• Title/Summary/Keyword: strontium doping

Search Result 18, Processing Time 0.024 seconds

Effect of Strontium Doped Porous BCP as Bone Graft Substitutes on Osteoblast (스트론튬(Strontium)이 도핑된 다공성 BCP 뼈 이식제가 조골세포에 미치는 영향)

  • Byun, In-Seon;Sarkar, Swapan Kumar;Seo, Hyung-Seok;Lee, Byong-Taek;Song, Ho-Yeon
    • Korean Journal of Materials Research
    • /
    • v.20 no.3
    • /
    • pp.155-160
    • /
    • 2010
  • In this study, we investigated primary biocompatibility and osteogenic gene expression of porous granular BCP bone substitutes with or without strontium (Sr) doping. In vitro biocompatibility was investigated on fibroblasts like L929 cells and osteoblasts like MG-63 cells using a cell viability assay (MTT) and one cell morphological observation by SEM, respectively. MTT results showed a cell viability percent of L929 fibroblasts, which was higher in Sr-BCP granules (98-101%) than in the non-doped granules (92-96%, p < 0.05). Osteoblasts like MG-63 cells were also found to proliferate better on Sr-doped BCP granules (01-111%) than on the non-doped ones (92-99%, p < 0.05) using an MTT assay. As compared with pure BCP granules, SEM images of MG-63 cells grown on sample surfaces confirmed that cellular spreading, adhesion and proliferation were facilitated by Sr doping on BCP. Active filopodial growth of MG-63 cells was also observed on Sr-doped BCP granules. The cells on Sr-doped BCP granules were well attached and spread out. Gene expression of osteonectin, osteopontin and osteoprotegrin were also evaluated using reverse transcriptase polymerase chain reaction (RT-PCR), which showed that the mRNA phenotypes of these genes were well maintained and expressed in Sr-doped BCP granules. These results suggest that Sr doping in a porous BCP granule can potentially enhance the biocompatibility and bone ingrowth capability of BCP biomaterials.

Effects of Sr Contents on Structural Change and Electrical Conductivity in Cu-doped LSM ($La_{1-x}Sr_xMn_{0.8}Cu_{0.2}O_{3{\pm}{\delta}}$)

  • Ryu, Ji-Seung;No, Tae-Min;Kim, Jin-Seong;Jeong, Cheol-Won;Lee, Hui-Su
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.10a
    • /
    • pp.33.1-33.1
    • /
    • 2011
  • Strontium doped lanthanum manganite (LSM) with perovskite structure for SOFC cathode material shows high electrical conductivity and good chemical stability, whereas the electrical conductivity at intermediate temperature below $800^{\circ}C$ is not sufficient due to low oxygen ion conductivity. The approach to improve electrical conductivity is to make more oxygen vacancies by substituting alkaline earths (such as Ca, Sr and Ba) for La and/or a transition metal (such as Fe, Co and Cu) for Mn. Among various cathode materials, $LaSrMnCuO_3$ has recently been suggested as the potential cathode materials for solid oxide fuel cells (SOFCs). As for the Cu doping at the B-site, it has been reported that the valence change of Mn ions is occurred by substituting Cu ions and it leads to formation of oxygen vacancies. The electrical conductivity is also affected by doping element at the A-site and the co-doping effect between A-site and B-site should be described. In this study, the $La_{1-x}Sr_xMn_{0.8}Cu_{0.2}O_{3{\pm}{\delta}}$ ($0{\leq}x{\leq}0.4$) systems were synthesized by a combined EDTA-citrate complexing process. The crystal structure, morphology, thermal expansion and electrical conductivity with different Sr contents were studied and their co-doping effects were also investigated.

