• 제목/요약/키워드: silicate phosphor

검색결과 42건 처리시간 0.028초

$Sr_2SiO_4:Eu^{2+}$ 형광체의 합성 및 발광특성 (Synthesis and luminescent properties of $Sr_2SiO_4:Eu^{2+}$ phosphors)

  • 김종민;박용서;최형욱
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.430-431
    • /
    • 2009
  • In this study, europium doped strontium silicate ($Sr_2SiO_4:Eu^{2+}$) phosphor has been synthesized by conventional solid-state method and investigated luminescent characteristic. $SrCO_3$ and $SiO_2$ were mixed together by 2:1 mole ratio. Also $NH_4Cl$ was added as a flux. The mixture were sintered at $800^{\circ}C$, $1000^{\circ}C$ for 3h under the atmosphere (5% $H_2$/95% $N_2$). This phosphor can be applicated to the yellow phosphor for white LED because it has yellow emission band (540nm), which emits efficiently under the 370nm excitaion energy.

  • PDF

Zn$_2SiO_4$ : Mn Phosphor Particles Prepared by Spray Pyrolysis Process

  • Kang, Yun-Chan;Park, Hee-Dong;Lim, Mi-Ae
    • Journal of Information Display
    • /
    • 제2권4호
    • /
    • pp.57-62
    • /
    • 2001
  • Green-emitting $Zn_2SiO_4$:Mn phosphor particles having a spherical shape and high luminescence intensities under VUV were prepared by spray pyrolysis process under severe preparation conditions. The type of precursor solutions affected the morphology and luminescence characteristics of the prepared particles. The particles prepared from the clear solution by laboratory-scale process had spherical shape and dense morphology, while the particles prepared from the severe preparation conditions had rough surface and collapsed structure. However, the particles prepared from the colloidal solution utilizing fumed silica were spherical in shape and filled morphology at the severe preparation conditions of high flow rate of carrier gas, high concentration of solution, and large reactor size. The prepared $Zn_2SiO_4$:Mn phosphor particles with complete spherical shape had higher photoluminescence intensity than that of the commercial product prepared by solid state reaction.

  • PDF

Luminescence property of Eu2+ in SiO2-Al2O3 glass phosphor

  • Chae, Ki Woong;Lee, Kyoung-Ho;Cheon, Chae Il;Cho, Nam In;Kim, Jeong Seog
    • Journal of Ceramic Processing Research
    • /
    • 제13권spc2호
    • /
    • pp.189-192
    • /
    • 2012
  • Manufacturing process for silicate glass phosphors containing Eu2+ activator and their photoluminescence property have been studied. We adopted powder sintering process instead of traditional glass melting process for making glass phosphor. At first, phosphor powders were synthesized at 1200 ℃ for 2-3 hours under a reducing atmosphere with 10% H2-90% N2 gas mixture. The reduced powders were compacted into discs and then the discs weresintered at 1400 ~ 1500 ℃ for 1 hr under a reducing atmosphere of 5H2-95% N2. The enhancement of PL intensity by Al2O3 addition, XPS binding energy shift of Si 2p and O 1s, sintering shrinkage, and crystallization were characterized.

LED용 (Sr,Ba)2Ga2SiO7:Eu2+ 녹색 형광체의 합성 및 발광특성 (Synthesis and Luminescent Characteristics of (Sr,Ba)2Ga2SiO7:Eu2+ Green Phosphor for LEDs)

  • 박정규;이승재;연정호;김창해
    • 대한화학회지
    • /
    • 제50권2호
    • /
    • pp.137-140
    • /
    • 2006
  • Eu2+를 활성제로 한(Sr,Ba)2Ga2SiO7 녹색 형광체를 일반적인 고상 반응으로 합성하였고, 그 합성된 형광체의 광발광 특성을 연구하였다. 형광체 제조 시, 마노유발에서 보다 효과적인 혼합을 위하여 아세톤을 사용하여 혼합하였다. 또한 25%H2/75%N2의 혼합기체를 이용한 환원조건에서 단순한 공정으로 형광체를 합성하였다. 이 형광체는 405 nm의 여기 파장하에서 효율적으로 발광되는 녹색 밴드(513 nm)를 갖고 있기 때문에 백색 LED(Light Emitting Diode)램프에 응용할 수 있다.

