Mechanical Properties and Wear Behaviour of $Al/SiC/Al_{2}O_{3}$ Composite Materials ($Al/SiC/Al_{2}O_{3}$복합재료의 기계적 성질 및 마멸특성)

  • 임흥준;김영한;한경섭
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.10
    • /
    • pp.2498-2508
    • /
    • 1993
  • $Al/SiC/Al_{2}O_{3}$ hybrid composites are fabricated by squeeze infiltration method. From the misconstructive of $Al/SiC/Al_{2}O_{3}$ hybrid composites fabricated by squeeze infiltration method, uniform distribution of reinforcements and good bondings are found. Hardness value of $Al/SiC/Al_{2}O_{3}$ hybrid composites increases linearly with the volume fraction of reinforcement because SiC whisker and $Al_{2}$O$_{3}$ fiber have an outstanding hardness. Optimal aging conditions are obtained by examining the hardness of $Al/SiC/Al_{2}O_{3}$ hybrid composites with different aging time. Tensile properties such as Young's modulus and ultimate tensile strength are improved up to 30% and 40% by the addition of reinforcements, respectively. Failure mode of $Al/SiC/Al_{2}O_{3}$ hybrid composites is ductile on microstructural level. Through the abrasive wear test and wear surface analysis, wear behaviour and mechanism of 6061 aluminum and $Al/SiC/Al_{2}O_{3}$ hybrid composites are characterized under various testing conditions. The addition of SiC whisker to $Al/SiC/Al_{2}O_{3}$ composites gives rise to improvement of the wear resistance. The wear resistance of $Al/SiC/Al_{2}O_{3}$ hybrid composites is superior to that of Al/SiC composites. The wear mechanism of aluminum alloy is mainly abrasive wear at low speed range and adhesive and melt wear at high speed range. In contrast, that of $Al/SiC/Al_{2}O_{3}$ hybrid composites is abrasive wear at all speed range, but severe wear when counter material is stainless steel. As the testing temperature increases, wear loss of aluminum alloy decreases because the matrix is getting more ductile, but that of $Al/SiC/Al_{2}O_{3}$ hybrid composites is hardly varied. Oil lubricant is more effective to reduce the wear loss of aluminum alloy and $Al/SiC/Al_{2}O_{3}$ hybrid composites at high speed range.

Characteristics of Elastic Paving Material Made of Sawdust and Urethane Resin Mixture (톱밥과 우레탄 수지 혼합물로 제조한 탄성 포장재의 특성)

  • Choi, Jae-Jin;Lee, Kwan-Ho;Moon, Seung-Kwon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.6
    • /
    • pp.673-680
    • /
    • 2017
  • Research and commercialization of wood chips-urethane resin mixtures as paving materials for park trails and tourist attractions are underway. The aim of this study was to expand the use of such paving materials to the playgrounds, where vigorous physical movements occur frequently. For this purpose, the physical properties and safety of the paving material, in which some or all of the wood chips(passing through a 10mm sieve and remaining in a 3mm sieve) were replaced with sawdust, were studied experimentally. Strength, elastic modulus, slip resistance, shock absorption and heavy metal content tests were carried out by varying the mixing ratio of urethane resin, sawdust and wood chip. As a result, in the case of wood chip-resin mixtures with mass ratios of the resin to total mass of sawdust and wood chips of 1.0 and 1.2 and having a ratio of sawdust mass to total mass of sawdust and wood chips of 0-0.4, it was found that the properties satisfied KS F 3888-2. On the other hand, in case of using sawdust only as a woody material, the shock absorbability was below standard, and the mass ratio of resin to sawdust required 1.2 or more to ensure the specified tensile strength.

