Fretting Wear and Friction of lnconel 690 for Steam Generator Tube in Elevated Temperature Water

  • Lee, Young-Ze;Lim, Min-Kyu;Oh, Se-Doo
    • KSTLE International Journal
    • /
    • 제3권1호
    • /
    • pp.49-53
    • /
    • 2002
  • Inconel 690 for nuclear steam generator tube has more chromium than the conventionally used Inconel 600 in order to increase the corrosion resistance. TD evaluate the tribological characteristics under fretting condition the fretting tests as well as sliding tests were carried out in elevated temperature water environment. Fretting tests of the cross-cylinder type were done under various vibrating amplitudes and applied normal loads in order to measure the friction forces and wear volumes. Also, the conventional sliding tests of pin-en-disk type were carried out to compare the test results. In fretting, the friction was very sensitive to the load and the amplitude. The friction coefficient decreased with increasing load and decreasing amplitude. Also, the wear of Inconel 690 can be predictable using the work rate model. Depending on normal loads and vibrating amplitudes, distinctively different wear mechanisms and of ten drastically different wear rates can occur. It was fecund that the fretting wear coefficients in water were increased as increasing the temperature of water.

20kW급 마이크로터빈용 저공해 연소기의 고압고온 성능실험 연구 (An Experimental Study on Low Nox Combustor Performance at High Pressure and Temperature for 20kW Class Microturbines)

  • 윤정중;오종식;이헌석
    • 유체기계공업학회:학술대회논문집
    • /
    • 유체기계공업학회 2002년도 유체기계 연구개발 발표회 논문집
    • /
    • pp.183-190
    • /
    • 2002
  • In order to reduce NOx emissions in the 20kw class microturbines under development, the low NOx characteristics, as being an application to the lean premixed combustion technology, have been investigated. The study has been conducted at the conditions of high temperature and pressure. Air from a compressor with the temperature of 500K to 650K and the pressure of 0.3bar gauge to 0.7bar gauge, was supplied to the combustor through an air preheat-treatment. Sampling exhaust gases were measured at the immediate exit of the combustor. for the effect of temperature on NO and CO emissions. though NOx was increased, CO was decreased with increasing inlet air temperature. With increasing inlet air pressure, NOx and CO were increased also. NOx was decreased, but CO was increased with increasing inlet air mass flow rate. The test has been performed on the equivalent ratios of 0.10 to 0.25 in a lean region. NOx was increased with increasing equivalent ratios, but CO was decreased as an influence of flame temperature. In the very lean region of the equivalent ratio below 0.12, CO was increased suddenly, due to instability. As the results of this study, NOx and CO are found to be reduced to the similar level at the same time when operated at optimal conditions.

  • PDF

카본블랙내 이온성 불순물들에 따른 반도전 재료(층)의 열적특성 (Thermal Properties of Semiconductive Materials(Shield) by Sonic Impurities in Carbon Black)

  • 이용성;최용성;박대희;이경용
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제54권4호
    • /
    • pp.149-153
    • /
    • 2005
  • We have investigated thermal properties showed by changing the content of carbon black which is the component parts of semiconductive shield in underground power transmission cable. Specimens were made of sheet with the nine of those for measurement. Heat capacity (${\Delta}$H), glass transition temperature (Tg) and melting temperature (Tm) were measured by DSC (Differential Scanning Calorimetry). The ranges of measurement temperature were from -100($^{\circ}C$) to 100($^{\circ}C$), and heating rate was 4($^{\circ}C$/min). And then thermal diffusivity was measured by LFA 447. The dimension of measurement temperature was 25[$^{\circ}C$]. Glass transition temperature of specimens was showed near -25[$^{\circ}C$] and the heat capacity and the melting temperature from the DSC results were simultaneously decreased according to increasing the content of carbon black, while thermal diffusivity was increased according to increasing the content of carbon black. Because ionic impurities of carbon black having Fe, Co, Mn, Al and Zn are rapidly passed kinetic energy increasing the number of times breaking during the unit time with the near particles according to increasing vibration of particles by the applied heat energy.

