Mechanical behaviors of concrete combined with steel and synthetic macro-fibers

  • Deng, Zongcai;Li, Jianhui
    • Computers and Concrete
    • /
    • v.4 no.3
    • /
    • pp.207-220
    • /
    • 2007
  • In this paper, hybrid fibers including high elastic modulus steel fiber and low elastic modulus synthetic macro-fiber (HPP) as two elements were used as reinforcement materials in concrete. The flexural toughness, flexural impact and fracture performance of the composites were investigated systematically. Flexural impact strength was analyzed with statistic analyses method; based on ASTM and JSCE method, an improved flexural toughness evaluating method suitable for concrete with synthetic macro-fiber was proposed herein. The experimental results showed that when the total fiber volume fractions ($V_f^a$) were kept as a constant ($V_f^a=1.5%$), compared with single type of steel or HPP fibers, hybrid fibers can significantly improve the toughness, flexural impact life and fracture properties of concrete. Relative residual strength RSI', impact ductile index ${\lambda}$ and fracture energy $G_F$ of concrete combined with hybrid fibers were respectively 66-80%, 5-12 and 121-137 N/m, which indicated that the synergistic effects (or combined effects) between steel fiber and synthetic macro-fiber were good.

Buckling performance of pultruded glass fiber reinforced polymer profiles infilled with waste steel fiber reinforced concrete under axial compression

  • Emrah, Madenci;Sabry, Fayed;Walid, Mansour;Yasin Onuralp, Ozkilic
    • Steel and Composite Structures
    • /
    • v.45 no.5
    • /
    • pp.653-663
    • /
    • 2022
  • This study reports the results of a series of tests of pultruded glass fiber reinforced polymer (P-GFRP) box section composite profile columns, geometrically similar with/without concrete core, containing 0-1-2-3% steel fiber, with different lengths. The recycled steel wires were obtained from waste tyres. The effects of steel fiber ratio on the collapse and size effect of concrete filled P-GFRP columns under axial pressure were investigated experimentally and analytically. A total of 36 columns were tested under compression. The presence of pultruded profile and steel wire ratio were selected as the primary variable. The capacity of pultruded profiles with infilled concrete are averagely 9.3 times higher than the capacity of concrete without pultruded profile. The capacity of pultruded profiles with infilled concrete are averagely 34% higher than that of the pultruded profiles without infilled concrete. The effects of steel wire ratio are more pronounced in slender columns which exhibit buckling behavior. Moreover, the proposed analytical approach to calculate the capacity of P-GFRP columns successfully predicted the experimental findings in terms of both pure axial and buckling capacity.

Compressive and Flexural Behavior of High-Strength Concrete Incorporating Different Types of Hooked-End Steel Fibers (강섬유 특성에 따른 고강도 콘크리트의 압축 및 휨 거동)

  • Jeong, Woo-Jin;Jin, Ai-Hua;Yun, Hyun-Do
    • Journal of Korean Association for Spatial Structures
    • /
    • v.23 no.2
    • /
    • pp.69-78
    • /
    • 2023
  • This paper investigates the effects of aspect ratio and volume fraction of hooked-end normal-strength steel fibers on the compressive and flexural properties of high-strength concrete with specified compressive strength of 60 MPa. Three types of hooked-end steel fibers with aspect ratios of 64, 67 and 80 were considered and three volume fractions of 0.25%, 0.50% and 0.75% for each steel fiber were respectively added into each high-strength concrete mixture. The test results indicated that the addition of normal-strength steel fibers is effective to improve compressive and flexural properties of high-strength concrete but fiber aspect ratio had little effect on the modulus of elasticity and compressive strength. As steel fiber content and aspect ratio increased, flexural beahvior of notched high-strength concrete beams was effectively improved.

Fire Resistance Test of Steel Fiber Reinforced Concrete (강섬유보강콘크리트의 내화성에 관한일실험)

  • 윤재환
    • Fire Science and Engineering
    • /
    • v.1 no.1
    • /
    • pp.19-26
    • /
    • 1987
  • In this study, fire resistance of steel fiber reinforced concrete was investigated Cylindrical and prismatic specimens made of Ordinary Portland Cement plain concrete and steel fiber reinforced concrete were exposed to heating in accordance with a standard time-temperature curve as specified in KS·F22 57, method of fire resistance test for structural parts of buildings, the period of heating was 1 hour and 2 hours. After the fire resistance test, mechanical properties of specimens such as compressive and bending strength, stress-strain curve, static and dynamic modulus of elasticity and bending toughness were investigated. Also the cracks and spallings of the specimens were observed. From the test results, it was confirmed that steel fiber reinforced concrete has a excellent fire resistance than plain concrete in the view of higher residual strength of concrete and smaller crackings because of steel fibers in concrete.

