• 제목/요약/키워드: rock-concrete disc

검색결과 9건 처리시간 0.02초

Investigation of ratio of TBM disc spacing to penetration depth in rocks with different tensile strengths using PFC2D

  • Sarfarazi, Vahab;Haeri, Hadi;Shemirani, Alireza Bagher;Hedayat, Ahmadreza;Hosseini, Seyed Shahin
    • Computers and Concrete
    • /
    • 제20권4호
    • /
    • pp.429-437
    • /
    • 2017
  • In this study, the effect of the tensile strength and ratio of disc spacing to penetration depth on the efficiency of tunnel boring machine (TBM) is investigated using Particle flow code (PFC) in two dimensions. Models with dimensions of $150{\times}70mm$ made of rocks with four different tensile strength values of 5 MPa, 10 MPa, 15 MPa and 20 MPa were separately analyzed and two "U" shape cutters with width of 10 mm were penetrated into the rock model by velocity rate of 0.1 mm/s. The spacing between cutters was also varied in this study. Failure patterns for 5 different penetration depths of 3 mm, 4 mm, 5 mm, 6 mm, and 7 mm were registered. Totally 100 indentation test were performed to study the optimal tool-rock interaction. An equation relating mechanical rock properties with geometric characteristics for the optimal TBM performance is proposed. The results of numerical simulations show that the effective rock-cutting condition corresponding to the minimum specific energy can be estimated by an optimized disc spacing to penetration depth, which, in fact, is found to be proportional to the rock's tensile strength.

The effect of ball size on the hollow center cracked disc (HCCD) in Brazilian test

  • Haeri, Hadi;Sarfarazi, Vahab;Zhu, Zheming;Moradizadeh, Masih
    • Computers and Concrete
    • /
    • 제22권4호
    • /
    • pp.373-381
    • /
    • 2018
  • Hollow center cracked disc (HCCD) in Brazilian test was modelled numerically to study the crack propagation in the pre-cracked disc. The pre-existing edge cracks in the disc models were considered to investigate the crack propagation and coalescence paths within the modelled samples. The effect of particle size on the hollow center cracked disc (HCCD) in Brazilian test were considered too. The results shows that Failure pattern is constant by increasing the ball diameter. Tensile cracks are dominant mode of failure. These crack initiates from notch tip, propagate parallel to loading axis and coalescence with upper model boundary. Number of cracks increase by decreasing the ball diameter. Also, tensile fracture toughness was decreased with increasing the particle size. In this research, it is tried to improve the understanding of the crack propagation and crack coalescence phenomena in brittle materials which is of paramount importance in the stability analyses of rock and concrete structures, such as the underground openings, rock slopes and tunnel construction.

Experimental study on rock-concrete joints under cyclically diametrical compression

  • Chang, Xu;Guo, Tengfei;Lu, Jianyou;Wang, Hui
    • Geomechanics and Engineering
    • /
    • 제17권6호
    • /
    • pp.553-564
    • /
    • 2019
  • This paper presents experimental results of rock-concrete bi-material discs under cyclically diametrical compression. It was found that both specimens under cyclical and static loading failed in three typical modes: shear crack, tensile crack and a combined mode of shear and wing crack. The failure modes transited gradually from the shear crack to the tensile one by increasing the interface angle between the interface and the loading direction. The cycle number and peak load increased by increasing the interface angle. The number of cycles and peak load increased with the interface groove depth and groove width, however, decreased with increase in interface groove spacing. The concrete strength can contribute more to the cycle number and peak load for specimens with a higher interface angle. Compared with the discs under static loading, the cyclically loaded discs had a lower peak load but a larger deformation. Finally, the effects of interface angle, interface asperity and concrete strength on the fatigue strength were also discussed.

Evaluation of rock cutting efficiency of the actuated undercutting mechanism

  • Jeong, Hoyoung;Wicaksana, Yudhidya;Kim, Sehun;Jeon, Seokwon
    • Geomechanics and Engineering
    • /
    • 제29권3호
    • /
    • pp.359-368
    • /
    • 2022
  • Undercutting using an actuated disc cutter (ADC) involves more complex cutting mechanism than traditional rock cutting does, requiring the application of various new cutting parameters, such as eccentricity, cutter inclination angle, and axis rotational speed. This study presents cutting-edge laboratory-scale testing equipment that allows performing ADC tests. ADC tests were carried out on a concrete block with a specified strength of 20 MPa, using a variety of cutting settings that included penetration depth (p), eccentricity (e), and linear velocity (v). ADC, unlike pick and disc cutting, has a non-linear cutting path with a dynamic cutting direction, requiring the development of a new method for predicting cutting force and specific energy. The influence of cutting parameters to the cutter forces were discussed. The ratio of eccentricity to the penetration depth (e/p) was proposed to evaluate the optimal cutting condition. Specific energy varies with e/p ratio, and exhibits optimum values in particular cases. In general, actuated undercutting may potentially give a more efficient cutting than conventional pick and disc cutting by demonstrating reasonably lower specific energy in a comparable cutting environment.

