Due to the recent environmental problems, lots of studies on the solutions to reduce the environmental pollutions are on the way. In the field of construction, concrete that we are currently consuming approximately 1 ton each year is the most common and cheap building material. We must cut down on this preoccupied use of this material and develop an alternative material as recommended by the late environmental standards. In this regard, this study propose the 'yellow soil' as the main substance that composes the final state, 'yellow soil concrete'. This study also aims to analyze the physical and chemical performances of this concrete mixed with the yellow soil by comparing it with the cement and assesses the possibility of its application to the cement. The results of the experiment shows that, assuming the solidity of the cement concrete to be around $210kg/cm^2$ (20.58MPa), the solidity of the yellow soil combined material may be around 45%~55% in terms of the range of W/B use, 200 to 400 in the per unit fission amount and less than 2% in the addition proportion of admixing agents. But the scope of the optimal concoction amount of the yellow soil concrete should better be limited as following. 40% to 50% in W/B, 300 to 400 in the per unit fission amount and less than 2% in the addition of admixing agents.
This study aims to provide basic data for soil packaging differing in accordance with the strength characteristics of mixed soil, using E.S.B. (Eco Soil Binder), an eco-friendly hardening agent, based on the type of soil. The soil used in this study is weathered granite soil readily collected in and around Korea, and is classified into SW, SP and SC according to soil classification systems. The test piece for the unconfined compressive strength test has dimensions of 50 mm in diameter and 100 mm in height, with the mix ratio of E.S.B. proportional to the weight of mixed soil changed from 5% to 10%, 15%, 20%, 25%, and 30%, where compactness of 90% and 100% were applied according to each condition to analyze the unconfined compressive strength characteristics at material ages of 3, 7, and 28 days. Also, the ratio of soil packaging standard strength and unconfined compressive strength was calculated to determine the optimal E.S.B. mix ratio, whereby the field applicability of the unconfined compressive strength using the estimation equation of ACI209R was evaluated.
A novel MgO-based binder was developed and applied to treat the anoxic sediment that was collected from Seonakdong river, Korea and was contaminated with heavy metals. The treated sediment was evaluated by measuring compressive strength, expansion, leaching of heavy metals and storage characteristics for $CO_2$. Initially, an optimal blending ratio of lime (L)/fly ash (FA)/blast furnace slag (BFS) that was to be mixed with MgO was screened to be $L_{0.3}-FA_{0.1}-BFS_{0.6}$. Long-term strengths of the sediments that were treated by various mixtures of MgO and $L_{0.3}-FA_{0.1}-BFS_{0.6}$ were then evaluated and the blending ratios between 4 : 6 and 6 : 4 were found optimal, which yielded a compressive strength of 4.09 MPa. On this basis, the optimal MgO-based binder was selected to be a 5 : 5 mixture of MgO and $L_{0.3}-FA_{0.1}-BFS_{0.6}$. The good performance of the MgO-based binder was believed to be due to the formation of Mg $(OH)_2$, which filled the micropores and also increased the density of the solidified matrices. The MgO-based binder exhibited an average stabilizing capacities for heavy metals of 92.9%, which was similar to or higher than that of Portland cement. It was found that 69.1 kg of carbon dioxide could be sequestrated after 365 days of curing when treating a ton of anoxic sediments.
Yun, Do Youn;Ahn, Jun-Young;Kim, Cheolyong;Kim, Tae Yoo;Hwang, Inseong
Journal of Soil and Groundwater Environment
/
v.21
no.6
/
pp.135-145
/
2016
MgO recently has been regarded as the alternative material for replacement of cement. The aim of this study is to investigate the effects of accelerated carbonation on the strength development of MgO-based binder which is binary mixtures of magnesium oxide (MgO) with portland cement (PC) or ground granulated blast furnace slag (GGBS) or fly ash (FA). The compressive strengths of all binders were higher in the 20% $CO_2$ condition and for longer curing time. The strength were generally higher as the following order: MgO/PC > MgO/GGBS > MgO/FA system. The binder composed of 20% MgO and 80% PC showed highest compressive strength (38.0MPa) which was higher than PC. The correlation analysis of the porosity and compressive strength showed that compressive strength was higher when porosity was lower. The hydration and carbonation products of MgO including brucite ($Ca(OH)_2$), magnesite ($MgCO_3$) and nesquehonite ($MgCO_3{\cdot}3H_2O$) presumably filled the pores and contributed to strength development. Thermogravimetric analyses elucidated that 0.34 kg of $CO_2$ could be stored the 50% MgO/50% PC binder which performed the maximum $CO_2$ uptake at 20% $CO_2$ condition.
