• Title/Summary/Keyword: vibrating .sample

Search Result 206, Processing Time 0.024 seconds

Electrically and magnetically Characterization for Ferroelectric/Ferrimagnetic ceramics (PZT/Ferrite 합성 세라믹의 전기적.자기적 특성연구)

  • 김장용;오준학;문병무
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.30-33
    • /
    • 2001
  • This thesis deal with ferroelectric and ferrimagnetic materials, PZT/Ferrite ceramics. We conducted test of magnetical and electrical measurement. From this measurement, We obtained tunability and we can control characteristic impedance(Z$_{0}$) from permeability($\mu$) and dielectric constant($\varepsilon$) for impedance matching in transmission line.e.

  • PDF

Magnetic Characteristics of BaFe12-2xCoxTixO19 Particles Prepared by Sol-gel Synthesis (졸-겔 합성에 의한 BaFe12-2xCoxTixO19 미립자의 자기적 특성)

  • 최현승;정지형;박효열;김태옥
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.1
    • /
    • pp.62-68
    • /
    • 2003
  • Ba-ferrite particles added with Co and Ti, which were known well the additives for the control in coercivity, were synthesized by sol-gel method. In the range 90 to 120 minute reaction time, a stable sol solution which showed no change with temperature, pH, viscosity and aging time. After dried and heat treatment of sol solution, Ba-ferrite phase formed at $700^{\circ}C$ with Differential Thermal Analysis(DTA) and X-Ray Diffractometer(XRD) measurement. The crystallinity became to be better with increasing the temperature. It were showed by Scanning Electron Microscopy(SEM) that Ba-ferrite increased to particle sizes as increasing heating temperature and obtained of narrow particles size distribution. Also, magnetic characteristics of Ba-ferrite powders Co and Ti added were observed by a Vibrating Sample Magnetometer(VSM). Saturation magnetization$(M_s)$ was not much changed, however. the coercivity$(H_c)$dramatically dropped with addition of Co and Ti.

Effects of Metal Ion Mole Ratio and Calcination Temperatures on Magnetic Properties and Microstructure of Ba2Co2Fe12O22 Powders Synthesized by Solid State Reaction (고상반응법으로 제조된 Ba2Co2Fe12O22분말의 자기적 성질과 미세구조에 미치는 금속이온몰비와 열처리 온도의 영향)

  • Cho, Kwang-Muk;Nam, In-Tak
    • Journal of the Korean Magnetics Society
    • /
    • v.19 no.6
    • /
    • pp.216-221
    • /
    • 2009
  • Y-type barium ferrite $Ba_2Co_2Fe_{12}O_{22}$ was synthesized by a solid state reaction method. Effects of metal ion mole ratio and calcination temperatures on magnetic properties and microstructures of the synthesized powders were investigated. Phase analysis and microstructure observation were performed with a XRD (X-ray diffractometer) and a FESEM (field effect scanning electron microscope), respectively. Magnetic properties of the powders were measured with a VSM (vibrating sample magnetometer). Single phase Y-type was synthesized when metal ion mole fraction $Fe^{3+}:\;Ba^{2+}:\;Co^{2+}$ was 6 : 1 : 1 and calcination temperature was $1050\;{^{\circ}C}$. High saturation magnetization value of 39.1 emu/g was obtained when metal ion mole fraction $Fe^{3+}:\;Ba^{2+}:\;Co^{2+}$ was 8 : 1 : 1 and calcination temperature was $1200\;{^{\circ}C}$.

Crystallographic and Mossbauer Studies of Magnetic Garnet $Y_{3-x}Bi_xFe_5O_{12}$ by a Sol-Gel Method (Sol-gel 합성에 의한 자성 garnet $Y_{3-x}Bi_xFe_5O_{12}$의 결정학적 및 Mossbauer 분광학 연구)

  • 엄영란;김철성;이재광
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.4
    • /
    • pp.203-209
    • /
    • 1998
  • Crystallographic and magnetic properties of single phase garnet $Y_{3-x}Bi_xFe_5O_{12}$ (x=0.0, 0.25, 0.5, 0.75, 1.0) were studied by using x-ray diffraction, Mossbauer spectroscopy and vibrating sample magnetometer (VSM). Ultra-fine polycrystalline cubic samples have been prepared by sol-gel method. The lattice constant increase linearly with increasing an amount of Bi. Annealing temperature was larger than 800 $^{\circ}C$ for the growth of a single-phase garnet powder. The second phase of garnet, $(BiFeO_3)$, was at 1000 $^{\circ}C$ for x=0.75, and 950 $^{\circ}C$ for x=1.00. From Mossbauer spectroscopy and VSM measurements, the magnetization and the coercivity were decreased and the Curie temperature $Y_{3-x}Bi_xFe_5O_{12}$(x=0.0, 0.25, 0.5, 0.75, 1.0) was slightly increased as increasing the Bi content.

