• 제목/요약/키워드: steel sheet joining

검색결과 130건 처리시간 0.027초

고장력강판 적용 샤시부품의 용접부 내구수명 향상기술 개발 (Development of Durability Enhancement Technology for Arc Weldings in Advanced High Strength Steel (AHSS) Chassis Parts)

  • 이광복;오승택
    • Journal of Welding and Joining
    • /
    • 제33권4호
    • /
    • pp.50-56
    • /
    • 2015
  • In general, discontinuity of metallurgical and structural points of weld zone could decline the fatigue strength. For the lightweight trend, the AHSS application in automotive chassis is in-progress. However, there are few research reports on AHSS welds fatigue strength in especially automotive chassis parts. Therefore, in this study, we evaluated the effects of the factors affecting the AHSS welding fatigue strength. As the result, the stress concentration of weld bead is the most important factor for welding fatigue strength. For the enhancement of welding fatigue strength, we focused on reducing the stress concentration of the welding beads. So, we applied and proved the plasma welding process and GTAW (Gas Tungsten Arc Welding) dressing method. It was verified by uniaxial fatigue specimen, fatigue performance increased from 40 to 60% by applying TIG dressing method compared to the conventional GMAW (Gas Metal Arc Welding). These results could be recommended the enhancement of fatigue performance of AHSS.

테일러드 블랭크용 박판 강재의 레이저 용접성 (1) (Laser Weldability of Sheet steels for Tailored Blank Manufacturing(1))

  • 김기철
    • Journal of Welding and Joining
    • /
    • 제16권1호
    • /
    • pp.77-87
    • /
    • 1998
  • This paper deals with the effect of laser welding parameters on the weld formation. Thin steels for automotive application were prepared so as to be welded with high power carbon dioxide laser system. Major process parameters were position of focus and travel speed. The effect of shielding gas was also discussed by employing the high speed photometry. Test results showed that the optimal position of focus varied in accordance with the joint configuration; bead-on-plate, butt or lap welding. It was recommended that the position of focus for the lap welding be located at slightly inner part of the material to be welded. In this case, however, it was noticeable that the weld penetration ratio, d/t$_{0}$ dropped drastically at the critical region. Results also demonstrated that both the bead width and penetration reduced as the travel speed increased. The penetration ratio showed two distinct regions; stabilized zone at the lower range of the travel spped and sudden drop zone at the higher range of travel speed. Lower limit of the penetration for acceptable weld was proved to be about 90% of the parent metal thickness based on the physical properties of the weld. Mixed gas application for both the shielding of molten metal and laser induced plasma control was recommended as far as the penetration was concerned.d.

  • PDF

Hole 클린칭을 이용한 고장력강판과 Al6061 이종소재의 접합 (Joining High-Strength Steel and Al6061 Sheet Using Hole Clinching Process)

  • 안남식;이찬주;이정민;고대철;이선봉;김병민
    • 대한기계학회논문집A
    • /
    • 제36권6호
    • /
    • pp.691-698
    • /
    • 2012
  • 일반적인 클린칭 접합공정에서 고장력강과 알루미늄의 이종소재간의 접합시 고장력강의 낮은 연신율과 높은 강도로 인해 클린칭 접합시 파단이 발생하거나 높은 클린칭 접합하중이 요구된다. 이러한 문제점을 해결하기 위해 본 연구에서는 클린칭 접합시 고장력강의 변형없이 알루미늄의 변형만을 이용한 홀 클린칭 접합공정을 개발하였다. 고장력강에 홀가공을 적용하여 고장력강의 변형을 배제하였다. 홀 클린칭 접합의 요구접합강도를 기초로 클린칭 접합의 기하학적 구속량을 결정하였으며, 홀 클린칭 금형의 형상은 성형체적 일정조건을 이용하여 설계하였다. 설계된 클린칭 접합공정의 유효성을 평가하기 위해 유한요소해석을 수행하여, 홀 클린칭 접합이 가능함을 확인하였다. 또한 홀 클린칭 접합의 접합강도는 인장전단시험을 통하여 평가하였다. 홀 클린칭 접합강도는 2.56kN으로 요구접합강도와 비교하여 동등수준 이상의 값을 가짐을 확인하였다.