고온 화염분무열분해법에 의해 합성된 장파장 자외선 하에서의 녹색 발광 실리케이트 형광체 (Green-Emitting Silicate Phosphor Under Long Wavelength Ultraviolet Prepared by High Temperature Flame Spray Pyrolysis)

  • 조중상;구혜영;이상호;강윤찬
    • 한국재료학회지
    • /
    • 제18권2호
    • /
    • pp.77-83
    • /
    • 2008
  • Green-emitting $Ba_{1.468}Sr_{0.5}SiO_4\;:\;Eu_{0.012},\;Y_{0.02}$ phosphor powders under long-wavelength ultraviolet light were prepared via high-temperature flame spray pyrolysis from spray solutions with and without $NH_4Cl$ flux. The effects of the temperature of the diffusion flame and the $NH_4Cl$ flux on the morphologies, crystal structures and photoluminescence intensities of the $Ba_{1.468}Sr_{0.5}SiO_4\;:\;Eu_{0.012},\;Y_{0.02}$ phosphor powders were investigated. The phosphor powders obtained from the spray solution with the $NH_4Cl$ flux had higher photoluminescence intensities compared to phosphor powders obtained from the spray solution without the flux. The photoluminescence intensity of the phosphor powders obtained from the spray solution without the flux decreased as the flow rate of the fuel gas increased. On the other hand, the photoluminescence intensity of the phosphor powders obtained from the spray solution with the flux increased as the flow rate of the fuel gas increased. The difference of in the phase purity and morphology of the powders affected the photoluminescence intensities of the phosphor powders.

Rietveld refinement study on variation of emission wavelength of $(Sr_{1-x},Ca_x)_2MgSi_2O_7:Eu^{2+}$ phosphor for white LED applications

  • Kwon, Ki-Hyuk;Im, Won-Bin;Jang, Ho-Seong;Yoo, Hyoung-Sun;Jeon, Duk-Young
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.565-568
    • /
    • 2008
  • In this study, a blue-emitting $Sr_2MgSi_2O_7:Eu^{2+}$ (SMS) phosphor for white light-emitting diodes is reported. Through transition of $4f{\rightarrow}5d$ in $Eu^{2+}$, SMS showed a strong blue emission under UV excitation. Additionally, the variation of emission wavelength of SMS is explained by crystal field effect and is supported by rietveld refinement.

  • PDF

Preparation and Luminescence Properties of PDP Green Phosphors using Polymer Matrix Technique

  • Jun, Sang-Bae;Lee, Dong-Kyu;Kim, Soo-Jong;Masaki, Takaki;Han, Chung-Hwa
    • Transactions on Electrical and Electronic Materials
    • /
    • 제8권3호
    • /
    • pp.121-124
    • /
    • 2007
  • The $Zn_2SiO_4:Mn$ phosphors were prepared using polymer matrix technique in order to improve the performance of green emitting phosphors for plasma display panel(PDP). $Zn_2SiO_4:Mn$ phosphor exhibits a strong green emission around 520-530 nm. The emission intensity and particle size of powders were controlled by sintering temperature and raw material composition. The zinc silicate $Zn_2SiO_4:Mn$ single phase were obtained at lower temperature than prepared by solid-state reaction method. PL luminance of $Zn_2SiO_4:Mn$ phosphor was similar to the commercial material.

Synthesis of Nanoparticles via Surface Modification for Electronic Applications

  • Lee, Burtrand I.;Lu, Song-Wei
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 2000년도 Proceedings of 2000 International Nano Crystals/Ceramics Forum and International Symposium on Intermaterials
    • /
    • pp.35-58
    • /
    • 2000
  • The demand for sub-micrometer or nanometer functional ceramic powders with a better suspension behavior in aqueous media in increasing. Redispersible barium titanate (BT) nanocrystals, green light emitting Mn2+ doped Zn$_2$SiO$_4$ and ZnS nanoparticle phosphors were synthesized by a hydrothermal method or chemical precipitation with surface modification. The nanoparticle redispersibility for BT was achieved by using a polymeric surfactant. X-ray diffraction(XRD) results indicated that the BT particles are of cubic phase with 80 nm in size. XRD results of zinc silicate phosphor indicate that seeds play an important role in enhancing the nucleation and crystallization of Zn$_2$SiO$_4$ crystals in a hydrothermal condition. This paper describes and discuss the methods of surface modification, and the resulting related properties for BT, zinc silicate and zinc sulfide.

  • PDF

Coating of ZnS phosphor by $SiO_2$ sol-gel

  • Lee, You-Hui;Han, Sang-Do;Han, Chi-Hwan;Yang, Hua;Singh, Ishwa
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2004년도 Asia Display / IMID 04
    • /
    • pp.719-723
    • /
    • 2004
  • Silica coating on ZnS particles with buffer solution has been investigated. Diluted sodium silicate in water was used as the precursor material and it was diluted in water. Sodium silicate was added drop-wise in the continuously stirred suspension of ZnS in the buffer solution at room temperature. Smooth and evenly distributed silica coated ZnS phosphors has been obtained when the pH of buffer solution was 10, the concentration of sodium silicate in water was 20 wt%, firing temperature was 500 $^{\circ}C$.

  • PDF