PURPOSES : This study aimed to analyze the experimental and numerical behavior of warm mix asphalt pavement prepared using steel slag and RAP and to conduct economic analysis of pavement construction. METHODS : For developing high performance asphalt pavement, we performed three evaluations: fundamental analysis, experimental testing, and 3D finite element analysis. In particular, 3D finite element analysis was conducted on several pavement structures by adopting the results of experimental tests. RESULTS : Through the various evaluations, it was established that steel slag was effective for use as asphalt mixture aggregate. Moreover, asphalt mixture constituting steel slag and RAP demonstrated higher performance behavior compared with conventionally used asphalt mixture. Furthermore, based on the 3D FE modeling, we established that the developed asphalt pavement constituting steel slag and RAP can be utilized for thin layer pavement with comparable performance behavior. CONCLUSIONS :Warm mix asphalt pavement prepared using steel slag and RAP is more competitive and economic compared to hot-mix asphalt pavement. Moreover, it can be applied for preparing thin layer asphalt pavements with reasonable performance. The developed warm mix asphalt pavement prepared using steel slag and RAP can be an alternative pavement type with competitive performance based on the reasonable economic benefit it provides.
본 논문은 준고온 첨가제가 혼입된 3 종류(일반아스팔트, SBS 및 SMA)의 아스팔트 혼합물 다짐도 변화에 대한 시험 결과이다. 다짐 특성을 조사 분석하기 위하여 다짐 시간 변화와 준고온 첨가제 함량 변화에 의한 다짐도 측정을 실시하였으며, 다짐 온도를 일반시료에 비하여 $30^{\circ}C$ 및 $50^{\circ}C$를 낮추어 밀도를 비교하였다. 선회 다짐 장비를 사용하여 다짐 횟수 변화에 따른 다짐밀도의 변화를 측정하였다. 다짐시간 경과와 다짐도의 관계는 3 종류의 준고온 첨가제를 일반 아스팔트에 첨가하여 다짐시간 변화와 첨가제 함량 변화에 따른 다짐도를 측정하였다. 온도 저감에 따른 다짐도 비교는 일반 아스팔트 혼합물, 고분자 개질 아스팔트 및 SMA 혼합물 3 종류의 혼합물을 사용하여 시험을 실시하였다. 준고온 아스팔트 혼합물은 다짐온도 저감으로 인하여 일반시료 아스팔트 혼합물과 밀도의 차이가 발생하지 않아서 다짐도가 안정된 상태를 나타냈다. 한편, 혼합물의 종류 및 준고온 첨가제의 종류에 따라 밀도의 차이, 다짐도 변화의 추이 변화가 발견되어 이들 두 인자 사이에 상관관계가 있는 것으로 나타났다.
본 연구는 준고온 공법을 이용한 재생 아스팔트 콘크리트의 강도특성을 평가하기 위해 이루어졌다. 굵은 골재 최대치수 13mm의 화강암과 침입도 60-80인 신규 바인더 60-80을 재생 혼합물을 제조하는데 사용하였다. 배합설계는 RAP(굵은 입자 : 잔입자=6 : 4) 첨가비율 20%와 30%를 사용하였고 GPC, 침입도, 절대점도, 동점도를 준고온 첨가제(Evotherm와 Sasobit)의 첨가 함량을 결정하기 위하여 측정하였다. LD(low-density poly ethylene)를 본 연구에서 준고온 재생 아스팔트 혼합물의 개질제로 사용하였다. 본 연구에서는 8개의 준고온 재생 혼합물(2 RAP함량 ${\times}$ 2 준고온 첨가제 ${\times}$ 2 개질제)뿐만 아니라 2개의 일반 재생 혼합물, 1개의 가열혼합 일반혼합물(control)까지 총 11개의 혼합물을 제조하였다. 변형강도 시험, 간접인장강도 시험, 수분민감성 시험, wheel tracking을 통한 소성변형 시험을 준고온 재생혼합물의 기본 특성을 평가하기 위하여 수행하였다.
The objective of this study is to analyze rut resistance and moisture susceptibility of warm mix asphalt(WMA) mixture. The deformation strength ($S_D$), which is known to have high correlations with the high-temperature deformation resistance of dense grade mixture, was used as a tool, together with wheel tacking (WT) test, for evaluating warm mix asphalt mixture's rut resistance.
