• Title/Summary/Keyword: self-etching adhesive

검색결과 105건 처리시간 0.018초

Effect of Hydrophobic, Neutral Adhesive on the Dentin Bond Strength of Self-etching Adhesive

  • Bae, Ji-Hyun;Choi, Yong-Hoon;Jung, Moon-Kyung;Cho, Byeong-Hoon
    • Journal of Korean Dental Science
    • /
    • 제2권2호
    • /
    • pp.5-11
    • /
    • 2009
  • Objectives : This study investigated the hypothesis that the dentin bond strength of self-etching adhesives (SEAs) may be improved by applying a coat of hydrophobic, neutral adhesive resin in addition to SEA. Method and Materials : The bond strengths of two SEAs - Experimental SEA (EX) and Adper Prompt (AP) - were measured with three bonding protocols. The D/E resin of All-Bond 2 was applied as the hydrophobic, neutral adhesive. Clearfil SE Bond (SE, self-etching primer system) and All-Bond 2 (AB, total etching system) were used as references. The following protocols were used: (1) EX1 (EX 1 coat); (2) EX2 (EX 2 coats); (3) EX+ (EX 1 coat + D/E resin); (4) AP1 (AP 1 coat); (5) AP2 (AP 2 coats); (6) AP+ (AP 1 coat + D/E resin); (7) SE (SE primer + SE bond); (8) SE+ (SE primer + D/E resin); (9) AB (etching + AB primer + D/E resin). Filtek Z250 composite resin was built up and the microtensile bond strength (MTBS) values of the specimens were compared. The fractured surfaces were observed using SEM. Results : When SEA was used as self-etching primer and hydrophobic, neutral adhesive was applied as well, MTBS was significantly higher than that when either one coat or two coats of SEA only were used (p < 0.05). Conclusion : The hydrophobic, neutral adhesive improved the integrity of the bonded interface obtained with SEA.

  • PDF

A comparative study on bond strength and adhesive failure pattern in bracket bonding with self-etching primer (Self-etching Primer를 이용한 교정용 브라켓 부착시 전단결합강도와 파절양상에 관한 비교연구)

  • Kim, You-Kyoung;Lee, Jin-Woo;Cha, Kyung-Suk
    • The korean journal of orthodontics
    • /
    • 제34권4호
    • /
    • pp.325-332
    • /
    • 2004
  • A self-etching primer that combines the etchant and primer in one chemical compound saves time and should be mote cost-effective to the clinician and patient. The purpose of this study was to evaluate the clinical effectiveness of a self-etching primer by measuring shear bond strengths according to various conditions and observing adhesive failure patterns. For this Investigation, 120 upper and lower premolars extracted for orthodontic purposes were used and randomly divided into six groups of twenty teeth each. Human premolars were embedded in a metal cylinder with orthodontic resin. Metal brackets and ceramic brackets were bonded with XT primer and self-etching primer by means of XT adhesive. Upon curing, plasma arc light and visible light were used. After bonding, the shear bond strength was tested by Instron universal testing machine, and the amount of residual adhesive that remained on the tooth after debonding was measured by stereoscope and assessed with an adhesive remnant index. The results were as fellows: 1. When brackets were bonded, if other conditions remained the same, there was no significant difference in shear bond strength due to the type of primer - either self-etching primer or XT primer. 2. When metal brackets were bonded, there was no significant difference in shear bond strength according to the source of light - plasma arc light or visible light - and type of primer. 3. There was a very significant difference in shear bond strength according to the type of brackets - metal or ceramic brackets. The shear bond strength of ceramic brackets was stronger than metal brackets. 4. When the adhesive failure patterns of metal brackets bonded with self-etching primer were observed by using the adhesive remnant index, the bond failure of the metal bracket occurred more frequently at the bracket-adhesive. The failure of the ceramic bracket, however, occurred more frequently at the enamel-adhesive interface. The adhesive failure patterns of metal brackets bonded with XT primer observed the same patterns. The above results suggest that self-etching primer can be clinically useful for bonding the brackets without fear of a decrease in shear bond strength.