Synthesis of Polyester Polyols by Using Double Metal Cyanide Catalyst and Physical Properties of Polyurethanes Produced by the Polyols (이중금속시안염 촉매에 의한 폴리에스테르 폴리올 제조 및 이를 이용한 폴리우레탄의 물성)

  • Kim, In-Ki;Seo, Hyun-Sook;Ha, Chang-Sik;Park, Dae-Won;Kim, Il
    • Clean Technology
    • /
    • v.14 no.1
    • /
    • pp.29-34
    • /
    • 2008
  • Copolymerizations of propylene oxide (PO) and phthalic anhydride (PA) have been performed in the presence of double metal cyanide (DMC) catalyst as a means of incorporating ester groups in the polyol backbone. DMC catalyst was effective for the copolymerization and the reactivity ratios measured by modified Kelen-$T{\ddot{u}}d{\ddot{o}}s$ equation were $r_1(PA)\;=\;0$, and $r^2(PO)\;=\;0.248$. Four different Polyol samples containing 1.0, 2.1, 7.52, and 11.42 mol% of PA unit were utilized for the synthesis of thermoplastic polyurethanes of their hard segments of 19 wt%. As the incorporated amount of PA increases, the elongation of the resulting polyurethane decreases and the tensile strength and the tensile modulus increase. The modulation of the incorporated amount of PA into polyol backbone was proven to be a feasible way to tune the physical properties of polyurethanes.

  • PDF

Effects of In Situ YAG on Properties of the Pressurless Annealed Sic-$TiB_2$ Electroconductive Ceramic Composites (무가압 어닐드한 Sic-$TiB_2$ 전도성 복합체의 특성에 미치는 In Situ YAG의 영향)

  • Shin, Yong-Deok;Ju, Jin-Young;Ko, Tae-Hun
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.57 no.5
    • /
    • pp.808-815
    • /
    • 2008
  • The composites were fabricated 61[vol.%] ${\beta}$-SiC and 39[vol.%] $TiB_2$ powders with the liquid forming additives of 8, 12, 16[wt%] $Al_2O_3+Y_2O_3$ as a sintering aid by pressureless annealing at 1650[$^{\circ}C$] for 4 hours. The present study investigated the influence of the content of $Al_2O_3+Y_2O_3$ sintering additives on the microstructure, mechanical and electrical properties of the pressureless annealed SiC-$TiB_2$ electroconductive ceramic composites. Reactions between SiC and transition metal $TiB_2$ were not observed in the microstructure and the phase analysis of the pressureless annealed SiC-$TiB_2$ electroconductive ceramic composites. Phase analysis of SiC-$TiB_2$ composites by XRD revealed mostly of ${\alpha}$-SiC(6H), ${\beta}$-SiC(3C), $TiB_2$, and In Situ YAG($Al_2Y_3O_{12}$). The relative density of SiC-$TiB_2$ composites was lowered due to gaseous products of the result of reaction between SiC and $Al_2O_3+Y_2O_3$. There is another reason which pressureless annealed temperature 1650[$^{\circ}C$] is lower $300{\sim}450[^{\circ}C]$ than applied pressure sintering temperature $1950{\sim}2100[^{\circ}C]$. The relative density, the flexural strength, the Young's modulus and the Vicker's hardness showed the highest value of 82.29[%], 189.5[Mpa], 54.60[Gpa] and 2.84[Gpa] for SiC-$TiB_2$ composites added with 16[wt%] $Al_2O_3+Y_2O_3$ additives at room temperature. Abnormal grain growth takes place during phase transformation from ${\beta}$-SiC into ${\alpha}$-SiC was correlated with In Situ YAG phase by reaction between $Al_2O_3$ and $Y_2O_3$ additive during sintering. The electrical resistivity showed the lowest value of 0.0117[${\Omega}{\cdot}cm$] for 16[wt%] $Al_2O_3+Y_2O_3$ additives at 25[$^{\circ}C$]. The electrical resistivity was all negative temperature coefficient resistance (NTCR) in the temperature ranges from $25^{\circ}C$ to 700[$^{\circ}C$]. The resistance temperature coefficient of composite showed the lowest value of $-2.3{\times}10^{-3}[^{\circ}C]^{-1}$ for 16[wt%] additives in the temperature ranges from 25[$^{\circ}C$] to 100[$^{\circ}C$].