Estimation of tensile strength and moduli of a tension-compression bi-modular rock

  • Wei, Jiong;Zhou, Jingren;Song, Jae-Joon;Chen, Yulong;Kulatilake, Pinnaduwa H.S.W.
    • Geomechanics and Engineering
    • /
    • 제24권4호
    • /
    • pp.349-358
    • /
    • 2021
  • The Brazilian test has been widely used to determine the indirect tensile strength of rock, concrete and other brittle materials. The basic assumption for the calculation formula of Brazilian tensile strength is that the elastic moduli of rock are the same both in tension and compression. However, the fact is that the elastic moduli in tension and compression of most rocks are different. Thus, the formula of Brazilian tensile strength under the assumption of isotropy is unreasonable. In the present study, we conducted Brazilian tests on flat disk-shaped rock specimens and attached strain gauges at the center of the disc to measure the strains of rock. A tension-compression bi-modular model is proposed to interpret the data of the Brazilian test. The relations between the principal strains, principal stresses and the ratio of the compressive modulus to tensile modulus at the disc center are established. Thus, the tensile and compressive moduli as well as the correct tensile strength can be estimated simultaneously by the new formulas. It is found that the tensile and compressive moduli obtained using these formulas were in well agreement with the values obtained from the direct tension and compression tests. The formulas deduced from the Brazilian test based on the assumption of isotropy overestimated the tensile strength and tensile modulus and underestimated the compressive modulus. This work provides a new methodology to estimate tensile strength and moduli of rock simultaneously considering tension-compression bi-modularity.

Simulation of fracture mechanism of pre-holed concrete model under Brazilian test using PFC3D

  • Sarfarazi, Vahab;Haeri, Hadi;Shemirani, Alireza Bagher
    • Smart Structures and Systems
    • /
    • 제22권6호
    • /
    • pp.675-687
    • /
    • 2018
  • In the previous studies on the porous rock strength the effect of pore number and its diameter is not explicitly defined. In this paper crack initiation, propagation and coalescence in Brazilian model disc containing a single cylindrical hole and or multiple holes have been studied numerically using PFC3D. In model with internal hole, the ratio of hole diameter to model diameter was varied between 0.03, 0.17, 0.25, 0.33, and 0.42. In model with multiple hole number of holes was different in various model, i.e., one hole, two holes, three holes, four holes, five holes, six holes, seven holes, eight holes and nine holes. Diameter of these holes was 5 mm, 10 mm and 12 mm. The pre-holed Brazilian discs are numerically tested under Brazilian test. The breakage load in the ring type disc specimens containing an internal hole with varying diameters is measured. The mechanism of cracks propagation in the wall of the ring type specimens is also studied. In the case of multi-hole Brazilian disc, the cracks propagation and b cracks coalescence are also investigated. The results shows that breaking of the pre-holed disc specimens is due to the propagation of radially induced tensile cracks initiated from the surface of the central hole and propagating toward the direction of diametrical loading. In the case of disc specimens with multiple holes, the cracks propagation and cracks coalescence may occur simultaneously in the breaking process of model under diametrical compressive loading. Finally the results shows that the failure stress and crack initiation stress decreases by increasing the hole diameter. Also, the failure stress decreases by increasing the number of hole which mobilized in failure. The results of these simulations were comprised with other experimental and numerical test results. It has been shown that the numerical and experimental results are in good agreement with each other.

