Analysis of the Wettability of Partially Fluorinated Polymers Reveals the Surprisingly Strong Acid-Base Character of Poly(vinylidene Fluoride)

  • Lee, Sang-Wha;Park, Joon-Seo;Lee, T. Randall
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권1호
    • /
    • pp.41-48
    • /
    • 2011
  • The wettabilities of the partially fluorinated polymers (ethylene-tetrafluoroethylene copolymer (ETFE), ethylenechlorotrifluoroethylene copolymer (ECTFE), and poly(vinylidene fluoride) (PVDF)) were investigated by contact angle measurements. Zisman plots for ETFE and ECTFE exhibited linear relationships, while the Zisman plot for PVDF showed a slight curvature, which was interpreted to indicate strong non-dispersive interactions between the surface and the contacting liquids. The Lifshitz-van der Waals forces of the fluoropolymers were estimated to increase in the order of ETFE < PVDF $\ll$ ECTFE. An evaluation of the polar or "acid-base" interaction energies showed that PVDF, which possesses the most acidic hydrogens among the examined fluoropolymers, has the strongest acid-base interactions.

Morphology and Crystallization in Mixtures of Poly(methyl methacrylate)-Poly(pentafluorostyrene)-Poly(methyl methacrylate) Triblock Copolymer and Poly(vinylidene fluoride)

  • Kim, Geon-Seok;Kang, Min-Sung;Choi, Mi-Ju;Kwon, Yong-Ku;Lee, Kwang-Hee
    • Macromolecular Research
    • /
    • 제17권10호
    • /
    • pp.757-762
    • /
    • 2009
  • The micro domain structures and crystallization behavior of the binary blends of poly(methyl methacrylate)-b-poly(pentafluorostyrene)-b-poly(methyl methacrylate) (PMMA-PPFS-PMMA) triblock copolymer with a low molecular weight poly(vinylidene fluoride) (PVDF) were investigated by small-angle X-ray scattering (SAXS), small-angle light scattering (SALS), transmission electron microscopy (TEM), optical microscopy, and differential scanning calorimetry (DSC). A symmetric, PMMA-PPFS-PMMA triblock copolymer with a PPFS weight fraction of 33% was blended with PVDF in N,N-dimethylacetamide (DMAc). In the wide range of PVDF concentration between 10.0 and 30.0 wt%, PVDF was completely incorporated within the PMMA micro domains of PMMA-PPFS-PMMA without further phase separation on a micrometer scale. The addition of PVDF altered the phase morphology of PMMA-PPFS-PMMA from well-defined lamellar to disordered. The crystallization of PVDF significantly disturbed the domain structure of PMMA-PPFS-PMMA in the blends, resulting in a poorly-ordered morphology. PVDF displayed unique crystallization behavior as a result of the space constraints imposed by the domain structure of PMMA-PPFS-PMMA. The pre-existing microdomain structures restricted the lamellar orientation and favored a random arrangement of lamellar crystallites.

폴리(메틸 메타크릴레이트)-폴리스티렌 이종 블록 공중합체/폴리(비닐리덴 플루오라이드) 블렌드의 미세 상분리와 결정화 (Microphase Separation and Crystallization in Binary Blends Consisting of Poly (methyl methacrylate)-block-Polystyrene Copolymer and Poly (vinylidene fluoride))

  • 김지선;이광희;조성무;류두열;김진곤
    • 폴리머
    • /
    • 제28권6호
    • /
    • pp.509-518
    • /
    • 2004
  • 비대칭 블록 공중합체와 단일고분자로 구성된 블렌드의 미세 도메인 구조와 결정화 거동을 소각 X-선 산란, 광학 현미경 및 DSC를 사용하여 조사하였다. 본 연구에서는 폴리(메틸 메타크릴레이트) 블록의 무게 분률이 0.53인 폴리(메틸 메타크릴레이트)-폴리스티렌 이종 블록 공중합체 (PMMA-b-PS)를 저분자량 폴리(비닐리덴 플루오라이드) (PVDF)와 혼합하였다. PVDF 함량 증가에 따라 블렌드 미세구조가 라멜라에서 실린더 구조로 전이하였으며, PVDF의 결정화는 결정화 이전에 형성된 미세구조의 배열을 교란시켜 질서도가 낮은 형태를 야기시켰다. 또한, PVDF 결정화 거동은 PMMA 블록과의 혼화성 및 미세 도메인에 의해 부가되는 공간적 제한에 큰 영향을 받았다.

Preparation of Poly(vinylidene fluoride)-g-poly(methacrylic acid) Composite Nanofiltration Membrane

  • Kim, Yong-Woo;Choi, Jin-Kyu;Koh, Joo-Hwan;Kim, Jong-Hak
    • Korean Membrane Journal
    • /
    • 제9권1호
    • /
    • pp.57-63
    • /
    • 2007
  • Amphiphilic graft copolymer from poly(vinylidene fluoride) (PVDF) was synthesized using atom transfer radical polymerization (ATRP) for composite nanofiltration membranes. Direct initiation of the secondary fluorinated site of PVDF facilitates grafting of tert-butyl methacrylate (tBMA). Amphiphilic PVDF-g-PMAA graft copolymer with a 51:49 wt ratio was obtained by hydrolyzing poly(tert-butyl methacrylate) (PtBMA) to poly(methacrylic acid) (PMAA). Wide angle X-ray scattering (WAXS) and differential scanning calorimetry (DSC) confirmed the decrease of crystallinity of PVDF upon graft copolymerization. Composite nanofiltration membranes were prepared from PVDF-g-PMAA as a top layer coated onto PVDF ultrafiltration (UF) support membrane. The morphology and hydrophilicity of membranes were characterized using scanning electron microscopy (SEM) and contact angle measurement. The rejections of composite membranes were 80.2% for $Na_2SO_4$ and 28.4% for NaCl, and the solution flux were 9.5 and $14.5\;L/m^2\;h$ at 1.0 MPa pressure.

