The aim of this study is to produce cokes which can be used for the production of ferroalloy, for this purpose, domestic anthracite mixed with plastic was sintered at various condition. The combustion and physical properties of anthracite and plastic, coal separation, and the influence of factors on the strength of coke were investigated. The results of this study are as follows: 1. The three kinds of anthracite from the Samcheok region contained 25 to 30% ash of $100{\mu}m$ over size, and have the caloric value of 5,205 cal/g(TaeAn), 4,893 cal/g(JangSung), 4,873cal/g(KyongDong). 2. The recommendable conditions for heavy-fluid separation of the Samcheok coal are to set the specific gravity of heavy fluid to 2.4 and control the size of coal to $35{\sim}140mesh$. 3. It is concluded that phenolic resin powder, liquefied phenolic resin, SAN, and melamine resin can be used as a binder for the anthracite cokes, from the thermal analysis of various plastics. Especially, the liquefied phenolic resin was considered as the most suitable binder as it would simplify the process.
Journal of the Korean Recycled Construction Resources Institute
/
v.7
no.1
/
pp.76-83
/
2012
In this study, the research examined the effect on FC, WG, RP replacement ratio on the quality improvement of BS mortar using the RA. First of all, the flow value increased as the FC contents increased, and decreased as the WG and RP contents increased. The air contents was reduced as the FC and RP contents increased, but was increased as the WG contents went up While the compressive strength of 1 : 7 mix proportion increased with the increase of the FC and WG contents, it decreased as there was more RP contents. The compressive strength of RP could increase as the mix proportion increased, but the difference depending on the improvement material type and replacement ratio decreased gradually. The absorption deteriorated as the FC and RP contents increased in all the mix proportions, but improved a little when WG was used. Meanwhile, the absorption decreased as the compressive strength improved in all the mix proportions as a correlation, but the order was FC, RP and WG depending on the quality improvement material types. The FC and WG were most favorable in terms of quality improvement as a total analysis, and the RP and WG was most effective in terms of economical efficiency and resource recycling.
Hong, Sun Chul;Han, Jung-Heon;Lee, Jundae;Ahn, Yul Kyun;Yang, Eun-Young;Chae, Soo Young;Kim, Su;Yoon, Jae Bok
Horticultural Science & Technology
/
v.31
no.6
/
pp.807-812
/
2013
In this study, we aimed to develop a simple analysis method for measuring the carotenoids content of pepper powder. A 96-wells polystyrene microplate and an ELISA reader were used for analysis. Although ELISA reader with 450 nm filter was applicable to measure carotenoid contents, the surface of microplates were degenerated by acetone used for carotenoids extraction. However, ten-folded dilute of the color extract with methanol did not affect the surface of polystyrene microplate and components of the color extract could be successfully measured by a ELISA reader, showing a high corelation with ASTA-20.1 method. In addition, this method uses 10 fold less acetone than ASTA-20.1 method resulting less acetone waste. The microplate method using ELISA reader has potential power for analyzing a large number of samples which may be very useful to the practical breeding program for high-colored peppers.
This study carried out an experiment in order to compare thermal characteristics after collecting dust generated in the process of disposing of waste tire, plywood flour in the process of manufacturing plywood, salicylic acid dust in the process of manufacturing functional soap, and dust in the process of manufacturing wheat powder, which has potential fire and explosion hazard. According to the results of experiment, the analysis showed that all samples subject to the experiment were in the condition where heat flux decreased and temperature decreased as the quantity of added talc was increased. This shows that decomposition rate decreased, and hazard decreased. However, in all of samples subject to the experiment, as heating rate increased, endothermic onset temperature moved to the low-temperature part, and the amount of absorbed heat was largely increased. This showed that the decomposition hazard of sample increased as heating rate increased, according to the analysis. Besides, TGA experiment results showed that thermal stability was secured because total weight loss decreased as the amount of talc was increased for all samples subject to the experiment regarding the ratio of weight loss. It is expected that the continuous research and supplementation of dust explosion mechanism in the future will contribute to the establishment of measures for the effective dust explosion prevention.
