  • Phosphorus is an essential and irreplaceable element for all living organisms and its resource is limited. Significant amount of used phosphorus is collected in sewage treatment plant as sludge. Sludge ash after incineration contains about 10% of phosphorus in dry mass basis, which is comparable to phosphate rocks, and it is an important source of phosphorus recovery. Acid and alkali were used to leach phosphorus from sludge ash and compared for their leaching kinetics and performance. Phosphorus leaching by NaOH was fast and 0.2 N and 2 N NaOH leached 49% and 56% of the total phosphorus in the sludge ash at the L/S ratio of 100. Phosphorus leaching by sulphuric acid and hydrochloric were very fast and most of the phosphorus was leached in 5 minutes. In case of sulphuric acid 95% of the total phosphorus in the sludge ash was leached by 0.2 N at the L/S ratio of 100 and 93% was leached by 1 N at the L/S ratio of 10. 1 N hydrochloric acid leached 99% of the total phosphorus at the L/S ratio of 10. The results showed acids were more effective than alkali for phosphorus leaching from sludge ash and hydrochloric acid leached more phosphorus than sulphuric acid.

탈황(脫黃) 폐촉매(廢觸媒)로부터 유가금속(有價金屬) 추출(抽出) (Extraction of Valuable Metals from Spent Desulfurizing Catalyst)

  • ;김동진;백승배;이성원
    • 자원리싸이클링
    • /
    • 제20권3호
    • /
    • pp.48-54
    • /
    • 2011
  • 황산으로 탈황 폐촉매를 침출한 결과 황산농도 1 M, 반응시간 1 hr인 실험조건에서 Ni 및 V은 95% 이상, 그리고 Mo은 30%가 침출되었다. 탈황 폐촉매의 Mo matrix 특성으로 인하여 다른 금속에 비하여 Mo의 침출율이 낮았으며, 본 침출반응은 확산반응에 의하여 제어되는 것으로 판단된다. Mo을 완전히 침출하기 위하여 유황성분이 제거된 폐촉매로 침출실험을 실시하였다. 1M 황산으로 처리후 탄산나트륨으로 세척시 Ni, Mo 그리고 V의 침출율은 99% 이었다. Ni 2 g/L; V 9 g/L, Mo 0.6 g/L 조성의 침출액을 LIX 841로 용매추출한 조건에서 A:O 비 5:2, 2단계로 처리시 Mo은 98% 이상 추출되었으며 A:O 비 5:3, 2단계로 처리시 V은 82%가 추출되었다.

소다배소 처리된 탈질 폐촉매로부터 황산침출과 가수분해 침전반응에 의한 TiO2의 회수 (Titanium Dioxide Recovery from Soda-roasted Spent SCR Catalysts through Sulphuric Acid Leaching and Hydrolysis Precipitation)

  • 김승현;친빅하;이재령
    • 자원리싸이클링
    • /
    • 제29권5호
    • /
    • pp.48-54
    • /
    • 2020
  • 소다배소 처리한 탈질폐촉매의 수침출 잔사로부터 TiO2 회수를 위하여 황산침출과 가수분해 반응을 실시하였다. Ti 성분의 황산침출은 70 ℃, 3 시간, 교반속도 500 rpm, 슬러리 농도 100 g/L로 고정하여 실시하였고, 황산농도는 4~8 M로 변화시키며 진행하였다. 침출액으로부터 Ti 성분의 침전회수는 가수분해반응을 이용하였으며, 실험조건은 100 ℃, 반응시간 2 시간으로 고정하였고, Ti 성분의 침전율은 침출액과 증류수의 혼합비와 침전반응 Seed 혼입유무에 따라 비교하였다. Ti의 침출율은 6 M에서 최대 95.2 %까지 도달 후 점차 감소하는 경향을 나타내었고, Si의 침출율은 황산농도 증가에 반비례하여 급격히 감소하여 91.7 %에서 8 M 조건에서는 3.0 %까지 억제되었다. 침출액을 이용한 가수분해는 부성분인 Si의 함량이 가장 낮은 8 M 침출액을 이용하여 진행하였다. 침출액의 혼합비에 의한 Ti의 침전회수율은 반응시간에 비례하였고 혼합비에 반비례하였다. 또한, 침전반응의 가속화를 위해 TiO2(#325~#400 mesh, 0.2 g) seed를 첨가하였을 경우에 모든 혼합조건에서 침전회수율이 상승하였으며, 혼합비(침출액:증류수) 1:9~3:7 구간에서 98.8~99.8 %의 침전율이 달성되었다. 회수된 TiO2의 순도는 침출액 혼합비 1:9~3:7 구간에서 혼합비가 낮을수록 증가하여 최대 99.46 %까지 상승함을 확인하였다.

