• 제목/요약/키워드: vacuum kinetic spray(aerosol deposition)

검색결과 2건 처리시간 0.017초

진공상온분사(VKS) 공정에서의 비행입자 가속 기구 및 속도제어를 위한 가스 유량 효과에 관한 연구 (Research on Acceleration Mechanism of Inflight Particle and Gas Flow Effect for the Velocity Control in Vacuum Kinetic Spray Process)

  • 박형권;권주혁;이일주;이창희
    • 한국재료학회지
    • /
    • 제24권2호
    • /
    • pp.98-104
    • /
    • 2014
  • Vacuum kinetic spray(VKS) is a relatively advanced process for fabricating thin/thick and dense ceramic coatings via submicron-sized particle impact at room temperature. However, unfortunately, the particle velocity, which is an important value for investigating the deposition mechanism, has not been clarified yet. Thus, in this research, VKS average particle velocities were derived by numerical analysis method(CFD: computational fluid dynamics) connected with an experimental approach(SCM: slit cell method). When the process gas or powder particles are accelerated by a compressive force generated by gas pressure in kinetic spraying, a tensile force generated by the vacuum in the VKS system accelerates the process gas. As a result, the gas is able to reach supersonic speed even though only 0.6MPa gas pressure is used in VKS. In addition, small size powders can be accelerated up to supersonic velocity by means of the drag-force of the low pressure process gas flow. Furthermore, in this process, the increase of gas flow makes the drag-force stronger and gas distribution more homogenized in the pipe, by which the total particle average velocity becomes higher and the difference between max. and min. particle velocity decreases. Consequently, the control of particle size and gas flow rate are important factors in making the velocity of particles high enough for successful deposition in the VKS system.

상온진공과립분사에 의한 TiO2 코팅층에 미치는 공정변수의 영향 (Effect of processing parameters on TiO2 film by room temperature granule spray in vacuum)

  • 김한길;박윤수;방국수;박동수;박찬
    • 한국결정성장학회지
    • /
    • 제27권1호
    • /
    • pp.22-27
    • /
    • 2017
  • 상온진공과립분사에 의해 slide glass 기판 위에 $1{\sim}30{\mu}m$의 두께를 가진 $TiO_2$ 코팅층을 제조하였다. $TiO_2$ granule 과립분말은 $1.5{\mu}m$의 평균 입도를 가진 Rutile 형태로 $600^{\circ}C$에서 4시간 하소 과정을 거쳤다. 공정변수로서는 반복횟수, 가스유량속도 및 과립투입속도로 하여 코팅층을 제조하였다. 반복횟수가 증가할수록 코팅층의 두께는 비례적으로 증가하였다. 이는 반복횟수의 증가에도 코팅층이 형성될 수 있는 적절한 운동에너지가 작용한 것을 알 수 있다. 가스유량속도에 따라 코팅층의 두께도 증가하였으나 1.7 V의 분말공급량에서는 25 LPM의 유량까지는 코팅층의 두께가 증가했지만, 35 LPM(L/min)의 유량에서는 두께가 감소하였다. 15 LPM의 낮은 유량속도에서는 분말공급량이 충분하더라도 성막에 필요한 운동에너지의 부족으로 코팅 층의 두께가 비례적으로 증가하지 않았다. $TiO_2$ 코팅층의 미세구조는 주사전자현미경 및 고성능 투과전자현미경을 이용하여 분석하였다.