Fatigue Behavior of K-Joint Structure for API 2W Gr.60 Steel (API 2W Gr.60 강재적용 K-Joint 구조의 피로성능평가)

  • Im, Sung-Woo;Chang, In-Hwa;Jo, Chul-Hee;Park, Kwan-Kyu
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2006.11a
    • /
    • pp.217-222
    • /
    • 2006
  • Large-scale model tests of welded tubular K-joints were carried out to observe the fatigue behavior of API 2W Gr.60 steel produced by POSCO. The fatigue crack behaviors for various loading conditions were measured and investigated around the critical joint sections. The experimental results have been verified with numerical approaches and also compared with the IIW, DnV RP-C203 and API RP 2A-WSD design curves. The hot spot stress method was applied in the study. The SCF factor for tubular K-joint was also obtained.

  • PDF

Residual static strength of cracked concrete-filled circular steel tubular (CFCST) T-joint

  • Cui, M.J.;Shao, Y.B.
    • Steel and Composite Structures
    • /
    • v.18 no.4
    • /
    • pp.1045-1062
    • /
    • 2015
  • Concrete-filled circular t steel tubular joints (CFSTJs) in practice are frequently subjected to fluctuated loadings caused by wind, earthquake and so on. As fatigue crack is sensitive to such cyclic loadings, assessment on performance of CFSTJs with crack-like defect attracts more concerns because both high stress concentration at the brace/chord intersection and welding residual stresses along weld toe cause the materials in the region around the intersection to be more brittle. Once crack initiates and propagates along the weld toe, tri-axial stresses in high gradient around the crack front exist, which may bring brittle fracture failure. Additionally, the stiffness and the load carrying capacity of the CFSTJs with crack may decrease due to the weakened connection at the intersection. To study the behaviour of CFSTJs with initial crack, experimental tests have been carried out on three full-scale CFCST T-joints with same configuration. The three specimens include one uncracked joint and two corresponding cracked joints. Load-displacement and load-deformation curves, failure mode and crack propagation are obtained from the experiment measurement. According to the experimental results, it can be found that he load carrying capacity of the cracked joints is decreased by more than 10% compared with the uncracked joint. The effect of crack depth on the load carrying capacity of CFCST T-joints seems to be slight. The failure mode of the cracked CFCST T-joints represents as plastic yielding rather than brittle fracture through experimental observation.

Thermal Characteristic of the Tubular Single tap Adhesively Bonded Joint bonded with filler containing epoxy adhesive (충전재가 함유된 단일겹치기 접착 조인트의 열적 특성에 관한 연구)

  • Kim, Jin-Kook;Lee, Dai-Gil
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.370-376
    • /
    • 2001
  • When an adhesive joint is exposed to high environmental temperature, the tensile load capability of the adhesive joint decreases because the elastic modulus and failure strength of structural adhesive decrease. The thermo-mechanical properties of structural adhesive can be improved by addition of fillers to the adhesive. In this paper, the elastic modulus and failure strength of adhesives as well as the tensile load capability of tubular single lap adhesive joints were experimentally and theoretically investigated with respect to the volume fraction of filler (alumina) and the environmental temperature. Also the tensile modulus of the fille containing epoxy adhesive was predicted using a new equation which considers filler shape, filler content and environmental temperature. The tensile load capability of the adhesive joint was predicted by using the effective strain obtained from the finite element analysis and a new failure model, from which the relation between the bonding length and the crack length was developed with respect to the volume fraction of filler.

  • PDF

A Study on Welding Distortion and Residual Stress for Tubular Welded Joint (튜브 용접부의 용접변형 및 잔류응력에 관한 연구)

  • Jin, Hyung-Kook;Shin, Sang-Beom;Lee, Dong-Ju;Park, Dong-Hwan
    • Journal of Welding and Joining
    • /
    • v.30 no.5
    • /
    • pp.51-56
    • /
    • 2012
  • The purpose of this study is to evaluate the distortion and the residual stress of GTA tubular welds between tube and head. In order to do it, the heat input model for GTA welding process was first developed by experiment and FE analyses. The welding distortion and the residual stress distribution of the tubular welds according to welding pass and various restraint degrees were evaluated by using FEA with the heat input model. From FEA results, it was found that the residual stress and the radial distortion at the weld toe of tube part decrease with a decrease in the number of welding pass. However, the maximum residual stresses in each direction of tubular welds are almost constant regardless of the external restraint degree. It was mainly due to the high internal restraint of the welds.

Chord bearing capacity in long-span tubular trusses

  • Kozy, B.;Boyle, R.;Earls, C.J.
    • Steel and Composite Structures
    • /
    • v.6 no.2
    • /
    • pp.103-122
    • /
    • 2006
  • The capacity of tubular truss chords subjected to concentrated reaction forces in the vicinity of the open end (i.e., the bearing region) is not directly treated by existing design specifications; although capacity equations are promulgated for related tubular joint configurations. The lack of direct treatment of bearing capacity in existing design specifications seems to represent an unsatisfactory situation given the fact that connections very often control the design of long-span tubular structures comprised of members with slender cross-sections. The case of the simple-span overhead highway sign truss is studied, in which the bearing reaction is applied near the chord end. The present research is aimed at assessing the validity of adapting existing specifications' capacity equations from related cases so as to be applicable in determining design capacity in tubular truss bearing regions. These modified capacity equations are subsequently used in comparisons with full-scale experimental results obtained from testing carried out at the University of Pittsburgh.

