정방정상과 능면체상의 경계조성 Pb(Zr, Ti)$O_3$ 세라믹스에서 화학조성의 불균일성이 상공존에 미치는 영향 (Effects of Chemical Inhomogeneity on Phase Coexistence in Pb(Zr, Ti))$O_3$ Ceramics at Morphotropic Tetragonal and Rhombohedral Phase Boundary)

  • 천채일;김호기
    • 한국세라믹학회지
    • /
    • 제27권8호
    • /
    • pp.1027-1033
    • /
    • 1990
  • In order to identify the origin of phase coexistence at morphotropic tetragonal and rhombohedral boundary in PZT ceramics, the effect of chemical inhomogeneity on phase coexistence region was investigated. Two kinds of PZT ceramics with different chemical homogeneity were prepared by conventional solid state reaction and co-precipitation method. There was coexistence of tetragonal and rhombohedral phase over a wide composition range in PZT ceramics calcined by solid state reaction, and there was also phase coexistence of which region was reduced considerably in sintered samples. And phase coexistence region was not observed in co-precipitated PZT ceramics(within 1 mole%). Therefore compositional fluctuation is considered to be major origin of the phase coexistence at morphotropic phae boundary in PZT ceramics.

  • PDF

Magnetic Properties of Ordered L12 FePt3: A First Principles Study

  • Kim, Dong-Yoo;Hong, Ji-Sang
    • Journal of Magnetics
    • /
    • 제16권3호
    • /
    • pp.197-200
    • /
    • 2011
  • Using the full potential linearized augmented plane wave (FLAPW) method, the influences of uniform and tetragonal strains on the magnetic state have been explored for chemically ordered bulk $L1_2$ $FePt_3$. The ordered state displays antiferromagnetic $Q_1$ (AFM-$Q_1$) state but it transitions into antiferromagnetic $Q_2$ (AFM-$Q_2$) state at about 10% uniform strain. The ferromagnetic (FM) state is observed at 11% uniform strain. For tetragonal strain, it is also seen that the transition from AFM-$Q_1$ to AFM-$Q_2$ depends on the strength and direction of the applied strain. The FM state does not appear in this case. Magnetocrystalline anisotropy (MCA) calculations for tetragonal distortion reveal that the spin reorientation transition occurs. In addition, we find that the direction of magnetization and the magnitude of magnetic anisotropy energy strongly depend on the c/a ratio.

금속 알콕사이드로부터 구형의 단분산 Y-doped $ZrO_2$ 미립자 제조 (Preparation of Spherical Monodispersed Y-doped ZrO2 Powders from Metal Alkoxide)

  • 김병익;이중윤;최상흘
    • 한국세라믹학회지
    • /
    • 제29권2호
    • /
    • pp.119-126
    • /
    • 1992
  • 3 mol% Y2O3-doped ZrO2 powders were prepared by hydrolysis with 0.1, 0.2, 0.3, 0.4, 0.5, 0.6 mol/ιH2O/ethanol into 0.1 mol/ι zirconium and yttrium alkoside/ethanol. Spherical monodispersed yttria-partially stabilized zirconia particles with an average diameter of about 0.5 ${\mu}{\textrm}{m}$ were prepared by hydrolysis with 0.2 mol/ιH2O/ethanol. The as-prepared powder was amorphous and with heating it transformed into cubic up to 80$0^{\circ}C$ and into tetragonal over 100$0^{\circ}C$. 3 mol% Y2O3-doped ZrO2 powders calcined over and up to 80$0^{\circ}C$ were a mixture of tetragonal and monoclinic and only tetragonal as determined by X-ray diffraction, respectively.

  • PDF

마게마이트(${\gamma}$-Fe$_2$O$_3$)의 구조에 대한 연구II -격자에너지 계산과 결정구조해석- (An Study on the Structure of Maghemite(${\gamma}$-Fe$_2$O$_3$) II -Lattice Energy Computation and Crystal Structure Analysis-)

  • 신형섭
    • 한국세라믹학회지
    • /
    • 제35권11호
    • /
    • pp.1182-1189
    • /
    • 1998
  • Crystal structure and structural stability of needle-shaped maghemite(${\gamma}$-{{{{ { {Fe }_{2 }O }_{3 } }}) have been studied by the computation and estimation of lattice energies interionic distances and site potentials. The refined struc-tures analyzed with cubic system(space group P4332) and tetragonal system(space group P4332) were used for these computations. The lattice energy of tetragonal system is -143.10eV/molecule. The maghemite structure with tetragonal system is more stable than that with cubic system. The ordering energy of the FE and cation vacancy within the octahedral site the 4b site of the structure with cubic system(space group P4332) is -0.95eV/molecule but this Fe has larger interionic distance and is very unstable.

  • PDF

Sol-Gel법에 의한$ZrO_2$ Ceramic Fiber 제조 ($ZrO_2$ Ceramic Fiber Fabrication by Sol-Gel Processing)

  • 김선욱;김성숭
    • 한국세라믹학회지
    • /
    • 제27권6호
    • /
    • pp.824-828
    • /
    • 1990
  • Zirconia gel fibers were fabricated by sol-gel processing using zirconium alkoxides and 2, 4-pentanedione. Their phase transformation and microstructural evolution were studied after heat treatments up to 150$0^{\circ}C$. Tetragonal ZrO2 began to form at 50$0^{\circ}C$ and followed by monoclinic, tetragonal phase during subsequent heat treatments at 1000, 150$0^{\circ}C$ for 1hour respectively. During cooling from 150$0^{\circ}C$, cracks were created, propagated along grain boundaries due to the volume change from tetragonal to monoclinic transformation.

