• Title/Summary/Keyword: wear behavior

Search Result 855, Processing Time 0.03 seconds

Effects of Carburizing Process on Sliding wear Behavior of Carburized SCM420H Steel (침탄처리한 SCM420H의 미끄럼 마모 특성에 미치는 침탄 조건의 영향)

  • Lee, Han-Young;Lee, Kyu-Hyun
    • Tribology and Lubricants
    • /
    • v.36 no.1
    • /
    • pp.18-26
    • /
    • 2020
  • The effects of the carburizing process on the sliding wear behavior of SCM420H steel have been investigated. In particular, the effects of grain boundary corrosion observed in the surface layer after gas carburizing and the effects of hardness of the carburized cases after heat-treatment on the sliding wear properties were examined. Pin specimens carburized by two methods (gas carburizing and vacuum carburizing) were tempered at two temperatures of 180℃ and 400℃ after oil-quenching, respectively. Sliding wear tests were carried out against heattreated SKH51 steel at several sliding speeds using a pin-on-disc type test machine. As results, it can be found that there is no difference in the wear behavior between the pins carburized using two methods. This implies that the grain boundary corrosion that formed in the surface layer after gas carburizing has no effect on the sliding wear behavior of carburized SCM420H steels. Additionally, there is no significant difference in the wear behavior between carburized pins tempered at 400℃ and at 180℃ after oil-quenching, regardless of the carburizing method. This is because carburized pins tempered at 400℃ have a troostite structure, which exhibits higher tribochemical reactivity even though its hardness is lower than that of martensite structure. In this respect, it can be considered that good wear resistance of carburized cases is maintained at least until the effective case depth.

The Study on the Wear Corrosion Behavior of Induction Hardening High Strength Cast Iron in the pH Environments (고주파 열처리한 강인주철재의 마멸부식거동에 관한 연구)

  • Park, Yun-Sik;Lim, Uh-Joh;Park, Dong-Gi
    • Journal of the Korean Institute of Gas
    • /
    • v.12 no.4
    • /
    • pp.52-57
    • /
    • 2008
  • This paper studies on the wear corrosion behavior of induction hardening high strength cast iron in the acidic environments. In a variety of pH solutions, wear corrosion behavior of GC 300 with a variety of contact pressures was investigated, and corrosion wear behavior after immersion test was considered. Also, electrochemical polarization test for GC 300 was carried out in various pH solutions. The main results are as following: In the strong acidic environment, wear corrosion rate of GC 300 appears highly and in the neutral environment is stable. Also, graphitic corrosion in the strong acidic environment occurs. The corrosion current density of GC 300 becomes high in a order of pH 1 > pH 2 > pH 4 > pH 6.5.

  • PDF

Effects of Ball Milling on Sliding Wear Behavior of Ni-Al Intermetallics Coated on Mild Steel through Induction Heating Process (고주파 연소합성 코팅된 Ni-Al계 금속간화합물의 미끄럼 마모 특성에 미치는 볼 밀링의 영향)

  • Lee, Han-Young
    • Tribology and Lubricants
    • /
    • v.34 no.6
    • /
    • pp.284-291
    • /
    • 2018
  • Ball-milling for reactant powders in advance and using an induction heating system for Ni-Al intermetallic coating process are known to enhance the reactivity of combustion synthesis. In this work, the effects of the charging weight ratio of ball to powder in ball-milling for reactant Ni-Al powders and the synthesizing temperature in induction heating on sliding wear behavior of the coating layers are investigated. Sliding wear behavior of the coating layers is examined against a tool steel using a pin-on-disc type sliding wear machine. As results, wear of the coating layer ball-milled without ball was severely worn out at the sliding speed of 2m/s, regardless of the synthesizing temperature in induction heating. However, the wear rate of the coating layers at the sliding speed was remarkably decreased with increasing the charging weight ratio of ball in ball-milling for reactant powders. This can be explained by the fact that the void in the coating layer is disappeared and the coating layer is densified by the ball-milling. The evidence showed that pitting damages were disappeared on the worn surface of ball-milled coating layer. Consequentially, the Ni-Al intermetallic coating layer could have better wear resistance at all sliding speed ranges with the ball-milling for reactant powders in advance.