  • PDF

M-Zn (M = Sb, V, and Nb) Substituted Strontium Hexaferrites with Enhanced Saturation Magnetization for Permanent Magnet Applications

  • Sapoletova, Nina;Kushnir, Sergey;Ahn, Kyunghan;An, Sung Yong;Choi, Moonhee;Kim, Jae Yeong;Choi, Changhak;Wi, Sungkwon
    • Journal of Magnetics
    • /
    • v.21 no.3
    • /
    • pp.315-321
    • /
    • 2016
  • M-Zn (M = Sb, V, Nb) substituted M-type strontium hexaferrites were prepared by a ceramic method. The phase composition, morphology and magnetic properties were studied by x-ray diffractometry, scanning electron microscopy and vibrating sample magnetometry. Saturation magnetization increases with a substitution up to 75.0 emu/g (2.5 % higher compared to unsubstituted hexaferrite) and then decreases with a further substitution. A coercive field of substituted hexaferrite powders with highest saturation magnetization is more than 3 kOe. Substituted strontium hexaferrite powders prepared in this work are a rare example of high $M_S$ compositions without doping rare-earth elements and would be a promising candidate for a permanent magnet application.

Sintering Behavior and Electrical Properties of Strontium Titanate-Based Ceramic Interconnect Materials for Solid Oxide Fuel Cells (고체산화물 연료전지용 Strontium Titanate 세라믹 접속자 소재의 소결 거동 및 전기적 특성)

  • Park, Beom-Kyeong;Lee, Jong-Won;Lee, Seung-Bok;Lim, Tak-Hyoung;Park, Seok-Joo;Song, Rak-Hyun;Shin, Dong-Ryul
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2010.11a
    • /
    • pp.80.1-80.1
    • /
    • 2010
  • A strontium titanate ($SrTiO_3$)-based material with a perovskite structure is considered to be one of the promising alternatives to $LaCrO_3$-based materials since $SrTiO_3$ perovskite shows a high chemical stability under both oxidizing and reducing atmospheres at high temperatures. $SrTiO_3$ materials exhibit an n-type semiconducting behavior when it is donor-doped and/or exposed to a reducing atmosphere. In this work, $Sr_{1-x}La_xTi_{1-y}M_yO_3$ materials doped with $La^{3+}$ in A-sites and aliovalent transition metal ions ($M^{n+}$) in B-sites were synthesized by the modified Pechini method. The X-ray diffraction analysis indicated that the materials synthesized by the Pechini process exhibited a single curbic perovskite-type structure without any impurity phases, and are tolerant, to some extent, to cation doping. The sintering behaviors of $Sr_{1-x}La_xTi_{1-y}M_yO_3$ in $H_2/N_2$ and air were characterized by dilatometry and microstructural observations. The electrical conduction mechanism and the dopant effect are discussed based on the defect structures and the electrical conductivities measured at various oxygen partial pressures and temperatures.

  • PDF

Dielectric properties of $BaTiO_3$ system Ceramics Doped with $Al_{2}O_{3}$ ($BaTiO_3$계 세라믹의 $Al_{2}O_{3}$ 첨가에 따른 유전 특성)

  • Heo, Young-Sik;Lee, Won-Sub;Lee, Sung-Gap
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.402-405
    • /
    • 2001
  • $(Ba_{0.6-x}Sr_{0.4}Ca_{x})TiO_{3}$ (x=0.10, 0.15, 0.20) ceramics were fabricated by the mixed-oxide method and their stuctural and dielectric properties were investigated with variation of composition ratio and an amount of $Al_{2}O_{3}$ (0.5, 1.0, 1.5. 2.0, 3.0 wt%) doping content. As a result of the X-ray diffraction BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with increase an $Al_{2}O_{3}$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing an amount of $Al_{2}O_{3}$ doping content. The dielectric loss is minimum for BSCT doped with 1.5wt% $Al_{2}O_{3}$ content. The tunability was decreased with increasing an Ca content and is about 4.2% for BSCT(50/40/10) doped with 2.0wt% $Al_{2}O_{3}$ content.