최근에 $135^{\circ}C^{\circ}C$ 이하의 온도에서 생산되는 중온형 아스팔트 혼합물의 새로운 생산 기술이 전세계적으로 개발되고 있다. 본 연구에서는 가열 아스팔트보다 낮은 온도에서 아스팔트를 효과적으로 골재에 분산시켜 코팅할 수 있는 폼드 아스팔트 기술을 이용하여 중온형 아스팔트 혼합물을 생산하였으며, 최근 개발된 새로운 Simple Performance Testing 장비를 이용하여 다양한 온도와 하중조건 하에서 중온형 폼드 아스팔트 혼합물의 공용성 특성을 평가하였다. 중온형 폼드 아스팔트 혼합물은 FG 64-22의 아스팔트를 거품상태로 만들어 중온으로 가열된 골재에 뿌려서 제조하였으며, 중온형 아스팔트 혼합물은 중온의 골재에 FG 64-22의 아스팔트를 액상 상태로 첨가하여 제조하였다. 중온형 폼드 아스팔트 혼합물은 중온형 아스팔트 혼합물보다 높은 동탄성계수와 Flow Number를 나타내었다. 따라서, $100^{\circ}C$로 가열된 골재를 사용하여 생산된 중온형 폼드 아스팔트 혼합물은 중온형 아스팔트 혼합물에 비하여 피로균열 및 소성변형 저항에 우수한 것으로 평가되었다.
PURPOSES : The main purposes of this study are to examine the influences of polyethylene wax-based WMA additive on the optimum asphalt content of warm-recycled asphalt mixture based on the Marshall mix design and to evaluate performance of warm-recycled asphalt mixture containing 30% RAP with polyethylene wax-based WMA additive. METHODS: Physical and rheological properties of the residual asphalt were evaluated in terms of penetration, softening point, ductility and performance grade (PG) in order to examine the effects of polyethylene wax-based WMA additive on the residual asphalt. Also, To evaluate performance characteristics of the warm-recycled asphalt mixtures using polyethylene wax-based WMA additive along with a control hot-recycled asphalt mixture, indirect tensile strength test, modified Lottman test, dynamic immersion test, wheel tracking test and dynamic modulus test were conduced in the laboratory. RESULTS : Based on the limited laboratory test results, polyethylene wax-based WMA additive is effective to decrease mixing and compacting temperatures without compromising the volumetric characteristics of warm-recycled asphalt mixtures compared to hot-recycled asphalt mixture. Also, it doesn't affect the optimum asphalt content on recycled-asphalt mixture. All performance test results show that the performance of warm-recycled asphalt mixture using polyethylene wax-based WMA additive is similar to that of a control hot-recycled asphalt mixture. CONCLUSIONS: Overall, the performance of warm-recycled asphalt mixture using polyethylene wax-based WMA additive is comparable to hot-recycled asphalt mixture.
본 연구는 원유정제과정에서 발생되는 산업부산물인 유황에 폴리머 성분의 첨가제를 혼입한 개질유황결합재를 사용하여 중온아스팔트 혼합물을 제조하고, 개질유황결합재를 사용한 중온아스팔트 혼합물의 간접인장강도, 수침전후 및 동결융해 전후 인장강도비와 휠트랙킹 시험에 의한 동적안정도 등의 역학 및 내구 특성을 평가하였다. 실험결과, 개질유황 결합재를 사용한 중온아스팔트 혼합물의 수침전후 인장강도비는 0.88로 중온 폼드 개질 아스팔트의 약 1.13배이며, 동결융해 전후의 인장강도비 또한 0.82로 인장강도비 KS 품질기준 값 0.75 이상을 모두 만족하였다. 간접인장강도는 1.60MPa로 KS 품질기준 값 0.80MPa의 2배, 일반가열아스팔트의 1.29MPa과 비교하여 약 1.24배 높은 간접인장강도를 나타내었다. 또한, 휠트랙킹 시험에 의한 동적안정도는 14,075회/mm로 일반가열아스팔트의 약 15배, 중온 폼드 개질 아스팔트의 약 3배로 피로균열 등 소성변형에 대한 저항성이 매우 우수하게 나타났다.
