• Title/Summary/Keyword: water-leaching

Search Result 574, Processing Time 0.025 seconds

해수-석탄회 상호작용에 의한 미량원소 용출특성:Batch 실험연구

  • 박성민;김강주;황갑수;김진삼
    • Proceedings of the Korean Society of Soil and Groundwater Environment Conference
    • /
    • 2004.09a
    • /
    • pp.295-298
    • /
    • 2004
  • It was revealed that leaching of elements were partly inhibited because seawater contains plenty of dissolved ions than fresh water. On the other hands, the low activity coefficient and the formation of complex with chloride and sulfate play roles in enhancing element leachability. However, the pH buffaring capacity of seawater is the most important factor that makes the leaching of elements and its chemical behavior in the seawater system different from those in the fresh water environments. In general, the leaching from the weathered ash was smaller than that from the fresh ash. However, it was revealed that the leaching of Si, Fe, Al, Mn, phosphate, and some other elements were independent of ash weathering. They were dependant only on the pH of the solutions.

  • PDF

Saikosaponin Contents and cAMP Phosphodiesterase Inhibitory Activities in Bupleuri Radix Extracts According to Extraction Conditions (추출조건에 따른 시호건근 추출액 중의 Saikosaponin함량 및 cAMP Phosphodiesterase 저해활성)

  • 김남수;박인선;강은미;박영현
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • v.29 no.2
    • /
    • pp.329-334
    • /
    • 2000
  • Two major oleananesaponins in Bupleuri radix, saikosaponin $\alpha$ and d, were extracted at various solvent compositions and leaching temperatures. Solvent composition was varied at 0 to 100%(v/v) of ethanol-water and methanol-water, whereas leaching temperature was adjusted to te range of 25~45$^{\circ}C$. The most effective extractant and leaching temperature were 70% ethanol and 45$^{\circ}C$, respectively. However, no major differences in saikosaponin content and cAMP phosphodiesterase inhibition were found at various leaching times. The cAMP phosphodiesterase inhibitions were alo the highest when 70% ethanol was used as the extractant.

  • PDF

Tungsten Recovery from Tungsten Carbide by Alkali Melt followed by Water Leaching (알칼리 용융 및 수 침출을 이용한 탄화텅스텐으로부터 텅스텐 회수)

  • Kim, Byoungjin;Kim, Suyun;Lee, Jaeryeong
    • Resources Recycling
    • /
    • v.26 no.6
    • /
    • pp.91-96
    • /
    • 2017
  • Tungsten (W) recovery from tungsten carbide (WC) was researched by alkali melt followed by water leaching. The experiments of alkali melt were carried out with the change of the sort of alkali material, heating temperature, and the heating duration. Water leaching of W was performed in the fixed conditions ($25^{\circ}C$, 2 hr., slurry density: 10 g/L). From the mixture of WC and sodium nitrate ($NaNO_3$) in the molar ratio of 1:2, treated at $400^{\circ}C$ for 6 hours, only 63.3% of W might be leached by water leaching. With the increase of sodium hydroxide (NaOH) as a melting additive, the leachability increased. Finally it reached to 97.8 % with the melted mixture of ($WC:NaNO_3:NaOH$) in the ratio of (1:2:2). This imply that NaOH may play a role as a reaction catalyst by lowering Gibb's free energy for alkali melt reaction for WC.

Analysis of Sediment Nutrients as Potential Sources of the Lake Water Quality (퇴적물 토양의 영양염류가 호소 수질에 미치는 잠재 요인 분석)

  • Jung, Joon-Oh;Kim, Young-Woo
    • Journal of Environmental Health Sciences
    • /
    • v.35 no.5
    • /
    • pp.376-385
    • /
    • 2009
  • The characteristics of Lake Cheonhoji water and sediment were investigated in oder to utilize these as fundamental materials for the management of lake water quality. The hydrographic properties of Lake Cheonhoji which are relatively low chance of nutrients loading from the watershed and a long retention time of lake water, lead to the probability of high lake productivity. It was also observed that lake water showed stratification during summer and complete mixing during fall, even though water depth was relatively shallow. The trophic state was eutrophic to hypertrophic from summer to late fall. The overall properties of the sediment were oligohumic, high ignition loss and high composition of NAIP and Resid.-P, which might serve as potential pollution sources of lake water quality. In laboratory scale experiments, it was observed that leaching potential of nutrients in the sediment was greatly dependant upon water temperature and dissolved oxygen. Finally, water pollution in Lake Cheonhoji was considered to be largely due to the adverse cycle of uncontrollable eutrophication, which resulted in the subsequent occurrence of dead algae and animal plankton, organic sedimentation, reduction of dissolved oxygen and nutrients leaching, which again reinforced the cycle of eutrophication in the lake.