  • PDF

Study of Superparamagnetic Microneedles containing Iron Oxide Nanoparticles (산화철 나노입자를 함유한 초상자성 마이크로니들에 관한 연구)

  • Lee, Seung-Jun
    • Applied Chemistry for Engineering
    • /
    • v.32 no.5
    • /
    • pp.556-561
    • /
    • 2021
  • Recently, iron oxide nanoparticles have been used as the subject of many studies on drug delivery system (DDS) due to their excellent magnetic properties and biocompatibility in response to external magnetic fields. In this study, hyaluronic acid-superparamagnetic microneedles (HA-SMNs) and carboxy methyl cellulose-superparamagnetic microneedles (CMC-SMNs) containing superparamagnetic iron oxide nanoparticles (SIONs) were prepared with HA and CMC as a matrix materials of MNs (microneedles). Various properties of SMNs were then investigated with scanning electron microscopy (SEM), superconducting quantum interference device-vibrating sample magnetometer (SQUD-VSM), frequency mixing magnetic detection (FMMD), and polymer/bio membrane. The SQUID-VSM measurements showed superparamagnetism of HA-SMNs and CMC-SMNs containing SIONs. The FMMD results demonstrated that the signal intensity changed significantly as the concentration of SIONs increased. In addition, SMNs exhibited the average skin permeability intensities on the bio membrane for HA-SMNs and CMC-SMNs were 92.5 and 98.5%, respectively. These results suggested that SMNs could be utilized as deliver materials for a TDDS and MR molecular imaging.

Crystallographic and Magnetic Properties of Li0.7Co0.2Ti0.2V0.2Fe1.7O4 Ferrite

  • Chae, Kwang-Pyo;Kwon, Woo-Hyun;Lee, Jae-Gwang
    • Journal of Magnetics
    • /
    • v.15 no.1
    • /
    • pp.25-28
    • /
    • 2010
  • This study examined the crystallographic and magnetic properties of vanadium-substituted lithium cobalt titanium ferrite, $Li_{0.7}Co_{0.2}Ti_{0.2}V_{0.2}Fe_{1.7}O_4$. Ferrite was synthesized using a conventional ceramic method. The samples annealed below $1040^{\circ}C$ showed X-ray diffraction peaks for spinel and other phases. However, the sample annealed above $1040^{\circ}C$ showed a single spinel phase. The lattice constant of the sample was $8.351\;{\AA}$, which was relatively unaffected by vanadium-substitution. The average grain size after vanadium-substitution was $13.90\;{\mu}m$, as determined by scanning electron microscopy. The M$\ddot{o}$ssbauer spectrum could be fitted to two Zeeman sextets, which is the typical spinel ferrite spectra of $Fe^{3+}$ with A and B sites, and one doublet. From the absorption area ratio of the M$\ddot{o}$ssbauer spectrum, the cation distribution was found to be ($Co_{0.2}V_{0.2}Fe_{0.6})[Li_{0.7}Ti_{0.2}Fe_{1.1}]O_4$. Vibrating sample magnetometry revealed a saturation magnetization and coercivity of 36.9 emu/g and 88.6 Oe, respectively, which were decreased by vanadium-substitution.

Magnetic Properties and the Crystallization of Amorphous Nd-Fe-Ti-B (Nd-Fe-Ti-B 비정질 합금의 자기적 성질 연구)

  • 이승화;안성용;김철성;김윤배;김창석
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.3
    • /
    • pp.140-145
    • /
    • 1997
  • The amorphous state of $NdFe_{10.7}TiB_{0.3}$ and its nanocrystallization have been studied by X-ray diffraction, 모스바우어 spectroscopy, and a vibrating sample magnetometer (VSM), $NdFe_{10.7}TiB_{0.3}$ amorphous ribbons were fabricated by a sigle-roll melt-spinning method. The average hyperfine field $H_{hf}$(T) of the amorphous state shows a temperature dependence of $[H_{hf}(T)-H_{hf}(0)]/H_{hf}(0)=-0.46(T/T_c)^{3/2}-0.34(T/T_c)^{5/2}$ for $T/T_c<0.7$ indicative of spin wave excitation. The quadrupole splitting just above the Curie temperature $T_c$ is 0.46 mm/s, whereas the average quadrupole shift below $T_c$ is zero. The Curie and crystallization temperatures are determined to be $T_c$=380K and $T_x=490K$, respectively, for a heating rate of 5 K/min. The occupied area of nanocrystalline phase at around 770K is about 65%. Above the Curie temperature, VSM data show magnetic moments increases again. The formation of $\alpha$-Fe is the main reason for the increasing moment as conformed with the 모스바우어 measurements.

