Fractionation and Pollution Index of Heavy Metals in the Sangdong Tungsten Mine Tailings (광미에 존재하는 중금속의 분획화와 오염도 평가)

  • Yang, Jae-E.;Kim, Hee-Joung;Jun, Sang-Ho
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.34 no.1
    • /
    • pp.33-41
    • /
    • 2001
  • Enormous volumes of mining wastes from the abandoned and closed mines are disposed without a proper treatment in the upper Okdong River basin at Southeastern part of Kangwon Province. Erosion of these wastes contaminates soil, surface water, and sediments with heavy metals. Objectives of this research were to fractionate heavy metals in the mine tailing stored in the Sangdong Tungsten tailing dams and to assess the potential pollution index of each metal fraction. Tailing samples were collected from tailing dams at different depth and analyzed for physical and chemical properties. pH of tailings ranged from 7.3 to 7.9. Contents of total N and organic matter were in the ranges of 3.2~5.5%, and 1.3~9.1%, respectively. Heavy metals in the tailings were higher in the newly constructed tailing dam than those in the old dam. Total concentrations of metals in the tailings were in the orders of Zn > Cu > Pb > Ni > Cd, exceeded the corrective action level of the Soil Environment Conservation Law and higher than the natural abundance levels reported from uncontaminated soils. Relative distribution of heavy metal fractions was residual > organic > reducible > carbonate > adsorbed, reversing the degree of metal bioavailability. Mobile fractions of metals were relatively small compared to the total concentrations. Distribution of metals in the tailing dam profiles was metal specific. Concentrations of Cu at the surface of tailing dams were higher than those at the bottom. Pollution index (PI) values of each fraction of metals were ranged from 4.27 to 8.51 based on total concentrations. PI values of mobile fractions were lower than those of immobile fractions. Results on metal fractions and PI values of the tailing samples indicate that tailing samples were contaminated with heavy metals and had potential to cause a detrimental effects on soil and water environment in the lower part of the stream. A prompt countermeasure to prevent surface of tailings in the dams from water and wind erosions is urgently needed.

  • PDF

An in vitro study of a few crystal growth solutions on the bracket shear bond strength (수종의 실험 결정형성용액에 의한 브라켓 전단결합강도의 비교)

  • Jeon, Yun-Ok;Lee, Ki-Soo
    • The korean journal of orthodontics
    • /
    • v.29 no.5 s.76
    • /
    • pp.613-625
    • /
    • 1999
  • The purpose of this study was to compare the bracket shear bond strengths of the crystal growth solutions with those of the $37\%$ phosphric acid etch technique. The 4 crystal growth solutions were made experimentally in the lab, that is, (1) $30\%$ polyacrylic acid solution containing 0.3 M sulfuric acid (ES 1), (2) $30\%$ polyacrylic acid solution containing 0.6M sulfuric acid (ES 2), (3) $30\%$ polyacrylic acid solution containing 0.3 M sulfuric acid and 0.6 M lithium sulfate(ES 3), and (4) $30\%$ polyacrlic acid solution containing 0.3 M sulfuric acid and $5\%$ phosphoric acid(ES4). The $37\%$ phosphoric acid solution used as a control. Bovine lower incisor tooth enamel was treated by the above solutions for 60 sec, washed out for 20 sec with slow water stream, and bonded lower anterior edgewise bracket with the light curing orthodontic composite resin adhesives. The teeth bonded brackets were stored in the distilled water at room temperature for 24 h, and followed to test the bracket shear bond strength. The acid etch technque showed 177.6 kg/$cm^2$ of mean shear bond strength which was the highest among the enamel treatment solutions. ES 1 shown 58.4 kg/$cm^2$ of mean shear bond strength and that of ES 4 showed 66.5 kg/$cm^2$. There was no significant difference between the two(p>0.05). ES2 showed 110.6kg/$cm^2$ of mean shear bond strength which was $62.3\%$ of that of acid etch technique. ES 3 showed 131.1 kg/$cm^2$ of mean shear bond strength which was the highest among experimental crystal growth solutions and which was $74\%$ of that of acid etch technique. The shear bond strengths of the crystal growth solutions were significantly lower that that of acid etch technique(p<0.05). The results sugest that although bracket shear bond strength of $30\%$ polyacrylic acid solution containing 0.3M sulfuric acid and 0.6 M lithium sulfate were showed the highest, it is low for the clinical application of this solution.