• Title/Summary/Keyword: shaving dust

Search Result 3, Processing Time 0.017 seconds

Properties of Light-weight Expanded Bonded Leather Using Thermal Expandable Microspheres (열 팽창성 Microsphere를 적용한 경량 발포 재생피혁 특성 분석)

  • Shin, Eun-Chul;Kim, Won-Ju;Kim, Yeong-Woo
    • Journal of Adhesion and Interface
    • /
    • v.21 no.3
    • /
    • pp.81-85
    • /
    • 2020
  • Shaving dust is a collagen fiber that is the leather waste occurred for thickness adjustment during the natural leather manufacturing process, and causes problems such as an environmental contamination because of a chromium (Cr) contained when it comes to reclaiming process. Various studies applying the shaving dust are currently being conducted in many countries across the world with an initiative by the EU. Of those applications, the bonded leather is being highlighted as a substitute for natural leather. Since the bonded leather, however, uses latex as a binder, accordingly it entails a high weight and a poor ventilation, which are deemed as disadvantages due to its dense internal tissues compared to other synthetic leathers. To address such disadvantages, this study employed the thermally expandable micro sphere to improve its air permeability and light weight by alleviating the internal structure. This is a study on the manufacturing of light bonded leather using the shaving dusts. In the study, the shaving dusts were forced to foam under 100~120℃ considering the heat resistance of collagen fiber after applying the thermally expandable micro sphere, and then the tendency was analyzed. In the analysis results, the most excellent foaming rate was exhibited when the shaving dusts were treated under 120℃ for 8 minutes and the variation of internal structure according to a foaming was observed through SEM analysis for the cross-section of the bonded leather.

Effective Chrome Removal Process from Shaving Dust (피혁분의 효율적인 탈 크롬 방법에 관한 연구)

  • Yun, Sun-Gyu;Park, Sung-Ha;Lee, Sang-Seob;Na, Jung-Won;Ko, Myung-Han
    • Applied Chemistry for Engineering
    • /
    • v.10 no.8
    • /
    • pp.1104-1108
    • /
    • 1999
  • In this study it was focused that if the chrome could be removed in the shaving dust, the reusable protein resource could be recycled from the shaving dust. As the chrome forms a Cr-collagenate by cross linking of collagen in the shaving dust, the dust was steeped for swelling and plumping by $Ca(OH)_2$ solution and then chromium in dust was resolved out by $H_2SO_4$ solution in the first stage process. In the second stage one, dust was swelled and plumped by NaOH solution and then the chromium in dust was oxygenated to a hexavalent chrome, which has high solubility in $H_2O_2$ solution. And then the chromium was removed byt he steeping of $H_2SO_4$ solution as the last process. The first stage process was consisted of the sequential steeping of 3%-$Ca(OH)_2$ and $0.8%-H_2SO_4$. In the second stage the total chrome was effectively removed by the sequential steeping of 0.1%-NaOH, $3%-H_2O_2$ and $1%-H_2SO_4$. In the completely dechromated dust, the humidity was measured as 10.68% and the crude protein was contained by 79.81%. Steeping solutions were reused 3 times for chrome removal process, the chrome was entirely removed in shaving dust.

  • PDF

A Study on Fabrication of Leather Brick by Using Leather Shaving Dust (피혁분을 이용한 가죽벽돌의 제조에 관한 연구)

  • 김영상
    • Journal of the Korean Professional Engineers Association
    • /
    • v.28 no.1
    • /
    • pp.119-125
    • /
    • 1995
  • To make the Leathen Bricks, We needed the hollouning Couchitions 1) During the water smoking, we must burn out the organic matenials completely by 600$^{\circ}$C 2) The optimum tempenatune to make the briks wan 1000$^{\circ}$C~1050$^{\circ}$C 3) The mixing ratio of the leathr dust was 6~8%

  • PDF