DLC 및 Re-Ir 코팅에 의한 성형용 코어면의 코팅 효과 (Coating Effect of Molding Core Surface by DLC and Re-Ir Coating)

  • 김현욱;차두환;이동길;김상석;김혜정;김정호
    • 한국정밀공학회지
    • /
    • 제26권1호
    • /
    • pp.51-56
    • /
    • 2009
  • Recently, with the increasing lightness and miniaturization of high resolution camera phones, the demand for aspheric glass lens has increased because plastic and spherical lens are unable to satisfy the required performance. An aspheric glass lens is fabricated by the high temperature and pressure molding using a tungsten carbide molding core, so precision grinding and coating technology for the molding core surface are required. This study investigates the effect of diamond-like carbon (DLC) and rhenium-iridium (Re-Ir) coating For aspheric molding core surface. The grinding conditions of the tungsten carbide molding core were obtained by design of experiments (DOE) for application in the ultra precision grinding process of the tungsten carbide molding core of the aspheric glass lens used in 5 megapixel, $4{\times}$ zoom camera phone modules. A tungsten carbide molding core was fabricated under this grinding condition and coated with the DLC and Re-Ir coating. By measurements, the effect of DLC and Re-Ir coating on the form accuracy and surface roughness of molding coer was evaluated.

Characteristics of tungsten coated graphite using vacuum plasma spraying method

  • Lim, Hyeonmi;Kang, Boram;Kim, Hoseok;Hong, Bong Guen
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.200.1-200.1
    • /
    • 2016
  • Tungsten coatings on the graphite (CX-2320) were successfully deposited using the vacuum plasma spraying (VPS) method. An optimum coating procedure was developed and coating thicknesses of $409{\mu}m$ (without an interlayer) and $378{\mu}m$ (with an interlayer) were obtained with no cracks and no signs of delamination. The mechanical characteristics and microstructure of the tungsten coating layers were investigated using a Vickers hardness tester, FE-SEM, EDS, and XRD. The effect of a titanium interlayer on the properties of the tungsten coating was investigated. It was shown that the titanium interlayer prevented the diffusion of carbon to the tungsten layer, thereby suppressing the formation of tungsten carbide. Vickers hardness data yielded values that were 62.5 ~ 80.46% of those for bulk tungsten, indicating that tungsten coatings on graphite can be utilized as a plasma-facing material. High heat flux tests were performed by using thermal plasma with a maximum flux of $10MW/^2$. Vickers hardness after the heat flux test is performed to see a change in the mechanical properties. The formationof a tungsten carbide and the effect of the titanium interlayer for the diffusion barrier are investigated by using energy dispersion spectroscopy (EDS).

  • PDF

Microstructure analysis of DLC thin film fabricated by filtered arc ion plating method

  • Park, Y.P.;Kim, T.G.;Cheon, M.W.
    • Journal of Ceramic Processing Research
    • /
    • 제13권spc2호
    • /
    • pp.363-367
    • /
    • 2012
  • DLC (diamond liked carbon) coating of the tungsten carbide (WC) alloy core surface for molding a glass aspheric lens improves the quality of glass lens and the molding core and is characterized by high hardness, high elasticity, abrasion resistance and chemical stability. In this study, the effect of DLC coating of a thin film by means of the filtered AIP (arc ion plating) technique was examined on Ra and shape of the coated surface. Roughness before and after DLC coating was measured and the result showed that the roughness was improved after coating as compared to before coating. It was observed that DLC coating of the WC alloy core surface for molding had an effect on improving the roughness and shape of the core surface. It is considered that this will have an effect on improving abrasion resistance and the service life of the core surface.

탄소섬유 강화 복합재 가공용 드릴 공구 개발 및 홀 가공성 평가 (Development of a Drill Tool for CFRP Machining and Evaluation of Drilling Processing)

  • 사민우
    • 한국기계가공학회지
    • /
    • 제19권3호
    • /
    • pp.8-13
    • /
    • 2020
  • Carbon fiber-reinforced plastics (CFRPs) are extremely strong and light fiber-reinforced plastics containing carbon fibers. CFRPs can be expensive to produce, but are commonly used wherever high strength-to-weight ratio and rigidity are required, such as in the aerospace, automotive, and ship superstructure industries. In CFRP drilling, the tool performance greatly varies depending on the tool shapes, cutting conditions, and diamond coating. This study developed a new type of tungsten carbide drill with multi-blade edges to evaluate the surface quality of CFRP materials according to the coating thickness of diamond-coated drills. Experiments on tool wear, surface roughness, and burr formation were conducted. The bore exit quality of a 12 mμ -coated drill was better than that of a 6 mμ -coated drill. The superior effects of the 12 mμ -coated drill and the good surface quality of CFRP were also demonstrated.