Oxidation Study on the Fabrication of Fe-36Ni Oxide Powder from Its Scrap

  • Yun, Jung Yeul;Park, Man Ho;Yang, Sangsun;Lee, Dong-Won;Wang, Jei-Pil
    • 한국분말재료학회지
    • /
    • 제20권1호
    • /
    • pp.48-52
    • /
    • 2013
  • A study of oxidation kinetic of Fe-36Ni alloy has been investigated using thermogravimetric apparatus (TGA) in an attempt to define the basic mechanism over a range of temperature of 400 to $1000^{\circ}C$ and finally to fabricate its powder. The oxidation rate was increased with increasing temperature and oxidation behavior of the alloy followed a parabolic rate law at elevated temperature. Temperature dependence of the reaction rate was determined with Arrhenius-type equation and activation energy was calculated to be 106.49 kJ/mol. Based on the kinetic data and micro-structure examination, oxidation mechanism was revealed that iron ions and electrons might migrate outward along grain boundaries and oxygen anion diffused inward through a spinel structure, $(Ni,Fe)_3O_4$.

STS 304강의 분위기온도에 따른 부식마멸기구에 관한 연구 (A Study on the Corrosive Wear Mechanism on Atmospherical Temperature of STS 304 Steel)

  • 전태옥;박흥식;주창식
    • 대한기계학회논문집
    • /
    • 제14권2호
    • /
    • pp.399-406
    • /
    • 1990
  • This paper is studied to know corrosive wear mechanism of STS304 steel on atmospherical temperature against mating material as the same. The corrosive test was carried out by rubbing the annular surface of two test pieces in distilled water and NaCl aqueous solution. The corrosive wear mechanism was investigated by S.E.M. The experimental results show that there is one Lcr transferring from severe wear to mild wear on change of NaCl concentration and atmospherical temperature, and which is the other still remaining in server wear state. It was found that the critical sliding distance Lcr shorten with increasing NaCl concentration but it is longer with ascending atmospherical temperature and the mild wear state still continues under the condition of high generation rate and elimination rate of the corrosive product. Considering upon the result, the model of corrosive wear mechanism is proposed.

고질소강 오스테나이트계 스테인레스강의 압축변형특성 (Deformation Characteristic by Compression in High-Nitrogen Austenitic Stainless Steel)

  • 이종욱;김동수;김병구;이명열
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.139-141
    • /
    • 2007
  • Compression tests were carried out to investigate morphologies of compressed specimen, deformation microstructure and stress-strain relation in high-nitrogen austenite stainless steel. Tests were performed under a wide range of temperature and, with true strain rates up to $\dot{\varepsilon}$ =0.05, 0.1, 0.5 and $1.0s^{-1}$. The activation energy of loading force was equal to plastic deformation energy within the temperature range of $900^{\circ}C$ to $1250^{\circ}C$. Dynamically recrystallized grain size decreased with an increasing strain rate and temperature. Flow stresses and deformation microstructures, were used to quantify the critical strain rate and recrystallized grain size. The grain size versus strain rate-temperature map obtained in the study was in good agreement with the deformation microstructures of compressed specimens.

  • PDF

승온속도에 따른 저온소결 PMN-PNN-PZT 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristic of Low Temperature Sintering PMN-PNN-PZT Ceramics according to the Heating Rate)

  • 김국진;류주현;홍재일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.253-254
    • /
    • 2007
  • In this study, in order to develop low temperature sintering multilayer piezoelectric actuator, PMN-PNN-PZT system ceramics were fabricated using $Li_2CO_3-Bi_2O_3$-CuO as sintering aids and their piezoelectric and dielectric characteristics were investigated as a function of heating rate. At sintering temperature of $900^{\circ}C$, with increasing heating rate, electromechanical coupling factor(kp), mechanical quality factor(Qm) and dielectric constant $({\varepsilon}_r)$ were increased.

