Washing Effects according to the Rinsing Conditions and the Characteristics of Soiled Fabrics (오염포의 특성과 헹구기 조건에 따른 세척 효과)

  • Jo, Won-Joo;Lee, Deug-Hee;Park, Eun-Jin;Lee, Jeong-Sook
    • Fashion & Textile Research Journal
    • /
    • v.13 no.3
    • /
    • pp.425-431
    • /
    • 2011
  • The purpose of this study was to investigate washing effects according to the rinsing conditions and the characteristics of soiled fabrics. In this study rinsing conditions including rinsing cycle, time, temperature, and bath ratio were examined. The foamability of rinsing bath was also examined. The quantity of LAS in the rinsing bath and extracts of test fabrics was analyzed after washing and rinsing, respectively. The results of these experiments were as follows: The washing effects of soiled fabrics were varied from the kinds of soils and rinsing conditions. The removal of soils from fabrics was increased by the first rinsing after washing effectively. The priorities of rinsing conditions were rinsing temperature> rinsing time > rinsing cycles> references. Foamability was result from residual LAS in rinsing bath and fabrics extracts after rinsing. The residual quantity of LAS was references > rinsing cycles> rinsing time> rinsing temperature, which shown rinsing temperature was the most efficient factor of the rinsing performance.

Effect of different chlorhexidine application times on microtensile bond strength to dentin in Class I cavities

  • Kang, Hyun-Jung;Moon, Ho-Jin;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.37 no.1
    • /
    • pp.9-15
    • /
    • 2012
  • Objectives: This study evaluated the effect of 2% chlorhexidine digluconate (CHX) with different application times on microtensile bonds strength (MTBS) to dentin in class I cavities and intended to search for ideal application time for a simplified bonding protocol. Materials and Methods: Flat dentinal surfaces with class I cavities ($4mm{\times}4mm{\times}2mm$) in 40 molar teeth were bonded with etch-and-rinse adhesive system, Adper Single Bond 2 (3M ESPE) after: (1) etching only as a control group; (2) etching + CHX 5 sec + rinsing; (3) etching + CHX 15 sec + rinsing; (4) etching + CHX 30 sec + rinsing; and (5) etching + CHX 60 sec + rinsing. Resin composite was builtup with Z-250 (3M ESPE) using a bulk method and polymerized for 40 sec. For each condition, half of the specimens were immediately submitted to MTBS test and the rest of them were assigned to thermocycling of 10,000 cycles between $5^{\circ}C$ and $55^{\circ}C$ before testing. The data were analyzed using two-way ANOVA, at a significance level of 95%. Results: There was no significant difference in bond strength between CHX pretreated group and control group at the immediate testing period. After thermocycling, all groups showed reduced bond strength irrespective of the CHX use. However, groups treated with CHX maintained significantly higher MTBS than control group (p < 0.05). In addition, CHX application time did not have any significant influence on the bond strength among groups treated with CHX. Conclusion: Application of 2% CHX for a short time period (5 sec) after etching with 37% phosphoric acid may be sufficient to preserve dentin bond strength.

A Facile synthesis of CoS by Successive Ionic Layer Adsorption and Reaction (SILAR) Process for Supercapacitors (스테인리스강 기판에 연속 이온 층 흡착 및 반응 (SILAR) 공정을 통한 CoS 코팅 및 슈퍼캐패시터 전극 특성)

  • Kim, Jaeseung;Lee, Jaewon;Kumbhar, Vijay S.;Choi, Jinsub;Lee, Kiyoung
    • Journal of Surface Science and Engineering
    • /
    • v.52 no.3
    • /
    • pp.130-137
    • /
    • 2019
  • In this study, the cobalt sulfide (CoS) nanosheet on stainless steel as a supercapacitor electrode is synthesized by using a facile successive ionic layer adsorption reaction (SILAR) method. The number of cycles for dipping and rinsing can control the nanosheet thickness of CoS on stainless steel. Field emission-scanning electron microscopy (FE-SEM) showed a layer structure of CoS particles coupled as agglomeration. And x-ray diffraction (XRD) showed the crystallinity of the CoS nanosheet. To investigate the characteristics of the CoS nanosheet electrode as the supercapacitor, analysis of electrochemical measurement was conducted. Finally, the CoS nanosheet of 70cycles on stainless steel shows the specific capacitance ($44.25mF/cm^2$ at $0.25mA/cm^2$) with electrochemical stability of 78.5% over during 2000cycles.

Effect of chlorhexidine application on the bond strength of resin core to axial dentin in endodontic cavity

  • Kim, Yun-Hee;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.37 no.4
    • /
    • pp.207-214
    • /
    • 2012
  • Objectives: This study evaluated the influence of chlorhexidine (CHX) on the microtensile bonds strength (${\mu}TBS$) of resin core with two adhesive systems to dentin in endodontic cavities. Materials and Methods: Flat dentinal surfaces in 40 molar endodontic cavities were treated with self-etch adhesive system, Contax (DMG) and total-etch adhesive system, Adper Single Bond 2 (3M ESPE) after the following surface treatments: (1) Priming only (Contax), (2) CHX for 15 sec + rinsing + priming (Contax), (3) Etching with priming (Adper Single Bond 2), (4) Etching + CHX for 15 sec + rinsing + priming (Adper Single Bond 2). Resin composite build-ups were made with LuxaCore (DMG) using a bulk method and polymerized for 40 sec. For each condition, half of specimens were submitted to ${\mu}TBS$ after 24 hr storage and half of them were submitted to thermocycling of 10,000 cycles between $5^{\circ}C$ and $55^{\circ}C$ before testing. The data were analyzed using ANOVA and independent t-test at a significance level of 95%. Results: CHX pre-treatment did not affect the bond strength of specimens tested at the immediate testing period, regardless of dentin surface treatments. However, after 10,000 thermocycling, all groups showed reduced bond strength. The amount of reduction was greater in groups without CHX treatments than groups with CHX treatment. These characteristics were the same in both self-etch adhesive system and total-etch adhesive system. Conclusions: 2% CHX application for 15 sec proved to alleviate the decrease of bond strength of dentin bonding systems. No significant difference was shown in ${\mu}TBS$ between total-etching system and self-etching system.