  • PDF

Effects of Vanadium Doping on Magnetic Properties of Inverse Spinel Fe3O4 Thin Films (역스피넬 Fe3O4 박막의 바나듐 도핑에 따르는 자기적 성질 변화)

  • Kim, Kwang-Joo;Choi, Seung-Li;Park, Young-Ran;Park, Jae-Yun
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.1
    • /
    • pp.18-22
    • /
    • 2006
  • Effects of V substitution of Fe on the magnetic properties of $Fe_3O_4$ have been investigated by x-ray diffraction (XRD), x-ray photoelectron spectroscopy (XPS), conversion electron Mossbauer spectroscopy (CEMS), and vibrating sample magnetometry (VSM) measurements on sol-gel-grown films. XRD data indicates that the $V_xFe_{3-x}O_4$ films maintain cubic structure up to x=1.0 with little change of the lattice constant. Analyses on V 2p and Fe 2p levels of the XPS data indicate that V exist as $V^{3+}$ mostly in the $V_xFe_{3-x}O_4$ films with the density of $V^{2+}$ ions increasing with increasing V content. Analyses on the CEMS data indicate that $V^{3+}$ ions substitute tetrahedral $Fe^{3+}$ sites mostly, while $V^{2+}$ ions octahedral $Fe^{2+}$ sites. Results of room-temperature VSM measurements on the films reveal that the saturation magnetization for the x=0.14 sample is larger than that of $Fe_3O_4$, while it becomes smaller than that of $Fe_3O_4$ for $x{\geq}0.5$. The coercivity of the $V_xFe_{3-x}O_4$ films is found to increase with x, attributed to the increase of anisotropy by the substitution of $V^{2+}(d^3)$ ions into the octahedral sites.

Immobilization of the Thenoyltrifluoroacetone on Sodium Dodecyl Sulfate Modified Magnetite Nanoparticles for Magnetic Solid Phase Extraction of Pb (II) from Water Samples

  • Sadeghi, Meysam;Yekta, Sina;Babanezhad, Esmaeil
    • Korean Chemical Engineering Research
    • /
    • v.54 no.5
    • /
    • pp.636-647
    • /
    • 2016
  • Magnetite nanoparticles ($Fe_3O_4$ NPs) were synthesized by co-precipitating method under optimized condition. The $Fe_3O_4$ NPs coated with sodium dodecyl sulfate-thenoyltrifluoroacetone ($Fe_3O_4$ NPs-SDS-TTFA) were then exerted as the magnetic solid phase extraction (MSPE) adsorbent for the extraction process prior to introducing to a flame atomic adsorption spectrometry (FAAS). The synthesized $Fe_3O_4$ NPs-SDS-TTFA were applied for the extraction of Pb(II) ions from different water samples. The characterization studies of nanoparticles were performed via scanning electron microscopy-energy dispersive micro-analysis (SEM-EDAX), X-ray diffraction (XRD) and vibrating sample magnetometer (VSM) techniques. The substantial parameters affecting the extraction efficiency were surveyed and optimized. A dynamic linear range (DLR) of $10-400{\mu}g\;L^{-1}$ was obtained and the limit of detection (LOD, n=7) and relative standard deviation (RSD%, n= 6, $C=20{\mu}g\;L^{-1}$) were found to be $2.3{\mu}g\;L^{-1}$ and 1.9%, respectively. According to the results, the proposed method successfully applied for the extraction of Pb(II) ions from different environmental water samples and satisfactory results achieved.

Effects of Sheet Thickness on the Electromagnetic Wave Absorbing Characterization of Li0.375Ni0.375Zn0.25-Ferrite Composite as a Radiation Absorbent Material

  • Kim, Dong-Young;Yoon, Young-Ho;Jo, Kwan-Jun;Jung, Gil-Bong;An, Chong-Chul
    • Journal of electromagnetic engineering and science
    • /
    • v.16 no.3
    • /
    • pp.150-158
    • /
    • 2016
  • This paper reports on a study of LiNiZn-ferrite composite as a radiation absorbent material (RAM). The electromagnetic (EM) wave absorbers are composed of an EM wave absorbing material and a polymeric binder. The surface morphology, chemical composition, weight percent of the ferrite composite of the toroid sample, magnetic properties, and return loss are investigated using field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDX), X-ray photoelectron spectroscopy (XPS), thermogravimetric analysis (TGA), vibrating sample magnetometer (VSM), and network analyzer. For preparing the absorbing sheet, chlorinated polyethylene (CPE) is used as a polymeric binder. The EM wave absorption properties of the prepared samples were studied at 4 - 8 GHz. We can confirm the effects of the thickness of the samples for absorption properties. An absorption bandwidth of more than a 10-dB return loss shifts toward a lower frequency range along with an increase in the thickness of the absorber.