RF magnetron sputtering 기술로 증착한 Undoped ZnO 박막의 증착 압력에 따른 구조적, 광학적 특성 (The Structural and Optical Properties of Undoped ZnO Thin Films Deposited by RF Magentron Sputtering System as Functions of Working Pressures)

  • 김재천;김명춘;김좌연
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.229-230
    • /
    • 2008
  • We have studied the structural and optical properties of ZnO thin film deposited on glass by RF magnetron sputtering as functions of working pressures. The grain sizes were decreased as the working pressures were increased. The average optical transmissions over all exceeded 80% for ZnO films deposited in 20, 25 and 300m torr working pressures. And the transmission spectra patterns were almost same. While the transmission spectra pattern of ZnO film deposited in 35nm torr was different with other spectra patterns obtained in 20, 25 and 30nm torr working pressures.

  • PDF

Undoped ZnO 박막에 Ampoule-tube 방법을 이용한 P와 As의 확산과 p형 ZnO 박막의 전기적 특성 (Phosphorus and Arsenic Diffusion used by Ampoule-tube Method into Undoped ZnO Thin Films and the Electrical Properties of p-type ZnO Thin Films)

  • 소순진;왕민성;박춘배
    • 한국전기전자재료학회논문지
    • /
    • 제18권11호
    • /
    • pp.1043-1047
    • /
    • 2005
  • To investigate the electrical properties of the ZnO films which are interested in the next generation of short wavelength LEDs and Lasers, our ZnO thin films were deposited by RF sputtering system. At sputtering process of ZnO thin films, substrate temperature, work pressure respectively is $300^{\circ}C$ and 5.2 mTorr, and the purity of target is ZnO 5N. The thickness of ZnO thin films was about $2.1\;{\mu}m$ at SEM analysis after sputtering process. Phosphorus (P) and arsenic (As) were diffused into the undoped ZnO thin films sputtered by RF magnetron sputtering system in ampoule tube which was below $5\times10^{-7}$ Torr. The dopant sources of phosphorus and arsenic were $Zn_3P_2$ and $ZnAs_2$. Those diffusion was perform at 500, 600, and $700^{\circ}C$ during 3 hr. We found the diffusion condition of the conductive ZnO films which had n- and p-type properties. Our ZnO thin film has not only very high carrier concentration of above $10^{17}/cm^3$ but also low resistivity of below $2.0\times10^{-2}\;{\Omega}cm$.

MgO 또는 ZnO를 첨가한 $LiNbO_3$단결정 성장 및 특성 : (II) 전기적 및 광학적 특성 (Single crystals growth and properties of $LiNbO_3$ doped with MgO or ZnO : (II) The electrical and optical properties)

  • 조현;심광보;오근호
    • 한국결정성장학회지
    • /
    • 제6권4호
    • /
    • pp.532-542
    • /
    • 1996
  • Floating zone(FZ)법으로 육성하고 annealing한 undoped $LiNbO_3$ 단결정 및 MgO 또는 ZnO를 첨가한 $LiNbO_3$ 단결정의 전기적,광학적 특성을 조사하였다. 전기전도도, 유전율 및 전이온도, 전기.기계결합계수등의 전기적 특성과 광투과율, 굴절율 등의 광학적 특성을 측정하였으며, 비선형 광학특성의 척도라 할 수 있는 비선형 굴절율을 이론적으로 계산하였다. Undoped $LiNbO_3$ 단결정과 MgO 또는 ZnO를 첨가한 $LiNbO_3$ 단결정의 전기적, 광학적 특성을 비교함으로서 MgO 또는 ZnO의 첨가가 $LiNbO_3$ 단결정의 전기적 및 광학적 특성에 미치는 영향을 조사하였다.

