소결된 텅스텐 재료의 용매에 의한 특성 평가 (Evaluation on Mechanical Properties of Sintered Tungsten Materials by Solvents)

  • 박광모;이상필;이진경
    • 한국산업융합학회 논문집
    • /
    • 제24권3호
    • /
    • pp.289-294
    • /
    • 2021
  • Tungsten (W) is used as a facing material for nuclear fusion reactors, and it is used in conjunction with structural materials such as copper alloy (CuCrZr), graphite, or stainless steel. On the other hand, since tungsten is a material with a high melting point, a method that can be manufactured at a lower temperature is important. Therefore, in this study, tungsten, which is a facing material, was attempted to be manufactured using a pressure sintering method. Material properties of sintered tungsten materials were analyzed for each solvent using two types of solvents, acetone and polyethylene glycol. The sintered tungsten material using acetone as a solvent exhibited a hardness value of about 255 Hv, and when polyethylene glycol was used, a hardness value of about 200 Hv was shown. The flexural strength of the sintered tungsten material was 870 MPa and 307 MPa, respectively, when acetone and polyethylene glycol were used as solvents. The sintered tungsten material using acetone as a solvent caused densification between particles, which served as a factor of increasing the strength.

소결첨가재에 의한 텅스텐의 기계적 특성평가 (Evaluation on Mechanical Properties of Tungsten by Sintering Additive Content)

  • 이상필;이진경
    • 한국산업융합학회 논문집
    • /
    • 제25권4_2호
    • /
    • pp.621-626
    • /
    • 2022
  • Tungsten is a high melting point metal unlike other steel materials, and it is difficult to manufacture because of its high melting temperature. In this study, pressure sintering process method was applied to manufacture the tungsten materials at low temperature. Therefore, it is necessary to densify the sintered material by using a sintering additive. Studies have been conducted on how the amount of titanium for sintering tungsten affects the mechanical properties of tungsten in this study. In order to secure the densification mechanism of tungsten powder during the sintering process, the characteristics of the sintered tungsten material according to the change of titanium content were evaluated. It was investigated the relationship between sintering parameters and mechanical properties for densification of microstructures. The sintered tungsten materials according to sintering additive content showed high sintered density (about 16.31g/cm3) and flexural strength (about 584 MPa) when the content of sintering additive was 3 wt%. However, as the content of the sintering additive increases, mechanical property of flexural strength is decreased, and the porosity is increased due to the heterogeneous sintering around titanium.

저온 열처리로 제작된 1.5 mol% 이트리아 안정화 지르코니아 세라믹스의 상 안정성 및 소결물성 (Phase stability and Sintered Properties of 1.5mol% Yttria-stabilized Zirconia Ceramics Fabricated by Low Temperature Sintering)

  • 김경태;최한철;박정식;이종국
    • 열처리공학회지
    • /
    • 제37권1호
    • /
    • pp.1-8
    • /
    • 2024
  • Phase stability of tetragonal crystals in yttria-stabilized zirconia ceramics is dependent on the content of yttria and the heat-treatment condition, related with mechanical properties. In this study, we fabricated the 1.5 mol% yttria-stabilized zirconia (1.5Y-YSZ) ceramics by cold isostatic pressing (CIP) and post-sintering at temperature range of 1200 to 1350℃ for 2 hours and investigated the sintered properties and microstructural evolution. Sintered and microstructural parameters, i.e, apparent density, grain size and phase composition of 1.5Y-YSZ ceramics were mainly dependent on the sintering temperature. Maximum sintered density of 99.4 % and average grain size of 200-300 nm could be obtained from the heat-treatment condition above sintering temperature at 1300℃ for 2 hours, possessing the superior mechanical hardness with 1200 Hv. However, phase stability of tetragonal grains in 1.5 YSZ ceramics is very low, inducing the phase transformation to monoclinic crystals on specimen surface during cooling after heat-treatment.