  • PDF

분말 열처리가 지르코니아 용사코팅층의 마모특성에 미치는 영향 (Effect of Heat Treatment of powder on the Tribological Behavior of the Plasma Sprayed Zirconia Coating)

  • 신종한;임대순;안효석
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제32회 추계학술대회 정기총회
    • /
    • pp.298-303
    • /
    • 2000
  • The 3 mol% yttria stabilized zirconia (3-Y PSZ) powder was heat treated at 50 0$^{\circ}C$ to evaporate the polymer binder and stabilize the tetragonal phase. The wear experiments were carried out on a ring-on-plate type reciprocating wear tester at selected temperatures with in the range room temperature to 600$^{\circ}C$ The results show that the heat treatment of powder decreases the wear rate due to the reduction of microcracks and pores in coatings and the stabilization of the tetragonal phase. Powder heat treatment enhanced the quality of the coating layer by removing remnant gases during coating process and the powder heat treatment at which tetragonal phase is stable diminished phase ratio of monoclinic. These two effects improved wear resistance characters.

  • PDF

고압 수증기에 따른 Low-Sn Zircaloy-4의 고온 산화 거동 (Steam Pressure Effects on the Oxidation of Low-Sn Zircaloy-4 at High Temperatures)

  • 양성우;박광헌
    • 한국표면공학회지
    • /
    • 제40권4호
    • /
    • pp.180-184
    • /
    • 2007
  • A new zirconium alloy, low-Sn Zircaloy-4 was investigated to see the effects of high pressure steam on the oxidation at high temperatures. High pressure steam turned out to enhance the oxidation at high temperatures below $1000^{\circ}C$. The oxide layer groved to deviate from the uniform layer under high steam pressures, and usually cracks were found at the thicker parts in the oxide layer. High pressure steam seems to destabilize the tetragonal oxides near the metal layer, and the monoclinic oxides transformed from the destabilized tetragonal oxides are structurally not sound, resulting in enhanced oxidation under high pressure steam.

고온수중에서 ZrO2의 코발트흡착 특성에 대한 연구 (A Study on the Adsorption Characteristic of Cobalt on ZrO2 in High-Temperature Water)

  • 김유환;배성렬
    • 공업화학
    • /
    • 제8권2호
    • /
    • pp.267-275
    • /
    • 1997
  • 본 연구는 졸-겔법을 이용하여 제조한 $ZrO_2$의 하소 온도에 따른 분말특성을 조사하고, 고온수에서 $ZrO_2$$Co^{2+}$ 흡착특성을 교반기가 달린 압력용기를 이용한 회분식 흡착 실험으로 알아보았다. 졸-겔법을 이용하여 $ZrO_2$분말을 제조하고, $600{\sim}1400^{\circ}C$로 하소한 후, X-선 회절법, SEM, BET 방법, Fourier transform 적외선 (FT-IR), 열중량 및 열시차분석법(TG-DTA)등을 이용하여 특성 변화를 조사하였다. 비정질의 질코니아는 $480^{\circ}C$부터 tetragonal 질코니아가 생성되고 $600{\sim}1000^{\circ}C$ 온도범위에서는 tetragonal 질코니아와 monoclinic 질코니아가 공존하며, $1200^{\circ}C$에서는 tetragonal 질코니아에서 monoclinic 질코니아로의 상변태가 나타났으며, 고온수에서 하소온도가 $600^{\circ}C$$ZrO_2$의 흡착제의 코발트 평형흡착용량은 0.16 meq/g 이었다. $125^{\circ}C$ 이상의 고온에서의 흡착반응은 비가역 흡열반응이며, $600^{\circ}C$에서 하소한 $ZrO_2$의 표준엔탈피 변화값(${\Delta}H^{\circ}$)은 약 18 kJ/gmol 이였다.

  • PDF

입방정과 사방정 PZT 요업체에서의 분극처리 후 유전율 (Permittivity in Tetragonal and Rhombohedral Phase PZT Ceramics after Poling)

  • 정훈택;김호기
    • 한국세라믹학회지
    • /
    • 제29권7호
    • /
    • pp.572-576
    • /
    • 1992
  • Dielectric constant of ferroelectric ceramics with poling is important in relation to the mechanism of dielectric breakdown. From the research about the dielectric constant variation with poling in tetragonal and rhombohedral phase PZT ceramics, it is known that the dielectric constant after poling is determined by competing effects between increasing effects (compressive stress induced by electrostriction of piezoelectric effects) and decreasing increase in large grain size with poling is smaller than in small grain size.

  • PDF

PZT계의 정방정상과 능면체정상의 경계조성에 대한 기계적 응력과 전기장의 영향 : 열역학적 고찰 (The Effect of Mechanical Stress and Electric Field on the Morphotropic Tetragonal and Rhombohedr Phase Boundary in PZT System : Thermodynamic Consideration)

  • 천채일;김호기
    • 한국세라믹학회지
    • /
    • 제30권10호
    • /
    • pp.859-865
    • /
    • 1993
  • Morphotropic tetragonal and rhombohederal phase boundary(MPB) in PZT system was calculated and the effect of mechanical stress and electric field on the MPB was examined using phenomenological thermodynamic theory proposed by Devonshire. Mechanical stress and electric field was calculated to change free energies of phases and shift MPB. The stable composition range of the phase, of which spontaneous strain and spontaneous polarization aligned to the direction of tensile stress or electirc field, was expanded.

  • PDF