Titanium has been used in various fields due to its good corrosion and erosion resistance, and superior mechanical properties. The process for selective electro-deposition on a titanium surface using laser beam is proposed in this paper. The process consists of laser irradiation, electro-deposition, and ultrasonic cleaning. Laser irradiation can change the surface morphology of titanium. Through laser irradiation, the surface cleaning effect and a rough surface can be achieved. The surface roughness of titanium was measured according to the laser beam conditions. The characteristics of selective electro-deposition on titanium surface according to surface roughness are investigated by various analytical methods such as SEM, and EDS.
Titanium is widely used in dentistry for its low density, high strength, fatigue resistance, corrosion resistance, and biocompatibility. But it has a tendency of surface damage under circumstance of friction and impact for its low hardness of the surface. Coating is one of methods fir increasing surface hardness. Its effect is to improve surface physical characteristics without change of titanium. Diamond-like carbon and titanium nitride are known for its high hardness of the surface. So that this study was aimed at the wear test and the cytotoxicity test of the commercially pure titanium and Ti-6Al-4V alloy which were deposited by diamond-like carbon film or titanium nitride film to acertain improvement of the surface hardness and the biocompatibility. A disk (25mm diameter, 2mm thickness) was made of commercially pure titanium and Ti-6Al-4V alloy and these substrates were deposited by diamond-like carbon film or titanium nitride film. Diamond-like carbon film was deposited by the method of radiofrequency plasma assisted chemical vapor deposition and titanium nitride film was deposited by the method of reactive arc ion plating. Then these substrates were tested about wear characteristics by the pin-on-disk type wear tester in which ruby ball was used as a wear causer under the load of 32N, The fracture cycles were measured by rotating the substrates until their films were fractured. The wear volume was measured after 150 cycles and 3,000 cycles using surface profiler. The cytotoxicity test was peformed by the method of the MTT assay. The results were as follows : 1. In the results of the wear volume test, commercially pure titanium and titanium alloy which were coated by diamond-like carbon film or titanium nitride aim had higher resistance against wear than the substrates which were not coated by any films (P<0.05). 2. In the results of the fracture cycle test and the wear volume test, diamond-like carbon film had higher resistance against wear than titanium nitride film (P<0.05). 3. In both coatings of diamond-like carbon aim and titanium nitride film, Ti-6Al-4V alloy had higher resistance against wear than commercially pure titanium (P<0.05) 4. In the results of the cytotoxicity test, diamond-like carbon film and titanium nitride film had little cytotoxicity as like commercially pure titanium or Ti-6Al-4V alloy (P>0.05).
Statement of problem. Nano-scale calcium-phosphate coating on the anodizing titanium surface using ion beam-assisted deposition (IBAD) has been recently introduced to improve the early osseointegration. However, not much is known about their surface characteristics that have influence on tissue-implant interaction. Purpose. This study was aimed to investigate microtopography, surface roughness, surface composition, and wettability of the titanium surface modified by the anodic oxidation and calcium phosphate coating using IBAD. Material and methods. Commercially pure titanium disks were used as substrates. The experiment was composed of four groups. Group MA surfaces represented machined surface. Group AN was anodized surface. Group CaP/AN was anodic oxidized and calcium phosphate coated surfaces. Group SLA surfaces were sandblasted and acid etched surfaces. The prepared titanium discs were examined as follows. The surface morphology of the discs was examined using SEM. The surface roughness was measured by a confocal laser scanning microscope. Phase components were analyzed using thin-film x-ray diffraction. Wettability analyses were performed by contact angle measurement with distilled water, formamide, bromonaphtalene and surface free energy calculation. Results. (1) The four groups showed specific microtopography respectively. Anodized and calcium phosphate coated specimens showed multiple micropores and tiny homogeneously distributed crystalline particles. (2) The order of surface roughness values were, from the lowest to the highest, machined group, anodized group, anodized and calcium phosphate deposited group, and sandblasted and acid etched group. (3) Anodized and calcium phosphate deposited group was found to have titanium and titanium anatase oxides and exhibited calcium phosphorous crystalline structures. (4) Surface wettability was increased in the order of calcium phosphate deposited group, machined group, anodized group, sandblasted and acid etched group. Conclusion. After ion beam-assisted deposition on anodized titanium, the microporous structure remained on the surface and many small calcium phosphorous crystals were formed on the porous surface. Nanoscale calcium phosphorous deposition induced roughness on the microporous surface but hydrophobicity was increased.
Journal of the Korean institute of surface engineering
/
v.35
no.5
/
pp.273-278
/
2002
We oxidized pure titanium by anodizing oxidation process in the range of 590V, within 1.5A, 30seconds. we investigated color evolution with a spectrophotometer. Surface images and surface roughness were characterized by an optical microscope and an atomic force microscope, respectively. Below the thickness of 40 $\mu\textrm{m}$, metallic yellow, blue, and pink colorsn were obtained. Lightness decreased, increased, and decreased again as titanium oxide thickness increased. Blue color at the applied voltage of 30V showed the best lightness and reproducibility with surface roughness below l$\mu\textrm{m}$. Bare titanium and titanium oxide films had micro pits more than 10ea/$\mu\textrm{m}^2$. We report that we successfully made colors by varing thickness below 40$\mu\textrm{m}$ with anodizing oxidation of method.