  • PDF

PLD법을 이용한 Buffer Layer 증착온도에 따른 As-doped ZnO 박막의 특성 (Characteristics of As-doped ZnO thin films with various buffer layer temperatures prepared by PLD method)

  • 이홍찬;심광보;오영제
    • 센서학회지
    • /
    • 제15권2호
    • /
    • pp.84-89
    • /
    • 2006
  • Highly concentrated p-type ZnO thin films can be obtained by doping of N, P and As elements. In this study, undoped ZnO buffer layers were prepared on a (0001) sapphire substrate by a ultra high vaccum pulsed laser deposition(UHV-PLD) method. ZnO buffer layers were deposited with various deposition temperature($400{\sim}700^{\circ}C$) at 350 mtorr of oxygen working pressure. Arsenic doped(1 wt%) ZnO thin films were deposited on the ZnO buffer layers by UHV-PLD. Crystallinity of the samples were evaluated by X-ray diffractometer and scanning electron microscopy. Optical, electrical properties of the ZnO thin films were estimated by photoluminescence(PL) and Hall measurements. The optimal condition of the undoped ZnO buffer layer for the deposition of As-doped ZnO thin films was at $600^{\circ}C$ of deposition temperature.

Preparation and EPR Characteristics of $ZnGa_2O_4$ : Mn Phosphor

  • 정하균;박도순;박윤창
    • Bulletin of the Korean Chemical Society
    • /
    • 제19권12호
    • /
    • pp.1320-1325
    • /
    • 1998
  • ZnGa2O4: Mn phosphors were prepared by a new chemical process, and their photoluminescence and electron paramagnetic resonance characteristics were investigated. The chemical method showed a low temperature formation of phosphors and a rod-type shape of particles. The strong ultraviolet emission was observed in the undoped ZnGa2O4 phosphor, while strong green emission in the Mn2+-activated ZnGa2O4 phosphor. The green emission intensity of the phosphor prepared by the chemical method was much stronger than that prepared by the conventional method. This difference with preparation methods was interpreted as due to the difference in the distribution of Mn2+ in the host lattice. From EPR results, it was explained that the line intensity of the undoped ZnGa2O4 is associated with the electrical conductivity of this material and the concentration quenching of green luminescence of ZnGa2O4: Mn at higher Mn2+ concentration is attributed to the coupling by exchange interaction between Mn2+ ions.

Properties of Aluminum Doped Zinc Oxide Thin Film Prepared by Sol-gel Process

  • Yi, Sung-Hak;Kim, Jin-Yeol;Jung, Woo-Gwang
    • 한국재료학회지
    • /
    • 제20권7호
    • /
    • pp.351-355
    • /
    • 2010
  • Transparent conducting aluminum-doped ZnO thin films were deposited using a sol-gel process. In this study, the important deposition parameters were investigated thoroughly to determine the appropriate procedures to grow large area thin films with low resistivity and high transparency at low cost for device applications. The doping concentration of aluminum was adjusted in a range from 1 to 4 mol% by controlling the precursor concentration. The annealing temperatures for the pre-heat treatment and post-heat treatment was $250^{\circ}C$ and 400-$600^{\circ}C$, respectively. The SEM images show that Al doped and undoped ZnO films were quite uniform and compact. The XRD pattern shows that the Al doped ZnO film has poorer crystallinity than the undoped films. The crystal quality of Al doped ZnO films was improved with an increase of the annealing temperature to $600^{\circ}C$. Although the structure of the aluminum doped ZnO films did not have a preferred orientation along the (002) plane, these films had high transmittance (> 87%) in the visible region. The absorption edge was observed at approximately 370 nm, and the absorption wavelength showed a blue-shift with increasing doping concentration. The ZnO films annealed at $500^{\circ}C$ showed the lowest resistivity at 1 mol% Al doping.