Freezing and Thawing Properties of Concrete Using Recycled Coarse Aggregate (재생굵은골재를 사용한 콘크리트의 동결융해 특성)

  • Sung, Chan-Yong;Youn, Joon-No;Kim, Young-Ik;Im, Sang-Hyuk;Jung, Duck-Hyun
    • Korean Journal of Agricultural Science
    • /
    • v.30 no.2
    • /
    • pp.154-163
    • /
    • 2003
  • This study was performed to examine the freezing and thawing properties of the high strength concrete using recycled coarse aggregate. The recycled coarse aggregate was replaced by 0%, 25%, 50%, 75% and 100% of natural crushed aggregate. The compressive strength of the concrete used recycled coarse aggregate was shown in more than $400kgf/cm^2$ at the curing age 28 days. The weight loss ratio by freezing and thawing was shown in less than 1% at all mix type. The pulse velocity and relative dynamic modulus were decreased with increasing the freezing and thawing cycles. Also, durability factor for the freezing and thawing were decreased with increasing the content of recycled coarse aggregate. But, recycled concrete replaced with recycled coarse aggregate 100% was shown in more than 60 by durability factor in freezing and thawing of 300cycles Accordingly, these recycled coarse aggregate can be used for high strength concrete.

  • PDF

Mechanical Properties of Strain Hardening Cement-Based Composite (SHCC) with Recycled Materials (자원순환형 재료를 사용한 변형경화형 시멘트 복합체(SHCC)의 역학적 특성)

  • Kim, Sun-Woo;Cha, Jun-Ho;Kim, Yun-Yong;Yun, Hyun-Do
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.5
    • /
    • pp.727-736
    • /
    • 2010
  • This paper describes results of an preliminary study to produce strain hardening cement-based composites (SHCCs)with consideration of sustainability for infrastructure applications. The aims of this study are to evaluate the influence of recycled materials on the mechanical characteristics of SHCCs, such as compressive, four-point bending, and direct tensile behaviors, and to give basic data for constitutive model for analyzing and designing infra structures with SHCCs. In this study, silica sand, cement, and PVA fibers, were partially replaced with recycled sand, fly-ash, and FET fibers in the mixture of SHCCs, respectively. Test results indicated that fly-ash could improve both bending and direct tensile performance of SHCCs due to increasing chemical bond strength at the interface between PVA fibers and cement matrices. However, SHCCs replaced with PET fibers showed much lower performance in bending and direct tensile tests due to originally low mechanical properties of own fibers, although compressive behavior is similar to PVA2.0 specimen. Also, it was noted that the recycled sand would increase elastic modulus of SHCCs due to larger grain size compared to silica sand. Based on pre-set target value to maintain the performance of SHCCs, it was concluded that the replacement ratio below 20% of fly-ash or below 50% of recycled sands would be desirable for creating sustainable SHCCs.

A Study on the Commercialization of Polyamide 66/Polypropylene Blend (폴리아마이드 66/폴리프로필렌 블렌드의 상업화 연구)

  • Kim, Seog-Jun;Nam, Byeong-Uk
    • Elastomers and Composites
    • /
    • v.38 no.3
    • /
    • pp.262-272
    • /
    • 2003
  • Maleic anhydride-grafted-polypropylene(PP-g-MA) were used as a blend component and a compatibilizer, respectively, for two reactive blends of polyamide 66(PA 66)PP-g-MA binary blends and PA 66/polypropylene(PP)/PP-g-MA ternary blends. The goal of this work was to investigate the property differences between binary and ternary blends. Tensile strength, flexural modulus, heat deflection temperature, impact strength, melt flow index, and the dependence of melt viscosity on the shear rate were examined. The impact strengths of binary blends were higher than those of ternary blends at all compositions, since the in situ synthesis of PP-g-PA 66 copolymer through the imide formation between the amine end group of PA 66 and the anhydride group of PP-g-MA gave the increase of molecular weight and was more popular in binary blends than in ternary blends. In case of ternary blends, most of the properties were superior to those of binary blends, owing to the better properties of PP compared with PP-g-MA. The toughened binary blends with 70/30(PA 66/PP-g-MA) and 80/20 ratios were not commercially applicable due to their poor processibility. So, the ternary blends which showed lower melt viscosities were recommended for the commercial applications.

