쇼트피이닝 가공된 스프링강의 저온 피로균열진전 평가 (A Study on the Shot Peening on the Low Temperature Fatigue Crack Propagation)

  • 박경동;정찬기;하경준;박상오;손명군;노영석
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 추계학술대회 논문집
    • /
    • pp.282-286
    • /
    • 2001
  • In this study, CT specimens were prepared from spring steel(SUP9) processed shot peening which was room temperature, low temperature and high temperature experiment. And we got the following characteristics from fatigue crack growth test carried out in the environment of room, low temperature and high temperature at $25^{\circ}C$,$-30^{\circ}C$,$-50^{\circ}C$,$-70^{\circ}C$ and $-100^{\circ}C$ in the range of stress ratio of 0.05 by means of opening mode displacement. The threshold stress intensity factor range $\Delta K_{th}$ in the early stage of fatigue crack growth (Region I ) and stress intensity factor range $\Delta K$ in the stable of fatigue crack growth (Region II) was decreased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature and high temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region.

  • PDF

해양구조용강의 피로강도향상 공법개발 (The Development Methods of Fatigue Strength Improvement for the Marine Structural Steel)

  • 박경동;정재욱
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2003년도 추계학술대회 논문집
    • /
    • pp.106-111
    • /
    • 2003
  • This study made an experiment On fatigue crack propagation da/dn, stress intensity factor range ${\Delta}K$ respectively in room temperature and in low temperature. And we got the following characteristics from fatigue crack growth test carried Out in the environment of room temperature and law temperature at $25^{\circ}C$, $-60^{\circ}C$, $-80^{\circ}C$, and $-100^{\circ}C$ in the range of stress ratio of 0.3 by means of opening made displacement. The threshold stress intensity factor range ${\Delta}Kth$ in the early stage of fatigue crack growth (Mode I) and stress intensity factor range ${\Delta}K$ in the stable of fatigue crack growth (Made II) was decreased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at law temperature and high temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region.

  • PDF

$MgB_2$ 초전도 박막의 경이온 조사에 의한 효과 (Effects of Light-ion Irradiation on Superconducting $MgB_2$ thin Films)

  • 이남훈;성원경;;김소연;박성하;강원남
    • Progress in Superconductivity
    • /
    • 제11권1호
    • /
    • pp.8-12
    • /
    • 2009
  • We investigated the effects of the irradiation of light-ions on the superconducting $MgB_2$ thin films fabricated by using HPCVD. Deuterium and helium ions were irradiated on $MgB_2$ thin films by various doses, from $1{\times}10^{10}cm^{-2}\;to\;8{\times}10^{15}cm^{-2}$. During these experiments some reasonable results and unpredictable results have been obtained. The reasonable results are that the peak of the reduced maximum pinning force shifts by increasing the pinning sites in $MgB_2$ films and the slightly change of critical current density of films. We obtained some unusual results, which are the increasing of the transition temperature and the change of residual resistance ratio. Among the data of deuterium and helium ion irradiation experiments, the results of helium ion irradiation have most notable points so we will discuss mainly about helium irradiation experiments.

  • PDF

실험적 감전 Stress 가 Escherichia coli 감염마우스의 기병에 미치는 영향 (Effect of Experimental Electrization Stress on the Pathogenesis of Escherichia coli in Mice)

  • 이방환
    • 대한수의학회지
    • /
    • 제13권2호
    • /
    • pp.119-129
    • /
    • 1973
  • A hypothesis that is a stress condition in animal may cause either enhancement or reduction of the host resistance against microbial infection was experimentally studied. Among of many processes for stress formation an experimental electrization in mice was devised, on the bases of blood picture analysis, and studied the effect of experimental electrization of mice on E. coll infection. The results obtained were as follows. 1. Electrization with ordinary current, A. C. 60 cps., on the path of symmetrical line of both posterior limbs at 20 to 100 volts (less than 10 mA) for 15 to 30 seconds was able to induce a stress reaction in blood pattern without showing any dangers of electrocution, electric burns and other residual signs, and no correlation between blood pattern of the reaction and an amount of current between 20 to 100 volts was observed. As the electrodes, two of 21 gauge hypodermic needles were used, when the electrization each of them were inserted into the center of toe tissue of the both legs. 2. Serum protein fractions following the experimental electrization showed a tendency of a low A/G ratio and a high value of ${\alpha}$-globulin. 3. In the studies on the effect of electrical stress on the pathogenesis of E. coli in mice, a group in which a simultaneous electrization and infection, and a group infected two hours after electrization showed 80 per cent mortality. On the other hand, infection after 20 hours electrization and control groups showed their mortality of 40 and 60 per cent respectively.

