• Title/Summary/Keyword: sliding wear behavior

Search Result 234, Processing Time 0.025 seconds

Effect of environment on the tribological behavior of Si-incorporated diamond-like carbon films (실리콘이 첨가된 다이아몬드상 카본 필름의 트라이볼로지적 특성에 미치는 환경변화의 영향)

  • 양승호;공호성;이광렬;박세준;김대은
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.42-48
    • /
    • 1999
  • An experimental study was performed to discover the effect of environment on the tribological behavior of Si-incorporated diamond-like carbon(Si-DLC) film slid on a steel ball. The films were deposited on Si(100) wafers from radio-frequency glow discharge of mixtures of benzene and dilute silane gases. Experiments using a ball-on-disk test-rig was performed under vacuum, dry air and ambient air conditions. It was observed that coefficient of friction was decreased as the environmental condition changes from vacuum, to dry air. It was also observed that the coefficient of friction decreased with increasing silicon concentration in the film. Chemical analyses of debris suggested that the low and stable friction coefficient is closely related to the silicon rich oxide debris and the rolling action.

  • PDF

Effect of Silver Particle Introduction on Rolling Friction (구름거동에 미치는 은 입자 투여의 영향에 대한 실험적 고찰)

  • 양승호;공호성;윤의성;김대은
    • Tribology and Lubricants
    • /
    • v.17 no.6
    • /
    • pp.417-426
    • /
    • 2001
  • The effect of silver particle introduction on the rolling friction of AISI 52100 steel pairs has been investigated. Experiments ware performed in dry conditions using a thrust bearing-type rolling test rig at a load range of 12-960 N and a sliding velocity range of 8-785 mm/sec with pure (99.99%) silver particles. Results showed that introduced silver particles formed transfer layers, which protected the virgin bearing surfaces and resulted in the low lolling friction. By changing the quantity of silver particles, transitions in the rolling friction were found. Results also showed that the variations in normal load and rolling speed also affected the rolling friction behavior. Analyses of SEM and EPMA showed that the formation the transfer layer was mainly governed by the silver particle quantity, normal load and rolling speed, and this resulted in the different behavior of rolling friction. In this study, it was found that the low and stable rolling friction was resulted from the, shakedown phenomena occurred at the silver transfer layer.

Effect of Environment on the Tribological Behavior of Si-incorporated Diamond-like Carbon Films (실리콘이 첨가된 다이아몬드상 카본 필름의 트라이볼로지적 특성에 미치는 환경변화의 영향)

  • 양승호;공호성;이광렬;박세준;김대은
    • Tribology and Lubricants
    • /
    • v.16 no.3
    • /
    • pp.188-193
    • /
    • 2000
  • An experimental study was performed to discover the effect of environment on the tribological behavior of Si-incorporated diamond-like carbon(Si-DLC) film slid on a steel ball. The films were deposited on Si(100) wafers by a radio-frequency glow discharge of mixtures of benzene and dilute silane gases. Experiments using a ball-on-disk test-rig was performed in vacuum, dry air and ambient air conditions. It was observed that coefficient of friction decreased as the environment changed from vacuum, to dry air. Chemical analyses of debris suggested that low and stable friction is closely related to the formation of silicon-rich oxide debris and the rolling action.

Tribological Characteristics of C/C-SiC-Cu Composite and Al/SiC Composite Materials under Various Contact Conditions (접촉 조건에 따른 C/C-SiC-Cu복합재와 Al/SiC복합재의 마모 특성에 관한 연구)

  • Kim, Byung-Kook;Shin, Dong-Gap;Kim, Chang-Lae;Goo, Byeong-Choon;Kim, Dae-Eun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.41 no.1
    • /
    • pp.21-30
    • /
    • 2017
  • The surface temperature of disc brakes varies during braking, which can affect the friction and wear behavior of braking systems. In order to develop an efficient braking system, the friction and wear behaviors of brake materials need to be clearly understood. In this work, the friction and wear behavior of the C/C-SiC-Cu composite and the Al/SiC composite, which are used in disc braking systems, were investigated. Both the surface temperature and contact pressure were studied. A pin-on-reciprocating tribotester was used for this purpose, in order to control temperature and load. Results showed that the friction varied significantly with temperature and sliding distance. It was found that a transfer layer of compacted wear debris formed on the wear track of the two materials. These layers caused the surface roughness of the wear track to increase. The outcome of this work is expected to serve as a basis for the development of braking systems under various operating conditions.