Defect-related yellowish emission of un doped ZnO/p-GaN:Mg heterojunction light emitting diode

  • Han, W.S.;Kim, Y.Y.;Ahn, C.H.;Cho, H.K.;Kim, H.S.;Lee, J.H.
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.327-327
    • /
    • 2009
  • ZnO with a large band gap (~3.37 eV) and exciton binding energy (~60 meV), is suitable for optoelectronic applications such as ultraviolet (UV) light emitting diodes (LEDs) and detectors. However, the ZnO-based p-n homojunction is not readily available because it is difficult to fabricate reproducible p-type ZnO with high hall concentration and mobility. In order to solve this problem, there have been numerous attempts to develop p-n heterojunction LEDs with ZnO as the n-type layer. The n-ZnO/p-GaN heterostructure is a good candidate for ZnO-based heterojunction LEDs because of their similar physical properties and the reproducible availability of p-type GaN. Especially, the reduced lattice mismatch (~1.8 %) and similar crystal structure result in the advantage of acquiring high performance LED devices. In particular, a number of ZnO films show UV band-edge emission with visible deep-level emission, which is originated from point defects such as oxygen vacancy, oxygen interstitial, zinc interstitial[1]. Thus, defect-related peak positions can be controlled by variation of growth or annealing conditions. In this work, the undoped ZnO film was grown on the p-GaN:Mg film using RF magnetron sputtering method. The undoped ZnO/p-GaN:Mg heterojunctions were annealed in a horizontal tube furnace. The annealing process was performed at $800^{\circ}C$ during 30 to 90 min in air ambient to observe the variation of the defect states in the ZnO film. Photoluminescence measurements were performed in order to confirm the deep-level position of the ZnO film. As a result, the deep-level emission showed orange-red color in the as-deposited film, while the defect-related peak positions of annealed films were shifted to greenish side as increasing annealing time. Furthermore, the electrical resistivity of the ZnO film was decreased after annealing process. The I-V characteristic of the LEDs showed nonlinear and rectifying behavior. The room-temperature electroluminescence (EL) was observed under forward bias. The EL showed a weak white and strong yellowish emission colors (~575 nm) in the undoped ZnO/p-GaN:Mg heterojunctions before and after annealing process, respectively.

  • PDF

RF Sputter 방법으로 제조한 투명전도막 ZnO 특성 (Properties of Transparent Conducting Zinc Oxide Films Prepared by RF Sputtering)

  • 최병호
    • 한국재료학회지
    • /
    • 제2권5호
    • /
    • pp.360-365
    • /
    • 1992
  • Ga 첨가효과 및 Sputter 제조조건이 전기적 특성에 미치는 영향을 고찰하기 위해 ZnO분말과 G$a_2O_3$분말을 소결하여 타겟트를 제조하여 Sputter법으로 유리기판에 Ga-doped ZnO 다결정박막을 제조하였다. RF 전력밀도, 아르곤 개스압력 및 Ga 함유량등을 최적화한 후 제조한 투명한 Ga-doped ZnO 박막의 비저항은 1$0^{-3}$ohm-cm이며, undoped 및 Ga-doped ZnO 박막의 전자농도는 각 $10^{18}$, $10^{21}$/c$m^2$이였다. 공기와 질소분위기에서 열처리를 행하였을 때 Ga-doped ZnO 박막의 비저항은 $10^{2}$ order 증가하였다. 가시광영역의 투과율은 80% 이상이였으며, Ga 함유량이 증가하면 optical band gap도 넓어졌다.

  • PDF

MgO 또는 ZnO를 첨가한 $LiNbO_{3}$ 단결정 성장 및 특성 : (I) 단결정 성장 및 결함구조 (Single crystals growth and properties of $LiNbO_{3}$ doped with MgO or ZnO : (I) Single crystals growth and their defect structure)

  • 조현;심광보;오근호
    • 한국결정성장학회지
    • /
    • 제6권3호
    • /
    • pp.368-376
    • /
    • 1996
  • 균일한 조성과 doping 효과를 얻을 수 있는 floating zone(FZ)법으로 조화용융조성의 undoped $LiNbO_{3}$ 및 5 mol%의 MgO 또는 ZnO를 각각 첨가한 $LiNbO_{3}$ 단결정을 육성하였다. 결정성장시 최적성장조건을 실험적으로 확립하였으며, 결정내에 존재하는 domain 구조, 전위구조, slip band, 미세쌍정등의 결함구조를 조사 및 분석하였다.

  • PDF