Temperature and leaching effects of zeolite-X derived from kaolin

  • Henry E. Mgbemere;Henry Ovri;Anna-Lisa Sargent
    • Advances in materials Research
    • /
    • 제13권2호
    • /
    • pp.103-114
    • /
    • 2024
  • Zeolites are microporous materials that find applications in different fields due to their numerous interesting properties. This research investigated the effect of leaching on unheated Ifon kaolin in dilute hydrochloric acid and sulphuric acid. The hydrothermal method synthesized zeolite-X type, and the resulting sample was characterized using different techniques. The silica/alumina ratio in the synthesized sample was approximately 5.6, while Infrared spectra confirmed that the synthesized material was Zeolite-X. Based on the X-ray diffraction patterns, other phases were also formed in addition to zeolite-X crystals. Thermogravimetry results indicated that the synthesized zeolite was relatively stable below 500℃, so its weight loss was only 13% after heating to about 200℃. A differential thermal analyzer confirmed this amount of weight loss, and endothermic and exothermic reactions were also observed for the samples calcined respectively at 700 and 900℃. Based on Brunauer-Emmett-Teller (BET) analyses, samples at 700℃ showed slower adsorption-desorption isotherms, pore volume, and sizes than those at 900℃. These results have shown that leaching and calcination temperature significantly affect the type of zeolite produced.

Rare earths from secondary sources: profitability study

  • Innocenzi, Valentina;De Michelis, Ida;Ferella, Francesco;Veglio, Francesco
    • Advances in environmental research
    • /
    • 제5권2호
    • /
    • pp.125-140
    • /
    • 2016
  • The paper is focused on the economic analysis of two hydrometallurgical processes for recovery of yttrium and other rare earth elements (REEs) from fluorescent phosphors of spent lamps. The first process includes leaching with sulphuric acid and precipitation of a mixture of oxalates by oxalic acid, the second one includes leaching with sulphuric acid, solvent extraction with D2EHPA, stripping by acid and recovery of yttrium and traces of other rare earths (REs) by precipitation with oxalic acid. In both cases the REEs were recovered as oxides by calcination of the oxalate salts. The economic analysis was estimated considering the real capacity of the HydroWEEE mobile's plant ($420kg\;batch^{-1}$). For the first flow-sheet the cost of recycling comes to $4.0{\euro}kg^{-1}$, while the revenue from the end-product is around $5.40{\euro}kg^{-1}$. The second process is not profitable, as well as the first one, taking into account the composition of the final oxides: the cost of recycling comes to $5.2{\euro}kg^{-1}$, while the revenue from the end-product is around $3.56{\euro}kg^{-1}$. The process becomes profitable if the final RE oxide mixture is sold for nearly $50{\euro}kg^{-1}$, a value rather far from the current market prices but not so unlikely since could be achieved in the incoming years, considering the significant fluctuations of the Res' market.