Influence of Coating Defect Ratio on Tribological Behavior Determined by Electrochemical Techniques (전기화학적 분석을 통해 산출된 코팅 결함율이 트라이볼로지적 특성에 미치는 영향 평가)

  • Lee Young-Ze;Kim Woo-Jung;Ahn Seung-Ho;Kim Ho-Gun;Kim Jung-Gu;Cho Chung-Woo
    • Tribology and Lubricants
    • /
    • v.20 no.6
    • /
    • pp.306-313
    • /
    • 2004
  • Many of the current development in surface modification engineering are focused on multilayered coatings, which have the potential to improve the tribological properties. Four different multilayered coatings were deposited on AISI D2 steel in this study. The prepared samples are designed as $WC-Ti_{0.6}Al_{0.4}N,\;WC-Ti_{0.53}Al_{0.47}N,\;WC-Ti_{0.5}Al_{0.5}N\;and\;WC-Ti_{0.43}Al_{0.57}N$. The multilayered coatings were investigated with respect to coating surface and cross-sectional morphology, roughness, adhesion, hardness, porosity and tribological behaviors. Especially, wear tests of four multilayered coatings were performed by using a ball-on-disc configuration with a linear sliding speed of 0.017 m/sec and a normal load of 5.38 N load. The tests were carried out at room temperature in air by employing AISI 52100 steel ball $(H_R\;=\;66) $ having a diameter of 10 mm. The surface morphology, and topography of the wear scars of samples and balls have been determined by using scanning electron spectroscopy (SEM). Also, wear mechanism was determined by using SEM coupled with energy-dispersive spectroscopy (EDS). Results have showed an improved wear resistance of the $WC-Ti_{1-x}Al_xN$coatings with increasing of Al (aluminum) concentration.

Selection of Optimum Clearance Considering the Dynamic Behavior of a High-pressure Injector (고압 인젝터의 동적 거동을 고려한 최적 틈새 조합에 관한 연구)

  • Ryu, Daewon;Kim, Dongjun;Park, Sang-Shin;Ryu, Bongwoo
    • Tribology and Lubricants
    • /
    • v.37 no.5
    • /
    • pp.172-178
    • /
    • 2021
  • An injector is a mechanical device present inside the engine. Its main function is to supply an appropriate volume of fuel into the combustion chamber, which is directly related to the overall engine efficiency of a car. During the operation of an injector, a magnetic force lifts the parts of the injector from closed position to open position which generates a horizontal force on the needle. The horizontal force acts on a different position from that of the center of mass of the needle. Therefore, this causes eccentricity in the needle and the generation of a tilting motion during the lifting operation which can result in wear. However, appropriate selection of clearances for these parts can prevent wear. In this study, lubrication analysis is conducted to determine the optimum clearance of parts with sliding motion inside the injector. The height functions are derived considering the dynamic behavior and relative velocity of the parts. Using the derived height function, the pressure profiles are calculated for the lubricated surfaces from the Reynolds' equation. Subsequently, the fluid reaction forces are calculated. The equations of motions are applied to the fluid reaction forces and external forces are solved to calculate the minimum film thickness between each part with variation in the clearances. Finally, the optimum clearances are determined. The effect of the clearances on the behavior of the moving parts is presented and discussed.

A STUDY OF ION BEAM ASSISTED DEPOSITION(IBAD) OF TiN ON Ni-Cr Be ALLOY FOR SURFACE CHARACTERISTIC (이온빔 보조 증착법에 의한 TiN 박막도포가 니켈-크롬-베릴륨 합금의 표면 성상에 미치는 영향에 관한 연구)

  • Choi, Soo-Young;Lee, Sun-Hyung;Chang, Ik-Tae;Yang, Jae-Ho;Chung, Hun-Young
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.2
    • /
    • pp.212-234
    • /
    • 1999
  • Dental restorative materials must have the physical properties to withstand wear and corrosion. Base metal alloys possess better mechanical properties and lower price than the gold alloys. For these reasons such alloys have largely replaced the precious metal alloys. One aspect to con-sider is the release of metal substances to oral environment. The release of elements from dental alloys is a continuing concern because the elements may have the potentially harmful biological effects on local tissues. The purpose of this study was to minimize metal release on the nonprecious metal surfaces by ion beam assisted deposition(IBAD) of titanium nitride (TiN) Ni-Cr-Be alloys with and without TiN coatings were secured in an wear test machine opposing ruby ball to determine their relative resistance to wear with loom, 200m, 300m and 400m sliding distance. And the corrosion behavior of the Ni-Cr-Be alloys with and without TiN coatings and 3 dental noble alloys have been studied. Potentiodynamic curves were used to analyse the corrosion characteristics of the alloys. The measurement of the released Ni and Cr ions was conducted by analysis of the electrolyte solution with atomic absorption spectroscopy. The results were as follows : 1. The critical sliding distance that wore down TiN coatings of $2.5{\mu}m$ thickness in this study condition was 300m. 2. Ion beam assisted deposition of TiN showed a good surface modification with respect to the properties of wear and corrosion resistance. 3. X-ray diffraction showed that the strongest peak of TiN is TiN(111) in the coatings. 4. The release of Ni and Cr ions from alloys measured by means of atomic absorption spectroscopy was reduced by ion beam assisted deposition of TiN.