In this study, the separation and recovery of cerium hydroxide was investigated from the wasted cerium polishing powders. Waste cerium polishing powder contains $64.5\;wt\%$ of rare earth oxide and the content of cerium oxide is $36.5\;wt\%$. Since cerium oxide, $56.3\%$ of rare earths, is the most stable state in rare earth, the dissolution of cerium oxide in acid solution is not easy. Therefore the process of rare earth oxide by sulfation and water leaching was examined in order to increase the recovery of rare earth. Rare earth elements were recovered in the form of $\Re{\cdot}Na(SO_{4})_{2}$ by the addition of sodium sulfate to leached solution. The slurry of rare earth hydroxide was prepared by the addition of $\Re{\cdot}Na(SO_{4})_{2}$ to sodium hydroxide solution. After the oxidation of cerous hydroxide($CE(OH)_{3}$) to ceric hydroxide($CE(OH)_{3}$) by aeration, ceric hydroxide was separated from other rare earth hydroxides by controlling the acidity of solution.
Kim, Jinhan;Kim, Yongcheol;Oh, Seung Kyo;Jeon, Jong-Ki
Clean Technology
/
v.27
no.2
/
pp.139-145
/
2021
The purpose of this study is to recover valuable metals from spent batteries using a dry process. We focused on the effect of the smelting temperature on the composition of recovered solid and liquid products and collected gaseous products. After removal of the cover, the spent battery was left in NaCl solution and discharged. Then, the spent battery was made into a powder form through a crushing process. The smelting of the spent battery was performed in a tubular electric furnace in an oxygen atmosphere. For spent lithium-ion batteries, the recovery yield of the solid product was 80.1 wt% at a reaction temperature of 850 ℃, and the final product had 27.2 wt% of cobalt as well as other metals such as lithium, copper, and aluminum. Spent nickel-hydrogen batteries had a recovery yield of 99.2 wt% at a reaction temperature of 850 ℃ with about 37.6 wt% of nickel and other metals including iron. For spent nickel-cadmium batteries, the yield decreased to 65.4 wt% because of evaporation with increasing temperature. At 1050 ℃, the recovered metals were nickel (41 wt%) and cadmium (12.9 wt%). Benzene and toluene, which were not detected with the other secondary waste batteries, were detected in the gaseous product. The results of this study can be used as basic data for future research on the dry recycling process of spent secondary batteries.
Park, Min Seok;Shin, Soo Beom;Kim, Ho Soo;Kim, Min Soo;Kim, Ha Sun;Jang, Jae Hyeok;Lee, Jin Kye;Lee, Dong Kuk
Applied Chemistry for Engineering
/
v.33
no.6
/
pp.581-587
/
2022
The leather industry generates a large amount of hazardous leather waste of various types every year. Among them, shaving scrap is difficult to recycle because it contains chromium ions. Many studies in recent years have shown that shaving scraps can be processed into various types of valuable products, such as adsorbent, filler, and poultry feed. In this study, collagen peptides were extracted from shaving scraps and structurally modified to be developed as new materials with improved physicochemical properties. First, the chromium ions contained in the shaving scraps were removed using a sodium hydroxide solution, and purified through concentration and low-temperature crystallization. The purified collagen peptide was used to prepare the powder using a spray dryer. The extracted collagen peptides were structurally modified by introducing double bonds by reacting with methacrylic anhydride (MAA), and the product was confirmed by 1H NMR spectroscopy. Next, a copolymer was prepared by redox polymerization of the modified collagen peptide (MCP) and 2-ethylhexyl acrylate (2-EHA). The structure of the copolymer was qualitatively confirmed by FT-IR. In conclusion, this study confirmed that collagen peptides can be extracted from shaving scrap and converted into new eco-friendly materials through certain treatments.
