• Title/Summary/Keyword: surface degradation

Search Result 1,509, Processing Time 0.029 seconds

Study on UV degradation in Polymeric Insulating Materials for Use in Outdoor Insulators by Corona-Charging (코로나 대전을 통한 옥외용 고분자 절연재료의 자외선 열화특성 연구)

  • Youn, Bok-Hee;An, Jong-Sik;Lee, Sang-Yong;Huh, Chang-Su
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.106-109
    • /
    • 2001
  • In this paper, we have investigated the degradation of shed materials of outdoor insulators by UV-radiation by using corona-charging and XPS analysis. The accumulated charges on polymeric surface having intrinsic hydrophobic property have a negative impact on retaining its hydrophobicity. Therefore, shorter decay times of surface charges are preferred. The surface voltage decay on UV-treated silicone rubber and EPDM show a different decay trend with UV treated time. From the XPS analysis, the oxidized groups of silica-like structure in silicone rubber increase with UV treatment time. For EPDM, the oxidized carbon groups of C=O, O=C-O increase as elapse of UV radiation time. These oxidized surface for each material have different electrostatic characteristics, so deposited charges may be expected to have different impacts on their surface hydrophobicity. The degradation mechanism based on our results is discussed.

  • PDF

Control of Enzymatic Degradability of Biodegradable Polylactide by Blending with Non-degradable Polymers (비 분해성고분자와 블렌드를 이용한 생분해성 폴리유산의 효소분해속도 조절)

  • Jang, Seong-Ho;Park, Sang-Bo;Lee, Won-Ki
    • Journal of Environmental Science International
    • /
    • v.19 no.9
    • /
    • pp.1161-1167
    • /
    • 2010
  • The effects of addition of non degradable polymers, polystyrene (PS) and poly(methyl methacrylate) (PMMA) on the rate of enzymatic degradation of biodegradable poly(l-lactide) (PLLA) have been studied in term of surface structure. Since a component in multicomponent polymeric system has shown surface enrichment, PS and PMMA which have lower surface energy than PLLA were selected as a minor blend component (5 wt%). Enzymatic degradation was carried out at $37^{\circ}C$ and pH 8.5 in the aqueous solution of Proteinase K. Two blend systems, partially miscible (PS/PLLA) and immiscible (PMMA/PLLA), showed the surface enrichment of 4 and 2 times of PS and PMMA, respectively. From the weight loss profile data, the slow degradation rate of both blend films was observed. This indicates that PS or PMMA domains which exist at surface act as a retardant of enzymatic attack.

Tracking Resistance of Epoxy Mold Insulating Materials by the Rotating Wheel Dip Test (회전윤법에 의한 에폭시 몰드 절연재료의 내트래킹성 평가)

  • Cho, Han-Goo;Yun, Mun-Su;Park, Yang-Kwan
    • Proceedings of the KIEE Conference
    • /
    • 2000.07c
    • /
    • pp.1590-1592
    • /
    • 2000
  • The time to tracking breakdown of treated filled specimen is longer than untreated filled specimen. And, after the RWDT, the surface of specimen by adding untreated filler appeared heavy erosion. It was found that the addition to surface treated filler. the better tracking resistance. In the RWDT, the breakdown specimen is not affected by the dry flashover voltage. despite the fact that the surface degradation of tracking test has different state on each specimen. This suggests that wet flashover voltage play an important role in evaluating of tracking and erosion on the surface degradation in tracking test. And, the flashover voltage of specimen under wet conditions are greatly affected by the salt concentration and degree of degradation by the RWDT. Because of hydrophobicity and degree of degradation by the RWDT, the flashover voltage of treated filled specimen is higher than that of untreated filled specimen. Different types of specimen may have different hydrophobicity and their surface state under contaminated conditions may not be the same. It is assumed that this phenomenon is related to the decrease in hydrophobicity of the surface of the materials.

  • PDF

Photoelectrocatalytic Degradation of Dyes in Aqueous Solution Using CNT/TiO2 Electrode

  • Zhang, Feng-Jun;Liu, Jin;Chen, Ming-Liang;Oh, Won-Chun
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.3
    • /
    • pp.263-270
    • /
    • 2009
  • The effect of photoelectrocatalytic (PEC) degradation for different dyes with the CNT/$TiO_2$ electrode was studied. The prepared electrode was characterized with surface properties, structural crystallinity, elemental identification, and PEC activity. The $N_2$ adsorption data showed that the composites had decreased surface area compared with the pristine CNT. This indicated the blocking of micropores on the surface of CNT, which was further supported by observation via FESEM. XRD patterns of the composites showed that the CNT/$TiO_2$ composite contained a mixing anatase and rutile phase. EDX spectra showed the presence of C, O and Ti peaks for all samples. The decomposition efifciency of the prepared electrode was evaluated by the PEC degradation of three dyes (methylene blue (MB), rhodamine B (RH.B), methyl orange (MO)). The variations of the FT-IR spectra and pH value of dye solutions were measured during the PEC system; it was found that the CNT/$TiO_2$ electrode has better PEC degradation for MB solution than that of RH.B and MO. The proposed degradation mechanism was present.