  • PDF

Dielectric Properties of $Al_2O_3-Doped\; (Ba, Sr, Ca)TiO_3$ Ceramics for Phased Array Antenna (위상배열 안테나용 $Al_2O_3가\; 첨가된\; (Ba, Sr, Ca)TiO_3$ 세라믹의 유전적 특성)

  • Lee, Seong-Gap;Lee, Yeong-Hui
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.11
    • /
    • pp.550-554
    • /
    • 2001
  • $(Ba_{0.6}Sr_{0.4}Ca_x)TiO_3 + yAl_2O_3$ wt% (x=0.10, 0.15, 0.20, y=0~3.0) ceramics were fabricated by the mixed-oxide method, and their structural and dielectric properties were investigated with variation of composition ratio and $Al_2O_3$ doping content. As results of the X-ray diffraction and microstructure analysis, all BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with an increase of $Al_2O_3$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing $Al_2O_3$doping content. The dielectric loss is minimum at BSCT doped with 1.5wt% $Al_2O_3$content. The tunability was decreased with increasing an Ca content and the BSCT(50/40/10) specimen doped with 2.0wt% $Al_2O_3$content showed the maximum value of 4.2%.

  • PDF

Dielectric properties of BaTiO$_3$ system Ceramics Doped with $Al_2$O$_3$ (BaTiO$_3$계 세라믹의 $Al_2$O$_3$ 첨가에 따른 유전 특성)

  • 허영식;이원섭;이성갑
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.402-405
    • /
    • 2001
  • (Ba$\_$0.6-x/Sr$\_$0.4/Ca$\_$x/)TiO$_3$(x=0.10, 0.15, 0.20) ceramics were fabricated by the mixed-oxide method and their structural and dielectric properties were investigated with variation of composition ratio and an amount of Al$_2$O$_3$(0.5, 1.0, 1.5, 2.0, 3.0 wt%) doping content. As a result of the X-ray diffraction BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with increase an Al$_2$O$_3$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing an amount of Al$_2$O$_3$ doping content. The dielectric loss is minimum for BSCT doped with 1.5wt% Al$_2$O$_3$ content. The tunability was decreased with increasing an Ca content and is about 4.2% for BSCT(50/40/10) doped with 2.0wt% Al$_2$O$_3$ content.

  • PDF

Electrochemical Performance of a Nd2-xSrxNiO4+δ/GDC(x = 0, 0.4, 0.6) as a SOFC Cathode Material (Nd2-xSrxNiO4+δ/GDC(x = 0, 0.4, 0.6) 공기극의 전기화학특성 평가)

  • Lee, Kyoung-Jin;Seo, Jeong-Uk;Lim, Ye-Sol;Hwang, Hae-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.1
    • /
    • pp.51-56
    • /
    • 2014
  • Mixed ionic and electronic conducting $K_2NiF_4$-type oxide, $Nd_{2-x}Sr_xNiO_{4+\delta}$ (x = 0, 0.4, 0.6) powders were synthesized by a solid-state reaction technique and solid oxide fuel cells consisting of a $Nd_{2-x}Sr_xNiO_{4+\delta}-GDC$ cathode, a Ni-YSZ anode and 8YSZ as an electrolyte were fabricated. The effect of strontium substitution for neodymium on the electrical and electrochemical properties was examined. The electrical conductivity increased with an increase in the Sr doping content, while it appears that the excess oxygen (${\delta}$) decreased. Sr doping into $Nd_2NiO_{4+\delta}$ resulted in an increase in the cathode polarization resistance and an decrease in the power density of the cell. These phenomena may be associated with the decreased amount of excess oxygen noted in the $Nd_{2-x}Sr_xNiO_{4+\delta}$ cathode.

Nb doped strontium titanate single crystal growth by floating zone method (Floating zone법에 의한 Nb를 첨가한 strontium titanate 단결정 성장)

  • Jeon, Byong-Sik;Cho, Hyun;Orr, Keun-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.5 no.3
    • /
    • pp.215-222
    • /
    • 1995
  • Nb doped strontium titanate single crystals were grown by the floating zone method. The doping amount of $Nb_2O_5$ was 0.2 wt %. Those crystals were grown in air and N z atmosphere and the growth rate was 5 mmlhr and rotation speed of upper and lower shaft was 30 rpm. The shapes of melt - feed rod interface depending on sintering temperatures were observed. In air atmosphere, the flow rate of air was 1.5 ${\ell}/min$ and in $N_2$ atmosphere, that of $N_2$ gas was 0.5 ${\ell}/min$. As grown crystals were analyseQ by XRD, Laue back - reflection and chemical etching. After annealing in $N_2$ atmosphere, resistivities of crystals were measured and the activation energies of each samples were calculated.

  • PDF