  • PDF

쇼트피이닝 가공된 차량용 스프링강의 피로수명에 미치는 고온의 영향 (A Study on The Effect of High Temperature on Fatigue Life of The Vehicle Spring Steel)

  • 박경동;하경준
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.167-172
    • /
    • 2002
  • In this study, CT specimens were prepared from spring steel(SUP9) processed shot peening which was room temperature, high temperature experiment. And ire got the following characteristics from fatigue crack growth test carried out in the environment of room, and high temperature at $25^{\circ}C,\;100^{\circ}C,\;150^{\circ}C$ and $180^{\circ}C$ in the range of stress ratio of 0.3 by means of opening mode displacement. The threshold stress intensity factor range ${\Delta}Kth$ in the early stage of fatigue crack growth (Region I) and stress intensity (actor range ${\Delta}K$ in the stable of fatigue crack growth (Region II) was decreased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at high temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region.

  • PDF

Seismic performance of RC bridge piers reinforced with varying yield strength steel

  • Su, Junsheng;Dhakal, Rajesh Prasad;Wang, Junjie;Wang, Wenbiao
    • Earthquakes and Structures
    • /
    • 제12권2호
    • /
    • pp.201-211
    • /
    • 2017
  • This paper experimentally investigates the effect of yield strength of reinforcing bars and stirrups on the seismic performance of reinforced concrete (RC) circular piers. Reversed cyclic loading tests of nine-large scale specimens with longitudinal and transverse reinforcement of different yield strengths (varying between HRB335, HRB500E and HRB600 rebars) were conducted. The test parameters include the yield strength and amount of longitudinal and transverse reinforcement. The results indicate that the adoption of high-strength steel (HSS) reinforcement HRB500E and HRB600 (to replace HRB335) as longitudinal bars without reducing the steel area (i.e., equal volume replacement) is found to increase the moment resistance (as expected) and the total deformation capacity while reducing the residual displacement, ductility and energy dissipation capacity to some extent. Higher strength stirrups enhance the ductility and energy dissipation capacity of RC bridge piers. While the product of steel yield strength and reinforcement ratio ($f_y{\rho}_s$) is kept constant (i.e., equal strength replacement), the piers with higher yield strength longitudinal bars are found to achieve as good seismic performance as when lower strength bars are used. When higher yield strength transverse reinforcement is to be used to maintain equal strength, reducing bar diameter is found to be a better approach than increasing the tie spacing.

쇼트피이닝 가공된 스프링강의 저.고온 피로균열진전 평가 (An Investigation on the Shot Peening on the Low.High Temperature Fatigue Crack Propagation)

  • 박경동;정찬기
    • 한국마린엔지니어링학회:학술대회논문집
    • /
    • 한국마린엔지니어링학회 2001년도 추계학술대회 논문집(Proceeding of the KOSME 2001 Autumn Annual Meeting)
    • /
    • pp.65-70
    • /
    • 2001
  • In this study, CT specimens were prepared from spring steel(SUP9) processed shot peening which was room temperature, low temperature and high temperature experiment. And we got the following characteristics from fatigue crack growth test carried out in the environment of room, low temperature and high temperature at $25^{\circ}C$, -3$0^{\circ}C$, -5$0^{\circ}C$, -7$0^{\circ}C$, -10$0^{\circ}C$ and 5$0^{\circ}C$, 10$0^{\circ}C$ , 15$0^{\circ}C$, 18$0^{\circ}C$ and in the range of stress ratio of 0.05 by means of opening mode displacement. The threshold stress intensity factor range $\DeltaK_{th}$ in the early stage of fatigue crack growth (Region I ) and stress intensity factor range ΔK in the stable of fatigue crack growth (Region II) was decreased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature and high temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region.

