주석 및 아연 박막이 코팅된 베어링 표면의 구름 저항 거동에 대한 실험적 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Tin and Zinc Films)

  • 양승호;공호성;윤의성;김대은
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제26회 추계학술대회
    • /
    • pp.51-58
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure tin and zinc coated 52100 bearing steel. Pure tin coatings ranging from 30 nm to 30,000 nm and pure zinc coatings ranging from 500 nm to 52,000 nm were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the effect of coating thickness on the tribological rolling behavior. Results showed that the existence of optimum film thickness which revealed minimum rolling resistance was discovered for tin and zinc coating. The compatibility of coating matehal to iron showed no significant effect on the rolling resistance behavior. The hardness of coating material revealed significant influence to the rolling resistance behavior.

  • PDF

은 박막의 미끄럼 마찰거동에 대한 실험적 고찰 (An Experimental Study on the Frictional Behavior of Silver Coating Films at Sliding Surfaces)

  • 양승호;공호성;윤의성;김대은
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.7-13
    • /
    • 1999
  • An experimental study was performed to discover the effect of silver coating on the frictional behavior of SM45C steel at sliding surfaces. Pure silver was coated the SM45C disk surfaces by a thermal evaporation method. Experiments using a pin-on-disk test-rig was performed under dry air and various humidity conditions. Friction coefficients increased to a high and unstable value after failure of coating, and friction coefficients increased with increasing the thickness of silver coated layer. But optimum coating thickness was not observed.

  • PDF

원자혼합법으로 증착된 은 박막의 트라이볼로지적 특성에 관한연구 (A Study on the Tribological Characteristics of Thermally Evaporated Silver Films Assisted by Atomic Mixing)

  • 양승호;공호성;윤희성
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제34회 추계학술대회 개최
    • /
    • pp.27-34
    • /
    • 2001
  • A new functionally gradient metal coating method using an atomic mixing technique was developed. In this work the effect of silver atomic mixing on the tribological characteristics of silver$.$ films. has been investigated experimentally. Atomic mixing was implemented by using the, bombardment .of accelerated Ar ions during the thermal evaporation coating process of silver films. Experiments were performed in dry conditions using a ball-on-disk test rig at a load range of 19.6 mN - 17.64 N and a sliding velocity of 20 mm/sec. Results showed that the life of functionally gradient silver coating was enhanced about 100 times more than that of thermally evaporated silver coating and 2 times more than that of IBAD silver coating. The functionally gradient. film also showed low friction and wear compared to those of the evaporated silver and

  • PDF

Influence of coating and annealing on the luminescence of Ga2O3 nanowires

  • Kim, Hyunsu;Jin, Changhyun;Lee, Chongmu;Ko, Taegyung;Lee, Sangmin
    • Journal of Ceramic Processing Research
    • /
    • 제13권spc1호
    • /
    • pp.59-63
    • /
    • 2012
  • Ga2O3-core/CdO-shell nanowires were synthesized by a two step process comprising thermal evaporation of GaN powders and sputter-deposition of CdO. Transmission electron microscopy (TEM) and X-ray diffraction (XRD) analyses revealed that the cores and the shells of the annealed coaxial nanowires were single crystal of monoclinic Ga2O3 and FCC CdO, respectively. As-synthesized Ga2O3 nanowires showed a broad emission band at approximately 460 nm in the blue region. The blue emission intensity of the Ga2O3 nanowires was slightly decreased by CdO coating, but it was significantly increased by subsequent thermal annealing in a reducing atmosphere. The major emission peak was also shifted from ~500 nm by annealing in a reducing atmosphere, which is attributed to the increases in the Cd interstitial and O vacancy concentrations in the cores.

연금속 박막이 코팅된 베어링 표면의 구름 저항 거동에 미치는 분위기의 영향에 대한 실험적 고찰 (An Experimental Study of Environmental Effects on the Rolling Resistance of Bearing Surfaces Coated by Soft Metallic Films)

  • 양승호;공호성;윤의성;김대은
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제27회 춘계학술대회
    • /
    • pp.47-54
    • /
    • 1998
  • An experimental study was performed to discover the effect of environmental conditions on the rolling resistance behavior of pure silver and lead coated 52100 bearing steel. Pure silver and lead coating were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed under vacuum, dry air and controlled humidity conditions. Results showed that agglomeration of particles were prevented in vacuum environment and as it showed low and stable rolling resistance by shakedown phenomena. Also, humidity relates closely to the agglomeration of particles and increased the rolling resistance after the failure of coated layer.