Assessment of Leaching Characteristics of Alkaline and Heavy Metal Ions from Recycled Concrete Aggregate (자원순환을 위한 폐콘크리트 순환골재의 알칼리 및 중금속 용출특성 평가)

  • Shin, Taek-Soo;Hong, Sang-Pyo;Kim, Kwang-Yul
    • Journal of Environmental Impact Assessment
    • /
    • v.22 no.5
    • /
    • pp.427-437
    • /
    • 2013
  • Generation rate of construction wastes in Korea has occupied preponderantly in recent years. To understand chemical properties of recycled concrete aggregate (RCA), RCA samples were tested for their leaching characteristics. Leaching tests were conducted according to Korean Standard Leaching Test (KLT) and Toxicity Characteristics Leaching Procedure (TCLP) respectively. The RCA samples were characterized using X-ray fluorescence (XRF). Alkalinity of the leachate was determined using a pH meter titration method. The XRF analysis result shows that the calcium oxide (CaO) content in the RCA sample is 25.3~50.4 %. When the RCA sample was mixed with water in a batch reactor, pH in the solution was rapidly increased, and 70% of the total pH change was found in 1 hour. The TCLP showed slightly higher efficiency for leaching heavy metals than the KLT. The leaching efficiency was also higher as the particle size of RCA sample was smaller. The leaching test results suggest that RCA can be generally classified as nonhazardous waste.

Leachability of lead, cadmium, and antimony in cement solidified waste in a silo-type radioactive waste disposal facility environment

  • Yulim Lee;Hyeongjin Byeon;Jaeyeong Park
    • Nuclear Engineering and Technology
    • /
    • v.55 no.8
    • /
    • pp.2889-2896
    • /
    • 2023
  • The waste acceptance criteria for heavy metals in mixed waste should be developed by reflecting the leaching behaviors that could highly depend on the repository design and environment surrounding the waste. The current standards widely used to evaluate the leaching characteristics of heavy metals would not be appropriate for the silo-type repository since they are developed for landfills, which are more common than a silo-type repository. This research aimed to explore the leaching behaviors of cementitious waste with Pb, Cd, and Sb metallic and oxide powders in an environment simulating a silo-type radioactive waste repository. The Toxicity Characteristic Leaching Procedure (TCLP) and the ANS 16.1 standard were employed with standard and two modified solutions: concrete-saturated deionized and underground water. The compositions and elemental distribution of leachates and specimens were analyzed using an inductively coupled plasma optical emission spectrometer (ICP-OES) and energy-dispersive X-ray spectroscopy combined with scanning electron microscopy (SEM-EDS). Lead and antimony demonstrated high leaching levels in the modified leaching solutions, while cadmium exhibited minimal leaching behavior and remained mainly within the cement matrix. The results emphasize the significance of understanding heavy metals' leaching behavior in the repository's geochemical environment, which could accelerate or mitigate the reaction.

Leaching of Black Dross by Hydrochloric Acid Solutions (염산용액에 의한 블랙드로스의 침출)

  • Nguyen, Thi Thuy Nhi;Nguyen, Thi Hong;Lee, Man Seung
    • Resources Recycling
    • /
    • v.26 no.6
    • /
    • pp.58-64
    • /
    • 2017
  • Leaching of black dross with HCl solution was conducted to find a suitable process to recover valauble materials. In this work, the leaching behavior of the components was compared between black dross and the residues after water treatment. All the components except $TiO_2$ in the black dross were dissolved by HCl solution in the experimental ranges. Treatment of the black dross with water to recover the salts has negative effect on the leaching of $Al_2O_3$, MgO and $SiO_2$. The reactions occuring during the leaching were discussed. At an optimum leaching condition of 3 M HCl and $90^{\circ}C$, the leaching percentage of $Al_2O_3$, MgO and $SiO_2$ was 85, 100 and 40%, respectively.

