• 제목/요약/키워드: tape

검색결과 1,905건 처리시간 0.025초

와이어링 PVC 테이프 내구 수명 예측 (Prediction Method of Useful Life of PVC Tape for Wiring Harness)

  • 김성우;정원욱;박종구;안미정
    • 한국신뢰성학회지:신뢰성응용연구
    • /
    • 제7권4호
    • /
    • pp.163-172
    • /
    • 2007
  • Phenomenon, such as hardening, cracking or breaking etc.. of PVC tape for wiring harness by aging were detected on driven automobile in field. Hardening or cracking of PVC tape were confirmed decline of elongation by surrounding stress. The accelerated heat aging test was carried out applying temperature most important factor of aging, and then deduced an equation of useful life using arrhenius model. Prediction method of useful life of PVC tape was developed using miner rule calculating damage value by thermal energy classified temperature by matching deduced equation of useful life and measured temperature value on driven automobile in field.

  • PDF

Bi-2223 테이프의 사고전류 특성 (Fault Current Characteristics of a Bi-2223 Tape)

  • 류경우;최병주;차귀수
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제3권1호
    • /
    • pp.29-34
    • /
    • 2001
  • A Bi-2223 tape has been developed for low-field Power applications such as Power cables or transformers working at liquid nitrogen temperature For such applications it is required to understand fault current characteristics of the Bi-2223 tape. In this paper we report fault current characteristics using two types of samples, straight sample and pancake coil sample. It was found that the fault current characteristics of the Bi-2223 tape are independent of external fields and frequencies . However they depend on electrical insulations and fault durations strong1y Also it was shown that the fault current characteristics in the insulated straight sample are similar to those in the pancake sample with a conductor insulation. Finally. it was shown that the Pancake sample with a layer insulation has better characteristics than that with a conductor insulation fur fault currents.

  • PDF

고온초전도 선재의 극저온 열전도도 측정 및 특성평가 (Evaluation of thermal conductivity for High temperature superconductor tape at low temperature)

  • 김정호;장석헌;김규태;주진호;나완수;강형구;고태국
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2002년도 학술대회 논문집
    • /
    • pp.153-155
    • /
    • 2002
  • The thermal conductivity of Ag and Ag alloys at low temperature (10~110 K) were evaluated by direct measurement technique. It was observed that thermal conductivity decreased with increasing the content of alloying elements such as Mg and Cu. Thermal conductivity of pure Ag tape at 20 K was measured to be 2794 W/m$\cdot$K. On the other hand, the corresponding values of Ag/Al tape and Ag/Al/sus315L tape were 1235 and 352 W/m$\cdot$K, respectively, indicating 2 to 8 times lower than that of pure Ag tape.

  • PDF

BSCCO(2223) 다심선재의 초전도 접합공정 연구 (Fabrication of Superconductive Joining of Multi-filamentary BSCCO(2223) Tape)

  • 김규태;김정호;장석헌;주진호;나완수
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2002년도 학술대회 논문집
    • /
    • pp.111-113
    • /
    • 2002
  • We jointed BSCCO multi-filament tapes and evaluated their electrical properties. In the process, two superconductive-joint methods were used; the two multi-filament tapes were directly connected each other(MM joint), and were connected through the single-filament tape inserted between them(MSM joint). It was observed that critical current ratio and n value were 25-29% and 2.5-2.8 for MM jointed tape, and 34-53% and 3.7-4.2 for MSM Jointed tape, respectively. The higher electrical properties for MSM tape is considered to be due to that the presence of single core results in better interconnections of multi-filaments from the two tapes.

  • PDF

수계공정에 의한 알루미나 테이프로 제조한 세라믹 인공치관용 알루미나 유리 복합체의 기계적 물성 (Mechanical Properties of Alumina-Glass Dental Composites Prepared from Aqueous-Based Tape Casting)

  • 이명현;김대준;이득용;이정훈;김창은
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1123-1131
    • /
    • 1999
  • Alumina-glass composites which are considered as the material of the choice for all dental crown was prepared by aqeous-based tape casting and sintering for 2h at 1120$^{\circ}C$ followed by glass infiltration for 2h at 1100$^{\circ}C$ Biaxial strength and fracture toughness of the composites were evaluated to determine the optimum composition of the tape as a function of the amount of constituent such as alumina binder and plasticizer. The strength and the fracture toughness of the alumina tape increased with increasing the contents of alumina and binder. These observations are consistent with in fluence of the constituents on mean alumuna particle distance in tapes suggesting that high strength of the glass infiltrated alumina composites is related to toughening by crack bowing. The biaxial strength and the fracture toughness of the composite containing the optimum constituent composition were 523 MPa and 3.3 MPa$.$1/2 respectively.

