The surface characteristics of polymers for liquid crystal alignment are studied by optical second-harmonic genertion (SHG) tecnique. Using SHG technique, the LC monolayers on rubbed polymer have already been studied. But, in this paper, the SH signals of polymer were observed and the orientational distribution of oriented polymer was studied. Te SHG experiments for side-chain type and main-chain type polymers are carried out as a function of rubbing strength. The orentational distribution of surface molecules of polymers is compared with the LC pretilt angle measured by the crystal rotation method.
Kim, Taekyeong;Park, Jihoon;Lee, Junheon;Kim, Taegun
Textile Coloration and Finishing
/
v.29
no.4
/
pp.223-230
/
2017
Three super hydrophobic fluorescence dyes were selected to dye high molecular weight polyethylene fiber and their molar absorptivity, emission spectrum, and quantum yield were measured. From the results of color strength on the fiber, all the three dyes exhibited linear increase according to the dye concentration and Fluoro3 dye showed the highest color strength among them. Emission strength of the fluorescence dyes on the fiber was investigated according to the dye concentrations. The emission was increased with the increase of the dye concentration at relatively low dye concentration and then after showing the maximum emission strength the emission was decreased at higher dye concentrations. The highest emission was obtained in Fluoro2 dye. Color fastness to washing and rubbing was generally good enough, however, especially to light, only Fluoro3 dye exhibited rating 3 acceptable practically and Fluoro1 and 2 was ratings 1 which is unacceptable level.
Proceedings of the Polymer Society of Korea Conference
/
2006.10a
/
pp.240-240
/
2006
Thin films of poly(vinyl cinnamate) (PVCi) were prepared on indium tin oxide (ITO) glass and silicon substrates by conventional spin coating and subsequent drying process. The thicknesses of the films ranged 50-120 nm. The films' surface was treated by rubbing, ultraviolet exposure or their combinations in various ways with changing rubbing strength and exposure dose. These films were examined in detail in the aspects of surface morphology and chain orientation. Further, the anchoring and orientation behaviors of liquid crystals on the film surfaces were investigated. All the results will be discussed in detail.
Kim, Hyungjin;Park, Seongmin;Kwon, Woong;Jeong, Euigyung
Textile Coloration and Finishing
/
v.34
no.1
/
pp.10-19
/
2022
Humectants are chemical compounds which added to water based pigment inks for DTP (Digital Textile Printing) to prevent evaporation of water. The humectants usually have diol or triol type chemical structures and their -OH groups have possibility to react with functional groups of the binder polymers, such as ester, carboxylic acid, and urethane groups, acting as a crosslinking agent. The crosslinking reactions between polymer binders and humectants in inks can affect touch of the printed fabrics. In this regard, this study aims to investigate effect of chemical structures and added amounts of humectants in pigment ink on touch of dyed fabrics by using 1,6-hexanediol, ethylene glycol, diethylene glycol, and 1,4-buthanediol with various amounts added to the mixture of a black pigment and a polyurethane type binder. Then, color, rubbing strength, touch of the fabrics dyed with the prepared pigment inks were evaluated.
Dyeing process of the natural indigo powder onto ramie and silk fabrics was investigated by using glucose and calcium hydroxide as a reducing system. Effect of reduction and dyeing conditions such as temperature and time of reduction/dyeing, and concentrations of glucose and calcium hydroxide on the dyeing process were explored. Indigo powder was obtained by drying the conventional niram paste in an oven at $50^{\circ}C$. Color strength of the dyed fabrics was evaluated by K/S value measured at the wavelength of maximum absorption(${\lamda}$max). Munsell color coordinates(H V/C) were used to compare fabric colors of ramie and silk. Ramie fabric showed purple-blue color for all the temperature and time. On the contrary, silk fabric showed wide range of color including brown, brown-green, green at the different temperature. With the increase of K/S value, the coordinate of value(lightness) decreased for both of ramie and silk fabrics. The coordinate of hue(shade) changed drastically with the increase of K/S value for silk fabric, compared with that of ramie fabric which showed nearly constant value at the whole range of K/S value. Optimum concentrations of calcium hydroxide were for 6 g/L for ramie and 4 g/L for silk at $60^{\circ}C$ and 50 min. K/S value increased with the indigo concentration. Maximum K/S value was shown at $10{\sim}12$ g/L of glucose concentration. For both of ramie and silk fabrics, the colorfastness of washing and light was lower than that of rubbing. All the colorfastness values were improved with the increase of color strength.