  • PDF

Properities of Freshly Mixed Concrete Using Recycled Coarse Aggregates and Steel Fiber (강섬유를 혼입한 굳지 않은 재생 콘크리트의 특성에 관한 연구)

  • 구봉근;김창운;김태봉;박재성
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.5
    • /
    • pp.93-99
    • /
    • 2000
  • The physical properties of freshly mixed steel fiber reinforced recycled concrete(SFRRC) were_investigated. Physical state and quality of fresh concrete were monitored batch by batch. the properties of freshly mixed SFRRC were determined in terms of slump, air content, superplasticizer, and bleeding ratio. Concrete mixtures were produced for three kinds of aggregate proportions. So, the experimental variables are various aggregate proportions, steel fiber contents(0, 0.5, 1.0, 1.5%) and steel length(30, 50, 60mm). From experimental results, optimum s/a by various experimental variables, variations of the slump by the air contents, and optimum superplasticizer to decrease unit water were presented.

Calculation of Crack Width in SFRC Structures (강섬유철근콘크리트 구조물의 균열폭 계산)

  • Kang Bo-Soon
    • Journal of the Korean Society for Railway
    • /
    • v.8 no.4
    • /
    • pp.293-298
    • /
    • 2005
  • A method is described for predicting crack with and spacing in Steel Fiber Reinforced Concrete (SFRC). The crack behavior of SFRC influenced by longitudinal reinforcement ratio, volume and type of sleet fiber, strength of concrete. It can be observed from experimental results that addition of steel fiber to reinforced concrete beam reduces crack width in serviceability limit stales. The proposed method predicts crack widths in cracking stage of the beam. Calculated crack widths obtained for reinforced concrete beams and different volume and type of steel fiber, strength of concrete showed good agreement with experimental results.

An Experimental Study on Eccentrically Loaded Steel Fiber Reinforced Concrete Columns (편심축하중을 받는 강섬유보강 콘크리트 기둥의 실험적 연구)

  • 박홍용;안영진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10b
    • /
    • pp.857-860
    • /
    • 2000
  • An experimental study on the behavior of Steel Fiber Reinforced Concrete Columns under eccentric compression are presented. Forth-one columns were tested; the variables were column type, eccentricity of load, fiber contents, and longitudinal reinforcement ratio. The column size was $250\times160$ mm in cross section with an effective length of 1150 mm. Eccentricity of load was varied in the range from 1/6 to 1/2 times the column depth. This paper is to provides a framework for basic understanding of the steel fiber concrete columns.

An Experimental Study on Flexural Behavior of Steel Fiber Reinforced Concrete Slab (강섬유보강 철근콘크리트 슬래브의 휨 거동에 관한 실험적 연구)

  • 박홍용;문정규
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10b
    • /
    • pp.861-866
    • /
    • 2000
  • This experimental were investigated on the influence of steel fiber reinforcement on flexural behavior characteristics of slabs with various steel fiber contents $V_f$ and aspect ratio($\ell $/$\phi$). Deflection, crack widths, and strains of steel bar were measured with every load step. In the results of this experimental, the addition of steel fibers to conventionally reinforced concrete slab increased the ultimate load, reduced the creak width, the average crack spacing, and deflection.

Investigation of Material Properties of the Steel Fiber Reinforced Concrete (강섬유 보강콘크리트의 재료적 성상에 관한 고찰)

  • 이현호;권영호;허무원;정현석
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.733-736
    • /
    • 2002
  • As composite materials, the addition of steel fiber in concrete significantly improves the engineering properties of structural members. The purpose of this study is to define the strengthening effect of steel fiber in a point of material usage. From tile material test. compression strength, tensile splitting strength and flexural strength were evaluated by steel fiber volume fraction ($V_f$) and aspect ratio (AR) of steel fiber. In case of AR 67, $V_f$ 2.0% could be achieved maximum steel fiber strengthening effect. And the AR 80 case, $V_f$ 1.0% could be achieved maximum effect than the effect of $V_f$ 1.5%.

  • PDF

Behavior of Steel Fiber Reinforced Concrete Columns under Cyclic Loading

  • Chang Kug-Kwan;Lee Hyun-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.3 s.81
    • /
    • pp.415-423
    • /
    • 2004
  • To improve the brittle column behavior during seismic excitation, benefits of using steel fiber reinforced concrete in columns were investigated. For experimental study, eight specimens were used to evaluate the shear enhancement effect. The variables in this study were amount of shear reinforcement ratio (i.e., 0.26, 0.21 $\%$) and steel fiber volume fraction (i.e., 0.0, 1.0, 1.5, 2.0$\%$). The test results indicated that the maximum enhancement of shear capacity was shown in $1.5\%$ steel fiber content. In addition, to predict the maximum shear strength, equations of ACI 318-99, AIJ MB, NZS 3101, Hirosawa and Priestley were reviewed. From the parametric and regression study, modified Priestely equation was proposed by adding steel fiber effect.