초경합금에 FVAS로 코팅한 DLC 박막의 특성 (Characteristic of DLC Thin Film Fabricated by FVAS Method on Tungsten Carbide)

  • 천민우;박용필;김태곤;이호식
    • 한국전기전자재료학회논문지
    • /
    • 제24권10호
    • /
    • pp.812-816
    • /
    • 2011
  • An optical lens is usually produced in the manner of high temperature compression molding with tungsten carbide alloy molding cores, it is necessary to develop and study technology for super-precision processing of molding cores and coating the core surface. As main methods used in surface improvement technologies using thin film, DLC present high hardness, chemical stability, and outstanding durability of abrasion to be extensively applied in various industrial fields. In this study, the effect of DLC coating of a thin film by means of the FVAS (filtered vacuum arc source) analyzed the characteristics of thin film. Surface roughness before and after DLC coating was measured and the result showed that the surface roughness was improved after coating as compared to before coating. In conclusion, it was observed that DLC coating of the ultra hard alloy core surface for molding had an effect on improving the surface roughness and shape of the core surface. It is considered that this will have an effect on improving abrasion resistance and the service life of the core surface.

고화소 카메라폰 모듈을 위한 Glass 렌즈 성형용 Silicon Carbide 코어의 초정밀 가공에 관한 연구 (A Study on Ultra Precision Grinding of Silicon Carbide Molding Core for High Pixel Camera Phone Module)

  • 김현욱;김정호;;곽태수;정상화
    • 한국정밀공학회지
    • /
    • 제27권7호
    • /
    • pp.117-122
    • /
    • 2010
  • Recently, aspheric glass lens molding core is fabricated with tungsten carbide(WC). If molding core is fabricated with silicon carbide(SiC), SiC coating process, which must be carried out before the Diamond-Like Carbon(DLC) coating can be eliminated and thus, manufacturing time and cost can be reduced. Diamond Like Carbon(DLC) is being researched in various fields because of its high hardness, high elasticity, high durability, and chemical stability and is used extensively in several industrial fields. Especially, the DLC coating of the molding core surface used in the fabrication of a glass lens is an important technical field, which affects the improvement of the demolding performance between the lens and molding core during the molding process and the molding core lifetime. Because SiC is a material of high hardness and high brittleness, it can crack or chip during grinding. It is, however, widely used in many fields because of its superior mechanical properties. In this paper, the grinding condition for silicon carbide(SiC) was developed under the grinding condition of tungsten carbide. A silicon carbide molding core was fabricated under this grinding condition. The measurement results of the SiC molding core were as follows: PV of 0.155 ${\mu}m$(apheric surface) and 0.094 ${\mu}m$(plane surface), Ra of 5.3 nm(aspheric surface) and 5.5 nm(plane surface).

비구면 Glass 렌즈 성형용 초경합금(WC) 코어의 DLC 코팅 효과 (DLC Coating Effect of WC Core Surface for Glass Molding Lens)

  • 김현욱;정상화;박용필;김상석;김혜정;김정호
    • 한국전기전자재료학회논문지
    • /
    • 제19권11호
    • /
    • pp.1050-1054
    • /
    • 2006
  • There have been intensive and continuous efforts in the field of DLC coating process because of their feature, like high hardness, high elasticity, abrasion resistance and chemical stability and have been applied widely the industrial areas. In this research, optimal grinding condition was investigated using Microlens Process Machine for the development of aspheric glass lens which is to be used for mobile phone module with 3 mega pixel and 2.5X optical zoom, and tungsten carbide(WC) mold cote was manufactured using high performance ultra precision machining and the effects of DLC coating on the form accuracy(PV) and surface roughness(Ra) of WC mold core was evaluated.