  • PDF

A Study on Contact Characteristics of Mechanical Face Seals for a Hydro-power Turbine Depending on the Rubbing Surface Geometry (소수력 터빈용 기계평면시일의 표면마찰형상에 따른 접촉특성 해석에관한 연구)

  • Kim Chung-Kyun
    • Tribology and Lubricants
    • /
    • v.22 no.3
    • /
    • pp.119-126
    • /
    • 2006
  • In this paper, the contact behavior characteristics of a primary sealing components such as a seal ring and a seal seat has been presented for a small hydro-power turbine. Using the non-linear FEM analysis, the maximum temperature, the axial displacement, radial differences between a seal ring and a seal seat, and maximum contact normal stress have been analyzed for three optimized sealing profiles in which are designed based on the FEM analysis and Taguchi's experimental method. The three primary sealing profiles between a seal ring and a seal seat are strongly related to a leakage of a water for a hydro-power turbine and wear of a primary sealing component. The computed results show that the contact rubbing area between a seal ring and a seal seat is very important for reducing a friction heating and wear in a sealing gap, and increasing a contact normal stress in primary sealing components. Based on the FEM computation, models II and III in which have a small rubbing surface of seal rings show low dilatation of primary sealing components, and high normal contact stress between a seal ring and a seal seat. Thus, the FEM computed results recommend a short contacting width of a primary sealing component for reducing a leakage and thermal distortions, and expanding a seal life. This means that a conventional primary sealing component may be switched to a reduced sealing face of seal rings.

Effects of Counterpart Materials on Dry Sliding Wear and Friction Behavior of Co-Fe, Co-Ni Bond Materials for Diamond Tools (다이아몬드 공구용 Co-Fe, Co-Ni 본드 소재의 마멸상대재에 따른 건식 미끄럼 마찰 및 마멸거동)

  • 권용진;김용석
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.03a
    • /
    • pp.28-28
    • /
    • 2003
  • 고온가압소결(Hot Pressing) 된 다이아몬드 공구용 Co-Fe, Co-Ni계 금속본드의 상온 건식 미끄럼 마멸시험을 행하고, 조성에 따른 각 본드의 마멸 특성을 비교하고 마멸 기구를 규명하였다. 미끄럼 마멸시험은 pin-on-disk 형태의 마멸시험기를 사용하여 각 조성의 성분, 적용하중 그리고 마멸상대재를 변수로 상온, 대기 중에서 실시되었다. 마멸속도는 마멸시험 전후의 시편의 무게 감량을 이론밀도와 거리로 나누어 계산되었다. 마멸기구의 규명을 위하여 시험된 시편의 마멸면과 마멸단면을 SEM과 EDS를 이용하여 분석하였다. 시험 결과 Co-Fe system의 경우 그 마멸속도는 마멸상대재의 영향보다는 Fe 첨가에 따른 시편의 미세조직과 기계적 성질의 차이에 따라 크게 변화하였다. 그러나 Co-Ni system의 마멸속도는 마멸 상대재에 따라 크게 변화하는 것이 관찰되었다. $Al_2$O$_3$를 상대재로 마멸된 경우에는 마멸속도가 시편/상대재 접촉면에서 형성되는 산화층의 영향을 크게 받았고, glass bead(83% SiO$_2$)를 상대재로 한 경우에는 시편의 경도와 마멸속도는 서로 반비례하였다.

  • PDF

An Investigation of Mechanical Properties and Sliding Wear Behavior of Ultra-Fine Grained 5052 Aluminum Alloy Fabricated by a Accumulative Roll-Bonding Process (누적압연접합공정에 의해 제조된 초미세립 5052 알루미늄 합금의 상온 기계적 특성 및 미끄럼 마멸거동에 대한 연구)

  • 하종수;강석하;김용석;신동혁
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.03a
    • /
    • pp.26-26
    • /
    • 2003
  • 본 연구에서는 누적압연접합공정(ARB)을 통하여 5052 알루미늄 합금의 결정립을 약 0.2$\mu\textrm{m}$ 크기로 미세화 하였다. 누적압연에 의한 변형량 증가에 따른 미세 조직 변화와 결정립 간의 상대적인 방위각 차이를 TEM을 이용하여 관찰하였다. 누적 변형량을 함수로 상온 인장특성을 분석하였고, 초미세립 소재를 후속 열처리한 후 미세 조직 변화를 관찰하여 제조된 초미세립 소재의 열적 안정성을 평가하였다. 상온 대기 중에서 pin-on-disk 형태의 마멸시험기를 사용하여 초미세립 소재의 미끄럼 마멸시험을 변형량과 하중을 변수로 행하였다. 강소성 변형에 의해 제조된 5052 알루미늄 합금 소재의 마멸저항성은 강소성 변형 전과 비교하여 소재의 경도가 크게 증가하였음에도 불구하고 오히려 감소하였다. 마멸시험 후 마멸면의 SEM, 마멸단면의 OM 관찰과 마멸면 직하의 깊이에 따른 경도측정을 통하여 초미세립 소재의 마멸기구를 분석하였고 마멸표면의 변형 층을 관찰하였다. 또한 마멸면 직하 조직의 TEM 관찰을 통해서 마멸시험 중의 미세 조직 변화를 연구하였다.

  • PDF