PURPOSES : The main distress of asphalt pavements in monsoon climate regions are caused by water damage and plastic deformation due to repeated rain season and increased heavy vehicle traffic volume. In this study, the mechanical properties of polymer-modified warm mix asphalt (PWMA) materials are evaluated to use in monsoon climate regions such as Indonesia. METHODS : Comprehensive laboratory tests are conducted to evaluate moisture resistance and permanent deformation resistance for three different asphalt mixtures such as the Indonesian conventional hot-mix asphalt (HMA) mixture, the polymer-modified asphalt mixture, and the polymer-modified warm mix asphalt (PWMA) mixture. Dynamic immersion test and indirect tensile strength ratio test are performed to evaluate moisture resistance. The wheel tracking test is performed to evaluate rutting resistance. Additionally, the Hamburg wheel tracking test is performed to evaluate rutting and moisture resistances simultaneously. RESULTS :The dynamic immersion test results indicate that the PWMA mixture shows the highest resistance to moisture. The indirect tensile strength ratio test indicates that TSR values of PWMA mixture, Indonesian PMA mixture, and Indonesian HMA mixture show 87.2%, 84.1%, and 67.9%, respectively. The wheel tracking test results indicate that the PWMA mixture is found to be more resistant to plastic deformation than the Indonesian PMA. The dynamic stability values are 2,739 times/mm and 3,150 times/mm, respectively. Moreover, the Hamburg wheel tracking test results indicate that PWMA mixture is more resistant to plastic deformation than Indonesian PMA and HMA mixtures. CONCLUSIONS :Based on limited laboratory test results, it is concluded that rutting resistance and moisture susceptibility of the PWMA mixture is superior to Indonesian HMA and Indonesian PMA mixtures. It is postulated that PWMA mixture would be suitable for climate and traffic conditions in Indonesia.
PURPOSES : This research was a laboratory study for evaluating the Reclaimed Asphalt Pavement (RAP) mixture added developed rejuvenator for warm mix recycling. Waste asphalt mixtures occupy about 18.2% of construction wastes in Korea. Moreover, most rejuvenators were imported from Europe or the U.S. Therefore, improving usage of RAP with a developed rejuvenator material provides environmental protection at a reduced cost. METHODS : The specimen used for this experiment was performed by only using RAP. A suitable rejuvenator for Target PG was then added. In addition, a conventional rejuvenator was selected to compare performance and specimens introduced with the same procedure as the developed rejuvenator was prepared. In order to evaluate rutting resistance and water susceptibility, we conducted a deformation strength test, a tensile strength ratio test, and a dynamic immersion test with the prepared mixtures. RESULTS :Laboratory test results indicated that both the developed additive and conventional additive improved performance of the recycled asphalt mixtures compared to mixtures without the rejuvenator. In addition, the deformation strength test and TSR test results satisfied standards for domestic recycling asphalt mixtures. The dynamic immersion test showed that the developed rejuvenator has superior scaling resistance than the conventional rejuvenator. CONCLUSIONS : In terms of rutting resistance and moisture susceptibility, the warm mix recycled asphalt mixtures with the developed rejuvenator appeared to effectively recovered performance.
PURPOSES : The purpose of this study is to evaluate of field application and laboratory performance of warm-mix asphalt (WMA) according to the dosage rate of organic-based WMA additive. METHODS: Three asphalt mixtures, i.e., hot mix asphalt (HMA), WMA with the dosage rate of 1.5%, WMA with the dosage rate of 1.0%, were sampled from the asphalt plant when the field trial project were constructed. With these mixtures, the laboratory testings were performed to evaluate the linear viscoelastic characteristics and the resistance to moisture, rutting and fatigue damage. RESULTS : From the laboratory test results, it was found that the WMA with the reduced dosage rate of additive would be comparable to HMA and WMA with the original dosage rate in terms of the dynamic modulus, tensile strength ratio, rutting resistance. However, the fatigue reisistance of WMA with the reduced dosage rate was slightly worse but it should be noted that the fatigue performance is necessarily predicted by combining the material properties and pavement structure. CONCLUSIONS: Through the field construction and laboratory testings, the dosage rate of organic-based WMA additive could be reduced from 1.5% to 1.0% without the significant decrease of compactability and laboratory performance. The long-term performance of the constructed pavement will be periodically monitored to support the findings from this study.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.