using a Coal-tar Pitch)

  • 이진용;서동수;임연수;이승구;박종규
    • 한국세라믹학회지
    • /
    • 제35권7호
    • /
    • pp.740-748
    • /
    • 1998
  • The inertia friction properties of C/C composites manufactured by the processes of pressure and at-mospheric carbonizaton with a commerciallized and two kinds of modified coal-tar pitch as a matrix pre-cursor were investigated. The modifications of a pitch such as the introduction of mesophase and the ad-dition of sulphur into a raw pitch were not effective for a impregnation efficiency conducted in a vacuum and at the same time in a pressure of 5kg/cm2 due to the increase of the pitch viscosity. There was not a difference in the densification increment between the pitch modifications however it was revealed that a pressure carbonization was more advantageous than an atmospheric in the densification and the formation of anisotropic carbon matrix. The friction and wear propertis of C/C having higher degree of matrix cry-stallization higher density and hardness of friction surface showed superiority. As the braking energy was increased the friction coefficients were decreased and reached almost same level at the high kinetic energy of 99.6kJ. The wear trends at 99.6kJ were different from the behaviors of friction ceofficient under the same energy in which an oxidation wear is being considered along with a mechnical wear although the wear rates were almost similar to the friction coefficient at the low energy.

  • PDF

방전 드릴을 이용한 미세 홀 관통 공정의 전극 소모량 실시간 예측 (Real-Time Prediction of Electrode Wear for the Small Hole Pass-Through by EDM-drill)

  • 최용찬;허은영;김종민;이철수
    • 한국생산제조학회지
    • /
    • 제22권2호
    • /
    • pp.268-274
    • /
    • 2013
  • Electric discharge machining drill (EDM-drill) is an efficient process for the fabrication of micro-diameter deep metal hole. As there is non-physical contact between tool (electrode) and workpiece, EDM-drill is widely used to machine the hard machining materials such as high strength steel, cemented carbide, titanium alloys. The electro-thermal energy forces the electrode to wear out together with the workpiece to be machined. The electrode wear occurs inside of a machining hole. and It causes hard to monitor the machining state, which leads the productivity and the quality to decrease. Thus, this study presents a methodology to estimated the electrode wear amount while two coefficients (scale factor and shape factor) of the logarithmic regression model are evaluated from the experiment result. To increase the accuracy of estimation model, the linear transformation method is adopted using the differences of initial electrode wear differences. The estimation model is verified through experiment. The experimental result shows that within minute error, the estimation model is able to predict accurately.