임플랜트 지대주 나사의 텅스텐 카바이드/탄소 코팅이나사풀림에 미치는 영향 (Influence of tungsten carbide/carbon coating of implant-abutment screw on screw loosening)

  • 박재경;정창모;전영찬;윤지훈
    • 대한치과보철학회지
    • /
    • 제46권2호
    • /
    • pp.137-147
    • /
    • 2008
  • 임플랜트 보철물에서 각 구성 요소를 연결하는 나사 풀림 현상이 흔히 발생하고 있다. 나사 풀림을 최소화하기 위해서 연결 구성 부품 사이의 압축력을 최대로 하는 것이 중요한데, 나사 신장의 허용 한계 내에서 조임회전력을 증가시켜 나사 내부의 인장력 즉 전하중을 극대화하기 위해서는 마찰 계수를 감소시켜 초기 조임회전력의 손실을 최소화해야 한다. 건조 윤활제를 나사 표면에 코팅한 나사들이 전하중을 증가시키고 나사 풀림을 감소시키나 나사의 반복체결에 따른 코팅표면의 마모가 문제점으로 지적되고 있다. 최근 내마모성이 우수하며 동시에 나사의 마찰 저항을 최소화할 수 있는 텅스텐 카바이드/탄소 코팅을 이용한 나사가 임상에 사용되고 있으나 실제적으로 연결부 안정성에 미치는 영향에 관한 연구는 미미한 편이다. 이에 본 연구에서는 external butt joint 형태를 가지는 US II 시스템과 one stage용 8도의 internal cone 연결형태의 SS II 시스템 및 11도의 internal cone 연결형태의 GS II 시스템에서 티타늄 합금 나사의 텅스텐 카바이드/탄소 코팅이 지대주 나사 풀림에 미치는 영향을 알아보기 위하여 100만 회 반복 하중 전후의 풀림회전력 및 상실률을 비교한 결과 다음과 같은 결론을 얻었다. 1. 초기 풀림회전력은 티타늄 합금나사보다 텅스텐 카바이드/탄소 코팅 나사를 사용한 경우 작게 나타났으며 (P<.01), 동일 나사를 사용한 경우에는 임플랜트 시스템 간에 차이가 없었다 (P>.05). 2. 반복하중에 따른 풀림회전력의 상실률은 두 나사 모두에서 external butt joint 형태의 US II 시스템이 internal cone 연결형태의 SS II 와 GS II 시스템 보다 크게 나타났으나, SS II 와 GS II 시스템 사이에는 차이를 보이지 않았다 (P<.01). 3. 텅스텐 카바이드/탄소 코팅 나사를 사용한 경우 티타늄 합금 나사에 비해 모든 시스템에서 반복하중 후 풀림회전력 상실률이 작게 나타났으며 (P<.01), 코팅 나사 사용으로 인한 상실률의 감소차는 임플랜트 시스템 간에 차이를 보이지 않았다 (P>.05).

임플랜트 지대주 나사의 텅스텐 카바이드/탄소 코팅이 전하중에 미치는 영향에 관한 연구 (INFLUENCE OF TUNGSTEN CARBIDE/CARBON COATING ON THE PRELOAD OF IMPLANT ABUTMENT SCREWS)

  • 최진욱;정창모;전영찬;임장섭;정희찬;엄태관
    • 대한치과보철학회지
    • /
    • 제44권2호
    • /
    • pp.229-242
    • /
    • 2006
  • Statement of problem: In order to increase preload with reducing the friction coefficient, abutment screws coated with pure gold and Teflon as dry lubricant coatings have been introduced. But the reported data indicate that if screw repeated tightening and loosening cycle, an efficiency of increasing preload was decreased by screw surface wearing off. Purpose: This study was to evaluate the influence of tungsten carbide/carbon coating, which has superior hardness and frictional wear resistance, on the preload of abutment screws and the stability of coating surface after repeated closures. Material and method: The rotational values of abutment screws and the compressive forces between abutment and fixture were measured in implant systems with three different joint connections, one external butt joint and two internal cones. Moreover the stability and the alteration of coating surface were examined by comparison of the compressive force and the removable torque values during 10 consecutive trials, observation with scanning electron microscope and analyzed the elemental composition with energy dispersive x-ray spectroscopy Results and conclusion: 1. Application of coating resulted in significant increase of compressive force in all implant systems(P<.05). The increasing rate of compressive force by coating in external butt joint was gloater than those in internal cones (P<.05). 2. Coated screw showed the significant additional rotation compared to non-coated screw in all implant systems (P<.05). There were no significant differences in the increasing rate of rotation among implant systems (P>.05). 3. Removable torque values were greater with non-coated screw than that with coated screw (P<.05). 4. Coated screw showed insignificant variations in the compressive forces during 10 consecutive trials(P>.05) 5. After repeated trials, the surface layer of coated screw was maintained relatively well. However surface wearing and irregular titanium fragments were found in non-coated screw.