Leaching Behaviour of vanadium from Orimulsion ash (오리멀젼회로부터 바나듐 침출특성에 관한 연구)

  • Park Kyung-Ho;Yoon Seung-Han;Nam Chul-Woo;Choi Yeung-Ki;Yoon Oh-Seub
    • Resources Recycling
    • /
    • v.13 no.4
    • /
    • pp.32-38
    • /
    • 2004
  • Recently, Orimulsion (a bitumen-in emulsion) has received increasing attention as an alternative fuel. Orimulsion combusion produces an ash rich in V, Ni and Mg which are processed to recover metals. As a basic study to recover V from Orimulsion ash, physico-chemcial properties and leaching behaviours were investigated. Orimulsion ash was fine size grains ($d_{50}$ 5.9 $\mu\textrm{m}$) with 16% V, 4 % Ni and 9% S. Vanadium was easily leached in water because Orimulsion ash was mainly constituted of metal sulfates. However, the increase of leaching temperature decreased the extraction percentage of vanadium because of hydrolysis of V(V) to vanadium pentoxide. The addition of sulfuric acid could increase the leaching percentage vanadium. In case of alkaline leaching for selective recovery of vanadium, the oxidzing agent such as $H_2$$O_2$ is required to improve the leaching per-centage

Determination of Leaching Requirements in the Unripened Tidal Reclaimed Paddy Fields (간척초기답의 제염용수량 결정을 위한 기초연구)

  • 손재권
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.42 no.2
    • /
    • pp.55-62
    • /
    • 2000
  • In order to make the reasonable irrigation plan in the unripended tidal reclaimed paddy fields, the estimation of irrigation water requirements by soil textures and water management methods for the normal growth of crops is very important . This study was carried out to determine leaching requirements before cultivating crops. For the purpose of this study, the physical and chemical properties of soil samples used in the desalinization experiments were analyzed, and change of salinity by supplying water and leaching water were investigated in the experimental field with lysimeters. As a result considering the soil textures, desalinization effects of good drainage soils(S1) were better than those of poor drainage soils (S2). In the changes of salinity of the soils with supplying water by water management methods, among the good grainage soils with culvert treatment(S1CW), salinity of S1CW3 with 1, 120mm and S1W4 with 1, 440mm supplying water were 2.6dS/m and 1.1dS/m respectively, and salinity of S1NW4 with 1.680mm among those non-culvert treatment (S1NW) was 3.0dS/m, less than critical salanity value 3.0dS/m. On the other hand, of the poor drainage soils with cultvert treatment , salinity of S2CW3 was ranged 9.4-6.0dS/m with supplied water, and that of non-culverted treatment S2NW as 12.3-8.4dS/m.

  • PDF

Leaching of Vanadium and Tungsten from Spent SCR Catalysts for De-NOx by Soda Roasting and Water Leaching Method (소다배소(焙燒) 및 수침출법(水浸出法)에 의한 탈질용(脫窒用) 폐(廢) SCR 촉매(觸媒)로부터 바나듐과 텅스텐 침출(浸出))

  • Kim, Hye-Rim;Lee, Jin-Young;Kim, Joon-Soo
    • Resources Recycling
    • /
    • v.21 no.6
    • /
    • pp.65-73
    • /
    • 2012
  • Selective catalytic reduction(SCR) catalysts are obtained from de-NOx system of thermoelectric power plant. A process was developed for valuable metals such as vanadium and tungsten recovery from spent SCR catalyst by using soda roasting followed by water leaching. Spent SCR catalyst having $V_2O_5$(1.23 mass %) and $WO_3$(7.73 mass %). For getting soluble metal forms of the targeted metals like vanadium and tungsten soda roasting process was implemented. In soda roasting process, sodium carbonate added 5 equivalent ratio at roasted temperature $850^{\circ}C$ with 120 min roasted time for $544{\mu}m$ particle size of spent SCR catalyst. After soda roasting process moved to water leaching for roasted spent catalyst. Before leaching process the roasted spent catalyst was grinded up to $-45{\mu}m$ size. The leaching time is 30 min at $40^{\circ}C$ temperature, 10 % pulp density. The final leaching efficiency obtained 46 % of vanadium and 92 % of tungsten from present process.