Journal of the Korea Institute of Building Construction
/
v.16
no.1
/
pp.45-52
/
2016
In this research, characteristic properties of gel time and homo gel strength of liquid chemical grouting material for soil grouting using non-cement binder(NCB) were measured according to kinds of liquid B's Binders, W/B of liquid B's Binders and the volume ratio between liquid A and liquid B in order to examine on the applicability of soil grouting material using non-cement binder. The test was performed using NCB-1, NCB-2, NCB-3 which are environment-friendly inorganic binders developed by means of collaboration by our research team and which are different from chemical composition ratio each other. In conclusion, it was found that NCB could be applied to liquid soil grouting material using non-cement binder and replace ordinary portland cement, because NCB had the most excellent performance in certain section of gel time and homo gel strength in condition of this experiment.
Fertilizer granulation test was carried out by a small pan granulator. A premixture composed of SOP 60%, urea 22% and RP powder 18% was rolled in the pan granulator while 10% phosphoric acid solution(binder) was sprayed on the rolling powder bed. Granules were developed very fast along with a little amount of binder. Hardness, brittle ratio in water and hygroscopicity of granules were improved enough to evaluate physical properties of the fertilizer. Growth responses of tobacco plant to the fertilizer were investigated at seedling and flowering stage by pot experiment under plastic film roof. Seedlings showed poor growth at nursery pot cell. In virgin soil with deficient available phosphate tobacco plant showed poor growth until budding and flowering stage but good growth in tillage soil with high cumulative phosphate.
Proceedings of the Korean Institute of Building Construction Conference
/
2023.11a
/
pp.73-74
/
2023
In this paper, the characteristics of soil concrete were examined using industrial waste red mud and construction waste circulating aggregate, and if unit cement of 250 kg/m3, it can be used as a soil packaging material by meeting the compressive strength standards for parking lots of SPS-KSCICO-001-2006:2020.
Arsenic is one of the most abundant contaminant found in waste mine tailings and soil around refinery, Because of its carcinogenic property, the countries like United States of America and Europe have made stringent regulations which govern the concentration of arsenic in soil. The study focuses on solidification/stabilization for removal of arsenic from soil. Cement was used to solidify/stabilize the abandoned soil primarily contaminated with arsenic (up to 68.92 mg/kg) in and around refinery. Solidified/stabilized (s/s) forms in the range of cement contents 5-30 wt % were evaluated to determine the optimal binder content. Revised Korean standard leaching tests (KSLT), toxicity characteristic leaching procedures (TCLP), Old Korea standard leaching test and revised Korea standard leaching test were used for chemical characterization of the S/S forms. The addition of 10 % cement remarkably reduced the leachability of arsenic in contaminated soil. The concentration of As in leachate of TCLP, KSLT, and old KSLT for soil are below the standard. However that in leachate of revised KSLT is above the standard. Because of extraction fluid used in revised KSLT is very strong acid. It is arsenic in s/s with binder should be exhaustingly leached. Therefore S/S process would not be available for As treatment in soil in Korea.
In this study, to determine characteristics of compaction and the soil water characteristic curve(SWCC) in decomposed granitic soils, compaction tests and SWCC tests were carried out for samples having various contents of coefficient of uniform($c_u$), By compacting their samples with standard Proctor density test, the effects of binder contents on maximum dry density and optimum moisture content were investigated and compared. Samples compacted with the maximum dry density and the optimum moisture content were tested by means of the SWCC, to determine their SWCC parameters, such as Brooks & Corey(${\lambda}$, ${\Psi}_b$), Van Genuchten (${\alpha}$, n, m), Fredlund & Xing(a, n, m).
Park, Kyu-Eun;Hong, Suk-Wo;Kim, Sang-Jin;Kang, Suk-Pyo
Proceedings of the Korean Institute of Building Construction Conference
/
2023.11a
/
pp.31-32
/
2023
In this paper, in order to utilize recycled aggregate as an alternative to natural resources in the construction industry, the physical properties of red mud-added soil concrete according to the type of aggregate and amount of binder were reviewed. The results of using waste asphalt concrete as a natural aggregate substitute were SPS-KSCICO- It was found to satisfy the compressive strength standards for parking lots of 001-2006, and its applicability in the construction industry was judged.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.