The influence of moisture control on bond strength of composite resin treated with self-etching adhesive system (Self-etching adhesive system에서 수분 조절이 레진의 치질접착강도에 미치는 영향)

  • Jin, Myoung-Uk;Kim, Young-Kyung;Park, Jeong-Won
    • Restorative Dentistry and Endodontics
    • /
    • 제27권4호
    • /
    • pp.363-369
    • /
    • 2002
  • 최근에 많이 사용되어지고 있는 치과용 접착제는 산 부식 후 수분이 있는 상태에서 적용하는 wet-bonding 술식을 많이 추천하고 있다. 하지만 self-etching primer의 경우 산부식과 priming 과정이 동시에 시행되고, 제조자들은 건조된 치아표면에 적용할 것을 추천하고 있다. 그러나 건조된 정도에 대하여서는 별다른 추천사항이 없으며. 수분이 self-etching primer에 어떤 영향을 미치는지에 대하여서는 별다른 연구가 이루어져 있지 않은 상태이다. 이에 본 연구에서는 치질 삭제 후 남아있는 수분이 self-etching primer의 레진 접착 강도에 어떤 영향을 미치는 지를 알아보고자 하였다. 발거한 대구치 96개를 이용하여 물기가 있는 상태에서 #600 사포로 표면을 연마하고, 법랑질 면을 노출시킨 군과 상아질을 노출시킨 군으로 분류 후, 30분 공기 중 방치 군 (1군), 5초 공기 건조 군 (2군), 1초 공기 건조 군 (3군), 솜으로 약간의 물기를 제거한 군(blot dry) (4군) 등 총 8개의 군으로 나누었다. Self-etching adhesive system인 Clearfil SE Bond primer를 20초간 적용하고, bonding제 도포 후 10초간 광중합 시행하였다. 접착제 처리한 치아면에 몰드를 고정한 후 Clearfil AP-X 복합레진을 2mm 충전하고, 40초간 광중합을 시행하였다. 24시간 후 전단 응력 결합강도를 측정하였으며, 그 결과는 다음과 같이 나타났다. 법랑질과 상아질 모두에서, 30분 건조군과 5초 공기건조군이 1초와 blot drying 군보다 높은 결합강도를 보였으며 통계학적으로 유의한 차이를 보였다(p<0.05). 본 실험 결과에 의하면 self-etching adhesive system을 사용함에 있어서 법랑질과 상아질군 공히 건조된 상태에서 사용하여야 하며 수분의 존재시 치아와의 결합력이 감소하는 것으로 나타났다. 따라서 임상에서 접착제의 적용시 수분의 조절에 주의하여야 할 것으로 사료된다.

Effect of moisture and drying time on the bond strength of the one-step self-etching adhesive system

  • Lee, Yoon;Park, Jeong-Won
    • Restorative Dentistry and Endodontics
    • /
    • 제37권3호
    • /
    • pp.155-159
    • /
    • 2012
  • Objectives: To investigate the effect of dentin moisture degree and air-drying time on dentin-bond strength of two different one-step self-etching adhesive systems. Materials and Methods: Twenty-four human third molars were used for microtensile bond strength testing of G-Bond and Clearfil $S^3$ Bond. The dentin surface was either blot-dried or air-dried before applying these adhesive agents. After application of the adhesive agent, three different air drying times were evaluated: 1, 5, and 10 sec. Composite resin was build up to 4 mm thickness and light cured for 40 sec with 2 separate layers. Then the tooth was sectioned and trimmed to measure the microtensile bond strength using a universal testing machine. The measured bond strengths were analyzed with three-way ANOVA and regression analysis was done (p = 0.05). Results: All three factors, materials, dentin wetness and air drying time, showed significant effect on the microtensile bond strength. Clearfil $S^3$ Bond, dry dentin surface and 10 sec air drying time showed higher bond strength. Conclusions: Within the limitation of this experiment, air drying time after the application of the one-step self-etching adhesive agent was the most significant factor affecting the bond strength, followed by the material difference and dentin moisture before applying the adhesive agent.