Study on the Surface Activity of Rhamnolipid (RL) and Function of RL in Liquid Detergent (람노리피드의 계면특성 및 액체세정제에서의 기능에 대한 연구)

  • Chi, Gyeong-Yup;Lim, JongChoo
    • Applied Chemistry for Engineering
    • /
    • v.29 no.6
    • /
    • pp.753-758
    • /
    • 2018
  • Surface activities including CMC, surface tension, foaming power etc. of the rhamnolipid (RL), a biosurfactant fermented by microorganism were investigated. Both the RL and liquid detergent contained RL showed a good surface activity. For the detergency test, the liquid detergent with RL showed a slightly better performance than that of using an fatty acid. However for the foaming profile, the liquid detergent with RL exhibited a lot of foam volume and the suppression of the rinsing and foaming during rinsing cycles with the RL was not seen. Therefore it can be concluded that RL can be used as a main surfactant or co-surfactant in liquid detergents without functions of foaming suppression or rinse-aid.

The Effects of Laundering Conditions on Calcium Deposition on the Fabric (세척조건이 직물에의 Calcium 침착에 미치는 영향)

  • Moon Young Ae;Kahng He Won;Kim Sung Reon
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.5 no.1
    • /
    • pp.9-14
    • /
    • 1981
  • The influence of laundering conditions on calcium deposition on the fabric was studied by repeated laundering the cotton fabric with soap in the hard water of 200 P.P.M. $CaCO_3$. The experimental variables were: 1) soap concentrations ($0.06\%$, $0.13\%$, $0.25\%$), 2) water contents in the fabric after hydroextraction. ($65\%$, $150\%$, $315\%$), 3) builders (Na-EDTA, sodium carbonate, sodium metasilicate), 4) washing cycle (5, 10, 15, 20 cycles). The fabric was washed for 15 minutes at $23\pm1^{\circ}C$ in a washing machine (Model; Gold Star Wp-2005) under the similar conditions with those of home laundering, and rinsed 5 times for 5 minutes. The amount of calcium deposits on the fabric was determined by the EDTA-Back titration method described by Wasserman and Basch. Results of this study were follows: 1) The amount of calcium deposits on the fabric increased with increasing wash cycles. 2) During the rinsing process, residual calcium content on the fabric increased with water content in the fabric after hydroextraction. 3) The amount of calcium deposits on the fabric decreased with the increasing soap concentration above the equivalent amount of calcium ion content in the water. 4) Sequestering agents and alkaline builders influenced the amount of calcium deposits on the fabric. The amount of calcium deposits on the fabric was in the order of sodium metasilicate, sodium carbonate, nonbuilder, and EDTA.

  • PDF

The Actual Management State of Trial Contact Lenses and Lens Care Products in Local Optical Shops (안경원의 시험착용 콘택트렌즈 및 관리용품 관리 실태)

  • Park, Mijung;Lee, Unjung;Kim, So Ra
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.16 no.4
    • /
    • pp.391-401
    • /
    • 2011
  • Purpose: In the present study, the actual management state of trial contact lenses and lens care products in local optical shops was surveyed and analyzed to reduce the risk of lens complication possibly induced by neglecting lens care. Methods: The feeling of contact lens wearers during the wear of trial contact lenses was surveyed. Futhermore, the actual management state of trial contact lenses such as cosmetic lens and RGP lens and lens care products was also investigated by surveying opticians who trade contact lenses in local optical shops. Results: It was found that consumers trusted the sanitary conditions of the lens since trial cosmetic contact lens and RGP lens were cleaned before and after trails by over 98% of opticians in local optical shops. For trial cosmetic lens, cleaning with normal saline, multipurpose solution for soft lens and combination of saline and multipurpose solution were 38.5%, 40.5% and 21%, respectively, before trials. After trials, cosmetic lenses were cleaned with normal saline, multipurpose solution for soft lens and a combination of saline and multipurpose solution were 13%, 75%, and 12%, respectively. On the other hand, cleaning with normal saline, multipurpose solution for RGP lens and combination of saline and multipurpose solution were 28.5%, 38.5% and 33%, respectively, before trying trial RGP lens. After trials, RGP lenses were cleaned with normal saline, multipurpose solution for RGP lens and a combination of saline and multipurpose solution were 2.5%, 70%, and 27.5%, respectively, indicating that relatively many opticians followed the lens cleaning regimen. In local optical shops, the cleaning trial cosmetic lens was mainly conducted at every 10 days or a month and the washing cycle of cosmetic lens case was in a month or 2~3 months. The cleaning interval of trial RGP lens was primarily in a month or 2~3 months. For those lens cases, more than 75% of opticians washed them with a surfactant and then rinsed with cold water. The storing periods of lens care products were primarily in a week for saline and in a month and 2~3 months indicating that storing period of lens care products was relatively well-kept in local optical shops. Conclusions: It is thought that the concern about any microbial infection is not that high since trial contact lenses and lens care products were generally well-managed by opticians in local optical shops from the results above. However, better public eye health and better public confidence in opticians may be possible if further strengthen in avoidance of lens cleaning with saline, keep of cleaning cycles within 2 weeks and rinsing of lens cases with hot water happens.