Effect of Applied Load and Sliding Speed on Wear Behavior of Thermally Sprayed STS316 Coating (STS316 용사코팅의 마모거동에 미치는 작용하중 및 미끄럼속도의 영향)

  • Lee, Jae-Hong;Kim, Yeong-Sik
    • Journal of Power System Engineering
    • /
    • v.18 no.5
    • /
    • pp.74-79
    • /
    • 2014
  • This article aims at investigating the effect of applied load and sliding speed on wear behavior of thermally spraryed STS316 coating. STS316 coatings were fabricated by flame spray process according to optimal parameters on steel substrates. Dry sliding wear tests were performed on STS316 coating using four different applied load as 10, 15, 20 and 25 N and four different sliding speed as 15, 30, 45 and 60 rpm. Wear behavior on worn surface was investigated using scanning electron microscope(SEM) and energy disperive X-ray spectroscopy(EDS). The dominant wear mechanism of STS316 coating under low applied load and sliding speed was oxidation on worn surface. However, under high applied load and sliding speed the principal wear mechanism was abrasion on oxidation film and damage of oxidation film.

Wear Behavior of SUS304 Stainless Steels in Corrosive Environment (부식 환경에서 SUS304 스테인레스 강의 마모 거동)

  • Lee Kwang-Jin;Yoon Sang-Don;Koo Young-Pil;Kim Hyung-Ja
    • Tribology and Lubricants
    • /
    • v.20 no.2
    • /
    • pp.91-96
    • /
    • 2004
  • Wear behavior of self-mated stainless steels in NaCl solution has been investigated. The experiment was done in the corrosive liquid of which NaCl concentration of $0\~3\%$ and temperature of $15\~90^{\circ}C$. Two kinds of wear type were observed: one is 'severe wear' type which shows gradually increasing wear volume with increasing sliding distances, the other is 'mild wear' type which shows change of wear rate from high value to low at transition distance. The specific wear rate in severe wear type was not sensitive to the liquid temperature and concentration of NaCl but stable at value of $1\times10^{-3}\;mm^3$ approximately.

A dry wear behavior as hardness difffrence in a dual disc on disc sliding wear tests (디스크 언 디스크 시스템에서 경도에 따른 건식 마모거동)

  • Kim Junghyun
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.13 no.5
    • /
    • pp.16-23
    • /
    • 2004
  • The wear behavior as the hardness of the sliding elements on the dry wear has been investigated using a disc on disc configuration. The materials of the specimens are used as ten kinds along their hardness. In this study, both upper and lower specimens have been used the same materials. Using experimental data, we figured the relationship between wear coefficient and friction coefficient, and the relationship between wear coefficient and friction temperature. Also we combined friction temperature and friction coefficient instead of wear coefficient. We substituted this into wear equation of Archard. The result had been derived a newly wear equation in disc on disc wear system.

A Study on the Variation of the Fretting Wear Mechanisms under Elastically Deformable Contacts

  • Lee, Young-Ho;Kim, Hyung-Kyu
    • KSTLE International Journal
    • /
    • v.10 no.1_2
    • /
    • pp.27-32
    • /
    • 2009
  • In this study, fretting wear tests of nuclear fuel rods have been performed by using two kinds of spacer grid springs with a concave and a convex shape in room temperature dry and distilled water conditions. The objectives were to examine the variation of the wear mechanism with increasing fretting cycles and to evaluate the difference of the wear debris detachment behavior at each test environment. From the test results, the wear volume of each spring condition increased with increasing fretting cycles regardless of the test environments. However, the wear rate did not show a regular tendency and apparently changed with increasing fretting cycles. This is because the formation of the wear particle layer and/or the variation of the contact condition between the fuel rod and spring surfaces could affect a critical plastic deformation for detaching the wear debris. Based on the test results, the relationship between the wear behavior of each spring shape and test environment condition, and the variation of the surface characteristics are discussed in detail.