Shear bond strength of brackets bonded with different self etching primers (Self etching primer를 사용하여 부착된 교정용 브라켓의 전단결합강도의 비교)

  • Yang, Jin-Young;Kim, Min-Ji;Lim, Yong-Kyu;Lee, Dong-Yul
    • The korean journal of orthodontics
    • /
    • 제37권4호
    • /
    • pp.283-292
    • /
    • 2007
  • The purpose of this study was to evaluate the clinical usefulness of 4 self etching primers by measuring the shear bond strength of orthodontic brackets and examining the failure pattern of bracket-tooth interfaces. Methods: Seventy-five, defect-free, premolars were randomly assigned into five groups: control group (37% phosphoric acid + Transbond XT primer) and self etching primer treated groups (Transbond Plus self etching primer, Unifil bond, Clearfil SE bond, and Adhese). The shear bond strength was measured with a universal testing machine and the amount of residual adhesive remaining on the brackets after debonding was assessed by the adhesive remnant index (ARI). Results: The results showed that the groups conditioned with self etching primer had significantly lower shear bond strength than the control group (p < 0.05), although clinically acceptable. However, there were no significant differences in shear bond strength among the self etching primer groups (p > 0.05). Evaluation of the ARI scores indicated there was less resin remnant on the teeth in the groups conditioned with self etching primers, although not statistically significant. Conclusion: The results of this study suggest that all four of the self etching primers have shown acceptable bond strength for clinical use.

Influence of application time of self-etching primer on bonding to dentin

  • Song, Ki-Gang;Lee, Young-Gon;Cho, Young-Gon
    • Proceedings of the KACD Conference
    • /
    • 대한치과보존학회 2003년도 제120회 추계학술대회 제 5차 한ㆍ일 치과보존학회 공동학술대회
    • /
    • pp.625-625
    • /
    • 2003
  • I. Objectives Self-etching primer adhesive system is affected to dentin surface conditioning and priming. Especially application time of self-etching primer is very important factor of clinical procedure which has direct influence on smear layer, etching reaction and primer penetration to dentin. This study evaluated the influence of application time of self-etching primers on microtensile bond strength (${\mu}{\;}TBS$) to dentin using three self-etching primer adhesive systems.(omitted)

  • PDF

Microtensile bond strength of silorane-based composite specific adhesive system using different bonding strategies

  • Bastos, Laura Alves;Sousa, Ana Beatriz Silva;Drubi-Filho, Brahim;Pires-de-Souza, Fernanda de Carvalho Panzeri;Garcia, Lucas da Fonseca Roberti
    • Restorative Dentistry and Endodontics
    • /
    • 제40권1호
    • /
    • pp.23-29
    • /
    • 2015
  • Objectives: The aim of this study was to evaluate the effect of pre-etching on the bond strength of silorane-based composite specific adhesive system to dentin. Materials and Methods: Thirty human molars were randomly divided into 5 groups according to the different bonding strategies. For teeth restored with silorane-based composite (Filtek Silorane, 3M ESPE), the specific self-etching adhesive system (Adhesive System P90, 3M ESPE) was used with and without pre-etching (Pre-etching/Silorane and Silorane groups). Teeth restored with methacrylate based-composite (Filtek Z250, 3M ESPE) were hybridized with the two-step self-etching system (Clearfil SE Bond, Kuraray), with and without pre-etching (Pre-etching/Methacrylate and Methacrylate groups), or three-step adhesive system (Adper Scotchbond Multi-Purpose, 3M ESPE) (Three-step/Methacrylate group) (n = 6). The restored teeth were sectioned into stick-shaped test specimens ($1.0{\times}1.0mm$), and coupled to a universal test machine (0.5 mm/min) to perform microtensile testing. Results: Pre-etching/Methacrylate group presented the highest bond strength values, with significant difference from Silorane and Three-step/Methacrylate groups (p < 0.05). However, it was not significantly different from Pre-etching/Silorane and Methacrylate groups. Conclusions: Pre-etching increased bond strength of silorane-based composite specific adhesive system to dentin.