Carbon diffusion behavior and mechanical properties of carbon-doped TiZrN coatings by laser carburization (레이저 침탄된 TiZrN 코팅에서 탄소확산거동과 기계적 특성)

  • Yoo, Hyunjo;Kim, Taewoo;Kim, Seonghoon;Jo, Ilguk;Lee, Heesoo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.31 no.1
    • /
    • pp.32-36
    • /
    • 2021
  • This study was investigated in carbon diffusion behavior of laser-carburized TiZrN coating layer and the changes of mechanical properties. The carbon paste was deposited on TiZrN coatings, and the laser was irradiated to carburize into the coatings. The XRD peak corresponding to the (111) plane shifted to a lower angle after the carburization, showing the lattice expansion by doped carbon. The decreased grain size implied the compression by the grain boundary diffusion of carbon. The XPS spectra for the bonding states of carbon was analyzed that carbon was substitute to nitrogen atoms in TiZrN, as carbide, through the thermal energy of laser. In addition, the combination of sp2 and sp3 hybridized bonds represented the formation of an amorphous carbon. The cross-sectional TEM image and the inverse FFT of the TiZrN coating after carburizing were observed as the wavy shape, confirming the amorphous phase located in grain boundaries. After the carburization, the hardness increased from 34.57 GPa to 38.24 GPa, and the friction coefficient decreased by 83 %. In particular, the ratio of hardness and elastic modulus (H/E) which is used as an index of the elastic recovery, increased from 0.11 to 0.15 and the wear rate improved by 65 %.

Mechanical Properties and Resistance to Freezing and Thawing of the Recycled Aggregate Concrete with Metakaolin (메타카올린을 혼합한 재생골재 콘크리트의 역학적 특성 및 동결융해 저항성)

  • Moon, Han-Young;Kim, Yang-Bae;Moon, Dae-Joong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.4
    • /
    • pp.270-278
    • /
    • 2005
  • Recycled aggregate concrete has lower strength and durability compared to concrete with natural aggregate. Therefore, metakaolin is used to improve the properties of recycled aggregate concrete. Main components of metakaolin are $SiO_2$ and $Al_2O_3$. and specific surface area is 9 times larger than that of ordinary portland cement. Quality of demolished-recycled aggregate(DRA) satisfies the type 1 of KS F 2573, but quality of source-recycled aggregate(SRA) does not satisfy with the type 2 of KS F 2573. When metakaolin was replaced with 20% of cement, compressive strength of concrete with SRA and DRA develops about 40~64% of control concrete. Water absorption ratio was reduced about 2% by replacing 20% metakaolin and it represents low compared to the natural aggregate concrete without metakaolin. In addition, the resistance to freezing and thawing, of concrete with DRA is indicated to remarkably enhanced due to the contribution of metakaolin. However, when metakaolin is replaced with 20% of cement, relative dynamic modulus of elasticity of concrete with SRA was below 60% at 210 freezing and thawing cycles.

The Thermal Properties Analysis of the Mixtures Composed with Epoxy Resin and Amine Curing Agent (에폭시 수지/방향족 아민 경화물의 배합비 변화에 따른 열적 특성 분석)

  • Kim, Daeyeon;Kim, Soonchoen;Park, Young-Il;Kim, Young Chul;Lim, Choong-Sun
    • Journal of Adhesion and Interface
    • /
    • v.15 no.3
    • /
    • pp.100-108
    • /
    • 2014
  • In this work, a series of molar ratios composed with YD-128 and DDM were chosen based on the viscosity analysis. The mixtures of YD-128 and DDM with the different molar ratios were cured at $170^{\circ}C$ for 15 min followed by post cure at $190^{\circ}C$ for two hours. The thermal properties of the cured samples were investigated with DSC, TGA, DMA, and TMA. The conversion ratio of the mixtures of YD-128 and DDM (1 : 1.1) was calculated by dividing ${\Delta}H$ obtained from DSC experiments for each cured sample by ${\Delta}H$. The TGA data of the cured samples showed that the thermal stability and thermal degradation activation energy were proportional to the amount of DDM in the mixtures. However, the highest tan ${\delta}$, and the lowest thermal expansion data with DMA and TMA respectively were obtained from the stoichiometric mixture of YD-128 and DDM. Furthermore, the different ratio of mixtures were applied to test specimens to be cured at $170^{\circ}C$ to measure single lap shear strength with universal testing machine.