Journal of the Korean Society of Clothing and Textiles
/
v.48
no.4
/
pp.707-728
/
2024
This study aimed to assess the colorizing properties of bacterial cellulose (BC) using plant-based dyes, namely spinach, beet, and banana peel, and determine the dyeing conditions of each dye based on color strength (K/S) values. Tannic acid and walnut shell powder were utilized as bio-mordants, and their effects on the dyeability of BC were compared to metallic mordants. Additionally, the type of mordant and the mordanting method were assessed according to their rubbing fastness and dry-cleaning fastness. The K/S values of the colorized and mordanted BCs were also compared to examine their mordanting conditions. Finally, the mordanting conditions for spinach, beet, and banana peel dyeing were selected as post-mordanting with tannic acid, meta-mordanting with tannic acid, and post-mordanting with walnut shell powder, respectively. Based on the results, the selected mordanting conditions improved both rubbing fastness and dry-cleaning fastness of BCs to grade 5, and the light fastness achieved grade 4-5. The tensile strength and flexibility of the dyed BCs were also enhanced and comparable to that of untreated cowhide leather.
In this paper, a new regenerated celluosic fiber, "Tencel" was treated with cellulase enzyme. Also Tencel fabrics were pretreated with NaOH and dyed with various reactive dyes, and subsequently finished with DMDHEU. $\Delta{E}^*_{ab}$ value was calculated by measuring color difference before and after wet abrasion test to rubbing. The fibrillation propensity was estimated on Tencel by means of weight loss, $\Delta{E}^*_{ab}$ value, and SEM observation. Weight loss of NaOH pretreated Tencel fabric is more lower than that of original fabric. The cellulase treatment decreased tensile strength but improved wet abrasion strength, wrinkle recovery, and bending properties. Tendency of fibrillation for Tencel fabric was reduced by NaOH-pretreatment, dyeing with multifunctional reactive dyes, and afterfinishing by DMDHEU.by DMDHEU.
Wool fabrics were treated with deep UV for 10 to 30min and then dyed with C.I. Acid Yellow 99, C.I, Acid Red 57 and C.I. Acid Blue 62. FT-IR and XPS have been used to prove the chemical composition of wool fiber surfaces. The mechanical property and colorfastness were also studied. The intencities of the peaks of C=O group at $1700^cm^{-1}$ were increased with increasing irradiation time. Relative $O_{1s},\; N_{1s}\; and\; S_{2p}$ intensities increased considerably and oxygen was incorporated in the form of CO and COO on the fiber surface. The dye uptakes of wool fabrics dyed with three acid dyes were proportional to irradiation times and in inversely proportional to irradiation distances. It was found that the tensile strength of wool fabrics were gradually deteriorated with the UV irradiation times. The colorfastness, such as washing, light and rubbing, of UV irradiated wool fabrics dyed with acid dyes were good.
This study investigated effect of particle sizes of polymer binders for digital textile printing(DTP) pigment inks on touch of fabrics. The polymer binders were synthesized via miniemulsion polymerization of methyl methacrylate(MMA), butyl acrylate(BA), N-ethylolacrylamide(NEA) and methacrylic acid(MAA). The prepared binders were applied to black pigment inks and those black pigment inks were used to dye cotton fabrics. Then, color strength, rubbing fastness, stiffness, surface and bending properties of the dyed fabrics were investigated. Depending on the particle size of the polymer binder used, color strength, friction fastness, stiffness, surface and bending properties change. Generally, the larger the particle size of the polymer binder, the softer properties.
The present study was conducted to investigate dyeing properties and functionality of silk fabrics dyed with extracts from buckwheat skin. Comparative results of color strength(K/S) values of dyed silk fabrics were studied to quantify the effects of dye concentrations, dyeing temperatures, dyeing time and the pH; the effect of mordants; and color changes. And also evaluated the fastness, antimicrobial property, ultraviolet protection properties of the dyed and mordanted silk fabrics. The color strength(K/S) values of silk generally increased depending on the increasing dye concentration, dyeing temperature, and dyeing time. And the highest color strength values were obtained at a dye concentration of 100%(v/v), a dyeing temperature of $90^{\circ}C$, a dyeing of time 80 minutes, and a dyebath of pH 2. The color fastness to light of dyed and mordanted silk fabrics were found to be good, and the drycleaning and rubbing fastness were excellent. The fade of washing fastness was not good, however, the stain of washing fastness and perspiration fastness showed relatively good grade. The Al, Cu, Fe mordanted silk fabrics(except Fe for Klebsiella pneumoniae) showed 99.9% reduction rate. The ultraviolet protection properties of the mordanted fabrics were generally improved. Moreover, the Cu and Fe mordnared fabrics showed very exceptional ultraviolet protection factors.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.