Degradation Behavior of 850 nm AlGaAs/GaAs Oxide VCSELs Suffered from Electrostatic Discharge

  • Kim, Tae-Yong;Kim, Tae-Ki;Kim, Sang-In;Kim, Sang-Bae
    • ETRI Journal
    • /
    • v.30 no.6
    • /
    • pp.833-843
    • /
    • 2008
  • The effect of forward and reverse electrostatic discharge (ESD) on the electro-optical characteristics of oxide vertical-cavity surface-emitting lasers is investigated using a human body model for the purpose of understanding degradation behavior. Forward ESD-induced degradation is complicated, showing three degradation phases depending on ESD voltage, while reverse ESD-induced degradation is relatively simple, exhibiting two phases of degradation divided by a sudden distinctive change in electro-optical characteristics. We demonstrate that the increase in the threshold current is mainly due to the increase in leakage current, nonradiative recombination current, and optical loss. The decrease in the slope efficiency is mainly due to the increase in optical loss.

  • PDF

A Study on Degradation Characteristic and Flow Behavior in De-NOx Catalyst (탈질촉매 내 열화특성과 유동상태에 관한 연구)

  • Hwang, Seung-Min
    • Journal of Environmental Science International
    • /
    • v.19 no.9
    • /
    • pp.1093-1101
    • /
    • 2010
  • In this study, the indirect correlation of degradation characteristic and flow behavior in the de-NOx catalyst is investigated experimentally. The inner flow behavior in the de-NOx catalyst is varied from turbulent flow to laminar flow and the degradation of the de-NOx catalyst is remarkably affected by the inner flow. The degradation of the catalyst is increased in the upstream region near the inlet because injected turbulent flow enhances the adhesion of ash particle on the catalyst surface. The degradation of the catalyst near the inlet also governs the overall efficiency of the catalyst. The amount of adhered ash particles on the catalyst surface decreases as they progress downstream. This is due to the inner flow transition from turbulent flow to laminar flow.

Surface Analysis Techniques for Studying Optical Degradation of Solar Coatings (태양에너지 박막의 광퇴화 연구를 위한 표면분석)

  • Lee, Kil-Dong
    • Journal of the Korean Solar Energy Society
    • /
    • v.29 no.2
    • /
    • pp.55-61
    • /
    • 2009
  • This paper reviews the state-of-the art in surface analysis techniques for solar coatings. For analyzing solar coatings and interfaces, surface properties were very important factor for obtaining the information related to the optical degradation processes and microstructure. Various types of analytical techniques for chemical composition, microstructure and surface topography analysis of solar coatings were discussed. In addition, the examples of solar selective coating analysis results for applications were demonstrated. Development and analysis technique of solar coating for energy conservation was felt to be necessary at this time.

The Application of IRR-Camera for the Diagnosis of Surface Degradation (표면열화진단을 위한 적외선카메라의 응용)

  • Lim, Jang-Seob;Jeong, Seung-Chun;Lee, Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05a
    • /
    • pp.61-65
    • /
    • 2001
  • The conventional tracking testing as IEC-60587 is widely used in surface aging measurement of outdoor insulator because those testing can carry out very short time in Lab-testing. Also IEC-60587 testing is able to offer the standard judgement of relative degradation level of outdoor HV machine/system. Therefore it is very useful method compare to previous conventional tracking testing method and effective Lab-testing method. But surface discharges(SD) have very complex characteristics of discharge pattern so it is required estimation research to development of precise analysis method. In recent, the study of IRR-camera is carrying out discover of temperature of power equipment through condition diagnosis and system development of degradation diagnosis. In this study, SD occurred from procelain insulator, used 22.9[KV] distribution, is measured with partial temperature distribution in real time, the degradation grade of SD is analyzed through produced patterns in SD concentration according to applied time.

  • PDF

Mechanism of Enzymatic Degradation of Poly(butylene succinate)

  • Lee, Chan-Woo;Kimura, Yoshiharu;Chung, Jin-Do
    • Macromolecular Research
    • /
    • v.16 no.7
    • /
    • pp.651-658
    • /
    • 2008
  • Poly(butylene succiate) (PBS), poly(butylene succinate-co-L-lactate) (PBSL), and poly(butylene succinate-co-6-hydroxycaproate) (PBSCL) polymers were degraded by lipase $PS^{(R)}$, and the enzymatic degradation mechanism of PBS was analyzed in detail. The enzymatic degradation of PBS gave 4-hydroxybutyl succinate (4HBS) as the main product. An exo-type hydrolysis mechanism was proposed based on this observation. The terminal chain of PBS had conformational similarity to ordinary tri- and diglycerides and could be incorporated as a substrate in the active site of this lipase. The surface adsorption of the lipase was much larger on PBS and its copolymer films than on the other polyester films because the lipase adhered quite strongly to the polymer terminal through a specific adsorption mechanism. Kinetic analysis showed that the total number of surface adsorption points per unit area of PBSL and PBSCL copolymers was larger than that of the PBS homopolymer.

Degradation characteristics of the FRP material for using as a PCB substrate (PCB 기판용 FRP 재료의 열화특성)

  • Park Jong Kwan
    • Journal of the Institute of Electronics Engineers of Korea SD
    • /
    • v.41 no.12
    • /
    • pp.1-6
    • /
    • 2004
  • In this study, heat and discharge treatments are arbitrary simulated for finding out the initiations and processes of surface degradation on the surface of polymer for using as a PCB substrate. Thermal-treatment changed the surface to the hydrophobic one with the increase of contact angle and surface potential decay, respectively. The XPS spectrum showed that the increased hydrophobicity in thermal treatment was originated from the continuous decrease of side-chains caused by secessions of oxygen groups and the increase of unsaturated double bond in carbon chains. Also, thermal-treatment caused the discoloration on the point of treated surface. These phenomena were attributed to the generation of ether group. In the chemical change by discharge treatment, a lot of side-chains occurred on the treated surface, and so the hydrophilicity increased as time elapsed.