Studies on the Bituminization Process of Radioactive Liquid Waste[I]

  • Lee, Sang-Hoon;Chun, Kwan-Sik;Lim, Eung-Keuk
    • Nuclear Engineering and Technology
    • /
    • 제7권3호
    • /
    • pp.213-222
    • /
    • 1975
  • 알카리로 처리한 국산 blown asphalt를 사용해서 방사성 폐액을 180-20$0^{\circ}C$ 범위 내에서 고화처리한 것이 산처리 한것보다 좋은 결과를 얻었으며, 방사선 조사선량이 4.0$\times$$10^{7}$ rad까지도 안정된 고화체로 존재하고 있다. 한편 40wt%의 고형분이 함유되어 있는 $^{137}$Cs-asphalt 고화체의 증류수에 의한 $^{137}$Cs의 용출율이 8.27$\times$$10^{-4}$ g/$\textrm{cm}^2$-day 인데 반하여 $^{90}$ Sr은 낮았으며, 일반적으로 증류수보다 해수때가 또한 pH가 증가함에 따라 용출율은 낮아진다.

  • PDF

인공 산성 빗물로 인한 잎으로부터의 양이온 이론

  • 류태선;김준호
    • The Korean Journal of Ecology
    • /
    • 제16권4호
    • /
    • pp.409-416
    • /
    • 1993
  • 인공산성빗물에 대두(Glycine max), 청갈참 (Quercus aliena var. pellucida) 및 리기다소나무(Pinus rigida)에 살포한 후 연속적으로 일정량을 받아서 이온량을 정량하였다. 모든 잎에서 세탈된 이온의 양은 초기에 많았으나 시간이 지날수록 감소하였으며, 세탈되는 이온량은 빗물의 pH가 낮을수록 세탈되는 이온량은 많았다. 총 세탈된 K의 양은 정상빗물(pH5.6) 보다 pH 4.0의 빗물에서1.04~1.46배, pH 3.5의 빗물에서 1.09~1.58배, 그리고 pH 3.0의 빗물에서 1.24~2.03배 만큼 많았다. 총 세탈된 Ca량은 정상빗물보다 ph 4.0의 빗물에서 1.23~1.47배, pH 3.5 빗물에서 1.50~1.92배, 그리고 pH3.0의 빗물에서 2.45~3.30배 만큼 많았다. 총 세탈액 속의 Ca/K의 비는 청갈참에서 1.10~2.91, 리기다소나무에서 1.68~2.98, 그리고 대두에서 0.66~0.91이었다. 조사된 모든 식물에서 빗물의 pH가 낮아질수록 Ca/K 비율이 커졌다. 산성빗물처리 후의 식물체를 분석한 결과 이온세탈 효과는 pH3.0 처리구에서만 유일하게 나타났다.

  • PDF

생물학적(生物學的) 방법(方法)에 의한 폐기물(廢棄物)의 재활용(再活用) (Waste Recycling Through Biological Route)

  • ;김동진;안종관;박경호;이승원
    • 자원리싸이클링
    • /
    • 제17권2호
    • /
    • pp.3-15
    • /
    • 2008
  • 다양한 독성 폐기물이 주변 환경에 배출되면 궁극적으로 모든 생명체의 생존에 위협이 된다. 박테리아 및 곰팡이종의 반응을 이용한 미생물침출 및 미생물복원을 포함하는 바이오 습식제련은 환경문제를 극복하는데 적합한 경제성이 있는 잠재기술이다. 미생물침출은 Thiobacillus ferrooxidans, Thiobacillus thiooxidans, Laptospirillum ferrooxidans와 같이 금속과 반응을 일으키는 박테리아를 이용하여 다양한 광물 및 폐기물로부터 금속 성분을 용해하는 것을 말한다. 일반적으로 미생물 침출반응은 직접 및 간접반응으로 나누어진다. 직접반응에서 박테리아는 성장 및 물질대사를 위하여 침출 기질로부터 전자를 받아 황산을 생산하므로써 황화광물을 산화시킨다. 반면 간접반응에서는 철산화 박테리아에 의해 생성된 $Fe^{3+}$가 황화광물을 산화시킨다. 이러한 침출기구를 통하여 저품위 광물 및 정광, 슬러지, 광미, 플라이 애쉬, 슬래그, 전자 스크랩, 폐밧데리 및 폐촉매 등으로부터 금속을 회수할 수 있다. 생물학적 방법은 폐기물의 매립을 극복할 수 있는 대체기술로서 건강하고 깨끗한 환경 보존에 기여할 수 있다.