가지형 공중합체/$TiO_2$ 나노복합 고분자 전해질막의 제조 및 분석 (Preparation and Characterization of Graft Copolymer/$TiO_2$ Nanocomposite Polymer Electrolyte Membranes)

  • 고종관;노동규;라즈쿠마 파텔;설용건;김종학
    • 멤브레인
    • /
    • 제20권1호
    • /
    • pp.1-7
    • /
    • 2010
  • 원자전달 라디칼 중합을 이용하여 poly(styrene sulfonic acid) 47 wt%를 가진 poly(vinylidene fluoride-co-chlorotrifluoroethylene)-g-poly(styrene sulfonic acid) (P(VDF-co-CTFE)-g-PSSA) 가지형 공중합체를 합성하였다. 티타늄 아이소프로폭사이드(TTIP)와 가지형 공중합체를 졸-겔 공정을 통하여 $TiO_2$/가지형 공중합체 복합막을 제조하였다. TTIP는 가지형 공중합체의 친수성을 가진 PSSA 영역에만 선택적으로 결합하였으며 그곳에 $TiO_2$ 나노 입자가 형성되어 성장하였다. 이와 같은 결과를 적외선과 자외선 분광학으로 확인할 수 있다. 함수량과 이온 교환 능력 (IEC)는 TTIP의 함량에 따라 감소하였고 이것은 막이 가진 술폰산의 수가 감소하기 때문이었다. TTIP가 5 중량%일 때, 막의 기계적 강도는 증가하고 수소이온 전도도도 유지되었다.

수소이온 전도성 가지형 공중합체 전해질막 제조 및 분석 (Synthesis and Characterization of Proton Conducting Graft Copolymer Membranes)

  • 노동규;고종관;서진아;김종학
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2010년도 춘계학술대회 초록집
    • /
    • pp.126.2-126.2
    • /
    • 2010
  • The "grafting from" technology to prepare the well-defined microphase-separated structure of polymer using atom transfer radical polymerization (ATRP) will be introduced in this presentation. Various amphiphilic comb copolymers were synthesized through this approach using poly (vinylidene fluoride) (PVDF), poly (vinylidene fluoride-co-chlorotrifluoroethylene) (P(VDF-co-CTFE) and poly(vinyl chloride) (PVC) as a macroinitiator. Hydrophilic side chains such as poly (styrene sulfonic acid) (PSSA) or poly (sulfopropyl methacrylate) (PSPMA) were grafted from the mains chains using direct initiation of the chlorine atoms. The structure of mass transport channels has been controlled and fixed by crosslinking the hydrophobic domains, which also provides the greater mechanical properties of membranes. Successful synthesis and microphase-separated structure of the polymer were confirmed by $^1H$ NMR, FT-IR spectroscopy and TEM. The grafted/crosslinked membranes exhibited good mechanical properties (400 MPa of Young's modulus) and high thermal stability (up to $300^{\circ}C$), as determined by a universal testing machine (UTM) and TGA, respectively.

  • PDF

비휘발성 메모리 응용을 위한 VF2-TrFE 박막의 제작 및 특성 (Fabrications and Properties of VF2-TrFE Films for Nonvolatile Memory Application)

  • 정상현;변정현;김현준;김지훈;김광호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.388-388
    • /
    • 2010
  • In this study, Ferroelectric vinylidene fluoride-trifluoroethylene (VF2-TrFE) copolymer films were directly deposited on degenerated Si (n+, $0.002\;{\Omega}{\cdot}cm$) using by spin coating method. A 1~5 wt% diluted solution of purified vinylidene fluoride-trifluoroethylene (VF2:TrFE = 70:30) in a dimethylformamide (DMF) solvent were prepared and deposited on silicon wafers at a spin rate of 2000 ~ 4000 rpm for 2 ~ 30 seconds. After annealing in a vacuum ambient at 100 ~ $200^{\circ}C$ for 60 min, upper aluminum electrodes were deposited by vacuum evaporation for electrical measurement. X-ray diffraction results showed that the VF2-TrFE films on Si substrates had $\beta$-phase of copolymer structures. The capacitance on highly doped Si wafer showed hysteresis behavior like a butterfly shape and this result indicates clearly that the copolymer films have ferroelectric properties. The typical measured remnant polarization ($P_r$) and coercive filed ($E_c$) values were about $5.7\;{\mu}C/cm^2$ and 710 kV/em, respectively, in an applied electric field of ${\pm}$ 1.5 MV/em. The gate leakage current densities measured at room temperature was less than $7{\times}10^{-7}\; A/cm^2$ under a field of 1 MV/cm.

  • PDF