  • PDF

은 박막이 코팅된 베어링 표면의 구름 저항 거동 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Silver Film)

  • 양승호;공호성;윤의성;권오관
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제25회 춘계학술대회
    • /
    • pp.101-110
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure silver coated 52100 bearing steel. Pure silver coatings ranging from 80 nm to several micrometers were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the influence of coating thickness on the tribological rolling behavior. The existence of optimum film thickness which revealed minimum rolling resistance was discovered. A careful analysis on the contact surfaces for the optimum film thickness has been performed. The contact patches produced by the transferred silver films played an important role for the rolling resistance to keep low.

  • PDF

은 박막이 코팅된 베어링 표면의 구름 저항 거동 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Silver Film)

  • 양승호;공호성;윤의성;권오관
    • Tribology and Lubricants
    • /
    • 제13권3호
    • /
    • pp.85-92
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure silver coated 52100 bearing steel. Pure silver coatings ranging from 80 nm to several micrometers were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the influence of coating thickness on the tribological rolling behavior. The existence of optimum film thickness which revealed minimum rolling resistance was discovered. A careful analysis on the contact surfaces for the optimum film thickness has been performed. The contact patches produced by the transferred silver films played an important role for the rolling resistance to keep low.

알루미늄의 진공증발과 열산화에 의한 알루미나 복합분리막의 제조 및 특성분석 (Synthesis and Characterization of Alumina Composite Membrane by Al Evaporation and Thermal Oxidation)

  • 이동호;최두진;현상훈
    • 한국세라믹학회지
    • /
    • 제32권3호
    • /
    • pp.349-358
    • /
    • 1995
  • The ceramic composite membrane was synthesized by thermal oxidation after evaporation of Al on the support prepared by slip casting process. Oxidation was performed at $700^{\circ}C$ and 80$0^{\circ}C$ under dry oxygen atmosphere. It was considered as optimum oxidation condition that the membrane showed a knudsen behaviro. A further oxidation resulted in an increase of gas permeability because top layer became densified. Then, a multi-layered composite membrane was synthesized through a sol-gel method, evaporation and thermal oxidation of Al coating processes. While the membrane was thermally stable up to 80$0^{\circ}C$, gas permeability was rapidly decreased even at a slight amount of deposition of Al.

  • PDF

연금속 박막이 코팅된 베어링의 구름 저항 거동에 미치는 분위기의 영향에 대한 실험적 고찰 (An Experimental Study of Environmental Effects on the Rolling Resistance of Bearings Coated by Soft Metallic Films)

  • 양승호;공호성;윤의성;김대은
    • Tribology and Lubricants
    • /
    • 제14권3호
    • /
    • pp.1-6
    • /
    • 1998
  • An experimental study was performed to discover the effect of environmental conditions on the rolling resistance behavior of pure silver and lead coated 52100 bearing steel. Pure silver and lead coatings were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed under vacuum, dry air and controlled humidity conditions. Results showed that agglomeration of particles were suppressed in vacuum environment and resulted in low and stable rolling resistance by shakedown phenomena. Also, humidity related closely to the agglomeration of particles and the rolling resistance after the failure of coated layer.

주석 및 아연 박막이 코팅된 베어링 표면의 구름 저항 거동에 대한 실험적 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Coated by Pure Tin and Zinc Films)

  • 양승호;공호성;윤의성;김대은
    • Tribology and Lubricants
    • /
    • 제14권1호
    • /
    • pp.1-6
    • /
    • 1998
  • An experimental study was performed to discover the tribological behaviors of pure tin and zinc coated 52100 bearing steel. Pure tin coatings ranging from 30 nm to 30,000 nm and pure zinc coatings ranging from 500 nm to 52,000 nm were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the effect of coating thickness on the tribological rolling behavior. Results showed that the existence of optimum film thickness which revealed minimum rolling resistance was discovered for tin and zinc coating. The compatibility of coating material to iron showed no significant effect on the rolling resistance behavior. The hardness of coating material revealed significant influence to the rolling resistance behavior.