Kim Young-Hwan;Yoon Ji-Sup;Jung Jae-Hoo;Jin Jae-Hyun;Hong Dong-Hee
Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
/
v.3
no.2
/
pp.77-84
/
2005
A voloxidizer for a hot cell demonstration, that handles spent fuels of a high radiation level in a limited space should be small and spent fuel powders should not be dispersed out of the equipment involved. In this study a density rate equation as well as the Stokes'equation has been proposed in order to obtain the theoretical terminal velocity of powders. The terminal velocity of U$_{3}$O$_{8}$ has been predicted by using the terminal velocity of SiO$_{2}$, and then determination has been the optimum air flow rate which is able to prevent powders from scattering. An equation which has shown a relationship between theoretical terminal velocities of U$_{3}$O$_{8}$ and SiO$_{2}$ has been derived with the help of the Stokes'equation, and then an experimental verification made for the theoretical Stokes' equation of SiO$_{2}$ by means of an experimental device made of acryl. The theoretical terminal velocity based on the proposed density rate equation has been verified by detecting U$_{3}$O$_{8}$ powders in a filter installed in the mock-up voloxidizer. As the results, the optimum air flow rates seem to be 20 LPM by the Stokes'equation while they are 14.5 L/min by the density rate equation. At the experiments with the mock-up voloxidizer, a trace amount of U$_{3}$O$_{8}$ seems to be detectable at the air flow rate of 14.5 L/min by the density rate equation, but U$_{3}$O$_{8}$ powders of 7$\mu$m diameter seem detectable at the air flow rate of 20 L/min by the Stokes'equation. It is revealed that 14.5 L/min is the optimum air flowe rate which is capable of preventing U$_{3}$O$_{8}$ powders from scattering in the UO$_{2}$ voloxidizer and the proposed density rate equation is proper to calculate the terminal velocity of U$_{3}$O$_{8}$ powders.
Kim, Sam-Soon;Lee, Ji-Yul;Park, Sung-Oh;Kim, Ki-Joo
The Korean Journal of Mycology
/
v.1
no.2
/
pp.15-23
/
1973
Mold producing cellulase were isolated from rotten woods, and identified as the three species: Aspergillus niger van Tieghem, Aspergillus schiemanni Thom and Trichoderma viride Pers. In this paper, culture conditions in the media and characteristics of these strains were investigated. Using these strains, we have conducted a research concerning the utilization of farm product waste materia's. 1. Optimum conditions for the cellulase formation were as follows. KM 10-1; pH 5.2-5.5, $35^{\circ}C$, incubation time 6 days. OL 11-1; pH 5.5, $30-35^{\circ}C$, incubation time 6 days. SH 9-2; pH 5.5, $30^{\circ}C$, incubatoin time 6 days. 2. Their cellulase activities in their optimum condition were as follows: KM 10-1; CMC-LP 78.5% CMC-SP 4.0 glucose mg/gm of the cultures/min. OL 11-1; CMC-LP 89.9%, CMC-SP 4.9 glucose mg/gm of the cultures/min. SH 9-2; CMC-I.P 77.4%, CMC-SP 3.9 glucose mg/gm of the cultures/min. 3. Hydrolysis of animal feed containing a large quantity (23-30%) of cellulose by means of the crude enzyme in the selected strains resolved 30% of the cellulose contained in the animal feed.
Recently, carbon capture and storage (CCS) techniques have been globally studied. This study was conducted to use waste cement powder as an efficient raw material of mineral carbonation for $CO_2$ sequestration. Direct aqueous carbonation experiment was conducted with injecting pure $CO_2$ gas (99.9%) to a reactor containing $200m{\ell}$ reacting solution and the pulverized cement paste (W:C = 6:4) having particle size less than 0.15 mm. The effects of two additives (NaCl, $MgCl_2$) in carbonation were analyzed. The characteristics of carbonate minerals and carbonation process according to the type of additives and pH change were carefully evaluated. pH of reacting solution was gradually decreased with injecting $CO_2$ gas. $Ca^{2+}$ ion concentration in $MgCl_2$ containing solution was continuously decreased. In none $MgCl_2$ solution, however, $Ca^{2+}$ ion concentration was increased again as pH decreased. This is probably due to the dissolution of newly formed carbonate mineral in low pH solution. XRD analysis indicates that calcite is dominant carbonate mineral in none $MgCl_2$ solution whereas aragonite is dominant in $MgCl_2$ containing solution. Unstable vaterite formed in early stage of experiment was transformed to well crystallized calcite with decreasing pH in the absence of $MgCl_2$ additives. In the presence of $MgCl_2$ additives, the content of aragonite was increased with decreasing pH whereas the content of calite was decreased.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.