  • PDF

Effects of Suspension Composition on Defects in Aqueous Tape Casting of Alumina Ceramics: A Rheological Study

  • Shin, Hyo-Soon
    • 한국세라믹학회지
    • /
    • 제42권1호
    • /
    • pp.1-6
    • /
    • 2005
  • In aqueous alumina tape casting, the effects of altering the composition of the suspensions, the binders and the casting thickness were studied. The rheological behavior of the suspensions and the defects of the dried tapes were examined and the relationships between them are discussed. The changes in the defect regions reported in the previous paper were related with the rheological properties with variations of the binder, the composition and the casting thickness. The shear thinning factor increased with the organic content and the solid content (the decrease of water content). The apparent viscosity increased with the shear thinning factor. The relation between the shear thinning factor and the log apparent viscosity was similar for all binder types. In the relation between the defect free region and the rheological properties, the defect free region became narrower with increasing casting thickness. The defect free region is independent of binder type. Therefore, the thicker tape is more difficult to produce in aqueous alumina tape casting. Knowledge of the rheological properties of the suspensions could help Predict the defect type and the possibility of defect free dried tapes.

Bi-2223초전도 선재의 접합공정 연구 (A study of joining method of BSCCO(2223) tape)

  • 김정호;김태우;주진호;서수정
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 1999년도 제1회 학술대회논문집(KIASC 1st conference 99)
    • /
    • pp.18-21
    • /
    • 1999
  • The effects of joining process such as contact method, shape of joined area and pressure on the properties of Bi-2223 superconducting tape have been optimized. In the process tapes were etched to expose the superconductor core in the shape of 'ㅁ' and 'ㄷ'. The exposed cores of the two tapes were brought into contact, uniaxially pressed and sintered. Subsequently, the current capacity of the joined tape was measured as a function of uniaxial pressure. It was observed that the current capacity was significantly dependent on uniaxial pressure. The joined tape, fabricated with a pressure of 1,600 MPa, showed the highest value of current capacity(90%) of highest value of current capacity is resulted from improvements in core density, contacting area and grain alignment, etc. In addition the effect of processing variables on microstructural evolution and mechanical property of joined tape will be presented.

  • PDF

줄자를 이용한 하지부피 측정시 부위별 검사자간, 검사자내 신뢰도 측정 (Intertester and Intratester Reliability of Tape Measurement on Lower Extremities)

  • 김성중;양회송;이충휘
    • 한국전문물리치료학회지
    • /
    • 제7권1호
    • /
    • pp.38-45
    • /
    • 2000
  • Tape measurement for evaluating edema is frequently used by clinicians. The primary purpose of this study is to determine the intertester and intratester reliability of tape measurement carried out by two physical therapists on lower extremities. The intertester and intratester reliability of six anatomical landmarks measurements were determined in six healthy subjects. The measurements were taken in five sessions by each tester. The intraclass correlation coefficients (2,1) were between .87 and .99 for intertester reliability. Intratester reliability was .93 and .99 for A tester and .82 and .99 for B tester. The average range of variation was .13 to .54 in six landmarks. The reliability of six volume measurements was very high. These results support the use tape measurement as a reliable tool for measuring limb girth.

  • PDF

초음파 분무를 이용한 세라믹 테이프의 성형 (fabrication of Ceramic Tape By Ultrasonic Spray)

  • 윤정한;박양수;심수만;이해원
    • 한국세라믹학회지
    • /
    • 제36권6호
    • /
    • pp.625-631
    • /
    • 1999
  • Ceramic tapes were fabricated by ultrasonically spraying slurries of monodispersed spherical and alumina powders. Effects of slurry compositions on tape forming were investigated. A relatively fast rate of solvent evaporation caused pores and cracks to be formed. A good chemical affinity between solvent and binder gave rise to binder separation resulting in inhomogeneous distribution of binder. Defect-free silica tapes with uniform distribution of particle packing and the binder were obtained from the solvent having a low chemical affinity and a slow evaporation rate and containing appropriate amounts of the binder and the plasticizer. Tape thickness could be controlled by adjusting solids loadings and slurry feed rates. It was possible to fabricate a tape in 15 $\mu\textrm{m}$ thickness from 7 vol% alumina slurry.

  • PDF

A Tape Feeder Inspection System for Measuring Feeding Accuracy

  • Cho, Tai-Hoon
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 2001년도 ICCAS
    • /
    • pp.98.4-98
    • /
    • 2001
  • A tape feeder of a SMD(Surface Mount Device) mounter is a device that sequentially feeds electronic components on a tape reel to the pick-up system of the mounter. As components are getting much smaller, feeding accuracy of a feeder becomes one of the most important factors for successful component pick-up. Therefore, it is critical to keep the feeding accuracy to a specified level in the assembly and production of tape feeders. This paper describes a tape feeder inspection system that was developed to automatically measure and inspect feeding accuracy using machine vision. It consists of a feeder base, an image acquisition system, and a personal computer. The image acquisition system is composed of CCD cameras with lens ...

  • PDF