  • PDF

3성분계 포졸란재를 이용한 반응성 분체 콘크리트(RPC)의 고온특성 (The mechanical properties of Reactive Powder Concrete using Ternary Pozzolanic Materials exposed to high Temperature)

  • 장칩도르지;소형석;이제방;소승영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 추계 학술논문 발표대회
    • /
    • pp.68-71
    • /
    • 2013
  • Reactive Powder Concrete (RPC) is an ultra high strength and high ductility cement-based composite material and has shown some promise as a new generation concrete in construction field. It is characterized by a silica fume-cement mixture with very low water-binder (w/b) ratio and very dense microstructure, which is formed using various powders such as cement, silica fume and very fine quartz sand (0.15~0.4mm) instead of ordinary coarse aggregate. However, the unit weight of cement in RPC is as high as 900~1,000 kg/㎥ due to the use of very fine sand instead of coarse aggregate, and a large volume of relatively expensive silica fume as a high reactivity pozzolan is also used, which is not produced in Korea and thus must be imported. Since the density of RPC has a heavy weight at 2.5~3.0 g/㎤. In this study, the modified RPC was made by the combination of ternary pozzolanic materials such as blast furnace slag and fly ash, silica fume in order to economically and practically feasible for Korea's situation. The fire resistance and structural behavior of the modified RPC exposed to high temperature were investigated.

  • PDF

Effect of Glass Fiber-Reinforced Connection on the Horizontal Shear Strength of CLT Walls

  • JUNG, Hongju;SONG, Yojin;HONG, Soonil
    • Journal of the Korean Wood Science and Technology
    • /
    • 제48권5호
    • /
    • pp.685-695
    • /
    • 2020
  • The connection performance between cross-laminated timber (CLT) walls and support has the greatest effect on the horizontal shear strength. In this study, the horizontal shear performance of CLT walls with reinforced connection systems was evaluated. The reinforcements of metal bracket connections in the CLT connection system was made by attaching glass fiber-based reinforcement to the connection zone of a CLT core lamina. Three types of glass fiber-based reinforcement were used: glass fiber sheet (GS), glass fiber cloth (GT) and fiber cloth plastic (GTS). The horizontal shear strength of the fabricated wall specimens was compared and evaluated through monotonic and cyclic tests. The test results showed that the resistance performance of the reinforced CLT walls to a horizontal load based on a monotonic test did not improve significantly. The residual and yield strengths under the cyclic loading test were 38 and 18% higher, respectively, while the ductility ratio was 38% higher than that of the unreinforced CLT wall. The glass fiber-based reinforcement of the CLT connection showed the possibility of improving the horizontal shear strength performance under a cyclic load, and presented the research direction for the application of real-scale CLT walls.

Experimental and numerical investigation on post-earthquake fire behaviour of the circular concrete-filled steel tube columns

  • Wang, Yu-Hang;Tang, Qi;Su, Mei-Ni;Tan, Ji-Ke;Wang, Wei-Yong;Lan, Yong-Sen;Deng, Xiao-Wei;Bai, Yong-Tao;Luo, Wei;Li, Xiao-Hua;Bai, Jiu-Lin
    • Steel and Composite Structures
    • /
    • 제38권1호
    • /
    • pp.17-31
    • /
    • 2021
  • Post-earthquake fire is a common disaster which causes serious safety issues to infrastructures. This study aims to investigate the residual loading capacities of circular concrete-filled steel tube (CFST) columns under post-earthquake fire experimentally and numerically. The experimental programme contains two loading steps - pre-damage cyclic loading at room temperature and transient state tests with constant compression loads. Three finite element models are developed and validated against the test results. Upon validation, a total of 48 numerical results were generated in the parametric study to investigate the effects of thickness and strengths of steel tube, axial compression ratio and damage degree on the fire resistance of circular CFST columns. Based on the analysis on experimental and numerical results, the loading mechanism of circular CFST columns is discussed. A design method is proposed for the prediction of fire resistance time under different seismic pre-damage and compression loads. The predictions by the new method is compared with the newly generated experimental and numerical results and is found to be accurate and consistent with the mean value close to the unity and a coefficient of variation around 1%.