  • PDF

플라즈마 화학증착법을 이용한 $\alpha$-Si:H박막의 제조 (Deposition of $\alpha$-Si:H thin films by PECVD method)

  • 정병후;문대규;임호빈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1991년도 추계학술대회 논문집
    • /
    • pp.63-67
    • /
    • 1991
  • Amorphous silicon films were deposited on glass, [100] single crystal silicon wafer with thermally grown silicon dioxide, and [100] silicon wafer substrates by Plasma Enhanced Chemical Vapor Deposition(with argon diluted silane source gas). Growth rate, UV optical band edge, and the hydrogen quantity in the amorphous silicon films have been investigated as a function of the preparation conditions by measuring film thickness, UV-absorbency, and FT-IR transmittance. The growth rate of the ${\alpha}$-Si:H films increases with increasing substrate temperture, flow rate and R.F. power density. The UV optical band edge shifts to blue with the increases in the deposition pressure. Increasing substrate temperature shifts the UV optical band edge of the films to red. Hydrogen quantity in the ${\alpha}$-Si:H films increases with an increases in the R.F. powr and decreases with an increase in the substrate temperature.

Effect of Heat Treatment and Platinum Loading on CdS Particles in the Photocatalytic Alanine Synthesis

  • Lee, Bu-Yong;Kim, Bong-Gon;Cho, Cheol-Rae;Sakada, Tadayoshi
    • Bulletin of the Korean Chemical Society
    • /
    • 제14권6호
    • /
    • pp.700-704
    • /
    • 1993
  • The photocatalytic alanine and hydrogen production reaction were studied by using CdS as a semiconductor photocatalysts. The rate of alanine and hydrogen production depends strongly on the temperature in heat treatment of CdS powder. In particular, the rate of alanine production, which was observed using Pt/CdS(A)-(CdS from Mitsuwa), was increased about six times than that of using Pt/CdS(B)-(CdS from Furruchi) under the same heat treatment condition at 500$^{\circ}$C. And the photocatalytic activity for alanine production using bare CdS(A) or Pt/CdS(A) was almost same with increasing temperature in heat treatment in the range of 100-600$^{\circ}$C. From X-ray diffraction data and photoluminescence spectrum, we conclude that the crystal structure changes of CdS(A) or strong interaction at interface of Pt and CdS contribute to increasing the rate of alanine and hydrogen production reaction.

Al-7wt%Si-0.3wt%Mg 합금의 응고 및 미세조직에 미치는 Sr 첨가와 금형예열온도의 영향 (The Effect of Sr Addition and Mold Preheating Temperature on the Solidification and Microstructure of Al-7wt%Si-0.3wt%Mg Alloy)

  • 권일수;김경민;윤의박
    • 한국주조공학회지
    • /
    • 제17권6호
    • /
    • pp.608-614
    • /
    • 1997
  • The effect of mold preheating temperature on the microstructure such as grain size, eutectic silicon morphology was investigated for the Al-7wt%Si-0.3wt%Mg alloy. Microstructural variations have been characterized as a function of Sr addition and cooling rate during solidification. Microstructures were correlated with cooling rate, local solidification time and eutectic nucleation temperature, etc. In this study, Sr addition caused increase of local solidification time, undercooling and reduction of eutectic plateau temperature. In logarithmic scale, local solidification time was in inverse proportion to cooling rate. Eutectic nucleation temperature was in inverse proportion to cooling rate of logarithmic scale. Increasing the cooling rate refined dendrite arm spacing and eutectic silicon. Dendrite arm spacing was logarithmically in inverse proportion to cooling rate. Without modifier addition, eutectic silicon was modified at cooling rate of $7^{\circ}C/s$ or higher.