Direct and indirect methods for determination of mode I fracture toughness using PFC2D

  • Sarfarazi, Vahab;Haeri, Hadi;Shemirani, Alireza Bagher
    • Computers and Concrete
    • /
    • 제20권1호
    • /
    • pp.39-47
    • /
    • 2017
  • In this paper, mode I fracture toughness of rock was determined by direct and indirect methods using Particle Flow Code simulation. Direct methods are compaction tension (CT) test and hollow centre cracked quadratic sample (HCCQS). Indirect methods are notched Brazilian disk (NBD) specimen, the semi-circular bend (SCB) specimen, hollow centre cracked disc (HCCD), the single edge-notched round bar in bending (SENRBB) specimen and edge notched disk (END). It was determined that which one of indirect fracture toughness values is close to direct one. For this purpose, initially calibration of PFC was undertaken with respect to data obtained from Brazilian laboratory tests to ensure the conformity of the simulated numerical models response. Furthermore, the simulated models in five introduced indirect tests were cross checked with the results from direct tests. By using numerical testing, the failure process was visually observed. Discrete element simulations demonstrated that the macro fractures in models are caused by microscopic tensile breakages on large numbers of bonded discs. Mode I fracture toughness of rock in direct test was less than other tests results. Fracture toughness resulted from semi-circular bend specimen test was close to direct test results. Therefore semi-circular bend specimen can be a proper test for determination of Mode I fracture toughness of rock in absence of direct test.

유도초음파의 반사법을 이용한 록볼트 그라우팅의 결함비율 평가 (Defect ratio evaluation of the rock bolt grouting using the reflection method of guided ultrasonic waves)

  • 유정동;배명호;한신인;이인모;이종섭
    • 한국터널지하공간학회 논문집
    • /
    • 제10권3호
    • /
    • pp.221-232
    • /
    • 2008
  • 록볼트는 지하구조물의 주지보재로 적용되고 있다. 록볼트 건전도 평가를 위한 비파괴 방법으로 유도초음파의 투과법을 이용한 기법이 우수한 결과를 보여주고 있다. 하지만 투과법은 철근의 양 끝단에 센서를 부착하기 때문에 암반에 이미 설치되어 있는 록볼트의 건전도 평가는 불가능하다. 본 연구의 목적은 록볼트 철근 두부에 가진센서와 수진센서를 나란히 설치하여 선단에서 반사되어 오는 파를 측정하는 반사법을 자유구속조건 및 지중관입조건에 적용하며, 이를 투과법과 비교하는데 있다. 유도초음파의 가진과 수진을 위해 피에조 디스크 엘리먼트와 AE 센서를 사용하였으며, 측정된 신호로부터 웨이브렛 변환을 통하여 에너지 속도를 산정하였다. 실험결과, 반사법의 결과가 투과법과 거의 일치하였으며, 결함비율이 증가함에 따라 에너지 속도가 증가하는 것으로 나타났다. 본 논문은 유도초음파의 반사법이 록볼트 건전도 평가에 있어 현장 적용 가능성 있는 방법이 될 수 있음을 보여준다.

  • PDF

암석재료 인장강도의 동적 증가계수 및 변형률 속도 의존성에 대한 실험적 연구 (An Experimental Study on the Dynamic Increase Factor and Strain Rate Dependency of the Tensile Strength of Rock Materials)

  • 오세욱;최병희;민경조;정용복;조상호
    • 화약ㆍ발파
    • /
    • 제39권1호
    • /
    • pp.10-21
    • /
    • 2021
  • 암석이나 콘크리트와 같은 취성재료는 재료에 동하중이 가해질 때에는 큰 변형률속도 의존성을 보인다. 이는 취성재료의 역학적 성질이 하중속도에 따라 크게 변화할 수 있음을 의미한다. 이런 성질 때문에 취성재료의 변형률속도 의존성은 발파공학이나 암석동역학 문제를 풀 때 반드시 고려해야 할 중요한 사항들 중의 하나이다. 하지만 불행하게도 국내의 경우, 암석이나 여타의 취성재료들의 동적물성을 특성화하는 연구들은 아직 미진한 상태에 있다. 본 연구에서는 거창 화강암과 고강도 콘크리트 시편의 동적특성을 파악하기 위해 홉킨슨 압력봉을 이용하여 동적 인장시험을 실시하였다. 시험방법으로는 ISRM이 제안한 동적 압열시험과 박리시험을 채택하였다. 일반적으로, 고변형률속도 하에서는 후자의 방법이 더 우수한 것으로 알려져 있다. 이들 두 종류의 시험을 실시한 결과, 시편들의 동적 인장강도가 거의 비슷하게 나타났다. 하지만 저자들은 애초에 시험방법에 따라 측정강도가 상이할 것으로 예상했었다. 따라서 서로 다른 방법을 적용했음에도 측정 강도가 비슷하게 나타난 것은 오히려 시험과정에서 어떤 오류가 개입된 것으로도 볼 수 있으므로 후속연구를 통해 이 부분에 대해 상세조사를 수행할 예정이다.