Change in shear bond strength of orthodontic brackets using self-etching primer according to adhesive types and saliva contamination (Self-etching primer를 사용하여 교정용 브라켓 접착 시 접착제와 타액오염에 따른 전단결합강도 변화)

  • Nam, Eun-Hye;Yoon, Young-Ah;Kim, Il-Kyu
    • The korean journal of orthodontics
    • /
    • 제35권6호
    • /
    • pp.433-442
    • /
    • 2005
  • The purpose of this study was to evaluate and compare the shear bond strength of orthodontic brackets depending on the variety of adhesives and whether saliva exists, by using self-etching primer (SEP). Groups were divided according to the type of adhesive into resin adhesive (Trans bond XT) and resin-modified glass ionomer cement (Fuji Ortho LC). One group of resin adhesive used XT primer after etching with 37% phosphoric acid, and the other group used self-etching primer. One group of resin-modified glass ionomer cement only used etching for bonding, and the other group used SEP. Each of the groups were also classified by whether saliva was contaminated or not. and then the shear bond strength was measured. The results showed that when using resin adhesive, the shear bond strength of SEP was lower than the XT primer. In the resin-modified glass ionomer cement groups, the shear bond strength which depends on the priming method, did not have a meaningful difference statistically When saliva was contaminated, the group which used SEP, regardless of the adhesive variety, had a greater shear bond strength than the normal priming group. From these results, SEP showed a shear bond strength that is possible to be used clinically, regardless of the adhesive variety. It can especially be clinically useful to use SEP to bond brackets even on tooth surfaces contaminated with saliva, because it offers the appropriate bonding strength as well as shorter treatment time and easy application.

RESIN TAG FORMATION OF SELF-ETCHING ADHESIVES (자가부식 접착제의 레진 Tag 형성)

  • Kim, Young-Jae;Jang, Ki-Taeg
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • 제30권1호
    • /
    • pp.143-152
    • /
    • 2003
  • The aims of the present study was to observe resin tag of the resin/enamel, dentin interface produced by self-etching adhesive systems and evaluate effect of additional acid etching on resin tag formation. Three self-etching primer(SE bond, AQ bond and L Pop) and an one bottle adhesive(Single bond) were used. Flat occlusal enamel and dentin disks were obtained from extracted human molars. A total of 20 surfaces were collected and divided into four groups of 5 samples. One-half of each specimen in each group was etched with 35% phosphoric acid prior to the application of each adhesive system, with the second half being kept unetched. Subsequently, resin composite was placed and polymerized. The samples were sliced and immersed into HCl and NaOCl solutions, followed by drying and sputter coating for examination with a SEM. The results were as follows; 1. Additional etching side of dentin displayed longer and thicker resin tag than unetched side in all self-etching adhesive groups. 2. In enamel, additional etching side displayed deeper and more distinct etching pattern than unetched side except L Pop. There is no difference between etched and unetched enamel in L Pop. The results obtained suggest the self-etching adhesive did not etch enamel and penetrate into dentinal tubule as deeply as did additional etching. Further research should include the evaluation of the relationship of boding strength, microleakage and resin tag morphology.

  • PDF

THE EVALUATION OF MICROLEAKAGE OF PIT AND FISSURE SEALANT BY USAGE OF SELF-ETCHING ADHESIVE SYSTEM (자가 산부식 접착제를 이용한 치면열구전색의 미세누출 평가)

  • Kim, Hyun-Jin;Lee, Nan-Young;Lee, Sang-Ho
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • 제35권2호
    • /
    • pp.216-224
    • /
    • 2008
  • The purpose of this study was to evaluate the effectiveness of fissurotomy and double application time of acidic primer of self-etching adhesive system of acid treatment on enamel surfaces for prevention of microleakage of pit and fissure sealants. The microleakage of pit and fissure sealants was evaluated by measuring the penetration depth of methylene blue solution. Specimens were divided by 4 groups according to the method of treatment. Group I: 35% phosphoric acid etching, 20 seconds. Group II: Priming with self-etching primer, 20 seconds. Group III: Priming with self-etching primer, 40 seconds. Group IV: Priming with self-etching primer, 20 seconds, after fissurotomy. The etched pattern produced on enamel was observed using a scanning electron microscope. Obtained data were analysed statistically using Kruscal-Wallis test followed by Mann-Whitney test for comparison of groups. The results are as follows: 1. Microleakage scores of group IV priming with self-etching primer 20 seconds after fissurotomy was the lowest. 2. Microleakage scores between group II and group III were not shown significant difference. 3. Enamel for 20 seconds etching with 35% phosphoric acid was observed the most effective etching pattern. And the etching pattern on the fissure enamel with self-etching adhesive 20 seconds after fissurotomy was more prominent than group II, III only using self-etching primer.

  • PDF