A Study on Use and Purchase Behavior of Sleeping wear for Summer in Chungchong area. (여름용 잠옷착용실태와 구매행동에 관한 연구-충청지역 도시를 중심으로-)

  • 권수애;김은영;최종명;이은경
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.24 no.6
    • /
    • pp.838-849
    • /
    • 2000
  • The purpose of this study was to investigate use and purchase behavior of sleeping wear for summer. Subjects in this study were composed of 591 males and females aged from twenties to fifties, living in Taejon and Chongju. For data analysis, descriptive analysis, $\chi$$^2$-test, t-test, ANOVA, and factor analysis were used. The results are as follows. First, subjects used sleeping wear(a night gown and pajamas), and home wear(T-shirts and sweat suit with zippered top) with similar rates. The subjects, who are females, married, older and have professional jobs, owned sleeping wear such as a night gown and pajamas more than home wear. Also, the mean of using pajamas was the highest, and they were satisfied with them more than others who didn't wear them. Second, one-third of consumers purchased sleeping wear once a year in a specialty store. Consumers mainly searched for information regarding sleeping wear in the display section. Most consumers weren't influenced by others when they made their purchases. When consumers decided to purchase a product, they considered six criteria such as fabric/management, wearing/fitness, esthetic, service, symbolic status, and economic for evaluating. Among them, the factor wearing/fitness was considered the most important. These results imply that consumers would be conscious of sleeping wear even though sleeping wear and home wear are used interchangeably. In addition, consumer behavior concerning sleeping wear is different from their characteristics such as sex, age, occupation, the level of education, and marital state. Therefore, the markets with sleeping wear would be able to be segmented based on consumers’characteristics. Also, marketers should focus on distribution channels to reform the markets of sleeping wear, that is, they may offer products in specialty stores. Additionally, market managers would be able to concentrate on visual merchandising in stores in order to increase brand awareness and market share.

  • PDF

The Effects of the Annealing Temperature and Environments on Room Temperature Wear Behavior of Plasma-Sprayed Partially Stabilized Zirconia Coatings (플라즈마 용사된 부분안정화 지르코니아 코팅의 상온 마모거동에 미치는 열처리온도 및 분위기의 영향)

  • 김장엽;임대순
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.10
    • /
    • pp.1176-1180
    • /
    • 1994
  • The sliding wear behavior of the plasma-sprayed zirconia containing 3 mol% yttria was investigated after the annealing at room temperature to 80$0^{\circ}C$ in various concentrations of humid atmosphere as laboratory, humid, dry argon atmosphere. Both of the friction coefficient and the wear loss increased with increasing temperature up to 80$0^{\circ}C$. Surface morphology of the worn samples changed with annealing temperature. The change of monoclinic/tetragonal (m/t) x-ray peak intensity ratio effected the wear behavior. The m/t ratio had maximum value at 20$0^{\circ}C$ and decreased with increased temperature in laboratory and humid atmosphere. In argon atmosphere the m/t ratio had no maximum value and decreased with increasing temperature. At all the annealing temperature humid atmosphere had more the m/t ratio value than any other atmosphere. The change of toughness was showed the inversed result of m/t ratio change. The results indicated that the resudial stress which was induced by the different amount of phase transformation takes a detrimental role in wear behavior.

  • PDF

Effect of Heat Treatment Conditions on the Microstructure and Wear Behavior of Ni-based Self-flux Alloy Coatings (니켈기 자융성 합금 코팅층의 미세구조 및 마모거동에 미치는 후열처리 조건의 영향)

  • Kim, K.T.;Oh, M.S.;Kim, Y.S.
    • Journal of Power System Engineering
    • /
    • v.11 no.1
    • /
    • pp.121-126
    • /
    • 2007
  • This study aims at investigating the effect of heat treatment conditions on the dry sliding wear behavior of thermally sprayed Ni-based self-flux alloy coatings. Ni-based self-flux alloy powders were sprayed onto a carbon steel substrate and then heat-treated at 700, 800, 900 and $1000^{\circ}C$ for 30 minutes in a vacuum furnace. Dry sliding wear tests were performed using sliding speed of 0.4 m/s and applied load of 6 N. AISI 52100 ball(diameter 8 mm) was used as counterparts. Microstructure and wear behavior of both as-sprayed and heat-treated Ni-based self-flux alloy coatings were studied using a scanning electron microscope(SEM), energy dispersive X-ray spectroscopy(EDX), electron probe micro-analysis(EPMA) and X-ray diffraction(XRD). It was revealed that microstructure and wear behavior of thermally sprayed Ni-based self-flux alloy coatings were much influenced by heat treatment conditions.

  • PDF