Nd:YAG 레이저빔을 이용한 아연도금강판(SECC)과 쾌삭강봉(SUM24L)의 용접에 관한 연구 (Welding behavior between Zn-coated steel plate and free cutting carbon steel rod by Nd:YAG laser beam)

  • 노영태;김병철;김도훈;윤갑식
    • 한국레이저가공학회지
    • /
    • 제4권3호
    • /
    • pp.30-39
    • /
    • 2001
  • This work was tamed out to apply a laser welding technique in joining between a Zn coated low carbon steel plate(SECC) and a free cutting carbon steel shaft(SUM24L) with or without W coating. Experiments were carried out and analysed by applying the FD(factorial design)method to obtain the optimum Laser welding condition. Optical microscopy, SEM, TEM and XRD analyses were performed in order to observe the microstructures in the fusion zone and the HAZ. Mechanical properties of the welded specimens were examined by microhardness test, tensile test and twist test. There was no flawed Zn in the fusion zone by EDS analysis. This means that during the welding process, Zn gas could be eliminated by appropriate shielding gas flow rate and butt welding gap. Ni coating itself did not influence on the tensile strength and hardness. However, twist bending strength and the weld depth of the Ni-coated free cutting carbon steel were lower as compared with those of the uncoated free cutting carbon steel. It was attributed to a lower absorbance of laser beam to the shin Ni surface. According to the results of the factorial design tests, the twist bending strength of welded specimens was primarily affected by pulse width, laser power, frequency and speed.

  • PDF

저항용접에서의 용접성 평가에 관한 연구 (A Study on the Evaluation of Weldability in Spot Welding)

  • 홍민성;김종민
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2003년도 추계학술대회
    • /
    • pp.301-306
    • /
    • 2003
  • Spot welding is frequently used for industrial purpose, such as automobile and aerospace industries and household appliances due to its high performance. In these day, robotization and systemization of welding process made it possible to produce more precise or smaller electric parts. And when it comes to welding of steel sheet, the size of nugget must be getting smaller. Therefore, welding conditions are limited to avoid defects, such as deformation, damage, weakening of joining area. In this research, the measurement of the nugget size by the nondestructive inspection has been conducted. As a result, the right estimation of the nugget size and void defects, the detection of corona bond near joining area, the selection of the optimum ultrasonic mode, and set up for ultrasonic inspection are studied. From the trustworthy solutions of nugget size estimated by results of measurement, the optimum inspection conditions depending upon the width of welding parts are determined as well.

  • PDF

레이저용접부 온도측정을 위한 적외선 온도측정장치의 개발에 관한 연구 (II) - 적외선 온도측정에서 제인자의 영향 - (A Study of the Infrared Temperature Sensing System far Measuring Surface Temperature in Laser Welding(II) - Effect of the System Parameter on Infrared Temperature Measurement -)

  • 이목영;김재웅
    • Journal of Welding and Joining
    • /
    • 제20권1호
    • /
    • pp.69-75
    • /
    • 2002
  • This study investigated the effect of the system parameters on penetration depth measurement using infrared temperature sensing system. The distance from focusing lens to detector was varied to diminish the error in measuring weld bead width. The effect of bead surface shape on measured surface temperature profile was evaluated using specimen heated by electric resistance. The measuring distance from laser beam was changed to optimize the measuring point. The results indicated that the monitoring device of surface temperature using infrared detector array was applicable to real time penetration depth control.

레이저용접부 온도측정을 위한 적외선 온도측정장치의 개발에 관한 연구(I) -용융부 형상에 따른 표면온도분포- (A Study of the Infrared Temperature Sensing System for Surface Temperature Measurement in Laser Welding(I) - Surface Temperature Profile According to Bead Shape -)

  • 이목영;김재웅
    • Journal of Welding and Joining
    • /
    • 제20권1호
    • /
    • pp.62-68
    • /
    • 2002
  • This study investigated the feasibility of penetration depth measurement using infrared temperature sensing on the weld surface. The detection point was optimized by FEM analysis in the laser keyhole welding. The profile of the weld surface temperature was measured using infrared detector array. Surface temperature behind the weld pool is proportional or exponentially proportional to penetration depth and bead width. From the results, the monitoring device of surface temperature using infrared detector array was applicable fur real time penetration depth control.

