Luminescence Characteristics of Blue Phosphor and Fabrication of a UV-based White LED (UV 기반 백색 LED용 청색 형광체의 발광특성 및 백색 LED 제조)

  • Jung, Hyungsik;Park, Seongwoo;Kim, Taehoon;Kim, Jongsu
    • Korean Journal of Optics and Photonics
    • /
    • v.25 no.4
    • /
    • pp.216-220
    • /
    • 2014
  • We have synthesized a $CaMgSi_2O_6:Eu^{2+}$ blue phosphor via a solid-state reaction method. The $CaMgSi_2O_6:Eu^{2+}$ phosphor has monoclinic structure with a space group of C2/c (15), and an emission band peaking at 450 nm (blue) due to the $4f^7-4f^65d$ transition of the $Eu^{2+}ion$. The emission intensity at $100^{\circ}C$ is 54% of the value at room temperature. A white LED was fabricated by integrating a UV LED (400 nm) with our blue phosphor plus two commercial green and red phosphors. The white LED shows a color temperature of 3500 K with a color rendering index of 87 (x = 0.3936, y = 0.3605), and a luminous efficiency of 18 lm/W. The white LED shows a luminance maintenance of 97% after operation at 350 mA for 400 hours at $85^{\circ}C$.

UV Absorption of Nano-thick $TiO_2$ Prepared Using an ALD (ALD 방법으로 제조된 나노급 $TiO_2$에 의한 자외선 차단효과 연구)

  • Han, Jeung-Jo;Song, Oh-Sung;Ryu, Ji-Ho;Yoon, Ki-Jeong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.8 no.4
    • /
    • pp.726-732
    • /
    • 2007
  • We fabricated UV absorption functional $10{\sim}50nm-TiO_{2-x}/quartz$ structures layer using ALD (atomic layer deposition) method. We deposited $10nm-TiO_{2-x}$ layer on quartz substrate using ALD, and film thickness was determined by an ellipsometer. The others specimen thickness was controlled by ALD time lineally. We characterized controlling phase UV and visible optical property using an X-ray difractometer, a UV-VIS-IR spectrometer and a digital camera. $ALD-TiO_{2-x}$ layers were non-stoichiometric $TiO_{2-x}$ form and amorphous phases comparing with bulk $TiO_2$. While the conventional bulk $TiO_2$ had band gap of $3.0{\sim}3.2eV$ resulting in absorption edges at 380 nm and 415 nm, $ALD-TiO_{2-x}$ layers showed absorption edges at 197 nm and 250 nm. Therefore, our nano-thick $ALD-TiO_{2-x}$ was able to absorb shorter UV region and showed excellent transmittance in visible region. Our result implies that our newly proposed nano-thick $TiO_{2-x}$ using ALD process may improve transmittance in visible rays and be able to absorb shorter UV light effectively.

  • PDF

A Study on the Tannin Weighting of Silk (견의 탄닌가공에 관한 연구)

  • Jeong, In-Mo;Lee, Yong-U;Lee, Gi-Won
    • Journal of Sericultural and Entomological Science
    • /
    • v.28 no.1
    • /
    • pp.72-78
    • /
    • 1986
  • The studies were performed to investigate the optimum conditions for tannic processing of silk by use Chinese Gallotannin and synthesized tannic acid, which are aimed at weighting, dyeing and physical properties of tannin treated silk. 1. It was reasonable that the concentration of tannin solution is 30 grams per liter of Chinese Gallotannin, 15 grams per liter of tannic acid for the efficient weighting of processed silk. The temperature and time for tannin treatment was optimum at 80$^{\circ}C$, 60 minutes and the acidity of tannin solution at pH 2 to 3. 2. In dyeing the tannintreated silk by Acid dye Orange II, the temperature and time was reasonable at 60$^{\circ}C$, 90 minutes to control the desorption of tannin components weighted onto silk. 3. The colour differences ($\Delta$E) of dyed silk fabric by soaping could be remarkably narrowed by tannin treatment, resulting in improving the washing fastness of tannin treated silk by two grades more than that of untreated one. 4. The light fastness of tannin treated silk could be drastically improved by reducing the dye-loss of dyed silk fabric which was coused from the Ultra-violet ray irrdiation. 5. The rubbing fastness and water repellency of tannin treated silk was at the same level with that of untreated one. However, the Drape coefficient of tannin treated silk was decreased more than that of untreated one, which is closely related with fabric softness and dressing appearence.

  • PDF

Development of Saccharomyces cerevisiae Strains with High RNA Content (리보핵산을 다량으로 함유하는 Saccharomyces cerevisiae 균주의 개발)

  • Kim, Jae-Sik;Kim, Jin-Wook;Shim, Won;Min, Byoung-Cheol;Kim, Jung-Wan;Park, Kwan-Hwa;Pek, Un-Hua
    • Korean Journal of Food Science and Technology
    • /
    • v.31 no.2
    • /
    • pp.465-474
    • /
    • 1999
  • RNase activity of Saccharomyces cerevisiae ATCC 7754 was investigated to obtain strains with high ribonucleic acid (RNA) content. The yeast strain contained two RNase activities; an acidic RNase with a optima of pH $3{\sim}4$ and an alkaline RNase with a optima pH 9. The acidic RNase activity was inhibited by $0.08\;M\;HgCl_{2}$ most drastically. The alkaline RNase activity was inhibited by 2.0 M NaCl or KCl, while enhanced by addition of $0.05\;M\;CaCl_{2},\;0.02\;M\;ZnSO_{4},\;or\;0.008\;M\;HgCl_{2}$. Various mutants of Saccharomyces cerevisiae ATCC 7754 were isolated by ethylmethane sulfonate (EMS) treatment or $\gamma$-ray/ultra violet irradiation. Among the mutants that were sensitive to high concentration of KCl which inhibits alkaline RNase, B24 was selected for high RNA content per culture volume. Growth characteristics of the mutant were comparable to those of the mother strain with optimum growth at pH $4.5{\sim}5.5$. The mutant accumulated higher content of RNA than the mother strain when glucose was used as the carbon source. However, both growth rate and total RNA content of the mutant were higher in molasses medium than in glucose medium. RNA content of the mutant increased rapidly during the early stage of growth, and then decreased gradually until the culture reached stationary phase by a fed-batch culture in a 5 L jar fermenter. Maximal cell harvest and the final RNA content using the mutant B24 were 69.6 g/L culture broth and 19.8 g/100 g of the dry cell while those using the mother strain were 68 g/L culture broth and 16.1 g/100 g of dry cell, respectively.