동계 소결마찰재의 소결조건에 따른 마찰특성 고찰 (The Effect of Sintering Condition On Tribological Behavior in the Cu-Base Sintered Friction Materials)

  • 김상호;김기열;정진현;이범주;정동윤
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제25회 춘계학술대회
    • /
    • pp.53-61
    • /
    • 1997
  • The effect of sintering condition on tribological behavior in the Cu-base sintered friction materials was studied through pin-on-disk type wear tester. Especially, the experiment was focused on making a comparative study between presstwed sintering and pressureless sintering. Pressureless sintering process showes more stable friction coefficient and lower wear rate than pressure sintering process. This result is related to pore size and density of pore in the sintered materials.

  • PDF

함유소결베어링과 빗살무늬 유체베어링의 마찰 특성 및 레이저 스캐너 모터에서의 전기적 특성 (Oil-impregnated Sintered-metal Bearing and Herringbone-grooved Fluid Bearing for High-speed Scanner Motors)

  • 이영제;정광섭;정성훈
    • Tribology and Lubricants
    • /
    • 제15권1호
    • /
    • pp.108-115
    • /
    • 1999
  • The electrical and frictional properties of oil-impregnated sintered-metal bearing (OSB) and herringbone-grooved fluid bearing (HFB) with varying loads and speeds were measured. OSB shows very good performance up to 20,000 rpm and 0.05 N, and HFB successfully works up to 35,000 rpm and 0.05 N. From the endurance tests on start-stop and continuous operation, it was confirmed that those bearings could be mass-produced fur use on scanner motor in a laser scanner unit.

다공성 소결금속의 단조한계해석 (ANALYSIS OF FORGING LIMIT FOR SINTERED POROUS METALS)

  • 한흥남;오규환;이동녕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1995년도 제2회 단조심포지엄 단조기술의 진보
    • /
    • pp.64-73
    • /
    • 1995
  • The forging limit curves of sintered porous metals have been calculated, in terms of the two principal strains, by the Lee-Kuhn initial imperfection model. The various yield functions for porous metal have been applied to the initial imperfection model. When the value of initial imperfection ratio equals the value of initial relative density of the sintered porous metals, the calculation values are in good agreement with the measured data. The slopes of the forging limit curves are about 0.5 as in the case of non-porous metals.

Tribological Properties of Sintered Diamonds with WC-Co Matrix

  • Umeda, Kazunori;Tanaka, Akihiro;Takatsu, Sokichi
    • The Korean Journal of Ceramics
    • /
    • 제3권3호
    • /
    • pp.169-172
    • /
    • 1997
  • Sintered diamond/(WC-Co) composites were prepared by spark plasma sintering technique. Tribological properties were measured at temperatures from RT to $500^{\circ}C$ in sliding tests with alumina ball. They show coefficient of friction of 0.1 and below at RT and wear of the diamond composites is hardly detected. Effects of diamond grit size, diamond content and test temperature on the coefficient of friction and the wear are discussed. The wear scars were analyzed.

  • PDF

Influence of Nitrogen/Hydrogen Atmospheres on Sintered Properties of P/M Components

  • Philips, Thomas;Koh, Kyung-Sug
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.818-819
    • /
    • 2006
  • The effect of individual gas constituents in a sintering atmosphere is examined to optimize the sintered properties of Iron-Carbon P/M components. The influence of sintered properties is reviewed as a function of hydrogen percentages and dew point in the sintering zone. Microstructures, porosity, pore morphology and dimensional changes are the subject of this review. The effects of CO containing atmospheres are compared against the non CO atmospheres in terms of hardness, carbon control and dimensional changes.

  • PDF

Development of High Performance Multi-lobe Fluid Dynamic Bearings Using a Sintered Material

  • Tokushima, Hidekazu
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.379-380
    • /
    • 2006
  • Recently, in spindle motors for hard disk drive (HDD) devices, fluid dynamic bearings (FDB) with herringbone grooves have come to be used instead of ball bearings due to the demand for high density recording of the devices etc. In this study, a 5-lobe bearing with high bearing stiffness using a sintered material was developed, and the bearing performance was examined by simulated calculations and experiments. As a result, it was clarified that the 5-lobe bearing had the required performance for practical use in the spindle motor for HDD

  • PDF