Evaluation of Installation and Arrangement Effects of Internal Ring Stiffener for Tubular K-joints with Axially Loaded Braces (지부재에 축하중을 받는 K형 관이음부의 내부 환보강재의 설치 및 배치효과 평가)

  • Cho, Hyun-Man;Ryu, Yeon-Sun;Lim, Dong-Joo
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.24 no.3
    • /
    • pp.267-274
    • /
    • 2011
  • The effect of internal ring stiffeners is numerically evaluated for reinforcement of tubular K-joints. Finite element analyses are performed to compute stress of un-stiffened and ring-stiffened K-joints subjected to axial loading. The influence of loading condition and geometrical parameters of ring stiffener on joint behavior is assessed to determine the installation effect of single and double ring stiffeners. The arrangement effect of ring stiffener are evaluated using quantitative analysis compared single ring with double ring stiffeners. Based on the numerical results, practical size of ring stiffener is proposed for design of tubular K-joints.

Evaluation of torsional natural frequencies for non-tubular bonded joints

  • Pugno, Nicola;Ruotolo, Romualdo
    • Structural Engineering and Mechanics
    • /
    • v.13 no.1
    • /
    • pp.91-101
    • /
    • 2002
  • During the last several years, research activity on non-tubular bonded joints has concentrated on the effects of normal stress, bending moments and shear. Nevertheless, in certain situations, the structure may be subjected to twisting moments, so that the evaluation of its dynamic behaviour to torsional vibrations becomes of great importance even though evaluations of such loading conditions is entirely lacking in the literature. The aim of this article is to show that torsional natural frequencies of the non-tubular joint can be evaluated by determining the roots of a determinantal equation, derived by taking advantage of some analytical results obtained in a previous paper dealing with the analysis of the state of stress in the adhesive. Numerical results related to clamped-free and clamped-clamped joints complete the article.

Ultimate Strength Interaction of Steel Tubular T-Joint Subjected to Concurrent Action of Compression and Bending (압축과 휨을 동시에 받는 강관 T조인트 극한강도 상호작용)

  • Kim, Kyung-Sik
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.1
    • /
    • pp.298-303
    • /
    • 2016
  • Owing to the advantages of reduced weight and wind effect, the space-framed towers that consist of vertical and horizontal members of circular hollow tubular sections have been adopted widely for various purposes. It is critical to guarantee the strengths of tubular joints where vertical and horizontal members are connected structurally to make the entire space-framed system behave as a single tower structure. In this study, a strength evaluation was conducted for T-type tubular joints subjected to the concurrent action of compression and bending. Three of the available design codes, i.e., AISC, Eurocode 3, ISO 19902 were investigated and a design equation was suggested for an ultimate strength interaction between the axial force and bending moment based on nonlinear finite element analyses by selecting the slenderness ratios at the joints as major parameters.

Experimental and numerical investigations on remaining strengths of damaged parabolic steel tubular arches

  • Huang, Yonghui;Liu, Airong;Pi, Yong-Lin;Bradford, Mark A.;Fu, Jiyang
    • Steel and Composite Structures
    • /
    • v.34 no.1
    • /
    • pp.1-15
    • /
    • 2020
  • This paper presents experimental and numerical studies on effects of local damages on the in-plane elastic-plastic buckling and strength of a fixed parabolic steel tubular arch under a vertical load distributed uniformly over its span, which have not been reported in the literature hitherto. The in-plane structural behaviour and strength of ten specimens with different local damages are investigated experimentally. A finite element (FE) model for damaged steel tubular arches is established and is validated by the test results. The FE model is then used to conduct parametric studies on effects of the damage location, depth and length on the strength of steel arches. The experimental results and FE parametric studies show that effects of damages at the arch end on the strength of the arch are more significant than those of damages at other locations of the arch, and that effects of the damage depth on the strength of arches are most significant among those of the damage length. It is also found that the failure modes of a damaged steel tubular arch are much related to its initial geometric imperfections. The experimental results and extensive FE results show that when the effective cross-section considering local damages is used in calculating the modified slenderness of arches, the column bucking curve b in GB50017 or Eurocode3 can be used for assessing the remaining in-plane strength of locally damaged parabolic steel tubular arches under uniform compression. Furthermore, a useful interaction equation for assessing the remaining in-plane strength of damaged steel tubular arches that are subjected to the combined bending and axial compression is also proposed based on the validated FE models. It is shown that the proposed interaction equation can provide lower bound assessments for the remaining strength of damaged arches under in-plane general loading.

Reserve capacity of fatigue damaged internally ring stiffened tubular joints

  • Thandavamoorthy, T.S.
    • Steel and Composite Structures
    • /
    • v.4 no.2
    • /
    • pp.149-167
    • /
    • 2004
  • Offshore platforms have to serve in harsh environments and hence are likely to be damaged due to wave induced fatigue and environmental corrosion. Welded tubular joints in offshore platforms are most vulnerable to fatigue damage. Such damages endanger the integrity of the structure. Therefore it is all the more essential to assess the capacity of damaged structure from the point of view of its safety. Eight internally ring stiffened fatigue damaged tubular joints with nominal chord and brace diameter of 324 mm and 219 mm respectively and thickness 12 mm and 8 mm respectively were tested under axial brace compression loading to evaluate the reserve capacity of the joints. These joints had earlier been tested under fatigue loading under corrosive environments of synthetic sea water and hence they have been cracked. The extent of the damage varied from 35 to 50 per cent. One stiffened joint was also tested under axial brace tension loading. The residual strength of fatigue damaged stiffened joint tested under tension loading was observed to be less than one fourth of that tested under compression loading. It was observed in this experimental investigation that in the damaged condition, the joints possessed an in-built load-transfer mechanism. A bi-linear stress-strain model was developed in this investigation to predict the reserve capacity of the joint. This model considered the strain hardening effect. Close agreement was observed between the experimental and predicted results. The paper presents in detail the experimental investigation and the development of the analytical model to predict the reserve capacity of internally ring stiffened joints.