Al분말 분사에 의해 생성된 Fe-Al합금 피막층의 열처리에 따른 영향 (Effects of heat treatment on Fe-Al Alloy Layers Formed by Al Powder Spray)

  • 양병모;박정직;박광정;박경채
    • Journal of Welding and Joining
    • /
    • 제14권1호
    • /
    • pp.92-98
    • /
    • 1996
  • Al-Fe alloy layers on heated steel sheet were made by Al powder spray for 30 minutes at $700^{\circ}C$, $800^{\circ}C$ and $1000^{\circ}C$, respectively. As a results, for alloy layers formed at $700^{\circ}C$ and $800^{\circ}C$, main phases were brittle phase $FeAl_3 and Fe_2Al_5$, hardnesses were very high (Hv 700~800), corrosion resistances were good and surfaces were smooth, but wear resistances were bad. For alloy layer formed at $1000^{\circ}C$, main phase was ductile phase $Fe_3Al$, hardness was low (Hv 300~400), corrosion and wear resistances were excellent, but surface was rough. Therefore, alloy layers that formed at $700^{\circ}C$ and $800^{\circ}C$ were heat treated at $1000^{\circ}C$ for 10 minutes for the purpose of smooth surface and excellent wear resistance in this study. It was investigated that brittle phase $FeAl_3 and Fe_2Al_5$ of alloy layers fromed by Al powder spray at $700^{\circ}C$ and $800^{\circ}C$ turn into ductile phase $Fe_3Al$ by heat treated at $1000^{\circ}C$ for 10 minutes without changing smooth surface. It was concluded that the alloy layers formed by Al powder spray on heated steel sheet at $700^{\circ}C$ and $800^{\circ}C$ for 30 minutes and heat treated at $1000^{\circ}C$ for 10 minutes were excellent on wear and smooth surface.

  • PDF

QUALITY ASSURANCE IN LASER-BEAM WELDING OF HEAVY SECTION STEEL SHEET

  • Dahmen, M.;Kaierle, S.;Kapper, G.;Michel, J.;Schulz, W.;Spielvogel, K.;Poprawe, R.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.589-594
    • /
    • 2002
  • In manufacturing of welded parts which require a proof on acceptance close observation of the process is mandatory. The manufacturer is obliged to document the welding process. An approach for monitoring and recording the process of laser beam welding combining theoretical knowledge, process monitoring and welding experience will be presented. The range of application of a device for co-axial process monitoring was extended up to 20 mm sheet thickness welded in one pass at beam powers of up to 20 kW. Crucial features of the process which refer to the formation of failures were observed. The results presented give rise to the general applicability of the approach for process monitoring and recording as well as failure management.

  • PDF

파이버 레이저의 스테인리스강 용접시 인프로세스 모니터링을 위한 유기 플라즈마와 방사신호간의 상관성 연구(I) - 박판 용접시 측정신호의 특성 변화 - (A Study on Correlationship between the Induced Plasma and Emission Signals for In-process Monitoring in Stainless Steel Welding of Fiber Laser (I) - Properties Changes of the Measured Signals in a Thin Plate Welding -)

  • 이창제;김종도
    • Journal of Welding and Joining
    • /
    • 제32권6호
    • /
    • pp.64-69
    • /
    • 2014
  • The applications by using fiber laser have increased recently. However, due to high beam quality of fiber laser, it is inappropriate to apply the existing laser welding monitoring technology to the fiber laser welding as it is. On this study, thus, we analyzed emission signal with RMS and FFT for the in-process monitoring during fiber laser welding. 12mm-thick 304L stainless steel sheet was used in fiber laser welding and the result showed as follows: The intensity changes in RMS did not clarify the distinction between full penetration and partial penetration. However, as welding speed increases, specific frequency also increases in regards of frequency analysis by using FFT.