Purpose: The purpose of this study was to observe the change of metal-mold reaction and surface roughness in titanium casting specimens for phosphate-silica alumina bonded investment with mold temperatures. Methods: The metal-phosphate silica alumina bonded mold interface reaction and surface roughness of titanium casting specimens according to mold temperatures were investigated. The Specimens were analysed by scanning electron microscopy and surface roughness tester. Results: The oxidation behavior indicated by the growth of oxide thickness. The titanium-oxide layer were consisted two layer of a porous external and a dense internal one. The reaction layer and surface roughness increased with increasing investment material temperature. Conclusion: In this work, The most suitable mold temperature in casting of pure titanium was $200^{\circ}C$.
For the purpose of surveying any possibility of anchoring titanium dioxide on activated carbons to promote their activities as catalysts and/or adsorbents, two activated carbons were oxidized with ammonium peroxydisulfate and followed by anchoring titanium dioxide. The anchoring of titanium dioxide on the oxidized activated carbons were performed via the adsorption of tetrabutyltitanate, hydrolysis with deionized water, and calcination. The effect of oxidizing and anchoring treatment on the surface element composition, surface area, and pore texture were analyzed by XPS, BET and TPD. The oxidation of activated carbons with ammonium peroxydisulfate introduced carboxyl groups on the surface of activated carbons and these carboxyl groups promoted the anchoring of titanium oxide on the activated carbons. However, the treatments affected the surface area and the porosity of activated carbons.
Journal of the Korean Society of Manufacturing Process Engineers
/
v.8
no.4
/
pp.20-27
/
2009
The characteristics of titanium alloy as a relatively advanced material is low density, avirulent and, superior corrosive resistant, therefore the use of titanium alloy is increasing lately in aerospace and mechanical technologies, precision machinery, electronics industry, petro-chemical industries and biomedical areas. In these days, the titanium alloy product is required various surface qualities of not only smooth surface but also rough surface depending on usages. The purpose of this experimental research is to find the optimum surface roughness of titanium alloy of Ti-6Al-4V, by micro abrasive blasting as depending variable conditions of working pressure, nozzle size, working time, stand of distance and power particle size.
The objective of this study was to evaluate the influence of surface modifications on the bonding characteristics and cytotoxicity of specific titanium porcelain bonded to milling titanium and cast titanium. Milling titanium and cast titanium samples were divided into 8 test groups. These groups are as follow: i) sandblasted with particles of different size of $220{\mu}m\;and\;50{\mu}m$, ii) different sequences of sandblasting treatment and etching treatment, iii) etched with different etching solutions, and iv) preheated or not. The surface characteristics of specimens were characterized by the test of mean roughness of surface and SEM. The bond strength of titanium-ceramic systems was measured by using three-point bending test and SEM. The results show that the mean roughness of surface of sample sandblasted with $220{\mu}m$ aluminum oxide increased and bond strength were higher than sample sandblasted with $50{\mu}m$ aluminum oxide. The mean roughness of surface decreased, but the bond strength increased when the samples sandblasted with $220{\mu}m$ aluminum oxide were preheated. The sample sandblasted with $220{\mu}m$ aluminum oxide after oxidized with occupational corrosive agent I (50% NaOH, 10% $CuSO_4{\cdot}5H_2O$) and II (35% $HNO_3$, 5% HF) showed higher bond strength than sample oxidized with 30% $HNO_3$ after sandblasted with $220{\mu}m$ aluminum oxide. Group NaCuNF220SP (milling Ti: 35.3985 MPa, casting Ti: 37.2306 MPa) which was treated with occupational corrosive agent I (50% NaOH, 10% $CuSO_4{\cdot}5H_2O$) and II (35% $HNO_3$, 5% HF), followed by sandblasting with $220{\mu}m$ aluminum oxide and preheating at $750^{\circ}C$ for 1 hour showed the highest bond strength and significant differences (P<0.05). The method for modifying surface of titanium showed excellent stability of cells.
Titanium implant is used as the most popular dental material for replacement of missing teeth recently. A lot of studies on the surface modification of titanium implant have been carried out for enhancing osseointegration. The surface modification techniques could be classified as follows; topographic modifications which provide roughness and porosity, chemical surface modificationss or deposition of osseoconductive materials, and biochemical modifications to immobilize bone growth factors on titanium surface. In this study, the current and ongoing surface modification techniques and its typical characteristics used in clinics were reviewed. In the future, study and implication about biochemical modifications including patient' s individual characteristics will be important.
Journal of the Korean Society of Manufacturing Process Engineers
/
v.11
no.3
/
pp.13-18
/
2012
We investigated the cell activity of controlled titanium surface using various grinding methods including ELID (Electrolytic In-Process Dressing) grinding method. The influence of titanium surface condition by each grinding process on the cell activity was evaluated by ALP activity of MSC(Mesenchymal Stem Cells). The ALP activity of controlled surface by ELID grinding process using # 2000 wheel was higher than that of other titanium surface. The morphological, chemical properties of machined surface by grinding method was observed using various analytical method.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.